Excellent magnetic and mechanical properties of the Sm2Co17-based magnets fabricated via microwave processing
Source abstract
Abstract
Abstract The development of high performance Sm2Co17-based permanent magnets (SCPMs) by employing efficient fabrication methods can be beneficial for many applications. In this study, we prove that Sm(CobalFe0.25Cu0.06Zr0.02)7.5 PMs with an improved energy product (BH)max (27.1–30.0 MGOe) and bending strength (168.2–177.5 MPa) can be achieved by using microwave (MW) ageing. During short-time MW-ageing at 840 °C for 1 h, phase separation was performed in the hexagonal Sm2Co17 (2:17H) supersaturated solid solution characterized with small wavelength of composition modulations (λ = 1–2 nm) and high density of pure-edge dislocations. This contributes to large gradient energy ΔGγ and high separation rate, thus results in the formation of 20-nm uniform nanoparticles. The nanoparticles grow into a homogeneous 50-nm cellular structure composed of rhombohedral Sm2Co17 (2:17R) cells and hexagonal SmCo5 (1:5H) cell boundaries after being MW-aged for 3 h, then the non-uniform grain growth to 80 nm takes place by further increasing the time to 5 h. Moreover, prolonging the ageing time from 3 to 5 h can increase the Cu enrichment in the 1:5H cell boundary phase and enhance the coercivity Hci from 17.4 to 23.1 kOe. As compared with conventional ageing, the MW ageing considerably reduces the ageing time and the MW-aged PMs exhibit finer and more homogeneous cellular structures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties of Alloys · Magnetic properties of thin films · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
2. Initial irreversible losses and enhanced high-temperature performance of rare-earth permanent magnets10.1002/adfm.201900690 ↗
3. Effect of pre-aging treatment on the microstructure and magnetic properties of Sm(Co,Fe,Cu,Zr)7.8 sintered magnets10.2320/matertrans.MBW201325 ↗
4. The microstructure of sintered Sm(Co0.72Fe0.20Cu0.055Zr0.025)7.5 permanent magnet studied by atom probe10.1016/j.actamat.2003.10.015 ↗
5. Microstructure and magnetic properties of Sm(CoFexCu0.128Zr0.02)7.0 magnets with Fe substitution10.1016/S0304-8853(00)00508-4 ↗
6. High-temperature magnetic properties and microstructural analysis of Sm(Co,Fe,Cu,Zr)z permanent magnets10.1016/S0304-8853(99)00322-4 ↗
7. Microstructure and its correlation to magnetic properties in 2:17 type (Sm,Gd)-Co-Fe-Cu-Zr alloys10.1023/B:JMSC.0000026946.89286.68 ↗
8. Dependence of macromagnetic properties on the microstructure in high-performance Sm2Co17-type permanent magnets10.1016/j.jmmm.2020.166942 ↗
9. Microstructures of precipitation-hardened SmCo permanent magnets10.1063/1.330867 ↗
10. Defects-aggregated cell boundaries induced domain wall curvature change in Fe-rich Sm–Co–Fe–Cu–Zr permanent magnets10.1007/s10853-020-04889-9 ↗
11. Correlation of microstructure and magnetic properties in Sm(CobalFe0.1Cu0.1Zr0.033)6.93 magnets solution-treated at different temperatures10.1007/s12598-018-1182-z ↗
12. Microstructural changes during the slow-cooling annealing of nanocrystalline SmCo 2:17 type magnets10.1016/j.jallcom.2012.08.131 ↗
13. Highly coercive rapidly solidified Sm-Co alloys10.1063/1.2173238 ↗
14. Material and magnetic properties of Sm2(Co, Fe, Cu, Zr)17 permanent magnets processed by Spark plasma sintering10.1016/j.jallcom.2018.08.186 ↗
15. Preparation of nanoscale Sm2Co17 flakes by ball milling in magnetic field10.1016/S1006-706X(14)60080-7 ↗
16. Fast development of high coercivity in melt-spun Sm(Co, Fe, Cu, Zr)z magnets10.1063/1.1450253 ↗
17. Structural, mechanical and thermal characteristics of Al-Cu-Li particle reinforced Al-matrix composites synthesized by microwave sintering and hot extrusion10.1016/j.compositesb.2019.01.063 ↗
18. Microwave processing and characterization of nickel powder based metal matrix composite castings
19. Characteristics of 14Cr-ODS ferritic alloy fabricated by mechanically alloying and microwave sintering10.1016/j.jnucmat.2015.01.030 ↗
20. Effect of microwave sintering over vacuum and conventional sintering of Cu based nanocomposites10.1016/j.jallcom.2013.11.222 ↗
21. A novel approach for fabrication of functionally graded W/Cu composites via microwave processing10.1016/j.jallcom.2018.01.372 ↗
22. X-band microwave absorption in Nd3+-substituted Mg–Cd spinel ferrites synthesized under microwave sintering10.1109/TMAG.2020.3014057 ↗
23. Magnetoelectric and magnetodielectric coupling in partially Ni-doped CoFe2O4 and 0.15(Ba0.7Ca0.3TiO3)–0.85(BaZr0.2Ti0.8O3) composites prepared via clean microwave sintering10.1016/j.jallcom.2020.156599 ↗
24. Microchemistry and magnetization reversal mechanism in melt-spun 2:17-type Sm-Co magnets10.1063/1.1611641 ↗
25. Enhanced the dielectric relaxation characteristics of BaTiO3 ceramic doped by BiFeO3 and synthesized by the microwave sintering method10.1016/j.matchemphys.2020.123034 ↗
26. High performance tungsten synthesized by microwave sintering method10.1016/j.ijrmhm.2012.02.016 ↗
27. The evolution of phase constitution and microstructure in iron-rich 2:17-type Sm-Co magnets with high magnetic performance
28. Investigation on structure-magnetic property correlation in melt-spun Sm(Co0.56Fe0.31Cu0.04Zr0.05B0.04)z ribbons
29. Phase evolution and its effects on the magnetic performance of nanocrystalline SmCo7 alloy10.1016/j.actamat.2010.11.047 ↗
30. Porter · 2014
31. Callister · 2001
32. Role of nanoscale interfacial defects on magnetic properties of the 2:17-type Sm–Co permanent magnets10.1016/j.jallcom.2019.152620 ↗
33. Mechanism of phase transformation in 2:17 type SmCo magnets investigated by phase stabilization10.1016/j.scriptamat.2015.10.041 ↗
34. Fracture toughness studies in sintered SmCo5 magnets10.1016/j.jmmm.2014.12.016 ↗