Effect of laser energy density on microstructural evolution of selective laser melted Ti-15Zr alloy
Source abstract
Abstract
Selective laser melting (SLM) has been widely applied to the design and production of alloys due to the efficiency in processing components with complex structures and large sizes, especially Ti alloys. However, SLMed Ti alloys always exhibit undesirable ductility since the amount and morphology of the acicular α′ martensite phase are difficult to control. In this study, a SLMed Ti-15Zr alloy with an excellent combination of strength (a yield strength of 792 ± 11 MPa, an ultimate strength of 837 ± 13 MPa) and ductility (18.7 ± 0.5 %) was successfully fabricated by adjusting laser energy density (E) during the SLM process and the subsequent heat treatment. The influence of E on densification and microstructural evolution was investigated. When E is in the range of 69–125 J/mm 3 , Ti-15Zr alloys can achieve a relative density greater than 99 %. With the increase of E, the coarse equiaxed α phase decreases, and the fine lamellar α phase increases in the alloys after the heat treatment, owing to the slow cooling rate in the molten pool at high E. The excellent mechanical properties were attributed to the coordinated effects of the coarse equiaxed α phase and the fine lamellar α phase.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. A review on biomedical titanium alloys: recent progress and prospect10.1002/adem.201801215 ↗
2. Development of new metallic alloys for biomedical applications10.1016/j.actbio.2012.06.037 ↗
3. Achieving high strength and large ductility via Zr-rich stripes in Ti-15Zr alloy10.1016/j.matlet.2022.132194 ↗
4. The effect of the solute on the structure, selected mechanical properties, and biocompatibility of Ti-Zr system alloys for dental applications10.1016/j.msec.2013.09.032 ↗
5. Degradative effects of the biological environment on metals and ceramics
6. A review of titanium zirconium (TiZr) alloys for use in endosseous dental implants10.3390/ma5081348 ↗
7. Microstructure and mechanical properties of Ti-15Zr alloy used as dental implant material10.1016/j.jmbbm.2016.05.008 ↗
8. Mechanical properties and microstructural evolution of TA15 Ti alloy processed by selective laser melting before and after annealing10.1016/j.msea.2019.138742 ↗
9. Development of biomedical implants through additive manufacturing: a review10.1007/s11665-021-05578-7 ↗
10. Powder based additive manufacturing for biomedical application of titanium and its alloys: a review10.1007/s13534-020-00177-2 ↗
11. Recent developments in metal additive manufacturing10.1016/j.coche.2020.03.001 ↗
12. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium10.1016/j.msea.2013.11.038 ↗
13. Ultrahigh-strength titanium gyroid scaffolds manufactured by selective laser melting (SLM) for bone implant applications10.1016/j.actamat.2018.08.005 ↗
14. Densification behavior, microstructure evolution, and mechanical performances of selective laser melted Ti-5Al-2.5 Sn α titanium alloy: effect of laser energy input10.1016/j.jallcom.2018.09.153 ↗
15. Effect of heat treatment on microstructure and mechanical properties of the selective laser melting processed Ti-5Al-2.5 Sn α titanium alloy10.1016/j.msea.2017.10.061 ↗
16. Effects of heat treatment on the microstructure evolution and mechanical properties of selective laser melted TC4 titanium alloy10.3390/met12050702 ↗
17. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
18. Microstructure and mechanical behaviour of Ti-6Al-7Nb alloy produced by selective laser melting10.1016/j.matchar.2011.03.006 ↗
19. Fabrication of microscaffolds from Ti-6Al-7Nb alloy by SLM10.1108/RPJ-10-2013-0101 ↗
20. Manufacture by selective laser melting and mechanical behavior of a biomedical Ti-24Nb-4Zr-8Sn alloy10.1016/j.scriptamat.2011.03.024 ↗
21. Simultaneous improvement in strength and plasticity of Ti-24Nb-4Zr-8Sn manufactured by selective laser melting10.1016/j.matdes.2018.07.036 ↗
22. Microstructure and mechanical properties of the near-beta titanium alloy Ti-5553 processed by selective laser melting10.1016/j.matdes.2016.04.103 ↗
23. On microstructural evolution and mechanical properties of Ti-5Al-5V–5Mo-3Cr alloy synthesised from elemental powder mixtures10.1016/j.matchemphys.2018.03.007 ↗
24. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
25. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
26. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
27. Microstructure evolution and density behavior of CP Ti parts elaborated by Self-developed vacuum selective laser melting system10.1016/j.apsusc.2013.04.090 ↗
