Improving the thermal expansion behavior and damping capacity of C/SiC composites by heat treatment
Source abstract
Abstract
Abstract The present study proposes the heat treatment method to optimize the coefficient of thermal expansion (CTE) and damping capacity of 2D C/SiC composites. Results demonstrated that CTE increased monotonically with measuring temperature and could be tuned in a wide range from 2.16 × 10−6 to 0.48 × 10−6 K−1 at 200 °C by controlling the HT temperature. CTE decreased significantly at HT temperatures below 1700 °C and remained constant above that value and up to 1900 °C. The damping capacity of C/SiC composites could be improved by increasing HT temperature up to 1700 °C by introduction of thermally-induced microcracking phenomena; thereafter further increase in HT temperature did not contribute to damping. Matrix microcracking due to heat treatment also relaxed the residual stress state of the material by counteracting part of the matrix extension through propagation inside the composites hence contributing to dissipation of imposed vibration energy. A HT temperature value of 1700 °C was identified as critical for the total relaxation of thermal stresses; further increase in HT temperature failed to create more microcracks.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Thermal properties of materials · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Design, fabrication and applications of C/C, C/Si and SiC/SiC composites
2. Stress-dependence and time-dependence of the post-fatigue tensile behavior of carbon fiber reinforced SiC matrix composites10.1016/j.compscitech.2011.05.013 ↗
3. High-temperature tensile properties and oxidation behavior of carbon fiber reinforced silicon carbide bolts in a simulated re-entry environment10.1016/j.carbon.2010.01.056 ↗
4. Carbon fiber reinforced CMC for high-performance structures10.1111/j.1744-7402.2004.tb00169.x ↗
5. Damage analysis of thin 3D-woven SiC/SiC composite under low velocity impact loading10.1016/j.compositesa.2011.10.013 ↗
6. Damage assessment of thin SiC/SiC composite plates subjected to quasi-static indentation loading10.1016/j.compositesa.2010.08.004 ↗
7. Large-scale fabrication of lightweight Si/SiC ceramic composite optical mirror10.1016/j.matlet.2003.09.010 ↗
8. Effect of materials and modelling on the design of the space-based lightweight mirror10.1016/j.matdes.2008.04.056 ↗
9. Effect of SiC coating and heat treatment on the thermal radiation properties of C/SiC composites10.1016/j.jeurceramsoc.2013.12.012 ↗
10. Increasing the strength and toughness of a carbon fiber/silicon carbide composite by heat treatment10.1016/j.carbon.2012.11.001 ↗
11. Enhancing the fracture resistance of composites by interface modification through a simple fiber heat-treatment process10.1016/j.carbon.2016.08.047 ↗
12. Effect of heat treatment on the mechanical of SiCf/BN/SiC fabricated by CVI10.1016/j.ceramint.2015.11.030 ↗
13. Effect of intermediate heat treatment on mechanical properties of SiCf/SiC composites with BN interphase prepared by ICVI10.1016/j.jeurceramsoc.2010.12.018 ↗
14. Thermal expansion behavior of carbon fiber reinforced chemical-vapor-infiltrated silicon carbide composites from room temperature to 1400°C10.1016/j.matlet.2006.02.088 ↗
15. Temperature dependence of internal friction and elastic modulus of SiC/SiC composites10.1016/S0925-8388(03)00252-4 ↗
16. Effect of SiC coating and heat treatment on damping behavior of C/SiC composites10.1016/j.msea.2007.06.049 ↗
17. Effect of heat treatment on the thermal expansion of 2D and 3D C/SiC composites from room temperature to 1400 °C10.1016/S0008-6223(03)00125-8 ↗
18. Scripta Metal. Metal matrix composites Al-1bAl2O3 studied by mechanical spectroscopy10.1016/0925-8388(94)90531-2 ↗
19. Silicon-carbide monofilament-reinforced silicon-nitride or silicon-carbide matrix composites10.1111/j.1151-2916.1989.tb06174.x ↗
20. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites. 1. experimental approach10.1111/j.1151-2916.1994.tb07096.x ↗