Abstract
Abstract SiC ceramic was successfully diffusion bonded to itself with a powder mixture of TiH2, Si and graphite by spark plasma sintering in the temperatures from 1150 °C to 1450 °C. The microstructure, phase formation and evolution, and the mechanical properties of the joints were evaluated. In-situ reaction in the powder mixture produced fine-grained Ti3SiC2 and TiCx (TiC and TiC0.625) composite in the joint. The grain morphology and size of carbides were determined. No reaction between the carbides and SiC ceramic was observed. The fraction of Ti3SiC2 in the composite joint had a strong effect on the joint strength, which increased with the increasing of Ti3SiC2 content. The highest shear strength of 80.5 ± 7.4 MPa was obtained at 1350 °C, due to the uniform distribution and inherent toughening characteristic of Ti3SiC2 phase. The decomposition of Ti3SiC2 occurred at 1450 °C led to the formation of TiCx and TiSi2, thereby lowering the shear strength. The hardness of the interlayer was dependent mainly on the fraction of TiCx phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Failure mechanisms in ceramic-fiber/ceramic-matrix composites10.1111/j.1151-2916.1985.tb15313.x ↗
2. High-temperature mechanical properties of a ceramic matrix composite10.1111/j.1151-2916.1987.tb05677.x ↗
3. Resistance to thermal shock and to oxidation of metal diborides-SiC ceramics for aerospace application10.1111/j.1551-2916.2007.01589.x ↗
4. Thermomechanical properties of a spark plasma sintered ZrC-SiC composite obtained by a precursor derived ceramic route10.1016/j.msea.2015.07.025 ↗
5. Prediction of grinding force for brittle materials considering co-existing of ductility and brittleness10.1007/s00170-016-8594-4 ↗
6. Reaction-composite brazing of carbon fiber reinforced SiC composite and TC4 alloy using Ag–Cu–Ti–(Ti+C) mixed powder10.1016/j.msea.2012.11.031 ↗
7. Interface structure and formation mechanism of diffusion-bonded SiC/TiAl joint10.1023/A:1006626132693 ↗
8. SiC/SiC composites through transient eutectic-phase route for fusion applications10.1016/j.jnucmat.2004.04.157 ↗
9. Joining of sintered silicon carbide ceramics for high-temperature applications10.1023/A:1006568124914 ↗
10. Y2O3–Al2O3–SiO2-based glass-ceramic fillers for the laser-supported joining of SiC10.1016/j.jeurceramsoc.2014.01.019 ↗
11. Joining of SiC ceramic-based materials with ternary carbide Ti3SiC210.1016/j.mseb.2010.09.002 ↗
12. Joining of C/SiC composites by spark plasma sintering technique10.1016/j.jeurceramsoc.2013.10.028 ↗
13. Spark plasma joining of ZrB2-SiC composites using zirconium-boron reactive filler layers10.1111/j.1551-2916.2011.04739.x ↗
14. Joining of β-SiC by spark plasma sintering10.1016/j.jeurceramsoc.2013.12.023 ↗
15. Influence of spark plasma sintering (SPS) processing parameters on microstructure and mechanical properties of nickel10.1016/j.msea.2014.08.070 ↗
16. The effect of electric field and pressure on the synthesis and consolidation of materials: a review of the spark plasma sintering method10.1007/s10853-006-6555-2 ↗
17. Mechanical properties of the MAX phases
18. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
19. Investigation of the mechanical behavior of MAX phases by acoustic emission technique10.1016/j.msea.2017.09.030 ↗
20. Damage mechanisms around hardness indentations in Ti3SiC210.1111/j.1151-2916.1997.tb02861.x ↗
21. Solid-state synthesis and characterization of the ternary phase Ti3SiC210.1007/BF00352037 ↗
22. Thermal properties of Ti3SiC210.1016/S0022-3697(98)00313-8 ↗
23. Fast joining SiC ceramics with Ti3SiC2 tape film by electric field-assisted sintering technology10.1016/j.jnucmat.2015.08.004 ↗
24. Joining of CVD-SiC coated and uncoated fibre reinforced ceramic matrix composites with pre-sintered Ti3SiC2 MAX phase using Spark Plasma Sintering10.1016/j.jeurceramsoc.2016.06.025 ↗
25. Microstructure and mechanical properties of SiC-SiC joints joined by spark plasma sintering10.1016/j.ceramint.2016.06.049 ↗
26. Pore formation process of porous Ti3SiC2 fabricated by reactive sintering10.3390/ma10020163 ↗
27. Interfacial study of NiTi-Ti3SiC2 solid state diffusion bonded joints10.1016/j.msea.2014.10.033 ↗
28. Reviewing the effects of different additives on the synthesis of the Ti3SiC2 MAX phase by mechanical alloying technique10.1016/j.ijrmhm.2016.08.003 ↗
29. Synthesis and reaction mechanism of Ti3SiC2 by mechanical alloying of elemental Ti, Si, and C Powders10.1111/j.1551-2916.2005.00417.x ↗
30. Effect of Al addition on phase purity of Ti3Si(Al)C2 synthesized by mechanical alloying10.1016/j.jmatprotec.2006.09.001 ↗
31. Synthesis of high-purity Ti3SiC2 polycrystals by hot-pressing of the elemental powders
32. Diffusion kinetics of the carburization and silicidation of Ti3SiC210.1063/1.366707 ↗
33. On physical and thermochemical properties of high-purity Ti3SiC210.1016/S0167-577X(01)00620-6 ↗
34. Phase evolution of Ti3SiC2 annealing in vacuum at elevated temperatures10.1111/j.1744-7402.2012.02760.x ↗
35. Elastic and mechanical properties of the MAX phases