Abstract

In this study, an AlSi10Cu4Mg alloy was prepared by selective laser melting (SLM) using a mixture of pre-alloyed AlSi10Mg and elemental Cu powders, followed by aging at 180 ℃ for 2 h. The high-temperature tensile properties of both the SLMed and SLM-aged samples were tested in the temperature range of 200–400 ℃, and the microstructure changes during deformation were compared. At the temperature of 200 ℃, the SLMed sample exhibits outstanding tensile properties with an ultimate tensile strength (UTS) of 327±2 MPa and an elongation (EL) of 25.5±0.5 %. This is mainly related to the strain hardening that caused by the accumulation of anomalous dislocations near the high-volume fraction of Si nano-particles within the grains. For the SLM-aged sample, the aging treatment is found to further increase the strength, yielding a UTS of 381±3 MPa. The metastable transition of the Al 2 Cu phase indirectly promotes the precipitation of the nano-sized Si phase during the aging process. As the testing temperature increases, the strength increment of the SLM-aged sample gradually diminishes, while the elongation increment increases. Due to the limited intrinsic thermal stability of Si nano-particles and θ′ phase, the coarsening of the precipitates can weaken the strengthening effect. The dynamic recrystallization process can be accelerated by the aging treatment, thereby helping to improve the elongation.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (72)

Show source-provided references
1. High-temperature mechanical properties of AlSi10Mg specimens fabricated by additive manufacturing using selective laser melting technologies (AM-SLM)
2. Study on mechanical properties of honeycomb pentamode structures fabricated by laser additive manufacturing: numerical simulation and experimental verification10.1016/j.compstruct.2019.111199 ↗
3. Use of power factor and specific point energy as design parameters in laser powder-bed-fusion (L-PBF) of AlSi10Mg alloy10.1016/j.matdes.2019.108018 ↗
4. Aluminium alloys for aerospace applications
5. Achieving superior strength and ductility of AlSi10Mg alloy fabricated by selective laser melting with large Laser power and high scanning speed10.1007/s40195-022-01410-w ↗
6. High-temperature mechanical properties of stress-relieved AlSi10Mg produced via laser powder bed fusion additive manufacturing10.3390/ma15207386 ↗
7. Additive manufacturing of nano-oxide decorated AlSi10Mg composites: a comparative study on Gd2O3 and Er2O3 additions10.1016/j.matchar.2022.112206 ↗
8. In situ alloying of AlSi10Mg-5 wt% Ni through laser powder bed fusion and subsequent heat treatment10.1016/j.jallcom.2022.164081 ↗
9. Mechanical properties of SLM-printed aluminium alloys: a review10.3390/ma13194301 ↗
10. Design and development of an experimental wrought aluminum alloy for use at elevated temperatures10.1007/BF02628387 ↗
11. Thermal exposure of Al-Si-Cu-Mn-Fe alloys and its contribution to high temperature mechanical properties10.1016/j.jmrt.2019.12.018 ↗
12. Effect of Cu/Mg-containing intermetallics on the mechanical properties of the as-cast HVDC AlSiMgMnCu alloys by SBFSEM at nano-scale10.1016/j.jallcom.2022.166837 ↗
13. Microstructural evolution and strengthening mechanisms in a heat-treated additively manufactured Al–Cu–Mn–Zr alloy10.1016/j.msea.2022.142928 ↗
14. On the origin of the high coarsening resistance of Ω plates in Al–Cu–Mg–Ag Alloys10.1016/S1359-6454(01)00155-0 ↗
15. Highly stable coherent nanoprecipitates via diffusion-dominated solute uptake and interstitial ordering10.1038/s41563-022-01420-0 ↗
16. Influence of Cu content on ageing behavior of AlSiMgCu cast alloys10.1016/j.matdes.2005.11.015 ↗
17. Alloying AlSi10Mg and Cu powders in laser single scan tracks, melt spinning, and laser powder bed fusion10.1016/j.jallcom.2019.153538 ↗
18. Influence of Sc addition on precipitation behavior and properties of Al-Cu-Mg alloy
19. Microstructural evolution and precipitation behavior of Al–7Si–3Cu alloy prepared under 5 GPa10.1016/j.jmst.2023.03.016 ↗
20. Schaffer · 1999
21. Verhoeven · 1975
22. Alloying AlSi10Mg and Cu powders in laser single scan tracks, melt spinning, and laser powder bed fusion10.1016/j.jallcom.2019.153538 ↗
23. Effect of direct aging on the microstructure and tensile properties of AlSi10Mg alloy manufactured by selective laser melting process10.1016/j.matchar.2021.111113 ↗
24. Microstructure and mechanical properties of Cu-modified AlSi10Mg fabricated by laser-powder bed fusion10.1016/j.mtla.2020.100590 ↗
25. Achieving high strength in selective laser melting AlSi10Mg alloy by adding microsized pure Cu particles10.1016/j.msea.2023.145357 ↗
26. An analytical model for the interaction between an insoluble particle and an advancing solid/liquid interface10.1007/BF02801184 ↗
