Abstract

Sm 2Co 17-type permanent magnets are the favorable choice for applications above 200 °C. Their performance can be enhanced by Zr alloying, mainly due to the formation of Zr-rich 1:3R Z-plates. Herein, the atomic-scale structures of the Z-plates in an 1.7 at% Zr alloyed Sm 2Co 17 -type magnet are unveiled using aberration-corrected STEM. Zr is observed to preferably replace the dumbbell Sm to form (Sm 1/3Zr 2/3)Co 3 Z-plates, which have a number density of 37.6 µm −1 along c-axis. The Z-plate with thickness of the reported one-unit cell is rarely seen, instead several anomalously stacked types are detected. Most of the Z-plates have a two-third stacking (2/3-stacked) of one-unit cell, some of them are lacking one Sm+Co layer while others have additional Sm+Co layers. Totally four types of single 2/3-stacked Z-plates are identified, acting as the basic units for thick Z-plates. A few Z-plates (number density 2.73 µm −1) have thickness of more than double 2/3-stacking, which deteriorate the oxidation-resistance of the magnet. Further, by analyzing the end regions of Z-plates, the diffusion-controlled mechanisms for the phase transformation from the 2:17R matrix to the 1:3R Z-plates are unraveled.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Hydrogen Storage and Materials · Magnetic properties of thin films

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Perspective and prospects for rare earth permanent magnets10.1016/j.eng.2018.11.034 ↗
2. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
3. Recent developments in hard magnetic bulk materials
4. Enhancement of the Curie temperature for exchange coupled Nd-Fe-B and Pr-Fe-B magnets10.1109/20.619607 ↗
5. Magnetic properties of a new type of rare-earth cobalt magnets Sm2(Co, Cu, Fe, M)1710.1109/TMAG.1977.1059703 ↗
6. Genesis of the cell microstructure in the Sm(Co, Fe, Cu, Zr) permanent magnets with 2:17 type10.1002/pssa.2211400104 ↗
7. The microstructure of sintered Sm(Co0.72Fe0.20Cu0.055Zr0.025)7.5 permanent magnet studied by atom probe10.1016/j.actamat.2003.10.015 ↗
8. Correlation of microchemistry of cell boundary phase and interface structure to the coercivity of Sm(Co0.784Fe0.100Cu0.088Zr0.028)7.19 sintered magnets10.1016/j.actamat.2016.12.050 ↗
9. Direct evidence for Cu concentration variation and its correlation to coercivity in Sm(Co0.74Fe0.1Cu0.12Zr.04)7.4 ribbons10.1016/j.scriptamat.2009.01.006 ↗
10. Effects of solution treated temperature on the structural and magnetic properties of iron-rich Sm(CoFeCuZr)Z sintered magnet10.1109/TMAG.2013.2247576 ↗
11. Microstructures of precipitation‐hardened SmCo permanent magnets10.1063/1.330867 ↗
12. Evolution of microstructure, microchemistry and coercivity in 2.17 type Sm-Co magnets with heat treatment10.1109/20.951223 ↗
13. High temperature 2:17 magnets: relationship of magnetic properties to microstructure and processing10.1109/20.908808 ↗
14. Coercivity of precipitation hardened cobalt rare earth 17:2 permanent magnets10.1016/0304-8853(82)90010-5 ↗
15. The evolution of phase constitution and microstructure in iron-rich 2:17-type Sm-Co magnets with high magnetic performance10.1038/s41598-018-27487-x ↗
16. Correlation between Fe content and z value in Sm(CobalFexCu0.06Zr0.025)z permanent magnets10.1016/j.jmmm.2018.11.008 ↗
17. Atomic structure and domain wall pinning in samarium-cobalt-based permanent magnets10.1038/s41467-017-00059-9 ↗
18. Magnetic characterization of the (Zr,Sm)Co3 phase in Sm(CoFeCuZr)z magnets10.1063/1.2709759 ↗
19. Effect of Zr on the microstructure and magnetic properties of Sm(CobalFe0.1Cu0.088Zrx)8.5 magnets10.1063/1.371874 ↗
20. High-temperature magnetic properties of Sm(CobalFe0.1Cu0.088Zrx)8.5 magnets10.1016/S0304-8853(99)00783-0 ↗
21. Effect of Zr on magnetic properties and electrical resistivity of Sm(CobalFe0.09Cu0.09Zrx)7.68 magnets10.1016/j.jallcom.2018.04.222 ↗
22. Atomic-scale structure clarification of the planar Z phase and its influence on the magnetic properties in Sm(CoFeCuZr)z permanent magnets10.1016/j.actamat.2022.117846 ↗
23. The oxidation morphology of SmCo alloys10.1016/j.jallcom.2009.07.115 ↗
24. High temperature oxidation and its induced coercivity loss of a 2:17 type SmCo-based magnet
25. Decomposition behavior in the early-stage oxidation of Sm2Co17-type magnets10.1016/j.scriptamat.2021.113911 ↗
26. Atomic-scale oxidation of a Sm2Co17-type magnet10.1016/j.actamat.2021.117343 ↗
27. Zirconium content induced mitigation of mechanical anisotropy in 2:17 type SmCo magnets10.1016/j.jre.2019.07.006 ↗
28. Anisotropic fracture behavior of sintered rare-earth permanent magnets10.1109/TMAG.2005.852948 ↗
29. Unconventional magnetization textures and domain-wall pinning in Sm–Co magnets10.1038/s41598-020-78010-0 ↗
30. Nanoscale short-range ordering induced cellular structure and microchemistry evolution in Sm2Co17-type magnets10.1016/j.actamat.2020.09.057 ↗
31. Atomic scale understanding of the defects process in concurrent recrystallization and precipitation of Sm-Co-Fe-Cu-Zr alloys10.1016/j.actamat.2020.10.067 ↗
32. Mechanism of phase transformation in 2:17 type SmCo magnets investigated by phase stabilization10.1016/j.scriptamat.2015.10.041 ↗
33. The formation mechanism of 1:5H phase in Sm(Co, Fe, Cu, Zr)z melt-spun ribbons with high iron content10.1016/j.jmmm.2019.165939 ↗
34. Koch · 2002
35. Twinning structure in Sm(Co,Fe,Cu,Zr)z permanent magnet10.1016/j.intermet.2010.02.008 ↗
36. Intermetallic compounds in the system samarium-cobalt10.1016/0022-5088(68)90037-4 ↗
37. Role of primary Zr-rich particles on microstructure and magnetic properties of 2:17-type Sm-Co-Fe-Cu-Zr permanent magnets10.1016/j.jmst.2020.04.018 ↗
38. Phase evolution and its effects on the magnetic performance of nanocrystalline SmCo7 alloy10.1016/j.actamat.2010.11.047 ↗
39. Temperature dependence of magnetization processes in Sm(Co, Fe, Cu, Zr)z magnets with different nanoscale microstructures10.1063/5.0048047 ↗