Fretting fatigue damage mechanism of Ti6Al4V dovetail joint specimens at high temperature treated with salt layer
Source abstract
Abstract
Salt layer preparation on the contact surface of Ti6Al4V dovetail joint specimens using solid NaCl and Na 2SO 4 deposition, the effect of hot salt layer on fretting fatigue properties of Ti6Al4V alloy at high temperature was studied. The maximum stress load and temperature are 10 kN and 500 °C, respectively. The results show that the average fatigue life of the base metal dovetail joint sample (BM sample) is 9.93×10 4, and the average fatigue life of the hot salt dovetail joint sample (HS sample) is increased to 69.9×10 4 . The increase in fatigue life stems from the fact that the hot salt layer promotes the generation of thicker loose oxides on the surface of the Ti6Al4V alloy, besides, the lubricating effect of the oxide with higher hardness and the wear debris alleviates the fretting damage between the dovetail joint sample and the contact surface of the fretting pad. Fracture analysis shows that the hot salt layer does not change the crack initiation mechanism, and all of them show single crack source propagation and ductile fracture mechanism. Analysis of crack formation zone by electron back-scattered diffraction (EBSD), it is found that the presence of less dislocation distribution in the HS sample relative to the BM sample. The dislocations are more concentrated on the crack propagation paths and the fretting fatigue contact surfaces. This indicates that the BM sample produced more significant plastic deformation in the crack formation zone, accelerating crack initiation. The contact surface plastic deformation of the HS sample is small and the fretting fatigue life is enhanced.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical stress and fatigue analysis · Metal Alloys Wear and Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Effects of microstructure on the dynamic properties of TA15 titanium alloy10.1016/j.mechmat.2019.103121 ↗
2. Institute of Metal Research, Chinese Academy of Sciences: aiming to achieve breakthroughs in the development of materials10.1093/nsr/nwx049 ↗
3. An assessment of the role of near-threshold crack growth in high-cycle-fatigue life prediction of aerospace titanium alloys under turbine engine spectra10.1007/BF00012671 ↗
4. A state-of-the-art review on passivation and biofouling of Ti and its alloys in marine environments10.1016/j.jmst.2017.11.021 ↗
5. A fracture mechanics life prediction methodology applied to dovetail fretting10.1016/j.triboint.2006.02.006 ↗
6. Fracture of aircraft titanium alloys under high-frequency loading10.1007/s42452-022-05266-8 ↗
7. Failure assessment of the first stage high-pressure turbine blades in an aero-engine turbine10.1111/ffe.12630 ↗
8. The role of crystallographic texture and basal plane slip on microstructurally short fatigue crack initiation and propagation in forged billet and rolled Bar Ti-6Al-4V Alloy10.1007/s11661-021-06344-z ↗
9. Fan Blade Fatigue Fractures in CFM56-7B Engines10.1007/s11668-023-01702-y ↗
10. Fretting fatigue in aircraft components made of Ti-Al-V alloys10.1016/j.proeng.2013.03.284 ↗
11. Fretting wear behaviour of machined layer of nickel-based superalloy produced by creep-feed profile grinding10.1016/j.cja.2021.10.007 ↗
12. A review of fretting study on nuclear power equipment10.1016/j.triboint.2019.106095 ↗
13. Investigation of fretting fatigue behavior of TI811 alloy at elevated temperature
14. Study on mixed-mode fracture behavior of TC4 titanium alloy10.1016/j.tafmec.2023.103911 ↗
15. High-temperature fatigue behavior of TC17 titanium alloy and influence of surface oxidation10.1016/j.ijfatigue.2023.107896 ↗
16. Corrosion degradation behaviors of Ti6Al4V alloys in simulated marine environments
17. Hot corrosion damage mechanism of Ti6Al4V alloy in marine environment10.1016/j.vacuum.2021.110350 ↗
18. Fretting fatigue behavior of Ti–6Al–4V under seawater environment10.1016/j.msea.2005.05.047 ↗
19. Fretting fatigue behavior of shot-peened Ti–6Al–4V under seawater environment10.1016/j.msea.2006.01.031 ↗
20. The fretting fatigue of titanium and some titanium alloys in a corrosive environment10.1016/0043-1648(73)90069-0 ↗
21. Environmental effects in the fretting fatigue of Ti-6Al-4V10.1016/0043-1648(80)90174-X ↗
22. Improved fretting fatigue mechanism of surface-strengthened Ti-6Al-4V alloy induced by ultrasonic surface rolling process10.1016/j.ijfatigue.2023.107567 ↗
