Effect of dislocation-induced aging precipitate bands on creep resistance of Mg-Gd-Y-Zr-Ag alloy
Source abstract
Abstract
This work investigates the effect of dislocation array induced β’ precipitation bands on the creep behavior in wrought Mg-8.9Gd-1.8Y-0.5Zr-0.2Ag (wt%) alloy. The alloy with β’ precipitate bands shows significantly enhanced creep resistance ranging from 448 to 548 K. Pipe diffusion-controlled grain boundary sliding (GBS) is suggested to be the main steady creep mechanism below 498 K. Cross-slip is suggested to be the main steady creep mechanism above 498 K. The characterization indicates that the precipitate bands separate the matrix into multiple units within the grains and restrict the long-distance slip of the dislocations. Bands with high thermal stability limit the diffusion of vacancies across the grain and prevent precipitation free zone (PFZ) broadening on the grain boundaries. For the alloy without precipitate bands, basal slip is initiated before the formation of β’, and it is easy to form broad PFZs on grain boundaries. Although cross-slip is still unavoidable at 523 K, these results provide guidance for improving the creep resistance of the deformed Mg-Gd series alloys.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Recent developments in high-strength Mg-RE-based alloys: focusing on Mg-Gd and Mg-Y systems10.1016/j.jma.2018.08.001 ↗
2. Creep resistance in magnesium alloys10.1179/095066010X12646898728327 ↗
3. The role of dislocation-solute interactions on the creep behaviour of binary Mg-RE alloys10.1038/s41598-021-82517-5 ↗
4. Enhanced age-hardening response and mechanical properties of the Mg-Gd-Y-Zn-Zr alloy by trace Ag addition10.1016/j.jallcom.2021.159825 ↗
5. Effects of trace Ag on precipitation behavior and mechanical properties of extruded Mg−Gd−Y−Zr alloys10.1016/S1003-6326(21)65737-0 ↗
6. The formation mechanism of a novel interfacial phase with high thermal stability in a Mg-Gd-Y-Ag-Zr alloy10.1016/j.actamat.2018.10.005 ↗
7. Effect of Ag on interfacial segregation in Mg–Gd–Y–(Ag)–Zr alloy10.1016/j.actamat.2015.05.020 ↗
8. Enhanced creep resistance in Mg-Y-Nd alloy via regulating prior thermo-mechanical treatment
9. Unraveling the individual effect of yttrium and neodymium on the precipitate-free zone development and the dislocation creep mechanism of Mg-Y-Nd alloy10.1016/j.matchar.2022.112537 ↗
10. A comparative study on the effects of Gd, Y and La rare-earth elements on the microstructure and creep behavior of AZ81 Mg alloy10.1016/j.msea.2020.139712 ↗
11. Microstructures and creep properties of Mg–4Al–(1–4) La alloys produced by different casting techniques10.1016/j.msea.2012.05.072 ↗
12. Highly improved creep resistance of hot-extruded Mg-0.9Mn-0.5Ce alloy by conventional forging10.1016/j.msea.2022.144083 ↗
13. Understanding solid solution strengthening at elevated temperatures in a creep-resistant Mg–Gd–Ca alloy10.1016/j.actamat.2019.09.058 ↗
14. Enhancing the creep resistance of a dilute Mg-1.5 wt%Nd alloy plate via pre-compression and subsequent peak-aging10.1016/j.jallcom.2020.158590 ↗
15. Effects of volume fraction of fine grains on the tensile creep properties of a hot-deformed Mg-Gd-Y-Zr alloy10.1016/j.msea.2020.139052 ↗
16. Development of high-strength magnesium alloys via combined processes of extrusion, rolling and ageing10.1016/j.scriptamat.2011.01.042 ↗
17. Enhanced strength and ductility of Mg–Gd–Y–Zr alloys by secondary extrusion10.1016/j.jma.2013.02.006 ↗
18. Microstructures and mechanical properties of high performance Mg–6Gd–3Y–2Nd–0.4Zr alloy by indirect extrusion and aging treatment10.1016/j.msea.2014.06.043 ↗
19. Microstructure evolution and mechanical properties of Mg-Gd-Y-Ag-Zr alloy fabricated by multidirectional forging and ageing treatment10.1016/j.msea.2017.06.038 ↗
20. Microstructure evolution and mechanical properties of a high strength Mg-11.7Gd-4.9Y-0.3Zr (wt%) alloy prepared by pre-deformation annealing, hot extrusion and ageing10.1016/j.msea.2017.06.096 ↗
21. Bulk nanocrystalline high-strength magnesium alloys prepared via rotary swaging10.1016/j.actamat.2020.09.024 ↗
