High temperature oxidation behavior and interface diffusion of Cr3C2-NiCrCoMo/nano-CeO2 composite coatings
Source abstract
Abstract
The high-temperature oxidation resistance of chromium carbide cermet coating was improved by developing a novel Cr 3C 2-NiCrCoMo/nano-CeO 2 (NCE) composite coating based on the collaborative modification of the multielement alloy adhesive phase. The present study aimed to investigate the influence of nano-CeO 2 on the high-temperature oxidation resistance, interfacial element diffusion and oxidation mechanism of the coating deposited by the high-velocity oxygen fuel spraying technology (HVOF). The results showed that the novel NCE coating with the addition of 4 wt% nano-CeO 2 resulted in lower oxidation rates of 0.10, 0.23 and 0.39 mg/cm 2 at 700–900 °C and superior oxidation resistance compared with the original Cr 3C 2 -NiCrCoMo (NCC) coating because of the improvement of the thickness and denseness of the oxide film. The addition of nano-CeO 2 promoted the reaction between oxides and the content of spinel phases generated in the NCE coating oxide film. The oxide film of NCE coating with high content of spinel phases strongly inhibited on the ion diffusion, thus reducing the decarburization of the Cr 3C 2 particles at the coating-oxide film interface. The present study will contribute to improving the service life of chromium carbide cermet coatings in high-temperature oxidation environments and extending the application of coating.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Engineering HVOF-sprayed Cr3C2-NiCr coatings: the effect of particle morphology and spraying parameters on the microstructure, properties, and high temperature wear performance10.1007/s11666-012-9833-3 ↗
2. Pulsed laser remelting supersonic plasma sprayed Cr3C2-NiCr coatings for regulating microstructure, hardness and corrosion properties10.1016/j.surfcoat.2021.127258 ↗
3. Microhardness variation in relation to carbide development in heat treated Cr3C2-NiCr thermal spray coatings10.1016/S1359-6454(03)00254-4 ↗
4. Effect of carbide dissolution on chlorine induced high temperature corrosion of HVOF and HVAF sprayed Cr3C2-NiCrMoNb coatings10.1007/s11666-017-0645-3 ↗
5. Comparison on multi-angle erosion behavior and mechanism of Cr3C2-NiCr coatings sprayed by SPS and HVOF10.1016/j.surfcoat.2020.126366 ↗
6. Cavitation erosion characteristics at various flow velocities in NaCl medium of carbide-based cermet coatings prepared by HVOF spraying10.1016/j.ceramint.2020.09.022 ↗
7. Hot corrosion behavior of HVOF-sprayed CoNiCrAlYSi coatings in a sulphate environment10.1016/j.vacuum.2015.09.015 ↗
8. High-temperature corrosion behaviour of air plasma sprayed Cr3C2-25NiCr and NiCrMoNb powder coating on alloy 80 A at 900 °C10.1016/j.surfcoat.2018.01.011 ↗
9. High temperature wear performance of HVOF-sprayed Cr3C2-WC-NiCoCrMo and Cr3C2-NiCr hardmetal coatings10.1016/j.apsusc.2017.04.132 ↗
10. Ultrasonic assisted incremental sheet forming: constitutive modeling and deformation analysis10.1016/j.jmatprotec.2021.117365 ↗
11. HVOF sprayed Ni3Ti and Ni3Ti+(Cr3C2 +20NiCr) coatings: microstructure, microhardness and oxidation behaviour10.1016/j.jallcom.2017.11.131 ↗
12. The high-temperature wear and oxidation behavior of CrC-based HVOF coatings10.1007/s11666-017-0637-3 ↗
13. Oxidation behavior of arc-sprayed FeMnCrAl/Cr3C2–Ni9Al coatings deposited on low-carbon steel substrates10.1016/j.surfcoat.2010.12.008 ↗
14. Hot corrosion behavior of HVOF-sprayed Cr3C2-WC-NiCoCrMo coating10.1016/j.ceramint.2017.04.109 ↗
15. High temperature oxidation and tribological behavior of Cr3C2-25CoNiCrAlY and Cr3C2-25NiCr coatings prepared by AC-HVAF
16. High temperature erosion of Cr3C2-NiCr thermal spray coatings - the role of phase microstructure10.1016/j.surfcoat.2008.10.008 ↗
17. Tribological properties of rare earth oxide added Cr3C2-NiCr coatings10.1016/j.apsusc.2006.09.040 ↗
18. Sliding wear behavior of HVOF-sprayed Cr3C2-NiCr/CeO2 composite coatings at elevated temperature up to 800 °C10.1007/s11249-009-9540-5 ↗
19. Microstructure and wear resistance of Co-based/Cr3C2 coatings with CeO210.1080/02670844.2017.1363484 ↗
20. Corrosion behavior of bare, Cr3C2-25%(NiCr), and Cr3C2-25%(NiCr)+0.4%CeO2-coated Superni 600 under molten salt at 900 °C10.1007/s11665-014-1177-3 ↗
21. Hot corrosion behaviour of detonation-gun sprayed Cr3C2–NiCr coating on Inconel-718 in molten salt environment at 900 °C10.1007/s12666-014-0383-x ↗
22. Effect of scanning speeds on microstructure and wear behavior of laser-processed NiCr-Cr3C2-MoS2-CeO2 on 38CrMoAl steel10.1016/j.optlastec.2015.08.008 ↗
23. Research on the high temperature oxidation mechanism of Cr3C2-NiCrCoMo coating for surface remanufacturing10.1016/j.jmrt.2020.12.049 ↗
24. Xiao · 1987
25. High temperature creep behavior of Cr3C2 ceramic composite10.1016/0921-5093(96)10167-2 ↗
26. High-temperature oxidation of HVOF thermally sprayed NiCr–Cr3C2 coatings: microstructure and kinetics10.1007/s10853-015-9238-z ↗
27. The effect of oxygen flow rate in HVOF spraying on oxidation behavior of Cr3C2 (7 mass% NiCr) coatings10.2320/matertrans.42.707 ↗
28. Zhao · 2008
29. Thermomagnetic study of the system CoO-NiO10.1051/jphysrad:01960002106055100 ↗
30. Fromme · 2001
31. Influence of heat treatment on the abrasive wear resistance of a Cr3C2-NiCr coating deposited by an ethene-fuelled HVOF spray process10.1016/j.surfcoat.2016.02.066 ↗
32. Microstructure dependent erosion in Cr3C2–20(NiCr) coating deposited by a detonation gun10.1016/j.surfcoat.2007.03.017 ↗
33. B. Zhang, X. Cheng, et al., Preparation and performance study of Co-Ce system doped NiCr-based infrared radiation coatings, National Thermal Spraying Annual Conference. China Surface Engineering Association Thermal Spraying Professional Committee, (2014).
34. The effect of bond composition on the strength of partially-bonded vitrified ceramic abrasives10.1007/BF00270963 ↗
35. Role of the oxygen partial pressure on the properties of undoped tin oxide films deposited at low temperature
36. High temperature erosion-oxidation of Cr3C2-NiCr thermal spray coatings under simulated turbine conditions10.1016/j.corsci.2013.01.030 ↗
37. Ultrasonic assisted incremental sheet forming: constitutive modeling and deformation analysis10.1016/j.jmatprotec.2021.117365 ↗