27. R.B. Bird, W.E. Stewart, E.N. Lightfoot, Notes on transport phenomena. 1958.
28. On the behaviour of foreign particles at an advancing solid-liquid interface10.1016/0022-0248(89)90097-3 ↗
29. Microstructure of selective laser melted AlSi10Mg alloy10.1016/j.matdes.2019.107677 ↗
30. Selective laser melting of a high strength AlMnSc alloy: alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
31. Influence of predeformation and ageing of an Al–Zn–Mg alloy—II. Modeling of precipitation kinetics and yield stress10.1016/S1359-6454(98)00296-1 ↗
32. Modelling precipitation hardening in an A356+ 0.5 wt% Cu cast aluminum alloy
33. Unraveling precipitation evolution and strengthening function of the Al-Zn-Mg-Cu alloys with various Zn contents: multiple experiments and integrated internal-state-variable modeling10.1016/j.jmst.2021.12.008 ↗
34. Processing of Al-Cu-Mg alloy by FSSP: Parametric analysis and the effect of cooling environment on microstructure evolution10.1016/j.matlet.2021.131157 ↗
35. Simultaneous segregation at coherent and semicoherent heterophase interfaces10.1103/PhysRevLett.105.076102 ↗
36. Solute segregation at the Al/θ′-Al2Cu interface in Al-Cu alloys10.1016/j.actamat.2017.09.020 ↗
37. Coupled segregation mechanisms of Sc, Zr and Mn at θ′ interfaces enhances the strength and thermal stability of Al-Cu alloys10.1016/j.actamat.2021.116634 ↗
38. Enhanced coarsening resistance of Q-phase in aluminum alloys by the addition of slow diffusing solutes10.1016/j.msea.2018.08.059 ↗
39. Elevated temperature mechanical properties of TiCN reinforced AlSi10Mg fabricated by laser powder bed fusion additive manufacturing10.1016/j.msea.2021.141025 ↗
40. The role of transition metal additions on the ambient and elevated temperature properties of Al-Si alloys10.1016/j.msea.2017.03.084 ↗
41. High temperature tensile deformation behavior and failure mechanisms of an Al–Si–Cu–Mg cast alloy—the microstructural scale effect10.1016/j.matdes.2015.07.084 ↗
42. Effect of microstructure and overaging on the tensile behavior at room and elevated temperature of C355-T6 cast aluminum alloy10.1016/j.matdes.2015.06.031 ↗
43. Effect of Zr on the high cycle fatigue and mechanical properties of Al–Si–Cu–Mg alloys at elevated temperatures10.1016/j.jallcom.2019.151795 ↗
44. A creep-resistant additively manufactured Al-Ce-Ni-Mn alloy10.1016/j.actamat.2022.117699 ↗
45. Microstructure, tensile properties and thermal stability of AlMgSiScZr alloy printed by laser powder bed fusion10.1016/j.jmst.2020.08.033 ↗
46. Microstructure and properties of a high temperature Al–Ce–Mn alloy produced by additive manufacturing10.1016/j.actamat.2020.07.014 ↗
47. Influence of Si precipitates on fracture mechanisms of AlSi10Mg parts processed by Selective Laser Melting10.1016/j.actamat.2019.06.013 ↗
48. Microstructure evolution and mechanical properties at high temperature of selective laser melted AlSi10Mg10.1016/j.jmst.2020.04.066 ↗
49. In-situ ebsd study of the active slip systems and lattice rotation behavior of surface grains in aluminum alloy during tensile deformation10.1016/j.msea.2013.05.046 ↗
