Abstract

Ceramic particles and cooling rates have important effect on the Strength and plasticity of aluminum-based materials. In this paper, the microstructure and mechanical properties of Al-4.5Cu alloy were controlled by adding ultra-trace amounts of in-situ synthesized TiB 2 particles and multiple cooling rates. The results show, that the average size of TiB 2 particles is about 86.35 nm. The lattice dis-registry between TiB 2 and α-Al was calculated to be 4.5 %, the TiB 2 particles can be used as α-Al heterogeneous nucleation cores. The average grain size and standard deviation of Al-4.5Cu alloy with the addition of 0.02 wt% TiB 2 and high cooling rate are 30.5 μm and 15.9, respectively. Compared with the Al-4.5Cu alloy without adding TiB 2 particles and at medium cooling rate, the average grain size and standard deviation decreased by 68.1 % and 44.2 %, respectively. It can be seen from the room temperature tensile properties of the alloy after T6 heat treatment, that the yield strength, tensile strength and elongation of the Al-4.5Cu alloys with the addition of 0.02 wt% TiB 2 and high cooling rate are 468.3 MPa, 513.9 MPa, and 13.4 %, respectively. Compared with the Al-4.5Cu alloy without adding ceramic particles and at medium cooling rate, the yield strength, tensile strength and elongation increased by 15.6 %, 9.2 % and 25.2 %, respectively.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. The growth behavior and kinetics of intermetallic compounds in Cu–Al interface at 600°C–800 °C10.1016/j.intermet.2024.108244 ↗
2. Anomalous two-step repair mechanism of Al–Cu alloy regulated by the surroundings during E-beam irradiation10.1016/j.jmrt.2024.01.011 ↗
3. Enhancement of mechanical properties of Al-Cu alloy composite reinforced by Ni element: A combination of mixture design of experiment and artificial neural network approach
4. Stress-induced symmetrical tilt boundaries in layer-structured Al-Cu eutectic alloys10.1016/j.scriptamat.2024.116025 ↗
5. The nucleation sequence of α-Al on TiB2 particles in Al-Cu alloys10.1016/j.actamat.2021.116652 ↗
6. Low-temperature CO preferential oxidation in H2-rich stream over Indium modified Pd-Cu/Al2O3 catalyst10.1016/j.jcis.2024.02.003 ↗
7. Microstructure evolution and strengthening mechanisms of a high-performance TiN-reinforced Al–Mn–Mg–Sc–Zr alloy processed by laser powder bed fusion10.1016/j.jmst.2023.11.033 ↗
8. Microstructure evolution and mechanical properties strengthening in laser powder bed fusion of high-strength SiC and TiB2 co-reinforced Al-Zn-Mg-Cu composites10.1016/j.jallcom.2023.171463 ↗
9. Interfacial strain evolution and abnormal Poisson's ratios in Al nuclei for the Al/TiB2 heterostructure10.1016/j.scriptamat.2023.115508 ↗
10. Interfacial precipitation of the in-situ TiB2-reinforced Al–Zn–Mg–Cu–Zr composite10.1016/j.matchemphys.2023.127561 ↗
11. Low-temperature synthesis and sinterability of high-purity submicron TiB2 powder via microwave-assisted carbothermal reduction10.1016/j.jeurceramsoc.2024.01.054 ↗
12. Achieving strength-ductility balance in a laser powder bed fusion fabricated TiB2/Al–Cu-Mg-Ag alloy10.1016/j.jallcom.2023.169311 ↗
13. On the preparation and mechanical properties of in situ small-sized TiB2/Al-4.5Cu composites via ultrasound assisted RD method10.1016/j.jallcom.2018.06.303 ↗
14. Effect of laser additive manufacturing on the microstructure and mechanical properties of TiB2 reinforced Al-Cu matrix composite10.1016/j.msea.2022.142950 ↗
15. Enhancing mechanical properties of uniformly distributed nano TiB2/2024 Al composite rolling sheet by pre-stretch aging10.1016/j.jallcom.2022.165172 ↗
16. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
17. Processing, multiscale microstructure refinement and mechanical property enhancement of hypoeutectic Al–Si alloys via in situ bimodal-sized TiB2 particles10.1016/j.msea.2020.139081 ↗
