journal article·2023-03

Modification of electrical properties of amorphous vanadium oxide (a-VOx) thin film thermistor for microbolometer

Dasom Wang, Jaeyeong Bae, Hyung-Jin Choi, Seung-Hyub Baek, Seungwan Woo, Donghee Park, Won Jun Choi

Publisher page

Abstract

This work reports on the modification of electrical properties of amorphous vanadium oxide (a-VO x ) thin film thermistor by growth temperature and its effects on the performances of a cooler-free microbolometer. The a-VO x thin films have been deposited by pulsed DC sputtering processes under various growth temperatures from 160 to 230 ℃. The sheet resistance of the samples at room temperature decreases from 330 to 70 kΩ/▢ with increasing growth temperature. This is due to the increase of oxygen vacancies at higher growth temperature, which have been confirmed by XPS analysis. Temperature dependence of resistance of a-VO x films shows non-hysteresis behaviors up to 120 ℃, which in turn shows clear activation energies. The activation energy of a-VO x films also decreases from 0.190 to 0.145 eV with increasing growth temperature, which confirms the decrease of temperature coefficient of resistance (TCR) from 2.80 to 2.44 (-%/K) at 25 ℃ and from 1.48 to 1.14 (-%/K) even at 120 ℃. The responsivities of fabricated microbolometers based on the a-VO x thin film thermistors have been measured from 3.04 × 10 3 to 1.14 × 10 3 V/W at room temperature and from 9.54 × 10 2 to 3.02 × 10 2 V/W even at 120 ℃ with increasing growth temperature.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Transition Metal Oxide Nanomaterials · Gas Sensing Nanomaterials and Sensors · Electrical and Thermal Properties of Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (69)

