Reducing stress corrosion cracking susceptibility of high-strength aluminum alloy and its fastener by a novel electromagnetic shocking treatment
Source abstract
Abstract
A novel electromagnetic shocking treatment (EST) is put forward to reduce the stress corrosion cracking (SCC) susceptibility of high-strength aluminum alloys and its fasteners by selectively modifying grain boundary (GB) microstructure. The effect of EST on the microstructure, mechanical properties and SCC susceptibility of T73-Al7075 alloy and its high-lock nuts has been investigated. Mechanical properties, electrochemical performance and constant strain SCC test have been carried out for T73-Al7075 alloy, microhardness test and SCC test under wet-dry cyclic condition have been carried out for its high-lock nuts, as well as microstructure characterizations via SEM, EBSD and TEM have been carried out for T73-Al7075 alloy. Comparing to the received sample, the strength of EST sample basically keep consistent while the elongation increases slightly, besides, the electrical conductivity and electrochemical corrosion performance improves. The SCC susceptibility of T73-Al7075 alloy and its high-lock nuts have been reduced after EST. Microstructure characterization shows that the grain morphology and matrix intragranular precipitate distribution of the EST sample keep almost the same as those of the received sample, which is consistent with the almost unchanged mechanical properties of alloy sample. However, EST induces the transformation of grain boundary precipitates (GBPs) and the formation of stripy/wavy GB as observed experimentally, which indicates that EST promotes nonlinear GB wetting or pre-melting and even grain bridging. The phase transformation and GB complexion transition induced by EST are main factors attributing to the obvious improvement of SCC resistance of T73-Al7075 alloy and its high-lock nuts. It can be deduced that anodic dissolution cracking will be relieved because of the dissolution and coarsening of GBPs. Hydrogen induced cracking and crack propagation can be relieved with the occurrence of grain bridging. They are both beneficial to improve SCC resistance of Al7075 alloys. This work provides a novel EST method to targetedly embellish GB microstructure, optimize GB complexion and connectivity, and then enhance the service performance of solid alloys and even finished parts.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electromagnetic Effects on Materials · Surface Treatment and Residual Stress · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (82)
Show source-provided references
1. Srinadh, Stress corrosion cracking behaviour of 7xxx aluminum alloys: a literature review10.1016/S1003-6326(16)64220-6 ↗
2. Role of grain size on the stress corrosion cracking of 7475 aluminum alloys10.1016/S0921-5093(96)10840-6 ↗
3. Role of temper conditions on the hydrogen embrittlement behavior of AA 7010
4. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
5. Mechanisms of hydrogen embrittlement in high-strength aluminum alloys containing coherent or incoherent dispersoids
6. Environmentally assisted cracking: overview of evidence for an adsorption-induced localised-slip process10.1016/0001-6160(88)90113-7 ↗
7. Hydrogen trapping and embrittlement in high-strength Al alloys10.1038/s41586-021-04343-z ↗
8. Revisiting stress-corrosion cracking and hydrogen embrittlement in 7xxx-Al alloys at the near-atomic-scale10.1038/s41467-022-31964-3 ↗
9. Environmental cracking performance of new generation thick plate 7000-T7x series alloys in humid air10.1016/j.corsci.2020.108701 ↗
10. Stress Corrosion Cracking Behavior of 2024 and 7075 High-Strength Aluminum Alloys in a Simulated Marine Atmosphere Contaminated with SO210.1007/s11665-019-04537-7 ↗
11. Effects of dry/wet ratio and pre-immersion on stress corrosion cracking of 7050-T7451 aluminum alloy under wet-dry cyclic conditions10.1016/j.cja.2018.01.008 ↗
12. Strain-rate effects on hydrogen embrittlement of 7075 aluminum10.1016/0036-9748(79)90177-7 ↗
13. Effect of minor Sc addition on microstructure and stress corrosion cracking behavior of medium strength Al-Zn-Mg alloy10.1016/j.jmst.2017.11.042 ↗
14. Two-stage double peaks ageing and its effect on stress corrosion cracking susceptibility of Al-Zn-Mg alloy10.1016/j.jmst.2017.05.008 ↗
