Single-boss crevice former for studying crevice corrosion of UNS S32003 in chloride-containing solution at high temperature
Source abstract
Abstract
Abstract We studied crevice corrosion of UNS S32003 using a single-boss crevice former. This crevice assembly with a single boss at the center is a modification of the commonly used multiple-crevice assembly (MCA). This design effectively prevents unwanted crevice corrosion outside the crevice of interest. Our single-boss crevice assembly produces comparable repassivation potentials obtained using cyclic potentiodynamic polarization (CPP), Tsujikawa–Hisamatsu Electrochemical (THE), potentiodynamic–galvanostatic–potentiodynamic (PD–GS–PD), and potentiostatic (PS) techniques. Considering the degree of attack, we found that the THE technique is the most powerful for forming a deep, wide, and continuous crevice corrosion site, while the PS technique is the least powerful technique at potentials slightly above the repassivation potential. A galvanostatic hold in step 2 of the THE and PD–GS–PD techniques successfully grows a deep localized corrosion site, as indicated by a deep crevice corrosion attack found in samples tested with these techniques. The PS step (step 3) in the THE technique allows the grown localized corrosion site formed by a previous step (a galvanostatic hold) to propagate inward and along the crevice mouth, creating a wide and continuous crevice corrosion attack along the crevice mouth. Metastable pits play a role in crevice corrosion of UNS S32003 alloy in this study, as indicated by a large number of metastable pits in the crevice region. The ferrite phase is preferentially attacked by metastable pits.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Effect of nitrogen on crevice corrosion in austenitic stainless steel10.1016/j.corsci.2005.09.010 ↗
2. Crevice corrosion behaviour of superaustenitic stainless steels: dynamic electrochemical impedance spectroscopy and atomic force microscopy studies10.1016/j.corsci.2008.11.008 ↗
3. An experimental study of crevice corrosion behaviour of 316L stainless steel in artificial seawater10.1016/j.corsci.2010.05.040 ↗
4. Determination of the crevice corrosion stabilization and repassivation potentials of a corrosion-resistant alloy10.5006/1.3500830 ↗
5. An approach for estimating anodic current distributions in crevice corrosion from potential measurements10.1149/1.2054731 ↗
6. Demonstration of crevice corrosion in alkaline solution without acidification10.1149/1.2086211 ↗
7. Effect of the applied potential on the potential and current distributions within crevices in pure nickel10.1016/S0010-938X(98)00103-6 ↗
8. IR voltage switch in delayed crevice corrosion and active peak formation detected using a repassivation-type scan10.1016/j.electacta.2004.12.017 ↗
9. Prediction of critical crevice potentials for Ni–Cr–Mo alloys in simulated crevice solutions as a function of molybdenum content10.5006/1.3430462 ↗
10. Effect of temperature on the crevice corrosion of type 304 stainless steel in chloride solution up to 250°C10.5006/1.3585174 ↗
11. Effects of test methods on crevice corrosion repassivation potential measurements of alloy 2210.5006/1.3319149 ↗
12. Effects of iron content on microstructure and crevice corrosion of grade-2 titanium10.5006/1.3287747 ↗
13. Crevice corrosion repassivation of alloy 22 in aggressive environments10.5006/1.3279917 ↗
14. The initiation of crevice corrosion in stainless steels10.1016/S0010-938X(97)00050-4 ↗
15. Crevice corrosion of stainless steels. I. Mathematical model10.1179/000705978798358671 ↗
16. New technique for predicting the performance of stainless steels in sea water and other chloride-containing environments10.1179/000705980798318654 ↗
17. The Role of inclusions on initiation of crevice corrosion of stainless steel. I. Experimental studies10.1149/1.2096896 ↗
18. The role of inclusions on initiation of crevice corrosion of stainless steel. II. Theoretical Studies10.1149/1.2096434 ↗
19. A Critical review of IR drops and electrode potentials within pits, crevices and cracks
20. The significance of the local electrode potential within pits, crevices and cracks10.1016/0010-938X(89)90039-5 ↗
21. The initial potential and current distributions of the crevice corrosion process10.1149/1.2056139 ↗
22. A clearer view of how crevice corrosion occurs10.1007/BF03221250 ↗
23. Metastable pitting processes and crevice corrosion on stainless steels
24. ASTM Standard G78-01 · 2012
25. FN speller award lecture: corrosion considerations related to permanent disposal of high-level radioactive waste10.5006/1.3287662 ↗
26. Pitting corrosion of metals a review of the critical factors10.1149/1.1838615 ↗
27. Using electrochemical methods to determine alloy 22’s crevice corrosion repassivation potential10.1007/s11837-005-0065-6 ↗
28. Metastable pitting of aluminum and criteria for the transition to stable pit growth10.1149/1.2059275 ↗
29. Effect of potential on crevice corrosion kinetics of alloy 2210.5006/1.3318286 ↗
30. Metastable pitting of stainless steel10.5006/1.3583880 ↗
31. Metastable pitting corrosion of stainless steel and the transition to stability10.1098/rsta.1992.0114 ↗
32. The use of pitting transients to test microscopic models of localized corrosion10.4028/www.scientific.net/MSF.192-194.649 ↗
33. Prediction of pitting potentials and critical pitting temperatures
34. Microelectrochemical studies on the influence of Cr and Mo on nucleation events of pitting corrosion10.1149/1.1393169 ↗