Investigation of the hot corrosion effects on the lifetime of TBCs with and without TC

Javad Rahimi, Naghdali Choupani, Esmaeil Poursaeidi, Farzam Montakhabi, Mohammadrasoul Javadi Sigaroodi, Yousef Yousefi Jamalabad

Publisher page

Abstract

This paper investigates the influence of hot corrosion on the lifetime of TBCs with and without top coat under cyclic thermal loading. The tests were performed on two types of samples: Type A coating consisting solely of a bond coat (BC) fabricated by the HVOF method, and type B coating comprising a BC fabricated by the HVOF method and a TC fabricated by the APS method. The lifetime and degradation mechanism of these two types of coatings under hot corrosion in the presence of sulfate and vanadate molten salts were compared. The lifetime of type A and B coatings under the hot corrosion test is 31 and 24 cycles, respectively. Results indicate that the TGO acts as a barrier against the penetration of corrosive salts and delays the degradation of the type A coating. XRD patterns reveal that the reaction products of BC with molten salts are (Co,Ni) 3(VO 4) 2 and (Cr,Al)VO 4. In the type B coating, YVO 4 is formed as a hot corrosion product due to the reaction of molten salts with yttria. With the depletion of yttria, the phase transition of zirconia from tetragonal to monoclinic causes volumetric expansion and coating degradation.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Impact of bond coat types on calcium-magnesium-alumina-silicate and hot corrosion behavior in thermal barrier coatings10.1016/j.corsci.2023.111742 ↗
2. Thermal insulation performance and thermal shock resistance of plasma-sprayed TiAlCrY/Gd2Zr2O7 thermal barrier coating on γ-TiAl alloy10.1016/j.surfcoat.2023.129715 ↗
3. Stiffening-resistant composite TBCs counteracting the substrate constraint effect during thermal exposure10.1016/j.jallcom.2023.172832 ↗
4. Improvement in hot corrosion resistance and chemical stability of YSZ by introducing a Lewis neutral layer on thermal barrier coatings10.1016/j.corsci.2020.108776 ↗
5. The effect of CMAS penetration on the microstructure and failure of the TBCs applied by APS/APS method10.1016/j.surfcoat.2022.129053 ↗
6. Effect of alloying elements on microstructure evolution and wear mechanism of MCrAlX-based coatings at 800 °C10.1016/j.surfcoat.2023.129266 ↗
7. The study of mechanical properties and corrosion behavior of the Fe-based amorphous alloy coatings using high velocity oxygen fuel spraying10.1016/j.jallcom.2021.159132 ↗
8. Heat treatment effect on coating shock resistance of thermal barrier coating system with different types of bond coat10.1016/j.jeurceramsoc.2023.01.035 ↗
9. The effects of TGO growth stress and creep rate on TC/TGO interface cracking in APS thermal barrier coatings10.1016/j.ceramint.2021.05.199 ↗
10. Engineered architectures of gadolinium zirconate based thermal barrier coatings subjected to hot corrosion test10.1016/j.surfcoat.2017.09.005 ↗
11. Hot corrosion studies on plasma sprayed bi-layered YSZ/La2Ce2O7 thermal barrier coating fabricated from synthesized powders10.1016/j.jallcom.2017.04.022 ↗
12. Corrosion products evolution and hot corrosion mechanisms of REPO4 (RE= Gd, Nd, La) in the presence of V2O5+ Na2SO4 molten salt10.1016/j.jeurceramsoc.2018.10.031 ↗
13. Oxidation and hot corrosion behavior of Al2O3/YSZ coatings prepared by cathode plasma electrolytic deposition10.1016/j.corsci.2016.03.017 ↗
14. The role of the surface morphology and segmented cracks on the damage forms of laser re-melted thermal barrier coatings in presence of a molten salt (Na2SO4+ V2O5)10.1016/j.corsci.2016.11.011 ↗
15. Hot corrosion behavior of YSZ, Gd 2 Zr 2 O 7 and YSZ/Gd 2 Zr 2 O 7 thermal barrier coatings exposed to molten sulfate and vanadate salt10.1016/j.apsusc.2017.09.047 ↗
16. Evaluation of Hot Corrosion Behavior of APS and HVOF Sprayed Thermal Barrier Coatings (TBCs) Exposed to Molten Na2SO4 + V2O5 Salt at 1000 °C10.1007/978-3-319-79005-3_28 ↗
17. Microstructure modification of Y2O3 stabilized ZrO2 thermal barrier coatings by laser glazing and the effects on the hot corrosion resistance10.1007/s40145-020-0363-z ↗
18. Hot corrosion behavior of plasma sprayed La2Ce2O7/YSZ thermal barrier composite coating in the presence of Sulfate and Vanadate molten Salts
19. Hot corrosion behavior of YSZ/ZrW2O8 composites exposed to V2O5 at 700 °C and 850 °C in air10.1016/j.ceramint.2020.10.201 ↗
20. Hot corrosion behavior of dense CYSZ/YSZ bilayer coatings deposited by atmospheric plasma spray in Na2SO4+ V2O5 molten salts10.1016/j.surfcoat.2021.128066 ↗