50. In-situ evidence for rotation of Si particles with respect to grains in tensile-deformed Al-Si alloys10.1016/S1003-6326(23)66211-9 ↗
51. Geometrically necessary dislocation and size-dependent plasticity10.1016/S1359-6462(02)00329-9 ↗
52. Recent progress in gradient-structured metals and alloys10.1016/j.pmatsci.2023.101194 ↗
53. Towards the work hardening and strain delocalization achieved via in-situ intragranular reinforcement in Al-CuO composite10.1016/j.actamat.2023.119110 ↗
54. A criterion for slip transfer at grain boundaries in Al10.1016/j.scriptamat.2019.12.010 ↗
55. Effect of thermal deformation parameters on the microstructure, texture, and microhardness of 5754 aluminum alloy10.1007/s12613-019-1852-3 ↗
56. Investigation of work softening mechanisms and texture in a hot deformed 6061 aluminum alloy at high temperature10.1016/j.msea.2014.03.086 ↗
57. Elevated temperature microstructural stability in cast AlCuMnZr alloys through solute segregation10.1016/j.msea.2019.138279 ↗
58. Cu-rich nanoprecipitates modified using Al to simultaneously enhance the strength and ductility of ferritic stainless steel10.1016/j.jmst.2021.12.061 ↗
59. In-situ tailoring microstructure by directly synthesized TiC–TiB2 nanoparticles to achieve well-balanced strength and ductility in Al–Cu alloy10.1016/j.msea.2023.145350 ↗
60. Nanoscale precipitates as sustainable dislocation sources for enhanced ductility and high strength10.1073/pnas.1914615117 ↗
61. Strain hardening mediated by coherent nanoprecipitates in ultrahigh-strength steels10.1016/j.actamat.2021.116984 ↗
62. An analysis of the influence of the precipitate type on the mechanical behavior of Al-Cu alloys by means of micropillar compression tests10.1016/j.actamat.2020.05.040 ↗
63. Microstructure, heat treatment and mechanical properties of TiB2/Al–7Si–Cu–Mg alloy fabricated by selective laser melting10.1016/j.msea.2021.140951 ↗
64. Strengthening of an Al–Cu–Sn alloy by deformation-resistant precipitate plates10.1016/j.actamat.2008.03.028 ↗
65. Strength and strain hardening of a selective laser melted AlSi10Mg alloy10.1016/j.scriptamat.2017.07.025 ↗
66. Effect of direct aging on the microstructure and tensile properties of AlSi10Mg alloy manufactured by selective laser melting process10.1016/j.matchar.2021.111113 ↗
67. Simultaneous enhancement in strength and ductility of Fe50Mn30Co10Cr10 high-entropy alloy via nitrogen alloying10.1016/j.jmst.2020.04.072 ↗
68. Effect of Coarse β (Al3Mg2) phase on microstructure Evolution in 573 K annealed Al-10Mg alloy by uniaxial compression
69. Microstructure and mechanical properties of S30432 steel modified by trace TiC/TiB2 nano-particles10.1016/j.msea.2023.145049 ↗
70. Deformation behavior and microstructural evolution of as-cast 904L austenitic stainless steel during hot compression10.1016/j.msea.2012.12.043 ↗
71. Mechanisms of DRX nucleation with grain boundary bulging and subgrain rotation during the hot working of nickel-based superalloys with columnar grains10.1016/j.jallcom.2019.01.334 ↗
72. Microstructural evolution and strengthening mechanisms in a heat-treated additively manufactured Al–Cu–Mn–Zr alloy10.1016/j.msea.2022.142928 ↗