Effects of TiC0.4 on microstructure and properties of WC composites
Source abstract
Abstract
WC composites with 5 wt% TiC 0.4 were fabricated by spark plasma sintering (SPS) at sintering temperature of 1400–1700 °C for 10 min under an external pressure of 50 MPa. It can be observed that the WC-5 wt% TiC 0.4 composites mainly consisted of WC phase and non-stoichiometric (W 1−x, Ti x)C n solid solution phase and the amount of WC dissolving in TiC 0.4 increased with sintering temperature. The (W 1−x, Ti x)C n solid solutions uniformly distributed around WC grains and formed a semi-coherency interface with WC, which restricted the growth of WC grains and enhanced mechanical properties of the WC-5 wt% TiC 0.4 composites. The average grain size of WC (251.5 ± 201.6 nm) in WC-5 wt% TiC 0.4 composite sintered at 1600 ℃ was considerably smaller compared to most of previously reported WC-based composites. The existence of high content of C vacancies in non-stoichiometric TiC 0.4 raised remarkably the diffusion rate of W and Ti atoms in the sintering process of WC-5 wt% TiC 0.4 composites in contrast with stoichiometric TiC. The WC-5 wt% TiC 0.4 composite sintered at 1600 ℃ possessed the optimum properties, with the hardness of 21.9 GPa, fracture toughness of 7.6 MPa·m 1/2 , flexural strength of 612 MPa and compressive strength of 2.7 GPa. Moreover, it can be confirmed that the oxidation resistance of WC-5 wt% TiC 0.4 composite at higher temperature outperformed that below 1218 ℃. In addition, the WC-5 wt% TiC 0.4 composite sintered at 1600 ℃ showed higher high-temperature hardness, lower thermal conductivity and better resistance to oxidation than those of conventional WC-Co composites.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Nanocrystalline WC-Co composite with ultrahigh hardness and toughness10.1016/j.compositesb.2020.108161 ↗
2. Oscillatory pressure sintering: a new method for preparing WC-Co cemented carbides10.1016/j.jallcom.2019.152521 ↗
3. Fabrication of dual-grain structure WC-Co cemented carbide by in-situ carbothermal reduction of WO3 and subsequent liquid sintering10.1016/j.ceramint.2020.02.045 ↗
4. Binderless WC with high strength and toughness up to 1500 °C10.1016/j.jeurceramsoc.2020.01.055 ↗
5. Electrical resistance flash sintering of tungsten carbide10.1016/j.matdes.2021.110330 ↗
6. A review on binderless tungsten carbide: development and application10.1007/s40820-019-0346-1 ↗
7. Microstructure and mechanical properties of oscillatory pressure sintered WC ceramics with different carbon sources10.1016/j.ceramint.2021.01.020 ↗
8. Influence and effectivity of VC and Cr3C2 grain growth inhibitors on sintering of binderless tungsten carbide10.1016/j.ijrmhm.2011.11.006 ↗
9. Consolidation of binderless WC-TiC by high frequency induction heating sintering10.1016/j.ijrmhm.2007.01.006 ↗
10. Effects of TaC and TiC addition on the microstructures and mechanical properties of binderless WC10.1016/j.ijrmhm.2019.04.012 ↗
11. Sintering of binderless WC-Mo2C hard materials by rapid sintering process10.1016/j.ceramint.2007.03.029 ↗
12. Effect of ZrC nano-powder addition on the microstructure and mechanical properties of binderless tungsten carbide fabricated by spark plasma sintering10.1016/j.ijrmhm.2014.10.013 ↗
13. Effect of Mo2C addition on the microstructures and mechanical properties of WC-SiC ceramics10.1016/j.ijrmhm.2016.12.018 ↗
14. Effects of ZrC and SiC addition on the microstructures and mechanical properties of binderless WC10.1016/j.ijrmhm.2017.09.002 ↗
15. Enhanced mechanical properties and consolidation of the ultra-fine WC-Al2O3 composites using pulsed current activated heating10.1016/j.ceramint.2016.02.113 ↗
16. ZrO2(3Y) toughened WC composites prepared by spark plasma sintering10.1016/j.jallcom.2013.03.259 ↗
17. Study of processing routes for WC-MgO composites with varying MgO contents consolidated by FAST/SPS10.1016/j.jeurceramsoc.2017.01.005 ↗
18. Effects and influence of Y2O3 addition on the microstructure and mechanical properties of binderless tungsten carbide fabricated by spark plasma sintering10.1016/j.ijrmhm.2017.11.016 ↗
19. Influence of nano-sized La2O3 addition on the sintering behavior and mechanical properties of WC-La2O3 composites10.1016/j.ceramint.2015.08.002 ↗
20. Microstructure and characterization of WC-2.8 wt% Al2O3-6.8 wt% ZrO2 composites produced by spark plasma sintering10.1016/j.ceramint.2016.06.044 ↗
21. In-situ elongated aluminium borate grains toughening WC-1.87 wt% Al2O3-4.13 wt% ZrO2 composite via spark plasma sintering10.1016/j.ceramint.2019.06.208 ↗
22. In‑situ elongated β‑Si3N4 grains toughened WC composites prepared by one/two‑step spark plasma sintering10.1016/j.msea.2012.10.059 ↗
23. Influence of Al2O3 whisker concentration on mechanical properties of WC-Al2O3 whisker composite10.1016/j.ceramint.2015.07.167 ↗