21. Tobergte · 2013 · 53
22. Mechanisms controlling the durability of thermal barrier coatings10.1016/S0079-6425(00)00020-7 ↗
23. Hot corrosion resistance of air plasma sprayed ceramic Sm2SrAl2O7 (SSA) thermal barrier coatings in simulated gas turbine environments10.1016/j.ceramint.2018.06.234 ↗
24. Hot corrosion behavior of the La2(Zr0.7Ce0.3)2O7 ceramic in molten V2O5 and a Na2SO4+V2O5 salt mixture10.1016/j.jallcom.2016.07.257 ↗
25. An investigation on hot corrosion behavior of YSZ-Ta2O5 in Na2SO4+ V2O5 salt at 1100° C10.1016/j.corsci.2013.06.025 ↗
26. Investigation of the Effect of BC Layer Surface Roughness and TC Layer Porosity on Stress Values in Plasma Sprayed Coatings Based on SEM Images10.1016/j.mtcomm.2022.104737 ↗
27. Characterization and hot corrosion behavior of the La2(Zr0.7Ce0.3)2O7/8YSZ:Eu double ceramic layer coating prepared by atmospheric plasma spraying
28. Thermal shock resistance of thermal barrier coating with different bondcoat types and diffusion pre-coating
29. A comparative study of oxidation kinetics and thermal cyclic performance of thermal barrier coatings (TBCs)10.1016/j.surfcoat.2018.12.082 ↗
30. Isothermal oxidation and TGO growth behavior of NiCoCrAlY-YSZ thermal barrier coatings on a Ni-based superalloy10.1016/j.jallcom.2020.156093 ↗
31. A novel structure of YSZ coatings by atmospheric laminar plasma spraying technology10.1016/j.scriptamat.2018.04.022 ↗
32. Experimental and numerical life evaluation of TBCs with different BC and diffusion coating under cyclic thermal loading10.1111/ijac.14426 ↗
33. Effect of heat treatment and synergistic rare-earth modified NiCrAlY on bonding strength of nanostructured 8YSZ coatings10.1016/j.apsusc.2019.02.247 ↗
34. Effect of microstructure on early oxidation of MCrAlY coatings10.1016/j.actamat.2018.08.018 ↗
35. Coatings for gas turbine materials and long term stability issues10.1016/j.matdes.2004.02.005 ↗
36. On the high-temperature oxidation of MCrAlY coatings10.3139/146.110201 ↗
37. Influence of the combined-effect of NaCl and Na2SO4 on the hot corrosion behaviour of aluminide coating on Ni-based alloys10.1016/j.jallcom.2019.03.165 ↗
38. Stepwise depletion of coating elements as a result of hot corrosion of NiCrAlY coatings10.1007/s11665-013-0774-x ↗
39. Degradation of free-standing air plasma sprayed CoNiCrAlY coatings by vanadium and phosphorus pentoxides10.1016/j.surfcoat.2008.08.068 ↗
40. Effect of crystal structure and grain size on corrosion properties of AlCoCrFeNi high entropy alloy10.1016/j.jallcom.2020.158056 ↗
41. Nano- and micro-mechanical properties and corrosion performance of a HVOF sprayed AlCoCrFeNi high-entropy alloy coating10.1016/j.jallcom.2022.165000 ↗
42. Dynamic multi-crack evolution and coupling TBC failure together induced by continuous TGO growth and ceramic sintering10.1016/j.ceramint.2022.02.132 ↗
43. Hot corrosion behavior of Sc2O3-Y2O3-ZrO2 thermal barrier coatings in presence of Na2SO4+V2O5 molten salt10.1016/j.corsci.2014.04.001 ↗
44. Thermal properties and phase stability of Yttria-Stabilized Zirconia (YSZ) coating deposited by Air Plasma Spray onto a Ni-base superalloy10.1016/j.ceramint.2017.11.109 ↗
45. Evaluation of hot corrosion behaviors of Al2O3-YSZ composite TBC on gradient MCrAlY coatings in the presence of Na2SO4-NaVO3 salt10.1016/j.vacuum.2018.04.042 ↗
46. Application of thermal gradient and thermal cycling tests to Al2O3/CYSZ functionally graded TBC in the presence of simultaneous hot corrosion and CMAS effects10.1016/j.surfcoat.2022.128688 ↗
47. Degradation of yttria-stabilized zirconia thermal barrier coatings by vanadium pentoxide, phosphorous pentoxide, and sodium sulfate10.1111/j.1551-2916.2007.01941.x ↗
48. Investigation of isothermal oxidation behavior of thermal barrier coatings (TBCs) consisting of YSZ and multilayered YSZ/Gd2Zr2O7 ceramic layers10.1007/s11085-016-9690-4 ↗
49. Isothermal oxidation and TGO growth behaviors of YAG/YSZ double-ceramic-layer thermal barrier coatings10.1016/j.ceramint.2021.05.144 ↗
50. Microstructures, properties and failure analysis of (ZrO2–8 wt%Y2O3)/((Co, Ni) Cr Al Y) Thermal Barrier Coatings10.1016/0921-5093(89)90213-X ↗
51. Oxygen transport by gas permeation through the zirconia layer in plasma sprayed thermal barrier coatings10.1016/j.surfcoat.2003.10.018 ↗
52. Role of Al and Cr on cyclic oxidation behavior of AlCoCrFeNi2 high entropy alloy10.1016/j.jallcom.2022.165820 ↗
53. Microcracking of high zirconia refractories after t→m phase transition during cooling: an EBSD study10.1016/j.jeurceramsoc.2011.02.033 ↗