Structural stability of Na-inserted spinel-type sodium titanium oxide
Source abstract
Abstract
Abstract Spinel-type sodium titanium oxide (Na3LiTi5O12, NTO), which has an analogous structure to Li4Ti5O12 (LTO), is prepared as a single-phase material for the negative electrode of Na-ion batteries. A superior Na insertion and extraction cycle performance is achievable based on its similarity with the LTO reaction mechanism. However, the detailed structure of the NTO material in the Na insertion state remains obscure. Consequently, the crystallographic features of the Na insertion mechanism have not been sufficiently elucidated. In this study, the structural analyses of NTO and Na-inserted NTO (Na-NTO) electrodes were performed via X-ray diffraction and Rietveld refinement. The Na occupation site of the NTO spinel lattice was altered from the oxygen tetrahedral to the octahedral site by the electrochemical Na insertion reaction. The lattice constants of NTO and Na-NTO were refined for aNTO = 8.73 A and aNa-NTO = 8.84 A; approximately 1% lattice expansion, which was caused by the local compressions of the Ti–O atomic distance existing in the NTO and their relaxation in the Na-NTO, was confirmed by Na insertion. Notably, Ti–O atomic distances in NTO are quite heterogeneous with values of 1.8 A and 2.2 A, while they are homogenized to 2.0 A, 2.1 A, and 2.2 A in the Na-NTO lattice. Furthermore, the oxygen position in the NTO lattice is modified to enhance lattice symmetry by Na insertion, similar to the Li insertion reaction of the LTO lattice. Thus, the Na-NTO lattice structure is considerably more stable than the NTO lattice, which promises stable Na insertion and extraction cycle performances for NTO materials toward Na-ion battery utilization.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Research development on sodium-ion batteries10.1021/cr500192f ↗
2. Electrode materials for rechargeable sodium-ion batteries: potential alternatives to current lithium-ion batteries10.1002/aenm.201200026 ↗
3. Room-temperature stationary sodium-ion batteries for large-scale electric energy storage10.1039/c3ee40847g ↗
4. Sodium-ion batteries: present and future10.1039/C6CS00776G ↗
5. Materials design for high-safety sodium-ion battery
6. Carbon anodes for nonaqueous alkali metal-ion batteries and their thermal safety aspects10.1002/aenm.201900550 ↗
7. Review—practical issues and future perspective for Na-ion batteries10.1149/2.0151514jes ↗
8. Mechanism of the Na-substituted spinel phase generation in a Li4Ti5O12 electrode via sodium-ion battery cycling10.5796/electrochemistry.18-00029 ↗
9. Spinel-type sodium titanium oxide: a promising sodium-insertion material of sodium-ion batteries10.1021/acsaem.9b00541 ↗
10. Realizing the single-phase spinel-type sodium titanium oxide with the Li4Ti5O12-like structure for building stable sodium-ion batteries10.1021/acsami.9b21925 ↗
11. Structure and electrochemistry of the spinel oxides LiTi2O4 and Li4/3Ti5/3O410.1016/0378-7753(89)80152-1 ↗
12. Zero-strain insertion material of Li[Li1/3Ti5/3]O4 for rechargeable lithium cells10.1149/1.2048592 ↗
13. Zero-strain insertion mechanism of Li[Li1/3Ti5/3]O4 for advanced lithium-ion (shuttlecock) batteries10.1016/j.electacta.2005.05.053 ↗
14. Three-dimensional visualization in powder diffraction10.4028/www.scientific.net/SSP.130.15 ↗
15. Evidence of two-phase formation upon lithium insertion into the Li1.33Ti1.67O4 spinel10.1149/1.1391692 ↗
16. A single-crystal study of the electrochemically Li-ion intercalated spinel-type Li4Ti5O1210.1016/j.ssi.2008.07.006 ↗
17. VESTA 3 for three-dimensional visualization of crystal, volumetric and morphology data10.1107/S0021889811038970 ↗
18. Über die Verfeinerung der Kristallstrukturbestimmung Einiger Vertreter des Rutiltyps: TiO2, SnO2, GeO2 und MgF210.1107/S0365110X56001388 ↗
19. Polyhedral thermal expansion in the TiO2 polymorphs: refinement of the crystal structures of rutile and brookite at high temperature sample at 425 degrees C
20. H in rutile-type compounds: I. Single-crystal neutron and X-ray diffraction study of H in rutile10.2138/am-1995-5-604 ↗
21. Horn · Z. für Kristallogr. - Cryst. Mater. · 1972 · 136 · 27310.1524/zkri.1972.136.16.273 ↗
22. Rietveld analysis of electron powder diffraction data from nanocrystalline anatase, TiO210.1016/S0304-3991(99)00189-8 ↗
23. Gitterstruktur der Oxide, Sulfide, Selenide und Telluride des Lithiums, Natriums und Kaliums
24. Revised effective ionic radii and systematic studies of interatomie distances in halides and chaleogenides10.1107/S0567739476001551 ↗
25. Why do batteries fail?10.1126/science.1253292 ↗
26. Degradation mechanisms in Li-ion batteries: a state-of-the-art review10.1002/er.3762 ↗
27. Ageing mechanisms in lithium-ion batteries10.1016/j.jpowsour.2005.01.006 ↗
28. Fundamental degradation mechanisms of layered oxide Li-ion battery cathode materials: methodology, insights and novel approaches10.1016/j.mseb.2014.11.014 ↗
29. Lithium ion battery anode aging mechanisms10.3390/ma6041310 ↗
30. Layered ternary MetalOxides: performance degradation mechanisms as cathodes, and design strategies for high-performance batteries10.1016/j.pmatsci.2020.100655 ↗