24. Influence of MgO whisker addition on microstructures and mechanical properties of WC-MgO composite10.1016/j.matchemphys.2019.121907 ↗
25. Mechanical properties and consolidation of nanostructured WC-CNT composites by high frequency induction heated sintering
26. Effect of sintering temperature on phase constitution and mechanical properties of WC-1.0 wt% carbon nanotube composites10.1016/j.ceramint.2017.09.154 ↗
27. Multilayer graphene reinforced functionally graded tungsten carbide nano‑composites10.1016/j.matdes.2017.08.041 ↗
28. Fabrication and properties of hot-pressing sintered WC-Al2O3 composites reinforced by graphene platelets10.1016/j.ijrmhm.2019.03.025 ↗
29. Processing and mechanical properties of nonstoichiometric TiCx (0.3≤x≤0.5)10.1016/j.ceramint.2018.07.141 ↗
30. Diffusion-controlled alloying of single-phase multi-principal transition metal carbides with high toughness and low thermal diffusivity10.1063/1.5054954 ↗
31. A novel non-stoichiometric medium-entropy carbide stabilized by anion vacancies10.1016/j.jmst.2020.02.049 ↗
32. Microstructural and mechanical behavior of spark plasma sintered titanium carbide with hybrid reinforcement of tungsten carbide and carbon nanotubes10.1016/j.msea.2017.06.108 ↗
33. Effect of SiC whisker addition on the microstructures and mechanical properties of Ti(C, N)-based cermets10.1016/j.matdes.2010.07.028 ↗
34. Effect of TiC addition on the mechanical behaviour of Al2O3-SiC whiskers composites obtained by SPS10.1016/j.jeurceramsoc.2016.01.050 ↗
35. High-entropy carbide ceramics with refined microstructure and enhanced thermal conductivity by the addition of graphite10.1016/j.jeurceramsoc.2021.03.053 ↗
36. Extraordinary toughening enhancement in nonstoichiometric vanadium carbide10.1016/j.jmst.2021.04.057 ↗
37. Densification behavior and mechanical properties of hot pressed TiC-WC ceramics10.1016/j.ceramint.2020.07.335 ↗
38. Spark plasma sintering of WC-Ti
39. Effects of powder preparation and sintering temperature on consolidation of ultrafine WC-8Co tool material produced by spark plasma sintering10.1016/j.ceramint.2019.06.227 ↗
40. Influence of Ni and ZrO2 contents on sintering and mechanical properties of WC-2 wt% ZrO2-1 wt% Ni composites10.1016/j.ceramint.2019.02.198 ↗
41. Stress corrosion cracking resistant nanostructured Al-Mg alloy with low angle grain boundaries10.1016/j.actamat.2021.117607 ↗
42. Vacancy effect on the preparation of high-entropy carbides10.1007/s10853-020-04471-3 ↗
43. Effect of nonstoichiometric TiN0.3 on diffusion behavior in TaC–TiN0.3 system10.1016/j.ceramint.2015.05.092 ↗
44. Spark plasma sintering of WC-VC0.5 composites with exceptional mechanical properties and high-temperature performance10.1016/j.msea.2021.142360 ↗
45. The influence of stacking faults on mechanical behavior of advanced materials10.1016/j.msea.2020.140696 ↗
46. Enhancement of the mechanical properties of ultrafine-grained WC-Co cemented carbides via the in-situ generation of VC10.1016/j.jallcom.2022.163961 ↗
47. Microstructure and properties of WC-CoCuFeNi composites fabricated by spark plasma sintering
48. Pressureless sintering of WC-TaC binderless carbide10.1016/j.ceramint.2020.08.045 ↗
49. Mechanism of grain boundary serration during hot deformation of AZ31 alloy: role of grain boundary dislocations and grain boundary sliding10.1016/j.ijplas.2019.09.003 ↗
50. Role of binder phase on the microstructure and mechanical properties of a mechanically alloyed and spark plasma sintered WC-FCC HEA composites10.1016/j.jallcom.2021.160265 ↗
51. A new model for thermal conductivity of “continuous matrix/dispersed and separated 3D-particles” type composite materials and its application to WC-M (M = Co, Ag) systems10.1016/j.jmst.2021.04.036 ↗
52. Influence of microstructure on hardness and thermal conductivity of hardmetals10.1016/j.ijrmhm.2019.105170 ↗
53. Study of thermal expansion and thermal conductivity of cemented WC-Co composite10.1016/j.ijrmhm.2014.06.009 ↗
54. Pressureless sintering and properties of (Hf0.2Zr0.2Ta0.2Nb0.2Ti0.2)C high-entropy ceramics: the effect of pyrolytic carbon10.1016/j.jeurceramsoc.2021.01.048 ↗
55. Mechanism of the early stages of oxidation of WC-Co cemented carbides10.1016/j.corsci.2015.11.007 ↗
56. High-temperature oxidation behaviour of vacuum hot-pressed WC-15 wt% Al2O3 composites10.1016/j.ceramint.2022.01.079 ↗
57. Effect of C/Ti ratio on densification, microstructure and mechanical properties of TiCx prepared by reactive spark plasma sintering10.1016/j.ceramint.2017.09.202 ↗
58. Preparation, mechanical and tribological properties of WC-Al2O3 composite doped with graphene platelets10.1016/j.ceramint.2020.01.045 ↗
59. Extraordinary high-temperature mechanical properties in binder-free nanopolycrystalline WC ceramic10.1016/j.jmst.2021.05.013 ↗
60. Toughening cemented carbides by phase transformation of zirconia10.1016/j.matdes.2021.109559 ↗