journal article·2024-08

Synergistic enhancement of strength-ductility balance of TZM alloy through c-ZrO2 combined with large deformation and annealing

Gaolong Tian, Liujie Xu, Hong Fang, Fengan Geng, Yuchen Zhou, Shizhong Wei

Publisher page

Abstract

In this work, new TZM alloys containing 0.5 wt% and 1.0 wt% ZrO 2 were prepared by powder metallurgy method, and their annealed microstructures and mechanical properties were studied. The TZM alloy sheet with 94 % deformation was recrystallized at 1200°C, and the elongation was greatly increased, and its UTS, YS and EL were 573 ± 10 MPa, 431 ± 7 MPa and 44 ± 0.2 %, respectively. After adding 0.5 wt% c-ZrO 2 , the best strength-ductility balance was achieved, and its UTS, YS, EL and PSE are 621 ± 3 MPa, 527 ± 4 MPa, 41.3 ± 0.58 % and 25.6 GPa·%, respectively, which was much larger than the PSE combinations of most Mo and TZM alloys. Microstructure analysis shows that the excellent synergistic effect arises from the low O impurity content and the control of dislocation density and dislocation slip by c-ZrO 2 and the annealing process. Within the alloy, Ti and Zr react with O to produce TiO 2 and ZrTiO 4, which reduces the content of O impurities. Annealing provides sufficient space for dislocation slip, which coordinates the rotation of grain orientation during the stretching process. Coupled with the low O impurity concentration, results in excellent ductility of TZM alloys. Additionally, c-ZrO 2 can effectively fix dislocations within the grains and interact strongly with dislocations, consequently enhancing the strength of the TZM alloy.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Titanium Alloys Microstructure and Properties · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. High temperature fatigue behaviour of TZM molybdenum alloy under mechanical and thermomechanical cyclic loads10.1016/S0022-3115(99)00240-8 ↗
2. Fabrication and structural of gold/cerium nanoparticles on tin disulfide nanostructures and decorated on hyperbranched polyethyleneimine for photocatalysis, reduction, hydrogen production and antifungal activities10.1016/j.jphotochem.2021.113316 ↗
3. A facile preparation method for efficiency a novel LaNiO3/SrCeO3 (p-n type) heterojunction catalyst in photocatalytic activities, bactericidal assessment and dopamine detection
4. Synthesis and its characterization of silver sulfide/nickel titanate/chitosan nanocomposites for photocatalysis and water splitting under visible light, and antibacterial studies10.1016/j.matchemphys.2021.124990 ↗
5. Processing and characterization of spark plasma sintered TZM alloy10.1016/j.jallcom.2016.06.161 ↗
6. Corrosion characteristics of Mo and TZM alloy for plasma facing components in molten lithium at 623 K10.1016/j.corsci.2022.110202 ↗
7. Mechanism analysation and parameter optimisation of electro discharge machining of titanium-zirconium-molybdenum alloy10.1016/j.jmapro.2018.03.002 ↗
8. Decoration of MoO3-x on clay mineral matrix with great phosphorescence properties for oxygen activation, photochemical properties, bactericidal and oxidase-like mimics for prompt detection of pesticide10.1016/j.mssp.2023.107847 ↗
9. Fracture behavior of the La-doped molybdenum-titanium-zirconium alloy10.1016/j.msea.2019.05.031 ↗
10. Oxygen content effect on mechanical properties and microstructure of TZM alloy
11. The synthesis of TiC dispersed strengthened Mo alloy by freeze-drying technology and subsequent low temperature sintering10.1016/j.scriptamat.2021.113831 ↗
12. Microstructure, mechanical properties, and strengthening mechanisms of nanostructural Y-Zr-O oxide dispersion-strengthened (ODS) Mo alloys10.1016/j.jallcom.2022.166155 ↗
13. Deformation behavior and microstructure evolution of TZM alloy with 1.0 wt%ZrO2 under high temperature compression10.1016/j.ijrmhm.2023.106382 ↗
14. Geometrically necessary dislocation density evolution as a function of microstructure and strain rate10.1016/j.msea.2021.142224 ↗
15. Geometrically necessary dislocations favor the Taylor uniform deformation mode in ultra-fine-grained polycrystals10.1016/j.actamat.2016.06.062 ↗
16. Sintering behavior and mechanical properties of Mo-TZM alloyed with nanotitanium carbide10.1016/j.ijrmhm.2016.10.002 ↗
17. High-energy ball milling and spark plasma sintering of molybdenum - lanthanum oxide (Mo-La2O3) and molybdenum – lanthanum zirconate (Mo-La2Zr2O7) composite powders10.1016/j.ijrmhm.2021.105717 ↗
18. Preparation and ductile-to-brittle transition temperature of the La-TZM alloy plates10.1016/j.ijrmhm.2015.05.006 ↗
19. Design and structural of Sm-doped SbFeO3 nanopowders and immobilized on poly(ethylene oxide) for efficient photocatalysis and hydrogen generation under visible light irradiation
20. Simultaneous improvement of strength and plasticity of TZM alloys by introducing α-Al2O3 ceramic particles
21. Low-temperature accelerated sintering of high-performance oxide dispersion strengthened ultrafine grained Mo alloy10.1016/j.jallcom.2022.163982 ↗
22. Defect evolution on the activity of samarium doped Na2TinO2n+1 with different sodium/titanium ratio for photocatalytic degradation of fluoroquinolones drugs, toxicity assessments and eco-toxicity prediction10.1016/j.ceramint.2024.01.097 ↗
