Nanoindentation mechanical properties of glassy Cu 29 Zr 32 Ti 15 Al 5 Ni 19
Source abstract
Abstract
Abstract Cylindrical high entropy metallic glass Cu29Zr32Ti15Al5Ni19 (φ1mm) was prepared via suction casting into a water-cooled mold. The mechanical properties of glassy Cu29Zr32Ti15Al5Ni19 were valued via nanoindentation with Continuous Stiffness Measurement (CSM) mode. The results show that glassy Cu29Zr32Ti15Al5Ni19 is of good plasticity and homogeneous. The average values of nano-hardness and modulus of high entropy bulk metallic glass Cu29Zr32Ti15Al5Ni19 are 7.45 GPa and 105.4 GPa, respectively. Creep can be observed at room temperature when the alloy is held with a constant load. The average creep degree in holding stage is 52.4%, and the creep rate in steady-state creep is about 0.007% s−1. The creep compliance begins with a constant and then increases with time.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · High Entropy Alloys Studies · Phase-change materials and chalcogenides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Pd20Pt20Cu20Ni20P20 high-entropy alloy as a bulk metallic glass in the centimeter10.1016/j.intermet.2011.05.030 ↗
2. Phase stability in high entropy alloys: formation of solid-solution phase or amorphous phase10.1016/S1002-0071(12)60080-X ↗
3. A senary TiZrHfCuNiBe high entropy bulk metallic glass with large glass-forming ability10.1016/j.matlet.2014.03.185 ↗
4. More than entropy in high-entropy alloys: forming solid solutions or amorphous phase10.1016/j.intermet.2013.05.002 ↗
5. High entropy Ti20Zr20Cu20Ni20Be20 bulk metallic glass10.1016/j.jnoncrysol.2013.01.022 ↗
6. High mixing entropy bulk metallic glasses10.1016/j.jnoncrysol.2011.07.016 ↗
7. Alloy design for high-entropy bulk glassy alloys10.1016/j.proeng.2012.03.035 ↗
8. A quinary TieZreHfeBeeCu high entropy bulk metallic glass with a critical size of 12 mm10.1016/j.intermet.2015.02.011 ↗
9. Nanoindentation mechanical properties of indium-alloyed Cu-based bulk metallic glasses10.1007/s11665-013-0765-y ↗
10. Evaluation of Cu-Zr-Ti-in bulk metallic glasses via nanoindentation10.1007/s11665-013-0519-x ↗
11. Nanoindentation and mechanical properties of solids in submicrovolumes, thin near-surface layers, and films: a review10.1134/S1063783408120019 ↗
12. Stress induced pop-in and pop-out nanoindentation events in CuAlBe shape memory alloys10.1016/j.msea.2013.08.052 ↗
13. 3D versus 2Dfinite element simulation of the effect of surface roughness on nanoindentation of hard coatings10.1016/j.surfcoat.2009.04.006 ↗
14. The characterization of creep and time-dependent properties of bulk metallic glasses using nanoindentation10.1016/j.msea.2007.06.015 ↗
15. A simple method to minimize displacement measurement uncertainties using dynamic nanoindentation testing10.1016/j.triboint.2013.10.013 ↗
16. Mechanical behaviour characterisation of silicon and effect of loading rate on pop-in: a nanoindentation study under ultra-low loads10.1016/j.msea.2008.11.021 ↗
17. Taihua · 2013
18. Modified method for continuous stiffness measurement10.1557/jmr.2009.0087 ↗
19. A review of nanoindentation continuous stiffness measurement technique and its applications10.1016/S1044-5803(02)00192-4 ↗
20. The continuous stiffness measurement technique in nanoindentation intrinsically modifies the strength of the sample10.1080/14786435.2012.722234 ↗
21. Mechanical properties of bulk metallic glasses10.1016/j.pmatsci.2010.04.002 ↗
22. Micro and nano indentation studies on Zr60Cu10Al15Ni15bulk metallic glass10.1016/j.matdes.2014.09.017 ↗
23. Designing plastic Cu-based bulk metallic glass via minor addition of nickel10.1016/j.matdes.2013.12.041 ↗
24. Analysis of the indentation size effect in brittle materials from nanoindentation load–displacement curve10.1016/j.jeurceramsoc.2010.05.006 ↗
25. Thermal analysis and nanoindentaion studies on nanocrystalline AlCrNiFeZn high entropy alloy10.1016/j.mspro.2014.07.079 ↗
26. Fischer-Cripps · 2011
27. The characterization of creep and time-dependent properties of bulk metallic glasses using nanoindentation10.1016/j.msea.2007.06.015 ↗
28. Room-temperature creep resistance of co-based metallic glasses
29. Nanoindentation characterized initial creep behavior of a high-entropy-based alloy CoFeNi10.1016/j.intermet.2014.05.007 ↗
30. Creep behaviour of eutectic SnBi alloy and its constituent phases using nanoindentation technique10.1016/j.jallcom.2013.04.057 ↗