Development of Fe-based diluted nanocrystalline alloy by substituting C for P in FeSiBCCu system
Source abstract
Abstract
Here, an Fe 85.7Si 1B 10C 1P 2Cu 0.3 diluted nanocrystalline alloy exhibiting relatively high B s of 1.69 T and low H c of 2.58 A/m is successfully developed. In addition, the effects of substituting C with P on the thermal behavior, magnetic properties, microstructure, and magnetic domains of Fe 85.7Si 1B 10C 3−xP xCu 0.3 (x = 0, 1, 2, and 3 at%) amorphous alloys are investigated. It is found that the addition of P not only improves glass forming ability, but also enhances thermal stability of the amorphous alloy. Furthermore, the suitable P addition can also optimize the soft magnetic properties under heat treatment. For the Fe 85.7Si 1B 10C 1P 2Cu 0.3 alloy, the improved B s is due to the formation of bcc-Fe crystals and the lowest H c is caused by the low magneto-crystalline anisotropy, which are both induced by the construction diluted nanocrystalline structure. The formation of this unique microstructure is due to the competition between stabilization effect on amorphous phase of higher crystallization activation energy and the facilitation effect on the formation of bcc-Fe crystal by atomic-scale preexisting crystal-like clusters.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Magnetic Properties of Alloys · Magnetic properties of thin films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Enlarging heat-treatment processing windows of Fe-Si-B-P-Cu-M nanocrystalline alloys by doping transition metal elements10.1016/j.jallcom.2020.158420 ↗
2. Soft magnetic material status and trends in electric machines10.1109/TIE.2016.2613844 ↗
3. Power electronic transformers: a review10.1016/j.measurement.2020.108848 ↗
4. An investigation of ferrite and nanocrystalline core materials for medium-frequency power transformers10.1007/s11664-016-4559-5 ↗
5. Structure, properties, and glass forming ability of melt-spun Fe-Zr-B-Cu alloys with different Zr/B ratios10.1007/s11661-010-0446-5 ↗
6. Solidification behavior, glass forming ability and thermal characteristics of soft magnetic Fe-Co-B-Si-Nb-Cu bulk amorphous alloys10.1016/j.intermet.2011.05.004 ↗
7. Evolution of microstructure at hot band annealing of ferritic FeSi steels10.1016/j.jmmm.2016.10.035 ↗
8. Magnetic materials and devices for the 21st century: Stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
9. Soft magnetic materials for a sustainable and electrified world10.1126/science.aao0195 ↗
10. Soft magnetic Fe-Co-based amorphous alloys with extremely high saturation magnetization exceeding 1.9 T and low coercivity of 2 A/m10.1016/j.jallcom.2017.06.192 ↗
11. Investigation of microstructure and magnetic properties of Fe81Si4B12−xP2Cu1Mx (M = Cr, Mn and V; x = 0, 1, 2, 3) melt spun ribbons10.1016/j.jallcom.2014.10.202 ↗
12. High saturation magnetization and soft magnetic properties of bcc Fe-Zr-B and Fe-Zr-B-M (M = Transition metal) alloys with nanoscale grain size10.2320/matertrans1989.32.93 ↗
13. Soft magnetic properties of Fe-based bulk amorphous alloys10.2320/matertrans1989.41.1471 ↗
14. Effect of Hf addition on the glass forming ability, thermal and magnetic properties in the (Fe86B13Cu1)100−xHfx alloys10.1016/j.jnoncrysol.2017.11.044 ↗
15. Exceptionally high saturation magnetic flux density and ultralow coercivity via an amorphous-nanocrystalline transitional microstructure in an FeCo‐based alloy
16. Magnetic properties of high Bs Fe-based amorphous material[J]10.1016/j.jmmm.2006.02.167 ↗
17. FeSiBP bulk metallic glasses with unusual combination of high magnetization and high glass-forming ability[J]10.2320/matertrans.MRP2007198 ↗
18. Improving the glass formation ability and magnetic properties by Nb in Fe-Si-B-P-Cu-Nb nanocrystalline alloys10.1016/j.mseb.2020.114942 ↗
19. Role of Mo addition on structure and magnetic properties of the Fe85Si2B8P4Cu1 nanocrystalline alloy10.1016/j.jnoncrysol.2017.12.003 ↗
20. Effect of P on glass forming ability, magnetic properties and oxidation behavior of FeSiBP amorphous alloys10.1016/j.intermet.2016.12.024 ↗
21. Materials science - confusion by design10.1038/366303a0 ↗
22. Composition design of high Bs Fe-based amorphous alloys with good amorphous-forming ability10.1016/j.jallcom.2015.09.216 ↗
23. Fe content dependence of magnetic properties and bending ductility of FeSiBPC amorphous alloy ribbons10.1016/j.jallcom.2016.10.107 ↗
24. Composition design for Fe-based soft magnetic amorphous and nanocrystalline alloys with high Fe content10.1016/j.matdes.2020.108511 ↗
25. Recent progress in high Bs Fe-based nanocrystalline soft magnetic alloys10.1088/0022-3727/44/6/064004 ↗
26. Ferromagnetic domain theory10.1016/S0081-1947(08)60136-8 ↗
27. Permeability-frequency spectra of (Fe1−xCox)73.5Cu1Nb3Si13.5B9 nanocrystalline alloys under different magnetic fields10.1016/j.jmmm.2006.01.023 ↗
28. Origin of low coercivity of Fe-(Al, Ga)-(P, C, B, Si, Ge) bulk glassy alloys10.2320/matertrans.44.2020 ↗
29. Direct observation of local atomic order in a metallic glass10.1038/nmat2897 ↗
30. Magnetic softness and magnetization dynamics of FeSiBNbCu (P,Mo) nanocrystalline alloys with good high-frequency characterization10.1016/j.jmmm.2019.01.116 ↗
31. Reaction kinetics in differential thermal analysis10.1021/ac60131a045 ↗
32. Soft magnetic materials-nanocrystalline alloys
33. Effect of P on crystallization behavior and soft-magnetic properties of Fe83.3Si4Cu0.7B12−xPx nanocrystalline soft-magnetic alloys10.1016/j.tsf.2011.03.110 ↗
34. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element10.2320/matertrans.46.2817 ↗
35. Effect of P to B concentration ration on soft magnetic properties in FeSiBPCu nanocrystalline alloys10.1063/1.3672082 ↗
36. Origin of low coercivity of Fe-(Al, Ga)-(P, C, B, Si, Ge) bulk glassy alloys10.2320/matertrans.44.2020 ↗