23. Achieving an unprecedented strength-ductility balance of molybdenum alloy by homogeneously distributing yttrium-cerium oxide10.1016/j.jallcom.2021.163110 ↗
24. Preparation and characterization of Mo/Al2O3 composites10.1016/j.ijrmhm.2015.07.033 ↗
25. The origins of high hardening and low ductility in magnesium10.1038/nature15364 ↗
26. Dislocation exhaustion and ultra-hardening of nanograined metals by phase transformation at grain boundaries10.1038/s41467-022-33257-1 ↗
27. Secondary phases strengthening-toughening effects in the Mo–TiC–La2O3 alloys10.1016/j.msea.2021.142271 ↗
28. Preparation and properties of high-strength molybdenum alloy sheets doped with Al2O3 particles10.1007/s12598-016-0726-3 ↗
29. Investigation of microstructure and tensile properties of as-processed TZM alloy at elevated temperature10.1016/j.matchar.2021.110933 ↗
30. La2O3 effects on TZM alloy recovery, recrystallization and mechanical properties10.1016/j.msea.2015.03.114 ↗
31. Excellent combination of strength and elongation of TZM alloys achieved by c-ZrO2 and single cross rolling10.1016/j.matchar.2024.113670 ↗
32. Effect of annealing treatment on texture evolution, microstructure and mechanical properties of an extruded Mg-Gd-Zn-Zr alloy10.1016/j.jmrt.2023.10.249 ↗
33. Secondary phases formation in lanthanum-doped titanium-zirconium-molybdenum alloy10.1016/j.jallcom.2018.05.103 ↗
34. Precise control of oxygen for titanium-zirconium-molybdenum alloy10.1016/j.ijrmhm.2021.105768 ↗
35. Quantitative measurement of displacement and strain fields from HREM micrographs10.1016/S0304-3991(98)00035-7 ↗
36. The effect of yttrium addition on the oxidation resistance of EPM TiAl-based intermetallics10.1016/S1359-6462(03)00134-9 ↗
37. Trace Y for as-cast Ti6Al4V to simultaneous enhance strength-ductility10.1016/j.jallcom.2023.169757 ↗
38. Simultaneous gettering of oxygen and chlorine and homogenization of the β phase by rare earth hydride additions to a powder metallurgy Ti–2.25Mo–1.5Fe alloy10.1016/j.scriptamat.2012.06.009 ↗
39. Effects of calcination temperature on grain growth and phase transformation of nano-zirconia with different crystal forms prepared by hydrothermal method10.1016/j.jmrt.2022.06.137 ↗
40. Reduced activation energy and crystalline size for yttria-stabilized zirconia nano-crystals10.1016/j.jcrysgro.2004.03.017 ↗
41. The mechanical properties and fracture mechanisms of wrought low carbon arc cast (LCAC), molybdenum–0.5pct titanium–0.1pct zirconium (TZM), and oxide dispersion strengthened (ODS) molybdenum flat products10.1016/j.msea.2005.11.030 ↗
42. Strengthening and elongation mechanism of Lanthanum-doped Titanium-Zirconium-Molybdenum alloy10.1016/j.msea.2016.10.013 ↗
43. Micro-nano secondary phase greatly increases the plasticity of titanium-zirconium-molybdenum alloy10.1016/j.ijrmhm.2023.106152 ↗
44. High temperature mechanical properties of TZM alloys under different lanthanum doping treatments10.1016/j.jallcom.2017.03.346 ↗
45. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility10.1038/nmat3544 ↗
46. Evaluation of oxide dispersion strengthened (ODS) molybdenum and molybdenum–rhenium alloys10.1016/S0263-4368(00)00028-7 ↗
47. Mechanical properties of a ZrC-dispersed Mo alloy processed by mechanical alloying and spark plasma sintering10.1016/S0921-5093(99)00481-5 ↗
48. Influences of annealing temperature on microstructure and mechanical properties of Mo–La2O310.1016/j.ijrmhm.2011.03.003 ↗
49. Low cycle fatigue behaviors of pure Mo and Mo-La2O3 alloys10.1016/j.msea.2017.09.064 ↗
50. Evaluation of tensile property and strengthening mechanism of Zirconia reinforced molybdenum alloy10.1016/j.jallcom.2023.171716 ↗
51. Preparation and characterization of Mo/ZrO2–Y2O3 composites10.1016/j.ijrmhm.2018.04.018 ↗
52. Microstructure and high-temperature mechanical properties of second-phase enhanced Mo-La2O3-ZrC alloys post-treated by cross rolling10.1016/j.jallcom.2019.04.348 ↗
53. Effect of secondary phases on the strength and elongation of a novel Mo-TiC-ZrC-C alloy10.1016/j.ijrmhm.2020.105336 ↗
54. In-situ EBSD study of the active slip systems and lattice rotation behavior of surface grains in aluminum alloy during tensile deformation10.1016/j.msea.2013.05.046 ↗
55. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
56. Effect of annealing temperature on microstructures and mechanical properties of a 5083 Al alloy deformed at cryogenic temperature10.1016/j.scriptamat.2004.02.037 ↗
57. Grain boundary segregation engineering in as-sintered molybdenum for improved ductility10.1016/j.scriptamat.2018.07.008 ↗
58. On grain boundary segregation in molybdenum materials10.1016/j.matdes.2017.09.019 ↗
59. The double-edge effect of second-phase particles on the recrystallization behaviour and associated mechanical properties of metallic materials10.1016/j.pmatsci.2017.10.004 ↗
60. In-situ investigation of tensile behaviors of Ti–6Al alloy with extra low interstitial10.1016/j.msea.2021.140958 ↗
61. Grain rotations during uniaxial deformation of gradient nano-grained metals using crystal plasticity finite element simulations10.1016/j.eml.2017.09.003 ↗