Forming mechanism of growth twins and microstructure evolution on improvement of strength and toughness properties by β-eutectoid element in Ti-7Mo-4Al-4Zr-3Nb-2Cr-xFe alloys
Source abstract
Abstract
To form growth twins and simultaneously improve strength and toughness by using a β-eutectoid element, Ti-7Mo-4Al-4Zr-3Nb-2Cr- x Fe alloys were prepared. The phase composition, morphology of growth twins, tensile properties and fracture toughness were tested. Also, the formation of growth twins and the strength-toughness mechanism were studied. The results show that α and β phases exist after heat treatment. The relative content of β phase increases from 6.1 % to 12.5 % with increasing Fe content. Dislocation entanglements and dislocation walls appear at the α/β interface. There are two kinds of α phases, which are α p and α s phases. The growth twin with a width of ∼20 nm is found in α s phase due to the mismatch with the matrix lattice during solidification process. The smallest size of α p phase is at 1.0 wt% Fe. As the stable element of the β phase, Fe increases the phase transformation resistance from β phase to α phase to limit the growth of α phase. When Fe content increases from 0 to 1.5 wt%, tensile strength increases from 1107 to 1314 MPa. By increasing Fe content from 0 to 1.0 wt%, fracture toughness and elongation increase from 64 to 80 MPa·m 1/2 and 5.4–7.1 %, respectively. The strength and toughness of the alloys increase simultaneously within 0–1.0 wt%Fe. The solution strengthening of Fe, the refinement of α p phase, and the formation of growth twins and dislocation walls are the main reasons for the improvement in strength and toughness.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Influence of annealing on the microstructure and Charpy impact toughness of wire arc additive manufactured Ti5111 alloy10.1016/j.msea.2022.144255 ↗
2. Multi-phase trajectory optimization of aerospace vehicle using sequential penalized convex relaxation10.1016/j.ast.2021.107175 ↗
3. High strength and toughness of Ti-6Al-4V sheets via cryorolling and short-period annealing10.1016/j.msea.2022.143766 ↗
4. Fracture toughness of a rejuvenated β-Ti reinforced bulk metallic glass matrix composite10.1016/j.jmst.2021.09.001 ↗
5. Microstructure tailoring and impact toughness of a newly developed high strength Ti-5Al-3Mo-3V–2Cr-2Zr-1Nb-1Fe alloy10.1016/j.matchar.2021.111103 ↗
6. Oxygen-gradient titanium with high strength, strain hardening and toughness10.1016/j.actamat.2023.118674 ↗
7. Microstructure evolution and mechanical properties of directionally solidified large size Ti-47Al-5Nb-0.18C-0.3Si alloy by electromagnetic confinement10.1016/j.jallcom.2021.161762 ↗
8. Design of high strength and wear-resistance β-Ti alloy via oxygen-charging10.1016/j.actamat.2022.117686 ↗
9. Effect of silicon addition on microstructure and mechanical properties of a high strength Ti-4Al-4Mo-4Sn alloy prepared by powder metallurgy10.1016/j.jallcom.2021.162267 ↗
10. High dislocation density-induced large ductility in deformed and partitioned steels10.1126/science.aan0177 ↗
11. Controlling the microstructure and fracture toughness of the Ti-5Al-5Mo-5V–1Cr-1Fe alloy by multiple heat treatments10.1016/j.jmrt.2022.02.020 ↗
12. Development of beta-type Ti-Nb-Zr-Mo alloys for orthopedic applications
13. Deformation mechanism of bimodal microstructure in Ti-6Al-4V alloy: the effects of intercritical annealing temperature and constituent hardness10.1016/j.jmst.2020.08.057 ↗
14. Yielding nature and Hall-Petch relationships in Ti-6Al-4V alloy with fully equiaxed and bimodal microstructures10.1016/j.scriptamat.2019.07.015 ↗
15. Double toughening Ti-based bulk metallic glass composite with high toughness, strength and tensile ductility via phase engineering
16. Microstructural strengthening and toughening mechanisms in Fe-containing Ti-6Al-4V: a comparison between homogenization and aging treated states10.1016/j.jmst.2021.04.063 ↗
17. Toughening effects of Mo and Nb addition on impact toughness and crack resistance of titanium alloys10.1016/j.jmst.2020.11.045 ↗
18. Exploring the elastic, mechanical and anisotropic response of Ti-5Al-XSn alloys through DFT calculations10.1016/j.cjph.2022.02.016 ↗
19. Microstructure evolution and deformation mechanism of α+β dual-phase Ti-xNb-yTa-2Zr alloys with high performance10.1016/j.jmst.2022.04.052 ↗
20. Enhanced strength-ductility synergy in fiber-like structural titanium matrix composites by controlling TiB content10.1016/j.jallcom.2022.165399 ↗
21. Corrosion behavior of dual-phase Ti-6Al-4V alloys: A discussion on the impact of Fe content10.1016/j.jallcom.2020.157708 ↗
22. Effect of Fe content on microstructure and hardness of Ti-4.5Mo-5Al-1.8Zr-2.5Cr-1.1Sn titanium alloy based on high-throughput diffusion couple10.1016/j.msea.2022.143089 ↗
23. Improved mechanical, bio-corrosion properties and in vitro cell responses of Ti-Fe alloys as candidate dental implants10.1016/j.msec.2021.111917 ↗
24. Phase decomposition upon heat-treatment of a eutectoid Ti-Fe alloy processed by dual-wire-arc additive manufacturing10.1016/j.matlet.2022.132305 ↗
