Fabrication of (TixZr1−x)B2-(ZrxTi1−x)N composites by reactive spark plasma sintering of ZrB2-TiN

Mohammad Reza Derakhshandeh, Ali Fazili, Raouf Behjat Golenji, Fardin Alipour, Mohammad Javad Eshraghi, Leila Nikzad

Publisher page

Abstract

Abstract In this study, microstructural and mechanical properties of (ZrxTi1−x)N-(TixZr1−x)B2 composite fabricated by reactive spark plasma sintering (SPS) of ZrB2 and TiN was investigated. ZrB2 and TiN starting materials with equimolar ratio were sintered at 2000 °C for 8 min under a pressure of 30 MPa. An expansion (about 4%) was observed during the sintering process of the composite in the temperature range between 1290 °C and 1625 °C, which was attributed to the reaction of the starting materials. XRD pattern of the fabricated composite revealed the formation of TiB2 and ZrN phases after the sintering process. It was found that (Ti0.91Zr0.09)B2 and (Zr0.92Ti0.08)N phases are formed after sintering. High values of Vickers microhardness (28 ± 0.2 GPa), flexural strength (706 ± 51 MPa) and fracture toughness (8.49 ± 0.92 MPa m1/2) were achieved for this composite. Fracture of the (ZrxTi1−x)N and (TixZr1−x)B2 phases and crack path deflection mechanisms was founded as dominant toughening mechanisms in this composite.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. ZrB2-based “Brick-and-Mortar” composites achieving the synergy of superior damage tolerance and ablation resistance10.1021/acsami.0c08206 ↗
2. High thermal-conductivity rGO/ZrB2-SiC ceramics consolidated from ZrB2-SiC particles decorated GO hybrid foam with enhanced thermal shock resistance10.1016/j.jeurceramsoc.2020.03.029 ↗
3. Mechanical and tribological properties of TiB2-SiC and TiB2-SiC-GNPs ceramic composites10.1016/j.jeurceramsoc.2020.04.045 ↗
4. ZrB2-SiC-WC coating with SiC diffusion bond coat on graphite by spark plasma sintering process10.1016/j.ceramint.2017.07.123 ↗
5. Influence of chromium diboride on the oxidation resistance of ZrB2-MoSi2 and ZrB2-SiC ceramics10.1016/j.jeurceramsoc.2020.12.036 ↗
6. Improvement of sinterability and mechanical properties of ZrB2 ceramics by the modified borothermal reduction methods10.1016/j.jeurceramsoc.2020.03.051 ↗
7. Effect of tantalum solid solution additions on the mechanical behavior of ZrB2
8. Oxidation resistance and thermal stability of the SiC‐ZrB2 composite ceramic fibers10.1111/jace.17554 ↗
9. Oxidation behaviour of plasma-sprayed ZrB2-SiC coatings10.1016/j.ceramint.2018.10.157 ↗
10. Improving oxidation resistance of ZrB2-based ceramics by LaF3 doping via oxidation-induced self-healing mechanism10.1016/j.ceramint.2020.12.084 ↗
11. Ultra-high temperature oxidation resistance of ZrB2-20SiC coating with TaSi2 addition on siliconized graphite10.1016/j.ceramint.2019.05.030 ↗
12. Oxidation behaviours of ZrB2-SiC-MoSi2 composites at 1800 °C in air with different pressures10.1016/j.corsci.2019.05.027 ↗
13. Reactive hot pressing route for dense ZrB2-SiC and ZrB2-SiC-CNT ultra-high temperature ceramics10.1016/j.jeurceramsoc.2020.07.039 ↗
14. Fabrication of Al2O3/(ZrB2 + TiB2) composite using MACS and microwaves10.1007/s11661-014-2246-9 ↗
15. Mechanical and tribological properties of TiB2-SiC and TiB2-SiC-GNPs ceramic composites10.1016/j.jeurceramsoc.2020.04.045 ↗
16. In situ reaction and solid solution induced hardening in (Ti, Zr) B2–(Zr, Ti) C composites10.1111/jace.17355 ↗
17. Design, fabrication and properties of TiB2/TiN/WC gradient ceramic tool materials10.1016/j.ceramint.2019.11.131 ↗
18. Microstructural evolution and mechanical properties of TiB2-TiC-SiC ceramics joint brazed using Ti-Ni composite foils10.1016/j.jeurceramsoc.2020.03.053 ↗
19. High-temperature reaction consolidation of TaC-TiB2 ceramic composites by spark-plasma sintering10.1016/j.jeurceramsoc.2014.08.007 ↗
20. High-temperature reactive spark plasma consolidation of TiB2–NbC ceramic composites10.1016/j.ceramint.2015.05.022 ↗