23. Fretting fatigue damage mechanism of Nickel-based single crystal superalloys at high temperature10.1016/j.ijmecsci.2020.105894 ↗
24. Tribocorrosion behavior of micro/nanoscale surface coatings10.3390/s22249974 ↗
25. An experimental investigation of adhesive wear extension in fretting interface: application of the contact oxygenation concept10.1016/j.triboint.2020.106266 ↗
26. An experimental investigation on fretting wear behavior of copper–magnesium alloy10.1016/j.wear.2020.203497 ↗
27. Study on fretting fatigue Behavior of TC4 titanium alloy
28. On the mechanisms of various fretting wear modes10.1016/j.triboint.2011.02.010 ↗
29. Fretting wear behavior and mechanism of inconel 690 alloy related to the displacement amplitude10.1080/10402004.2016.1230686 ↗
30. RA-based fretting fatigue life prediction method of Ni-based single crystal superalloys10.1016/j.triboint.2019.01.036 ↗
31. Fretting fatigue characteristic of Ti–6Al–4V strengthened by wet peening10.1016/j.ijfatigue.2015.12.013 ↗
32. Fretting wear and friction reduction of CP titanium and Ti–6Al–4V alloy by ultrasonic nanocrystalline surface modification10.1016/j.surfcoat.2012.06.046 ↗
33. Influence of counterbody material on fretting wear behaviour of surface mechanical attrition treated Ti–6Al–4V10.1016/j.triboint.2012.07.021 ↗
34. Tribological investigations of wear resistant layers developed through EDA and WEDA techniques on Ti6Al4V surfaces: Part I – ambient temperature10.1016/j.wear.2020.203409 ↗
35. The influence of higher surface hardness on fretting fatigue life of hard anodized aerospace AL7075-T6 alloy10.1016/j.msea.2012.09.082 ↗
36. Study on the fretting wear performance and mechanism of GH4169 superalloy after various laser shock peening treatments10.1016/j.optlastec.2023.110301 ↗
37. Effect of ultrasonic surface rolling process on the microstructure and corrosion behavior of zirconium alloy in high-temperature water condition10.1016/j.matchemphys.2023.128546 ↗
38. Investigating the fretting fatigue life of thin film titanium nitride coated aerospace Al7075-T6 alloy10.1016/j.msea.2012.08.123 ↗
39. Mechanisms of sliding wear of metals and alloys at elevated temperatures10.1016/j.triboint.2007.10.003 ↗
40. The influence of contacting Ni-based single-crystal superalloys on fretting fatigue of Ni-based polycrystalline superalloys at high temperature10.1016/j.triboint.2014.01.011 ↗
41. Friction and wear characteristics of single crystal Ni-based superalloys at elevated temperatures10.1007/s11249-018-0994-1 ↗
42. Crystal orientation effect on fretting fatigue induced geometrically necessary dislocation distribution in Ni-based single-crystal superalloys10.1016/j.actamat.2019.08.035 ↗
43. Corrosion fatigue behavior of Fe-16Mn-0.6C-1.68Al twinning-induced plasticity steel in simulated seawater10.1016/j.corsci.2021.109282 ↗
44. Investigation of shot peening combined with plasma-sprayed CuNiIn coating on the fretting fatigue behavior of Ti-6Al-4V dovetail joint specimens10.1016/j.surfcoat.2018.12.006 ↗
45. Improvement in fretting fatigue life of GH4169 dovetail joint component by bonded solid lubricant coating at 500 ℃10.1016/j.triboint.2024.109415 ↗
46. Improving high temperature fretting fatigue performance of nickel-based single crystal superalloy by shot peening10.1016/j.ijfatigue.2023.107563 ↗
47. Quasi cleavage fracture of the bimodal size lamellar O phase microstructure of a Ti2AlNb based alloy10.1016/j.jallcom.2019.05.157 ↗
48. Enhancement in fatigue property of Ti-6Al-4V alloy remanufactured by combined laser cladding and laser shock peening processes10.1016/j.surfcoat.2022.128671 ↗
49. Investigation on microstructure and fracture behaviour of titanium alloy castings
50. Nanograin formation and cracking mechanism in Ti alloys under very high cycle fatigue loading10.1016/j.ijfatigue.2022.107331 ↗
51. Microstructural characterization of Ti-6Al-4V subjected to fretting10.1115/1.1792677 ↗
52. Comparison of surface integrity of GH4169 superalloy after high-energy, low-energy, and femtosecond laser shock peening10.1016/j.vacuum.2022.111740 ↗
53. Effects of temperature and load on fretting fatigue induced geometrically necessary dislocation distribution in titanium alloy10.1016/j.msea.2020.140308 ↗
54. Microstructural considerations of enhanced tensile strength and mechanical constraint in a copper/stainless steel brazed joint10.1016/j.msea.2020.139992 ↗