18. Microstructure evolution and properties improvement of in-situ TiB2/6061 composites via trace Mn addition10.1016/j.molstruc.2023.137423 ↗
19. Synergistic optimization in solidification microstructure and mechanical performance of novel (TiC N − TiB2)p/Al nanocomposites: Design, tuning and mechanism10.1016/j.compositesa.2022.106843 ↗
20. Enhanced combination of strength and ductility in the semi-solid rheocast hypereutectic Al Si alloy with the effect of in-situ TiB2 particles10.1016/j.matchar.2021.111143 ↗
21. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron10.1007/BF03037838 ↗
22. Manufacturing of (Al–10Zn) / TiB2 in-situ nanocomposites by reactive liquid metallurgy and hot-extrusion for enhanced interfacial bonding and mechanical properties10.1016/j.msea.2022.144200 ↗
23. Integrated model for describing the microstructure evolution of the inoculated Al-Zn-Mg-Cu alloys in continuous solidification10.1016/j.rinp.2021.104465 ↗
24. Correlation between tensile properties, microstructure, and processing routes of an Al–Cu–Mg–Ag–TiB2 (A205) alloy: additive manufacturing and casting10.1016/j.msea.2022.142989 ↗
25. Enhancing strength-ductility synergy and mechanisms of Al-based composites by size-tunable in-situ TiB2 particles with specific spatial distribution10.1016/j.compositesb.2021.108912 ↗
26. Effect of high cooling rate on the solidification microstructure of Al–Cu/TiB2 alloy fabricated by freeze-ablation casting10.1016/j.jmrt.2023.05.215 ↗
27. Effects of cooling rates on the solidification behavior, microstructural evolution and mechanical properties of Al–Zn–Mg–Cu alloys10.1016/j.jmrt.2022.12.082 ↗
28. Effects of nano-TiCp on the microstructures and tensile properties of TiCp/Al–Cu composites10.1016/j.matchar.2014.05.012 ↗
29. Investigation on work hardening rate of Al-Zn-Mg-Cu alloy under solid solution process and thermomechanical coupled multi-step fast aging process10.1016/j.jallcom.2024.174892 ↗
30. Effect of Mg on the microstructure evolution and mechanical properties of 5%TiB2/Al−4.5%Cu composites
31. Effects of cooling rate and TiC nanoparticles on the microstructure and tensile properties of an Al–Cu cast alloy10.1016/j.msea.2020.139737 ↗
32. Effects of nanoparticles on the solution treatment and mechanical properties of nano-SiCp/Al-Cu composites10.1016/j.jmatprotec.2021.117195 ↗
33. Enhanced age-hardening behavior in Al–Cu alloys induced by in-situ synthesized TiC nanoparticles10.1016/j.jmst.2018.09.029 ↗
34. Improving the strength-ductility trade-off of TiB2/Al-4.5%Cu composites via Mg–Ag microalloying and multi-step heat treatment10.1088/2053-1591/ac0264 ↗
35. The nano-sized TiC particle reinforced Al–Cu matrix composite with superior tensile ductility10.1016/j.msea.2014.11.006 ↗
36. Controlling the sizes of in-situ TiC nanoparticles for high-performance TiC/Al–Cu nanocomposites10.1016/j.ceramint.2021.07.017 ↗
37. In-situ investigation on the microstructure evolution and plasticity of two magnesium alloys during three-point bending10.1016/j.ijplas.2015.05.010 ↗
38. Annealing behavior of a cast Mg-Gd-Y-Zr alloy with necklace fine grains developed under hot deformation10.1016/j.msea.2017.02.008 ↗
39. Role of {10–12} twinning characteristics in the deformation behavior of a polycrystalline magnesium alloy10.1016/j.actamat.2010.07.002 ↗
40. Basal slip mediated tension twin variant selection in magnesium WE43 alloy10.1016/j.actamat.2019.03.018 ↗
41. Grain fragmentation associated continuous dynamic recrystallization (CDRX) of hexagonal structure during uniaxial isothermal compression: High-temperature α phase in TiAl alloys10.1016/j.intermet.2020.107028 ↗
42. Acquiring Mg-Ag microalloying TiB2/Al-4.5Cu composite simultaneously with ultrahigh strength and ductility via optimized salt-metal reaction and multistage heat treatment10.1016/j.matdes.2022.111252 ↗