15. Effects of quenching agents, two-step aging and microalloying on tensile properties and stress corrosion cracking of Al-Zn-Mg-Cu alloys10.1016/j.jmrt.2020.07.014 ↗
16. Synchronous improvement of mechanical properties and stress corrosion resistance by stress-aging coupled with natural aging pre-treatment in an Al-Zn-Mg alloy with high recrystallization fraction10.1016/j.jmst.2021.11.068 ↗
17. Correlations between intergranular stress corrosion cracking, grain-boundary microchemistry, and grain-boundary electrochemistry for Al-Zn-Mg-Cu alloys10.1016/j.corsci.2010.08.024 ↗
18. Some effects of alloy composition on stress corrosion cracking in Al-Zn-Mg-Cu alloys10.1016/j.corsci.2015.05.016 ↗
19. Enhanced mechanical properties and corrosion resistance of an Al-Zn-Mg aluminum alloy through variable-rate non-isothermal aging
20. The dependence of precipitate morphology on the grain boundary types in an aged Al–Cu binary alloy10.1007/s10853-020-05239-5 ↗
21. Effect of of Yb, Cr and Zr additions on recrystallization and corrosion resistance of Al–Zn–Mg–Cu alloys10.1016/j.msea.2008.07.028 ↗
22. Microstructure, mechanical properties and stress corrosion cracking of Al–Zn–Mg–Zr alloy sheet with trace amount of Sc10.1016/j.jallcom.2015.08.011 ↗
23. Microstructure and stress corrosion cracking resistance of Al-6.5Zn-2Cu-1.5Mg-0.05Ti alloy modified by Cr addition10.1016/j.matchar.2021.111621 ↗
24. Effects of severe cold rolling on tensile properties and stress corrosion cracking of 7050 aluminum alloy10.1016/j.matchemphys.2009.05.048 ↗
25. Correlation between stress corrosion cracking resistance and grain-boundary precipitates of a new generation high Zn-containing 7056 aluminum alloy by non-isothermal aging and re-aging heat treatment
26. Surface characteristics and stress corrosion behavior of AA 7075-T6 aluminum alloys after different shot peening processes10.1016/j.surfcoat.2022.128481 ↗
27. The effect of laser surface treatment on stress corrosion cracking behaviour of 7075 aluminium alloy10.1016/S0167-577X(03)00583-4 ↗
28. Effect of the deep cryogenic treatment on the stress corrosion cracking behaviour of AA 2017-T4 aluminium alloy10.1002/maco.201508586 ↗
29. Wear and corrosion performance of two different tempers (T6 and T73) of AA7075 aluminium alloy after nitrogen implantation10.1016/j.apsusc.2014.11.111 ↗
30. Crack growth behaviour of high strength aluminium alloy in 3.5%NaCl solution with corrosion inhibiting pigments10.1016/S0142-1123(01)00188-8 ↗
31. Microstructure of nanometer Al2O3 particles reinforced aluminum matrix composites processed by high pulsed electromagnetic field10.1016/j.matlet.2013.02.089 ↗
32. Electropulsing induced evolution of grain-boundary precipitates without loss of strength in the 7075 Al alloy10.1016/j.matchar.2015.05.007 ↗
33. Reversion of sub-boundaries into dense dislocations in aluminum by electric pulsing treatment10.1016/j.scriptamat.2019.03.043 ↗
34. Fatigue crack healing by a controlled high density electric current field10.1016/j.msea.2011.11.024 ↗
35. Self-healing of damage inside metals triggered by electropulsing stimuli10.1038/s41598-017-06635-9 ↗
36. Tailoring the residual stress and mechanical properties by electroshocking treatment in cold rolled M50 steel10.1016/j.msea.2020.139171 ↗
37. Effect of an electric field on the superplasticity of 7475 Al10.1016/0036-9748(89)90514-0 ↗
38. Effects of alternating magnetic field aged on microstructure and mechanical properties of AA2219 aluminum alloy10.1016/j.jallcom.2015.05.183 ↗
39. Simultaneously enhanced strength and ductility of Al-Mg-Si alloys during aging process induced by electro-pulsing treatment10.3390/ma12091383 ↗
40. intergranular corrosion performance regeneration below the precipitates solvus temperature in Al-Mg alloy10.1016/j.jmst.2020.01.071 ↗
41. Regulating solute partitioning utilized to decorate grain boundary for improving corrosion resistance in a model Al-Cu-Mg alloy
42. a pulsed electric current to reduce the susceptibility of high-strength steel to the stress corrosion cracking caused by hydrogen10.1016/j.ijhydene.2020.01.055 ↗
43. Structural and phase changes under electropulse treatment of fatigue-loaded titanium alloy VT1-010.1016/j.jmrt.2018.09.008 ↗
44. Removing hydrogen in solid metal using electric current pulse10.1016/j.jallcom.2020.156083 ↗
45. Investigation of the electroplastic effect using nanoindentation
