Microstructure and properties of a novel ultra-high strength, high elasticity and high plasticity Cu–20Ni–20Mn-0.3Nb-0.3Cr-0.1Zr alloy
Source abstract
Abstract
Abstract The elongation of high-strength copper alloy with tensile strength over 1300 MPa is generally less than 3%. In this paper, a novel Cu–20Ni–20Mn-0.3Nb-0.3Cr-0.1Zr (wt.%) alloy with high strength, high elasticity and high plasticity was prepared. Its tensile strength, elastic modulus and elongation is 1445 MPa, 147 GPa and 6.8%, respectively. On the basis of Cu–20Ni–20Mn alloy, microalloying Nb, Cr, Zr elements were added to restrain discontinuous precipitation and improve the properties of the alloys. By matching reasonable heat treatment process, a fine and highly uniform grain structure was obtained, which is the main reason for the increase of elongation. TEM and 3DAP results suggested that a large number of nanoscale NiMn precipitates are the main source of high strength in the alloy. The designed alloy has excellent comprehensive properties, which can be used for the preparation of precision sensing parts, elastic components.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. The effect of Co addition on the modulated structure coarsening and discontinuous precipitation growth kinetics of Cu–15Ni–8Sn alloy10.1016/j.jallcom.2020.155275 ↗
2. Microstructural characterization of cold-drawn Cu–Ni–Si alloy having high strength and high conductivity10.1016/j.jallcom.2020.155059 ↗
3. Effect of cold rolling and aging treatment on the microstructure and properties of Cu–3Ti–2Mg alloy10.1016/j.jallcom.2019.152915 ↗
4. Thermodynamics and kinetics of discontinuous precipitation in Cu–9Ni–xSn alloy10.1016/j.jallcom.2020.154314 ↗
5. The effect of cold rolling on age hardening of Cu-3Ti-3Ni-0.5Si alloy10.1016/j.jallcom.2019.05.091 ↗
6. Co effects on Cu-Ni-Si alloys microstructure and physical properties10.1016/j.jallcom.2019.05.135 ↗
7. Influence of microstructure on the Young’s modulus in a Cu-2Be (wt%) alloy10.1016/j.jallcom.2017.09.121 ↗
8. Precipitation behavior, microstructure and properties of aged Cu-1.7 wt% Be alloy10.1016/j.jallcom.2018.09.296 ↗
9. Precipitation behavior and properties of aged Cu-0.23Be-0.84Co alloy10.1016/j.jallcom.2015.10.290 ↗
10. Microstructure, mechanical properties and aging behaviour of nanocrystalline copper–beryllium alloy10.1016/j.msea.2018.12.011 ↗
11. Re-aging behavior of Cu–15Ni–8Sn alloy pretreated by dynamic strain aging10.1016/j.msea.2019.02.073 ↗
12. Effect of thermo-mechanical treatments on corrosion behavior of Cu-15Ni-8Sn alloy in 3.5 wt% NaCl solution10.1016/j.matchemphys.2017.06.041 ↗
13. Microstructural evolution, phase transition, and physics properties of a high strength Cu–Ni–Si–Al alloy10.1016/j.matchar.2018.11.018 ↗
14. Dynamics of phase transformation of Cu-Ni-Si alloy with super-high strength and high conductivity during aging10.1016/S1003-6326(09)60249-1 ↗
15. Phase transformation behaviors and properties of a high strength Cu-Ni-Si alloy10.1016/j.msea.2017.05.001 ↗
16. Effects of pre-deformation on precipitation behaviors and properties in Cu-Ni-Si-Cr alloy10.1016/j.msea.2018.11.045 ↗
17. Precipitation behavior of Cu-3.0Ni-0.72Si alloy10.1016/j.actamat.2018.12.047 ↗
18. Microstructure and properties of Cu–3Ti–1Ni alloy with aging process10.1016/S1003-6326(16)64450-3 ↗
19. Effect of prior cold work on age hardening of Cu–4Ti–1Cr alloy10.1016/j.msea.2005.05.072 ↗
20. Fabrication of high-strength and high-conductivity Cu-Ti alloy wireby aging in a hydrogen atmosphere10.1016/j.jallcom.2013.03.216 ↗
21. Age hardening studies in a Cu–4.5Ti–0.5Co alloy10.1016/S0921-5093(00)01834-7 ↗
22. Effects of multiple trace alloying elements on the microstructure and properties of Cu-4 wt% Ti alloys10.1016/j.msea.2017.09.072 ↗
23. Influence of Silver nanoparticles addition on the phase transformation, mechanical properties and corrosion behaviour of Cu–Al–Ni shape memory alloys10.1016/j.jallcom.2014.05.173 ↗
24. Phase transformation behavior of Cu–10Ni–3Al–0.8Si alloy10.1016/j.matchemphys.2016.02.033 ↗
25. Study of Cu–18Ni–20Zn Nickel Silver and other Cu-based alloys in artificial sweat and physiological solution10.1016/j.electacta.2007.04.105 ↗
26. Study by DSC and HRTEM of the aging strengthening of Cu–Ni–Zn–Al alloys10.1016/j.matdes.2015.12.030 ↗