28. Microstructure and mechanical properties investigation of CP titanium processed by selective laser melting (SLM)10.1016/j.jmatprotec.2016.10.022 ↗
29. The microstructure and tensile properties of additively manufactured Ti-6Al-2Zr-1Mo-1V with a trimodal microstructure obtained by multiple annealing heat treatment10.1016/j.msea.2021.142241 ↗
30. Globularization using heat treatment in additively manufactured Ti-6Al-4V for high strength and toughness10.1016/j.actamat.2018.09.064 ↗
31. Achieving an ideal combination of strength and plasticity in additive manufactured Ti-6.5 Al-2Zr-1Mo-1V alloy through the development of tri-modal microstructure10.1016/j.msea.2022.142944 ↗
32. Selective laser melting produced Ti-6Al-4V: post-process heat treatments to achieve superior tensile properties10.3390/ma11010146 ↗
33. Microstructure and mechanical properties of Ti-Zr-Cr biomedical alloys10.1016/j.msec.2015.02.028 ↗
34. New high strength titanium Alloy Ti-Zr for dental use
35. Development and properties of dental Ti-Zr binary alloys10.1016/j.jmbbm.2020.104048 ↗
36. Microstructure and tensile properties of hot-rolled Zr50-Ti50 binary alloy10.1016/j.msea.2014.10.079 ↗
37. Structure and mechanical properties of TiZr binary alloy after Al addition10.1016/j.msea.2013.08.029 ↗
38. Shape memory behavior in Ti-Zr alloys10.1016/j.scriptamat.2010.11.048 ↗
39. Development and mechanical characterization of porous titanium bone substitutes10.1016/j.jmbbm.2012.01.008 ↗
40. Titanium alloyed with rhenium by selective laser melting10.1016/j.msea.2014.10.021 ↗
41. Additive manufacturing of 24CrNiMo low alloy steel by selective laser melting: influence of volumetric energy density on densification, microstructure and hardness10.1016/j.msea.2021.140957 ↗
42. Densification behavior, microstructural evolution, and mechanical properties of TiC/316L stainless steel nanocomposites fabricated by selective laser melting10.1016/j.matdes.2017.10.039 ↗
43. Effect of C and Cu addition on the densification and microstructure of iron powder in direct laser sintering process10.1016/j.matlet.2008.01.113 ↗
44. Correlation between porosity and processing parameters in TiAl6V4 produced by selective laser melting10.1016/j.matdes.2016.05.070 ↗
45. Multi-laser powder bed fusion of Ti-6.5 Al-2Zr-Mo-V alloy powder: Defect formation mechanism and microstructural evolution10.1016/j.powtec.2021.02.010 ↗
46. Multi-scale defects in powder-based additively manufactured metals and alloys10.1016/j.jmst.2022.02.015 ↗
47. Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron Beam Melting10.1016/j.actamat.2017.09.047 ↗
48. The effect of laser energy input on the microstructure, physical and mechanical properties of Ti-6Al-4V alloys by selective laser melting10.1080/17452759.2016.1142215 ↗
49. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
50. Effects of selective laser melting build orientations on the microstructure and tensile performance of Ti-6Al-4V alloy10.1016/j.msea.2020.139001 ↗
51. Optimisation of process parameters to address fundamental challenges during selective laser melting of Ti-6Al-4V: a review10.1016/j.ijmachtools.2018.01.003 ↗
52. Additive manufacturing of metals: Microstructure evolution and multistage control10.1016/j.jmst.2021.06.011 ↗
53. Formation of equiaxed grains in selective laser melted pure titanium during annealing10.1016/j.jmrt.2021.01.008 ↗
54. Abnormal grain growth in commercially pure titanium during additive manufacturing with electron beam melting10.1016/j.mtla.2019.100281 ↗
55. Effect of initial microstructure on plastic flow and dynamic globularization during hot working of Ti-6Al-4V10.1007/s11661-999-0232-4 ↗
56. A novel ultra-high strength titanium alloy via hierarchical α/α' precipitation strengthening10.1016/j.msea.2022.142878 ↗
57. Slip band-grain boundary interactions in commercial-purity titanium10.1016/j.actamat.2014.05.015 ↗
58. Additive manufacturing of high strength near β titanium alloy Ti-55511 by engineering nanoscale secondary α laths via in-situ heat treatment10.1016/j.msea.2021.141245 ↗
59. Variation of hardness of metals with grain size10.1038/173948b0 ↗
60. Quantitative strengthening evaluation of powder metallurgy Ti-Zr binary alloys with high strength and ductility10.1016/j.jallcom.2020.156954 ↗
61. Strengthening mechanism of Ti-W composites with heterogeneous microstructures10.1080/21663831.2022.2049907 ↗
62. Measurement of geometrically necessary dislocation density with high resolution electron backscatter diffraction: effects of detector binning and step size10.1016/j.ultramic.2012.11.003 ↗
63. Quantitative strengthening evaluation of powder metallurgy titanium alloys with substitutional Zr and interstitial O solutes via homogenization heat treatment10.3390/ma14216561 ↗