46. Extraordinary effect of the δ phase on the electrically-assisted deformation responses of a Ni-based superalloy10.1016/j.matchar.2018.08.018 ↗
47. Magnetic induced re-dissolution and microstructure modifications on mechanical properties10.1016/j.jallcom.2021.160471 ↗
48. Progress in the investigations of grain boundary relaxation
49. Micro texture of titanium alloys excited nonlinearly by electromagnetic pulse10.1016/j.scriptamat.2021.113828 ↗
50. A novel electromagnetic shock treatment to selectively modify grain boundary and improve the corrosion resistance of aluminium alloy10.1016/j.matlet.2022.133703 ↗
51. On the theory of inhomogeneous electroelastic plates
52. Magnetoelasticity of highly deformable thin films: Theory and simulation10.1016/j.ijnonlinmec.2011.05.004 ↗
53. Defect reconfiguration in a Ti-Al alloy via electroplasticity10.1038/s41563-020-00817-z ↗
54. Role of thermo-mechanical gyrations on the α/β interface stability in a Ti6Al4V AM alloy10.1016/j.scriptamat.2021.114134 ↗
55. Mechanical properties, corrosion behavior and microstructures of a non-isothermal ageing treated Al-Zn-Mg-Cu alloy10.1016/j.msea.2017.01.086 ↗
56. Precipitation strengthening of aluminum alloys by room-temperature cyclic plasticity10.1126/science.aav7086 ↗
57. Pseudopartial grain boundary wetting: key to the thin intergranular layers10.4028/www.scientific.net/DDF.333.175 ↗
58. Grain boundary complexions and pseudopartial wetting10.1016/j.cossms.2016.05.006 ↗
59. Wetting of grain boundaries in Al by the solid Al3Mg2 phase10.1007/s10853-009-4014-6 ↗
60. Phase field modeling of formation mechanism of grain boundary allotriomorph in β→α phase transformation in Ti-6Al-4VAlloy
61. Theory of Ostwald ripening: competitive growth and its dependence on volume fraction10.1063/1.446427 ↗
62. The conflicts between strength and toughness10.1038/nmat3115 ↗
63. An evaluation of the contributions of skin, pinch and heating effects to the electroplastic effect in titatnium198010.1016/0025-5416(80)90216-5 ↗
64. Electromigration in metals10.1088/0034-4885/52/3/002 ↗
65. A survey of the main aspects of magnetic forces and mechanical behaviour of ferromagnetic materials under magnetisation
66. A theoretical analysis of the breakdown of electrostrictive oxide film on metal10.1016/j.jmps.2010.11.002 ↗
67. The effect of grain boundary serration on creep resistance in a wrough nickel-based superalloy10.1016/j.msea.2009.03.071 ↗
68. Deformation behavior and formability of solid solution state Al-Li alloy in electromagnetic forming10.1016/j.msea.2022.143858 ↗
69. Ultrafine grained structures resulting from SPD-induced phase transformation in Al-Zn alloys10.1002/adem.201500151 ↗
70. Study on hot compressive deformation behaviors and corresponding industrial extrusion of as-homogenized Al-7.82Zn-1.96Mg-2.35Cu-0.11Zr alloy10.1007/s10853-018-2388-z ↗
71. Deformation behavior and microstructure evolution of Al-5.06Mg-1.67Li-0.51Zn alloy under hot compression10.1016/j.jmrt.2021.10.084 ↗
72. Microstructure and mechanical properties of Al-Mg-Si alloy during solution heat treatment and forging integrated forming process10.1016/j.matchar.2022.111762 ↗
73. Grain boundary films in Al–Zn alloys after high pressure torsion10.1016/j.scriptamat.2013.09.019 ↗
74. Achieving microstructures prone to superplastic deformation in an Al-Zn-Mg-Cu alloy by equal channel angular pressing10.1016/j.jallcom.2012.08.084 ↗
75. The effect of extrusion temperature on the development of deformation microstructures in 5052 aluminium alloy processed by equal channel angular extrusion10.1016/S1359-6454(02)00607-9 ↗
76. On the relationship between grain boundary connectivity, coincident site lattice boundaries, and intergranular stress corrosion cracking10.1016/j.corsci.2004.01.019 ↗
77. The effect of grain boundary sliding and strain rate sensitivity on the ductility of ultrafine-grained materials
78. Overview no.49: on the mechanisms for the electroplastic effect in metals10.1016/0001-6160(86)90001-5 ↗
79. Magnetoplastic effect in metals in strong pulsed magnetic fields10.1134/S1063783415100297 ↗
80. The effect of grain boundary character distribution on the mechanical properties at different strain rates of a 316L stainless steel10.1007/s10853-017-1695-0 ↗
81. On the origins of fatigue strength in crystalline metallic materials10.1126/science.abn0392 ↗
82. Improvement of fatigue crack growth resistance by serrated grain boundary at high temperature10.1115/1.2903389 ↗