27. Impression creep behavior of a Cu–6Ni–2Mn–2Sn–2Al alloy10.1016/j.msea.2011.12.065 ↗
28. Effects of trace zirconium on the initiation and propagation behavior of fatigue cracks in Cu–6Ni–2Mn–2Sn–2Al alloy10.1016/j.matlet.2008.01.057 ↗
29. Combustion behaviour and mechanism of a Cu-Ni-Mn alloy in an oxygen enriched atmosphere10.1016/j.corsci.2019.108253 ↗
30. Thermal treatments and transformation behavior of Cu–Al–Be shape memory alloys10.1016/j.jallcom.2012.02.006 ↗
31. Diffusion behavior and atomic mobilities for fcc Cu–Cr–Ni alloys10.1016/j.jallcom.2015.06.226 ↗
32. Temperature-minimum line in the Cu-Ni-Mn phase diagram10.3103/S0967091210030071 ↗
33. MECHANICAL PROPERTIES OF Cu-6Ni-2Mn-2Sn-xAl ALLOYS10.1016/S1359-6462(99)00317-6 ↗
34. Grain boundary reaction in a Cu-Ni-Mn alloy10.2320/jinstmet1952.46.3_301 ↗
35. Aging characteristics and precipitate analysis of Cu–Ni–Mn–P alloy10.1016/j.msea.2006.12.074 ↗
36. Thermodynamic description of the Cu–Mn–Ni system at the Cu–Ni side10.1016/j.calphad.2003.08.003 ↗
37. Etude du stade initial de la transformation structurale de l’alliage Cu-Ni-Mn 60, 20, 2010.1016/0001-6160(78)90121-9 ↗
38. Experimental investigation and thermodynamic modeling of the Cu–Mn–Ni system10.1016/j.calphad.2009.07.003 ↗
39. Microstructure evolution and properties of Cu–20Ni–20Mn alloy during aging process10.1016/S1003-6326(15)63960-7 ↗
40. Dislocation substructure-controlled softening of Cu-20Ni-20Mn alloy10.1016/j.matchar.2018.11.013 ↗
41. Effects of Nb addition on the microstructures and mechanical properties of a precipitation hardening Cu-9Ni-6Sn alloy10.1016/j.msea.2018.01.022 ↗
42. Effect of V addition on microstructures and mechanical properties of Cu-15Ni-8Sn alloy10.1016/j.msea.2019.01.084 ↗
43. Study of Cu–18Ni–20Zn Nickel Silver and other Cu-based alloys in artificial sweat and physiological solution10.1016/j.electacta.2007.04.105 ↗
44. Effects of silicon and thermo-mechanical process on microstructure and properties of Cu–10Ni–3Al–0.8Si alloy10.1016/j.matdes.2014.04.053 ↗
45. The precipitation behavior and strengthening of a Cu–2.0wt% Be alloy10.1016/j.msea.2012.08.007 ↗
46. Contribution of Zr to strength and grain refinement in Cu-Cr-Zr alloy10.1016/j.msea.2019.04.053 ↗
47. Work softening behavior of Cu-Cr-Ti-Si alloy during cold deformation10.1016/j.jmrt.2019.01.012 ↗
48. Solidification microstructure of Cu-Cr and Cu-Cr-In alloys10.1088/2053-1591/ab8259 ↗
49. Grain refinement during high temperature tensile testing of prior cold worked and peak aged Cu–Ti alloys: evidence of superplasticity10.1016/j.msea.2008.08.029 ↗
50. Effects of aging on a spray-formed Cu-Al-Ni-Mn-Nb high temperature shape memory alloy10.1016/j.msea.2019.03.024 ↗
51. Microstructure and properties of a Cu–Ni–Si–Co–Cr alloy with high strength and high conductivity10.1016/j.msea.2019.05.003 ↗
52. Phase transformations behavior in a Cu–8.0Ni–1.8Si alloy10.1016/j.jallcom.2010.12.115 ↗
53. Ageing behavior in the Cu–10wt.%Al and Cu–10wt.%Al–4wt.%Ag alloys10.1016/j.jallcom.2008.05.072 ↗
54. Aging behavior and phase transformation of the Cu-0.2 wt%Zr-0.15 wt%Y alloy10.1016/j.vacuum.2018.10.054 ↗
55. Effect of aging treatment on damping capacity in Cu–Al–Mn shape memory alloy10.1016/j.jallcom.2019.153213 ↗
56. The effect of the processing parameters on the martensitic transformation of Cu-Al-Mn shape memory alloy10.1016/j.jallcom.2018.06.250 ↗
57. Effect of aluminum on microstructure and property of Cu–Ni–Si alloys10.1016/j.msea.2013.02.024 ↗
58. Effects of non-isothermal aging on mechanical properties, corrosion behavior and microstructures of Al-Cu-Mg-Si alloy10.1016/j.jallcom.2019.152960 ↗
59. Mechanical behaviour and damping properties of Ni modified Cu–Zn–Al shape memory alloys
60. A novel Cu–Ni–Zn–Al alloy with high strength through precipitation hardening10.1016/j.msea.2010.04.089 ↗
61. Cohesion in alloys-fundamentals of a semi-empirical model10.1016/0378-4363(80)90054-6 ↗
62. Energy effects and charge transfer in metal physics: modelling in real space10.1016/0921-4526(92)90565-A ↗
63. Effect of coherency on coarsening of second-phase precipitates in Cu-base alloys10.1007/s10853-007-2373-4 ↗
64. Hydrogen in aluminum: first-principles calculations of structure and thermodynamics10.1103/PhysRevB.69.144109 ↗