22. Abnormal creep behavior of Mg–12Gd–1MM–0.6Zr (wt%) alloy at 300°C10.1016/j.matlet.2021.129861 ↗
23. The effect of grain size on the tensile and creep properties of Mg–2.6Nd–0.35Zn–xZr alloys at 250°C10.1016/j.msea.2012.09.052 ↗
24. Grain boundary diffusion of Al in Mg10.1016/j.scriptamat.2014.02.008 ↗
25. Analysis of Creep Deformation Due to Grain-Boundary Diffusion/Sliding
26. Atomistic study of grain-boundary segregation and grain-boundary diffusion in Al-Mg alloys10.1016/j.actamat.2020.10.029 ↗
27. Dislocations-induced precipitates and their effect on mechanical properties of Mg-Gd-Y-Zr alloy10.1016/j.jma.2019.05.009 ↗
28. Dislocation arrays, precipitate bands and free zones in forged Mg-Gd-Y-Zr alloy10.1016/j.msea.2019.138789 ↗
29. Dislocation-induced β’ precipitation behavior and strength-ductility synergistic enhancement in Mg-Gd-Y-Zr-Ag alloy10.1016/j.jallcom.2023.169187 ↗
30. Dislocation configurations in an extruded ZK60 magnesium alloy10.1007/s11661-008-9621-3 ↗
31. Dynamic recrystallization mechanism of Mg-8.5Gd-2.5Y-0.4Zr alloy during hot ring rolling10.1016/j.matchar.2017.07.015 ↗
32. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
33. Effects of precipitate shape and orientation on dispersion strengthening in magnesium alloys10.1016/S1359-6462(02)00497-9 ↗
34. A detailed HAADF-STEM study of precipitate evolution in Mg–Gd alloy10.1016/j.jallcom.2018.10.193 ↗
35. The role of pyramidal 〈 + 〉 dislocations in the grain refinement mechanism in Ti-6Al-4V alloy processed by severe plastic deformation10.1016/j.actamat.2020.08.076 ↗
36. Microstructure evolution in a Mg–15Gd–0.5Zr (wt%) alloy during isothermal aging at 250°C10.1016/j.msea.2006.06.018 ↗
37. Microstructure and super high strength of cast Mg-8.5Gd-2.3Y-1.8Ag-0.4Zr alloy10.1016/j.msea.2010.09.004 ↗
38. Temperature dependency of slip and twinning in plane strain compressed magnesium single crystals10.1016/j.actamat.2010.11.064 ↗
39. Temperature effects on the mobility of pyramidaldislocations in magnesium10.1016/j.scriptamat.2016.09.002 ↗
40. Effective values of critical resolved shear stress for slip in polycrystalline magnesium and other hcp metals10.1016/j.scriptamat.2010.05.047 ↗
41. Tensile creep behavior and microstructure evolution of extruded Mg–10Gd–3Y–0.5Zr (wt%) alloy10.1016/j.msea.2013.04.068 ↗
42. Effects of precipitate origin and precipitate-free zone development on the tensile creep behaviors of a hot-rolled Mg-13wt%Gd binary alloy10.1016/j.matchar.2021.111303 ↗
43. Effect of the precipitation state on high temperature tensile and creep behaviors of Mg-15Gd alloy10.1016/j.jma.2021.06.016 ↗
44. Effects of heat treatment before extrusion on dynamic recrystallization behavior, texture and mechanical properties of as-extruded Mg-Gd-Y-Zn-Zr alloy10.1016/j.msea.2021.142479 ↗
45. Creep behaviors of a highly concentrated Mg-18 wt%Gd binary alloy with and without artificial aging10.1016/j.jallcom.2018.10.013 ↗
46. Tensile and compressive creep behavior of extruded Mg–10Gd–3Y–0.5Zr (wt%) alloy10.1016/j.matchar.2014.11.006 ↗
47. Deformation mechanisms in h.c.p. metals at elevated temperatures—II. Creep behavior of a Mg-0.8% Al solid solution alloy10.1016/0001-6160(82)90009-8 ↗
48. Effects of alloying elements on creep properties of Mg-Gd-Zr alloys10.1007/s11661-014-2335-9 ↗
49. Effect of initial temper on the creep behavior of a Mg–Gd–Nd–Zr alloy10.1016/j.msea.2008.03.009 ↗
50. Creep in commercially pure metals10.1016/j.actamat.2005.08.021 ↗
51. A comparative study of the role of Ag in microstructures and mechanical properties of Mg-Gd and Mg-Y alloys10.1016/j.msea.2018.06.084 ↗
52. Investigation on β′ phase inversion of peak-aging hot extruded GW84 alloy after short high temperature secondary aging10.1016/j.matlet.2021.129824 ↗
53. Investigation of tensile creep behavior of Mg–Gd–Y–Zr alloy based on creep constitutive model10.1016/j.msea.2020.140567 ↗
54. HRTEM observation of the age hardening precipitates in Mg-15wt%Gd-Zr alloy10.4028/www.scientific.net/AMR.15-17.445 ↗