25. Influence of Fe on the microstructure, superplasticity and room-temperature mechanical properties of Ti-4Al-3Mo-1V-0.1B alloy10.1016/j.msea.2022.143245 ↗
26. On the influence of the heat treatment on microstructure formation and mechanical properties of near-α Ti-Fe alloys
27. Corrosion behavior of dual-phase Ti-6Al-4V alloys: a discussion on the impact of Fe content10.1016/j.jallcom.2020.157708 ↗
28. Development of Ti-Mo-Fe alloys combining different plastic deformation mechanisms for improved strength-ductility trade-off and high work hardening rate
29. Refinement of αs phase and formation of nano-twins of Ti-7Mo-4Al-3Nb-2Cr alloyed by Zr element10.1016/j.jmrt.2022.10.129 ↗
30. Unravelling the competitive effect of microstructural features on the fracture toughness and tensile properties of near beta titanium alloys10.1016/j.jmst.2021.04.032 ↗
31. A review of microstructure and texture evolution during plastic deformation and heat treatment of β-Ti alloys10.1016/j.jallcom.2021.163242 ↗
32. Plane strain fracture behavior of a new high strength Ti-5Al-3Mo-3V–2Zr-2Cr-1Nb-1Fe alloy during heat treatment10.1016/j.msea.2020.140080 ↗
33. Strength and fracture toughness of TC21 alloy with multi-level lamellar microstructure10.1016/j.msea.2018.10.056 ↗
34. The effect of surface oxidation behavior on the fracture toughness of Ti-5Al-5Mo-5V–1Cr-1Fe titanium alloy10.1016/j.jallcom.2015.05.211 ↗
35. Effect of electroshocking treatment on the microstructure and mechanical properties of laser melting deposited near-β Ti-55531 thin-wall10.1016/j.jallcom.2022.168187 ↗
36. Fracture toughness anisotropy of Ti17 billet processed by the β forging10.1016/j.msea.2021.140825 ↗
37. The interdependence of microstructure, strength and fracture toughness in a novel β titanium alloy Ti-5Al-4Zr-8Mo-7V10.1016/j.msea.2020.139248 ↗
38. The relationship between flow behavior and initial microstructure of Ti-10V–2Fe-3Al alloy during subtransus deformation10.1016/j.jallcom.2022.166302 ↗
39. Effect of heat treatments on microstructure and property of a high strength/toughness Ti-8V-1.5Mo-2Fe-3Al alloy10.1016/j.msea.2014.08.025 ↗
40. Generalized stacking fault energies and critical resolved shear stresses of random α-Ti-Al alloys from first-principles calculations10.1016/j.jallcom.2020.156314 ↗
41. Deformation-induced γ↔α2 phase transformation in TiAl alloy compressed at room temperature10.1016/j.intermet.2006.10.016 ↗
42. Stacking faults observed in {1012̅} extension twins in a compressed high Sn content Zr alloy10.1016/j.scriptamat.2017.07.028 ↗
43. Balancing strength and ductility by controllable heat-treatment twinning in a near β-Ti alloy10.1016/j.jmrt.2020.04.045 ↗
44. Additive manufacturing of TTFNZ (Ti-4.5Ta-4Fe-7.5Nb-6Zr), a novel metastable β-titanium alloy for advanced engineering applications10.1016/j.jallcom.2022.165899 ↗
45. In-situ investigation of plasticity in a Ti-Al-V-Fe (α+β) alloy: slip mechanisms, strain localization, and partitioning10.1016/j.ijplas.2021.103131 ↗
46. The effect of Si additions on the sintering and sintered microstructure and mechanical properties of Ti-3Ni alloy10.1016/j.msea.2011.06.029 ↗
47. The effects of Fe content on the microstructural evolution and tensile properties in Ti-6Al-4V-(2, 4)Fe alloys fabricated by thermomechanical powder consolidation10.1016/j.msea.2021.141877 ↗
48. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
49. Surface nanocrystallization of body-centered cubic beta phase in Ti-6Al-4V alloy subjected to ultrasonic surface rolling process10.1016/j.surfcoat.2019.01.045 ↗
50. Modelling strengthening mechanisms in beta-type Ti alloys10.1016/j.msea.2019.04.027 ↗
51. Effect of grain size and temperature on the yield stress of the intermetallic compound TiAl10.1016/0036-9748(89)90434-1 ↗
52. Yielding nature and Hall-Petch relationships in Ti-6Al-4V alloy with fully equiaxed and bimodal microstructures10.1016/j.scriptamat.2019.07.015 ↗
53. Fracture characteristics analysis related to the microstructures in titanium alloys10.1016/0921-5093(96)10239-2 ↗
54. Multistage work hardening assisted by multi-type twinning in ultra-fine-grained heterostructural eutectic high-entropy alloys10.1016/j.mattod.2020.09.029 ↗
55. An X-ray method for the determination of stored energies in texture components of deformed metals; application to cold worked ultra high purity iron10.1016/S1359-6454(99)00457-7 ↗
56. A precipitation-hardened high-entropy alloy with outstanding tensile properties10.1016/j.actamat.2015.08.076 ↗
57. Microstructural evolution and strain-hardening in TWIP Ti alloys10.1016/j.actamat.2019.11.009 ↗
58. Mechanical properties and deformation mechanisms of Ti-15Nb-5Zr-4Sn-1Fe alloy with varying α phase fraction
59. Novel transformation pathway and heterogeneous precipitate microstructure in Ti-alloys10.1016/j.actamat.2020.06.048 ↗
60. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al(Sc) alloys10.1016/S1359-6454(02)00201-X ↗
61. Tensile properties of copper with nano-scale twins10.1016/j.scriptamat.2005.01.033 ↗
62. Dislocation nucleation governed softening and maximum strength in nano-twinned metals10.1038/nature08929 ↗