Abstract

In the selective laser melting (SLM) process, the transient nature of the molten pool and rapid cooling rate facilitates partial homogenization of components, resulting in attaining a finer scale concentration modulation and spatial heterostructure. However, the SLM-processed Ti6Al4V alloys have long suffered from the problem of both large detrimental columnar grains and poor work-hardening capacity. In this study, a high entropy alloy of FeCoNiCrMo particles was incorporated into the Ti6Al4V alloy and fabricated by the SLM technique. The resulting alloys exhibited a fine-scale modulated β + α` spatial heterostructure, delivering a notable tensile strength of 1366.4 MPa and a uniform elongation of approximately 8.7% with an excellent work-hardening capacity exceeding 300 MPa. This outstanding performance can be attributed to the progressive transformation-induced plasticity (TRIP) effect and hetero-deformation induced (HDI) strengthening within the ultra-refined α` martensite and metastable β phase regions. This work provided a compelling model of additive manufacture of heterogeneous structures while offering new insights and directions for the development of metallic materials with high strength-ductility characteristics.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Novel transformation pathway and heterogeneous precipitate microstructure in Ti-alloys10.1016/j.actamat.2020.06.048 ↗
2. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
3. Additive manufacturing of dense components in beta‑titanium alloys with crystallographic texture from a mixture of pure metallic element powders10.1016/j.matdes.2019.107771 ↗
4. Recent developments and opportunities in additive manufacturing of titanium-based matrix composites: a review10.1016/j.ijmachtools.2018.06.003 ↗
5. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
6. A systematic review of process uncertainty in Ti6Al4V-selective laser melting10.1016/j.cirpj.2021.12.005 ↗
7. Development of a high strength and high ductility near β-Ti alloy with twinning induced plasticity effect10.1016/j.scriptamat.2018.07.012 ↗
8. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
9. Deformation mechanisms in a metastable beta titanium twinning induced plasticity alloy with high yield strength and high strain hardening rate10.1016/j.actamat.2018.04.035 ↗
10. A new titanium alloy with a combination of high strength, high strain hardening and improved ductility10.1016/j.scriptamat.2014.09.005 ↗
11. Doubled strength and ductility via maraging effect and dynamic precipitate transformation in ultrastrong medium-entropy alloy10.1038/s41467-023-35863-z ↗
12. In situ design of advanced titanium alloy with concentration modulations by additive manufacturing10.1126/science.abj3770 ↗
13. Effect of scanning strategies on residual stress and mechanical properties of selective laser melted Ti6Al4V10.1016/j.msea.2017.11.103 ↗
14. Heterostructured materials10.1016/j.pmatsci.2022.101019 ↗
15. Laser additive manufacturing of titanium alloys with various Al contents10.1080/21663831.2023.2165418 ↗
16. Microstructure and mechanical properties of a novel β titanium metallic composite by selective laser melting10.1016/j.actamat.2014.01.018 ↗
17. Microstructural engineering of a dual-phase Ti-Al-V-Fe alloy via in situ alloying during laser powder bed fusion
18. Loss-free tensile ductility of dual-structure titanium composites via an interdiffusion and self-organization strategy
19. Additive manufacturing of fine-grained high-strength titanium alloy via multi-eutectoid elements alloying10.1016/j.compositesb.2022.110399 ↗
20. High-entropy alloys10.1038/s41578-019-0121-4 ↗
21. Selective laser melting of lattice structures: a statistical approach to manufacturability and mechanical behavior10.1016/j.rcim.2017.06.006 ↗
22. Selective laser melting of Ti6Al4V alloy: process parameters, defects and post-treatments10.1016/j.jmapro.2021.01.009 ↗
23. Homogenization timing effect on microstructure and precipitation strengthening of 17–4PH stainless steel fabricated by laser powder bed fusion
24. Crystal growth mechanism and mechanical properties of Ti-6Al-4 V alloy during selective laser melting10.1016/j.matchar.2022.112455 ↗
25. The martensitic transformation and mechanical properties of Ti6Al4V prepared via selective laser melting10.3390/ma12020321 ↗
26. Superior titanium from hybridised microstructures – a new strategy for future alloys10.1016/j.scriptamat.2019.07.031 ↗
27. Designing against phase and property heterogeneities in additively manufactured titanium alloys
28. Design of titanium alloys by additive manufacturing: a critical review
29. Trifunctional nanoprecipitates ductilize and toughen a strong laminated metastable titanium alloy
30. In-situ tailoring microstructures to promote strength-ductility synergy in laser powder bed fusion of NiCoCr medium-entropy alloy10.1007/978-3-031-04721-3 ↗
31. Back-stress-induced strengthening and strain hardening in dual-phase steel10.1016/j.mtla.2019.100376 ↗
32. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility10.1073/pnas.1517193112 ↗
33. Strong yet ductile nanolamellar high-entropy alloys by additive manufacturing10.1038/s41586-022-04914-8 ↗
34. Back stress strengthening and strain hardening in gradient structure10.1080/21663831.2016.1153004 ↗