Show source-provided references
1. Single-side fabricated p+Si/Al thermopile-based gas flow sensor for IC-foundry-compatible, high-yield, and low-cost volume manufacturing10.1109/TED.2018.2878469 ↗
2. Pedestrian detection with thermopiles using an occupancy grid
3. Transient radiation effects in ultra-low noise HgCdTe IR detector arrays for space-based astronomy10.1109/TNS.2005.860732 ↗
4. CMOS-SOI-MEMS transistor for uncooled IR imaging10.1109/TED.2009.2026523 ↗
5. Thermal sensors for contactless temperature measurements, occupancy detection, and automatic operation of appliances during the COVID-19 pandemic, A review10.3390/mi12020148 ↗
6. Uncooled microbolometer FPA sensor with wafer-level vacuum packaging, J. Sens
7. MEMS-based uncooled infrared bolometer arrays10.1117/12.755128 ↗
8. Spectral selectivity in infrared thermal detection10.1038/lsa.2012.24 ↗
9. A new uncooled thermal IR detector using silicon diode
10. Fabrication of microbolometer arrays based on polymorphous silicon–germanium10.3390/s20092716 ↗
11. 320×240 silicon microbolometer uncooled IR FPAs with on-chip offset correction10.1117/12.243062 ↗
12. Low-cost microbolometer type infrared detectors10.3390/mi11090800 ↗
13. Fabrication process for 256×256 bolometer-type uncooled infrared detector
14. Vanadium oxide microbolometer with gold black absorbing layer10.1117/1.OE.51.7.074003 ↗
15. Amorphous silicon thin-films for uncooled infrared microbolometer sensors10.1117/12.850545 ↗
16. Characterization of platinum and titanium thermistors for terahertz antenna-coupled bolometer applications10.1016/j.sna.2018.02.014 ↗
17. Vanadium oxide compounds: structure, properties, and growth from the gas phase10.1002/cvde.201400057 ↗
18. Stoichiometry and microstructural effects on electrical conduction in pulsed dc sputtered vanadium oxide thin films10.1557/jmr.2009.0183 ↗
19. Effects of postdeposition annealing on the metal-insulator transition of VO2-x thin films prepared by RF magnetron sputtering10.7567/JJAP.53.033201 ↗
20. Low temperature growth of amorphous VO2 films on flexible polyimide substrates with a TiO2 buffer layer10.1116/1.5019388 ↗
21. Influence of oxygen flow rate on metal–insulator transition of vanadium oxide thin films grown by RF magnetron sputtering10.1007/s00339-017-0779-7 ↗
22. Pulsed DC reactive magnetron sputtering of vanadium dioxide thermochromic thin films10.1179/175355511X12941605982307 ↗
23. High-performance thermal sensitive VO2(B) thin films prepared by sputtering with TiO2(A) buffer layer and first-principles calculations study10.1039/C7RA03239K ↗
24. Selective growth and texturing of VO2(B) thin films for high-temperature microbolometers10.1016/j.jeurceramsoc.2020.05.052 ↗
25. Spectroscopic characterization of electron-beam evaporated V2O5 thin films10.1016/S0040-6090(97)00141-7 ↗
26. Dependence of optical properties of vanadium oxide films on crystallization and temperature10.1016/j.tsf.2011.11.028 ↗
27. Low temperature charge carrier hopping transport mechanism in vanadium oxide thin films grown using pulsed dc sputtering10.1063/1.3139864 ↗
28. P-type amorphous vanadium oxide thin film fabricated by pulsed laser deposition10.35848/1347-4065/ab9ef7 ↗
29. Atomic layer deposition of vanadium dioxide and a temperature-dependent optical model
30. High temperature coefficient of resistance and low noise tungsten oxide doped amorphous vanadium oxide thin films for microbolometer applications10.1016/j.tsf.2019.137590 ↗
31. The microstructures and electrical properties of Y-doped amorphous vanadium oxide thin films10.1016/j.infrared.2016.12.013 ↗
32. Doped vanadium oxide for optical switching films10.1016/0165-1633(86)90047-X ↗
33. Fabrication of vanadium oxide thin film with high-temperature coefficient of resistance using V2O5/V/V2O5 multi-layers for uncooled microbolometer10.1016/S0040-6090(02)01263-4 ↗
34. Wide-temperature (up to 100 °C) operation of thermostable vanadium oxide based microbolometers with Ti/MgF2 infrared absorbing layer for long wavelength infrared (LWIR) detection10.1016/j.apsusc.2021.149142 ↗
35. Low temperature fabrication of vanadium oxide films for uncooled bolometric detectors10.1016/j.infrared.2005.04.001 ↗
36. A relationship between the V4+/V5+ ratio and the surface dispersion, surface acidity, and redox performance of V2O5-WO3/TiO2 SCR catalysts10.1039/C8RA02857E ↗
37. Substrate temperature effects on the structural, compositional, and electrical properties of VO2 thin films deposited by pulsed laser deposition10.1002/sia.6368 ↗
38. Structural and electrical properties of sputtered vanadium oxide thin films for applications as gas sensing material10.1063/1.363973 ↗
39. Raman and XPS characterization of vanadium oxide thin films with temperature10.1016/j.apsusc.2017.01.160 ↗
40. Stoichiometric vanadium oxides studied by XPS10.1002/sia.3844 ↗
41. Physical analysis of VO2 films grown by atomic layer deposition and RF magnetron sputtering10.1149/2.006406jss ↗
42. Growth and properties of strained VOx thin films with controlled stoichiometry10.1103/PhysRevB.69.075404 ↗
43. Tuning the properties of VO2 thin films through growth temperature for infrared and terahertz modulation applications10.1063/1.4821846 ↗
44. Oxygen vacancies allow tuning the work function of vanadium dioxide10.1002/admi.201801033 ↗
45. Effect of oxygen content on the electrical properties of sputter deposited vanadium oxide thin-films10.1016/j.mssp.2018.07.040 ↗
46. Role of oxygen vacancies in vanadium oxide and oxygen functional groups in graphene oxide for room temperature CO2 gas sensors10.1016/j.sna.2019.04.037 ↗
47. Influence of post-annealing on resistivity of VOx Thin Film10.1109/LED.2014.2326691 ↗
48. Electrical and optical properties of sputtered amorphous vanadium oxide thin films10.1063/1.3702451 ↗
49. Electrical and Infrared Optical Properties of Vanadium Oxide Semiconducting Thin-Film Thermometers10.1007/s11664-017-5571-0 ↗
50. High temperature coefficient of resistance and low noise tungsten oxide doped amorphous vanadium oxide thin films for microbolometer applications10.1016/j.tsf.2019.137590 ↗
51. Synthesis and phase stability of metastable bixbyite V2O3 colloidal nanocrystals10.1021/cm401530t ↗
52. Synthesis and optical properties of V2O5 nanorods10.1063/1.2722746 ↗
53. Effects of annealing ambient on oxygen vacancies and phase transition temperature of VO2 thin films10.1039/C6RA13189A ↗
54. Low temperature fabrication of VOx thin films for uncooled IR detectors by direct current reactive magnetron sputtering method10.1016/j.infrared.2007.12.002 ↗
55. Physical interpretation, modeling and impact on phase change memory (PCM) reliability of resistance drift due to chalcogenide structural relaxation
56. Physical mechanism and temperature acceleration of relaxation effects in phase-change memory cells
57. Reliability impact of chalcogenide-structure relaxation in phase-change memory (PCM) cells-Part I: Experimental study10.1109/TED.2009.2016397 ↗
58. Measurements of thermal characteristics in silicon germanium un-cooled micro-bolometers, Phys. Status Solidi Curr. Top
59. Noise performance of NbN hot electron bolometer mixers at 2.5 THz and its dependence on the contact resistance
60. Optically Immersed Bolometer IR Detectors Based on V2O5 Thin Films with Polyimide Thermal Impedance Control Layer for Space Applications10.1007/s10762-017-0446-2 ↗
61. Performance improvement of Y-doped VOx microbolometers with nanomesh antireflection layer10.1364/OE.386438 ↗
62. Performance improvement in amorphous silicon based uncooled microbolometers through pixel design and materials development10.1117/12.884249 ↗
63. Thermal conductivity control by oxygen defect concentration modification in reducible oxides: The case of Pr0.1Ce0.9O2−δ thin films10.1063/1.4865768 ↗
64. Review on texturization effects in thermoelectric oxides10.1007/s40243-019-0163-y ↗
65. Investigation of the thermal conductivities across metal-insulator transition in polycrystalline VO210.1007/s11434-012-5294-9 ↗
66. An all-ZnO microbolometer for infrared imaging10.1016/j.infrared.2014.07.023 ↗
67. IR detectors with adaptive responsivity and wavelength
68. Characterization of uncooled bolometer with vanadium tungsten oxide infrared active layer10.1016/j.sna.2005.04.024 ↗
69. Reliable determination of chemical state in x-ray photoelectron spectroscopy based on sample-work-function referencing to adventitious carbon: resolving the myth of apparent constant binding energy of the C 1s peak10.1016/j.apsusc.2018.04.226 ↗