Morphology and properties of Mg2Si phase modified by Ge in Mg-Si alloys
Source abstract
Abstract
The modification effects of Ge on Mg 2 Si phase in a Mg-2.5Si alloy were studied by computational simulation and experimental investigation. Based on first-principles structural prediction and electronic structure calculation, Mg 2(Si xGe 1-x) phases were structurally stable and had sufficient hardness and inherent toughness as a reinforcement phase. With the increase of Ge content, due to the preferential adsorption of Ge atoms on the {100} planes of Mg 2Si crystal, the morphology of primary Mg 2Si crystal changed from equilateral-dendrite to polygonal, and finally to quadrilateral. In Mg-2.5Si-0.5Ge alloy, Ge was almost completely dissolved in the Mg 2Si phase, but a small amount of dispersed solute segregation with a size of 10–20 nm can be observed. In Mg-2.5Si-1Ge alloy, many Mg 2 Ge precipitates with a small amount of Si dissolved having a size of 20–50 nm and a lattice constant a of 0.644 nm were uniformly distributed in primary Mg 2Si, and only one orientation relationship (OR) in form of [001] Mg2Ge || [001] Mg2Si, (001) Mg2Ge || (001) Mg2Si with a tiny rotational angle of 0.39° was found. The stiffness and hardness of Mg 2Si phase decreased with the increase of Ge content. Despite Mg 2(Si xGe 1-x ) crystal models only considering the solid solution of Ge and neglecting segregation and precipitation, the theoretical predictions of mechanical properties remained consistent with experimental results. This agreement was primarily due to the unique OR between Mg 2Ge precipitates and Mg 2Si phase.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. Current and Future Use of Magnesium in the Automobile Industry10.4028/www.scientific.net/MSF.419-422.51 ↗
2. Advanced metals for aerospace and automotive use10.1016/0921-5093(94)91026-X ↗
3. Magnesium: properties-applications-potential10.1016/S0921-5093(00)01351-4 ↗
4. Effect of hot extrusion on mechanical properties of a Mg-Si-Al alloy10.1016/0167-577X(94)90165-1 ↗
5. High strength and high strain rate superplasticity in a Mg-Mg2Si composite10.1016/0956-716X(95)00140-Q ↗
6. Effect of solidification cooling rate on the morphology and number per unit volume of primary Mg2Si particles in a hypereutectic Al-Mg-Si alloy10.1007/s11661-005-0228-7 ↗
7. Nonfaceted growth of intermetallic Mg2Si in Al melt during rapid solidification10.1016/j.jallcom.2007.08.037 ↗
8. Recent advances of high strength Mg-RE alloys: Alloy development, forming and application10.1016/j.jmrt.2023.08.055 ↗
9. High temperature tensile properties of modified Mg/Mg2Si in situ composite10.1016/j.matdes.2011.05.001 ↗
10. Effects of alternating current imposition and alkaline earth elements on modification of primary Mg2Si crystals in hypereutectic Mg-Si alloy10.1016/S1003-6326(08)60405-7 ↗
11. Effect of high-intensity ultrasonic treatment on modification of primary Mg2Si in the hypereutectic Mg–Si alloys10.1016/j.jallcom.2013.06.189 ↗
12. Structural, electronic, elastic and thermal properties of Mg2Si10.1016/j.jpcs.2010.01.017 ↗
13. Magnesium and magnesium-silicide coated silicon nanowire composite anodes for lithium-ion batteries10.1039/C2TA00769J ↗
14. Synthesis and characterization of Mg2Si/Si nanocomposites prepared from MgH2 and silicon, and their thermoelectric properties10.1039/c2jm35257e ↗
15. Thermodynamic evaluation of hypereutectic Al-Si (A390) alloy with addition of Mg10.1016/j.actamat.2010.02.017 ↗
16. Morphological evolution and growth mechanism of primary Mg2Si phase in Al–Mg2Si alloys10.1016/j.actamat.2010.10.036 ↗
17. Microstructure and mechanical properties of mechanically alloyed intermetallic Mg2Si-Al alloys
18. Modification of Mg2Si in Mg-Si alloys with K2TiF6, KBF4 and KBF4 + K2TiF6
19. Development of an effective modifier for hypereutectic Mg–Si alloys10.1016/j.jallcom.2007.08.082 ↗
20. Modification of Mg2Si in Mg-4Si Alloys with B10.2355/isijinternational.48.1662 ↗
21. Effect of Ca on the microstructure and tensile properties of Mg-Zn-Si alloys at ambient and elevated temperature10.1016/j.jallcom.2012.05.047 ↗
22. Effect of hot extrusion on microstructure and tensile properties of Ca modified Mg-Mg2Si composite10.1016/j.mspro.2015.11.053 ↗
23. Modification of Mg2Si in Mg-Si alloys with yttrium10.1016/j.msea.2004.09.007 ↗
24. Modification of Mg2Si in Mg-Si alloys with neodymium10.1016/S1003-6326(13)62847-2 ↗
25. The microstructure and creep characteristics of cast Mg-3Si and Mg-3Si-1Gd alloys10.1016/j.msea.2016.07.026 ↗
26. Modification of Mg2Si morphology in Mg-Si alloys with Bi10.1016/j.jmatprotec.2007.12.038 ↗
27. Morphology modification of Mg2Si by Sr addition in Mg-4%Si alloy