21. AlN-induced reinforcement of nano-amorphous B–C–N compound for TiB2–B4C ceramic composite10.1016/j.jallcom.2020.154074 ↗
22. Densification behavior and mechanical properties of spark plasma reaction sintered ZrB2–ZrC-B4C ceramics from B4C-Zr system10.1016/j.ceramint.2019.03.112 ↗
23. B deficiency in TiB2 and B solid solution in TiN in TiN-TiB2 composites prepared by spark plasma sintering10.1016/j.jeurceramsoc.2012.06.024 ↗
24. Densification behavior and microstructure development in TiB2 ceramics doped with h-BN10.1016/j.ceramint.2020.04.223 ↗
25. Characterization of TiB2-AlN composites for application as cutting tool10.1016/j.jmrt.2018.07.010 ↗
26. Mechanical properties and tribology of Si3N4–TiB2 ceramic composites produced by hot pressing and hot isostatic pressing10.1016/S0955-2219(00)00294-6 ↗
27. Spark plasma sintering of ceramic matrix composite of ZrB2 and TiB2: microstructure, densification, and mechanical properties—a review
28. Erosion resistance of TiB2–ZrB2 composites10.1016/j.wear.2009.01.037 ↗
29. Tribological properties of TiB2 and TiB2–MoSi2 ceramic composites10.1016/j.jeurceramsoc.2005.01.054 ↗
30. High toughness TiB2–Al2O3 composite ceramics produced by reactive hot pressing with fusible components10.1179/1743676114Y.0000000202 ↗
31. Reactive hot pressing and properties of Zr1-xTixB2-ZrC composites10.1111/jace.13350 ↗
32. Role of carbon nanotubes on mechanical properties of SiC-B4C-Ni hybrid composites fabricated by reactive spark plasma sintering10.1016/j.ceramint.2021.04.186 ↗
33. Preparation, microstructures, mechanical properties and oxidation resistance of SiBCN/ZrB2–ZrN ceramics by reactive hot pressing10.1016/j.jeurceramsoc.2015.08.010 ↗
34. Development and characterization of metal-diboride-based composites toughened with ultra-fine SiC particulates10.1016/j.solidstatesciences.2005.02.007 ↗
35. Reactive hot pressing of super hard (Ti,Ta)(B,C)–(Ta,Ti)C composites10.1016/j.msea.2020.140292 ↗
36. Synthesis, microstructure and mechanical properties of (Zr,Ti)B2-(Zr,Ti)N composites prepared by spark plasma sintering10.1016/j.jallcom.2010.01.006 ↗
37. Evolution of c-ZrN nanopowders in low-carbon MgO–C refractories and their properties10.1016/j.jeurceramsoc.2020.07.062 ↗
38. Djerdj · 2019
39. International Standard, ISO 28079, Hardmetals – Palmqvist Toughness Test, 2009.
40. Super hard carbon microtubes derived from natural cotton for development of high performance titanium composites10.1016/j.jallcom.2018.10.121 ↗
41. Effects of 211 and 413 ordering on the corrosion behavior of V-Al-C MAX phases prepared by spark plasma sintering10.1016/j.jeurceramsoc.2021.03.001 ↗
42. Preparation of in-situ formed TiN0.3-Ti5Si3-TiN composites through reactive spark plasma sintering of Ti and Si3N410.1016/j.ceramint.2018.12.136 ↗
43. Improved electrochemical and mechanical performance of WC-Co cemented carbide by replacing a part of Co with Al2O310.1016/j.jallcom.2020.153857 ↗
44. Comparison of spark plasma and microwave sintering of mullite based composite: mullite/Ta2O5 reaction10.1016/j.ceramint.2018.04.142 ↗
45. Effect of Co addition on microstructural and mechanical properties of WC-B4C-SiC composites10.1016/j.ceramint.2021.02.149 ↗
46. D. Lide, CRC Handbook of Chemistry and Physics: A Ready Reference Book, 2002.
47. Solid solution formation during spark plasma sintering of ZrB2–TiC–graphite composites10.1016/j.ceramint.2019.09.287 ↗
48. Vickers indentation fracture toughness of Y-TZP dental ceramics10.1016/j.ijrmhm.2016.12.016 ↗
49. Co-reinforcing of mullite-TiN-CNT composites with ZrB2 and TiB2 compounds10.1016/j.ceramint.2019.07.072 ↗
50. Effects of ZrB2 reinforcement on microstructure and mechanical properties of a spark plasma sintered mullite-CNT composite10.1016/j.ceramint.2019.05.113 ↗
51. Preparation of mullite-TiB2-CNTs hybrid composite through spark plasma sintering10.1016/j.ceramint.2019.05.154 ↗