28. Comparison about effects of Sb, Sn and Sr on as-cast microstructure and mechanical properties of AZ61-0.7Si magnesium alloy
29. Fractal dimension analysis of Mg2Si particles of Al-15%Mg2Si composite and its relationships to mechanical properties
30. Morphology and properties of Mg2Si and Mg2(SixSn1-x) reinforcements in magnesium alloys10.1016/j.jmst.2016.11.017 ↗
31. Thermal stability and elastic properties of Mg2X (X = Si, Ge, Sn, Pb) phases from first-principle calculations10.1016/j.commatsci.2011.07.012 ↗
32. Primary Mg2Si phase and Mg2Si /α-Mg interface modified by Sn and Sb elements in a Mg-5Sn-2Si-1.5Al-1Zn-0.8Sb alloy10.1016/j.jma.2021.02.003 ↗
33. Thermodynamic modeling of the Mg-Ge-Si, Mg-Ge-Sn, Mg-Pb-Si and Mg-Pb-Sn systems10.1002/chin.201020007 ↗
34. Solid-State Synthesis of Thermoelectric Materials in Mg-Si-Ge System10.2320/matertrans.46.1490 ↗
35. Hu · 2010 · 238
36. First principles study of Mg2X (X=Si, Ge, Sn, Pb): Elastic, optoelectronic and thermoelectric properties10.1016/j.mssp.2015.06.075 ↗
37. First-principles and experimental studies of impurity doping into Mg2Si10.1016/j.intermet.2007.12.001 ↗
38. Experimental study of ternary Ca-Mg-Si phase equilibria and thermodynamic assessment of Ca-Si and Ca-Mg-Si systems10.1016/j.intermet.2003.07.001 ↗
39. Lattice dynamics of Mg2Ge10.1016/0022-3697(65)90206-4 ↗
40. A.A. Nayeb, Phase diagrams of binary magnesium alloys. 1988.
41. The thermoelectric properties of mixed crystals of Mg2GexSi1-x10.1149/1.2425689 ↗
42. Stacking faults in B2-structured magnesium alloys from first principles calculations10.1016/j.commatsci.2011.06.001 ↗
43. First principles study of Mg2X (X=Si, Ge, Sn, Pb): elastic, optoelectronic and thermoelectric properties10.1016/j.mssp.2015.06.075 ↗
44. Ideal strength of Mg2X (X = Si, Ge, Sn and Pb) from first-principles10.1016/j.jma.2013.06.002 ↗
45. Temperature dependent elastic coefficients of Mg2X (X=Si, Ge, Sn, Pb) compounds from first-principles calculations10.1016/j.jallcom.2010.03.153 ↗
46. Morphology and Properties of Mg2Si Phase Modified by Pb in As-Cast Mg-2.5Si-xPb Alloys10.3390/ma17081811 ↗
47. Stability and elasticity of metastable solid solutions and superlattices in the MoN-TaN system: first-principles calculations10.1016/j.matdes.2018.02.033 ↗
48. Applicability of Born's stability criterion to face-centered-cubic crystals in [111] loading10.1063/1.2149151 ↗
49. Hardness of covalent compounds: roles of metallic component and d valence electrons10.1063/1.2956594 ↗
50. Morphological evolution of TiC from octahedron to cube induced by elemental nickel10.1039/c1ce06205k ↗
51. Formation and growth mechanism of ZrC hexagonal platelets synthesized by self-propagating reaction10.1016/j.jcrysgro.2008.07.016 ↗
52. Molecular-dynamics simulation of the effect of temperature of the growth environment on diamond habit10.1016/S0925-9635(99)00023-0 ↗
53. Extracting convergent surface energies from slab calculations10.1088/0953-8984/8/36/005 ↗
54. A kinetic model for crystal growth from aqueous solution in the presence of impurity10.1016/0022-0248(95)00128-X ↗
55. Synthesis of octahedron and truncated octahedron primary Mg2Si by controlling the Sb contents10.1039/c2ce26649k ↗
56. Explanation of some peculiarities of crystal morphology deduced from the BFDH law10.1016/j.jcrysgro.2004.06.046 ↗
57. Application of Bravais-Friedel-Donnay-Harker, attachment energy and Ising models to predicting and understanding the morphology of molecular crystals10.1088/0022-3727/24/2/001 ↗
58. Nanometre moire fringes in scanning tunnelling microscopy of surface lattices10.1088/0957-4484/15/8/022 ↗
59. Microstructural evolution behavior of Mg-5Si-1Al alloy modified with Sr-Sb during isothermal heat treatment10.1016/j.jallcom.2009.02.044 ↗
60. Revealing modification mechanism of Mg2Si in Sb modified Mg2Si/AZ91 composites and its effect on mechanical properties10.1016/j.jallcom.2020.156877 ↗
61. Effect of Sr on microstructure, tensile properties and wear behavior of as-cast Mg-6Zn-4Si alloy10.1016/j.matdes.2013.07.004 ↗
62. Liu, C. M., Zhu, X.R., Zhou, H.T., Phase diagrams of magnesium alloys, first edition ed, Central South University Press 2006, pp:25,50.
63. Thermal and solute diffusion in α-Mg dendrite growth of Mg-5wt%Zn alloy: a phase-field study10.1016/j.jmrt.2023.05.024 ↗
64. Solid solution and precipitation strengthening effects in basal slip, extension twinning and pyramidal slip in Mg-Zn alloys10.1016/j.actamat.2021.117374 ↗
65. Vacancy hardening and softening in transition metal carbides and nitrides10.1103/PhysRevLett.86.3348 ↗
66. Hardness of covalent crystals10.1103/PhysRevLett.91.015502 ↗
67. Insight into the mechanical, thermodynamics and superconductor properties of NbRuB via first-principles calculation