journal article·2024-03

CALPHAD-aided design of high-strength Al-Si-Mg alloys for sufficient laser powder bed fusion processability

Yuki Otani, Keito Saki, Naoki Takata, Asuka Suzuki, Makoto Kobashi, Masaki Kato

Publisher page

Abstract

This study proposes a design concept for an Al-Si-Mg ternary alloy to achieve both high strength and laser-based powder bed fusion (PBF-LB) processability using calculation of phase diagrams (CALPHAD). The thermodynamic calculations using the CALPHAD method evaluated the Al-10Si-4.5Mg (wt%) alloy composition for strengthening by both the Si and Mg 2Si phases and high PBF processability by reducing the risk of hot tearing behind the small freezing range of 27 °C and crack susceptibility index (|d T/d( F s 1/2 )|) of 77 °C. The PBF-LB Al-10Si-4.5Mg alloy sample (processed by laser power of 128 W and laser scanning velocity of 1000 mm/s) exhibited a fine three-phase microstructure and exceptional hardness of 199 HV. No hot tearing occurred, whereas many cracks preferentially propagated along the melt pool boundaries during the PBF-LB process. The severe lateral cracking resulted in a maximum relative density of 96 % in the Al-10Si-4.5Mg alloy samples. Preferential cracking could be responsible for the localization of the relatively coarse particles of the brittle Mg 2 Si phase in the cellular microstructures of the melt pool boundaries. Understanding the lateral cracking mechanism can provide new insights into alloy modification using the controlled solidification path to avoid a specific two-phase eutectic reaction (L→α-Al+Mg 2 Si) to improve the PBF processability. A modified alloy composition of Al-10Si-3Mg (wt%) was assessed using the CALPHAD approach. PBF-LB processing using the modified alloy powder alleviated cracking and improved the maximum relative density to 98 % for the PBF-LB manufactured samples. This result accentuated the validity of the design strategy for Al-Si-Mg ternary alloy utilizing the CALPHAD method.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (91)

Show source-provided references
1. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
2. The biomimetic design and 3D printing of customized mechanical properties porous Ti6Al4V scaffold for load-bearing bone reconstruction10.1016/j.matdes.2018.04.065 ↗
3. A review of selective laser melting of aluminum alloys: processing, microstructure, property and developing trends10.1016/j.jmst.2018.09.004 ↗
4. Unravelling the multi-scale structure–property relationship of laser powder bed fusion processed and heat-treated AlSi10Mg10.1038/s41598-021-85047-2 ↗
5. Fast scanning calorimetry study of Al alloy powder for understanding microstructural development in laser powder bed fusion10.1016/j.matdes.2022.110830 ↗
6. In-situ characterization of laser-powder interaction and cooling rates through high-speed imaging of powder bed fusion additive manufacturing10.1016/j.matdes.2017.09.044 ↗
7. Tuning strength-ductility combination on selective laser melted 316L stainless steel through gradient heterogeneous structure
8. Additively manufactured hierarchical stainless steels with high strength and ductility10.1038/nmat5021 ↗
9. Anomalous strengthening by supersaturated solid solutions of selectively laser melted Al–Si-based alloys
10. A review of laser powder bed fusion additive manufacturing of aluminium alloys: microstructure and properties
11. Wavelength dependant ablation rates for metals and silicate glasses using homogenized laser beam profiles — implications for LA-ICP-MS10.1016/S0169-4332(01)00465-2 ↗
12. Enabling high-performance 3D printing of Al powder by decorating with high laser absorbing Co phase
13. Density and solidification shrinkage of hypoeutectic aluminum-silicon alloys10.1007/s11661-001-0050-9 ↗
14. Aluminium die casting alloys: alloy composition, microstructure, and properties-performance relationships10.1179/imr.1995.40.6.221 ↗
15. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
16. A comparison of Selective Laser Melting with bulk rapid solidification of AlSi10Mg alloy10.1016/j.jallcom.2018.01.309 ↗
17. Alloying AlSi10Mg and Cu powders in laser single scan tracks, melt spinning, and laser powder bed fusion10.1016/j.jallcom.2019.153538 ↗
18. Susceptibility of ternary aluminum alloys to cracking during solidification10.1016/j.actamat.2016.12.028 ↗
19. Crack free metal printing using physics informed machine learning10.1016/j.actamat.2021.117612 ↗
20. A simple test for assessing solidification cracking susceptibility and checking validity of susceptibility prediction10.1016/j.actamat.2017.09.065 ↗
21. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
22. A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting10.1016/j.msea.2021.141638 ↗
23. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
24. Influence of erbium addition on the defects of selective laser-melted 7075 aluminium alloy10.1080/17452759.2021.1990358 ↗
25. Effects of the addition of silicon to 7075 aluminum alloy on microstructure, mechanical properties, and selective laser melting processability10.1016/j.msea.2020.139079 ↗
26. Application of base plate preheating during selective laser melting10.1016/j.procir.2018.08.002 ↗
27. Effect of processing parameters on the densification of an additively manufactured 2024 Al alloy10.1016/j.jmst.2020.03.070 ↗
28. Review of high-strength aluminium alloys for additive manufacturing by laser powder bed fusion10.1016/j.matdes.2022.110779 ↗
29. An integrated computational materials engineering-anchored closed-loop method for design of aluminum alloys for additive manufacturing10.1016/j.mtla.2019.100574 ↗
30. Towards a high strength aluminium alloy development methodology for selective laser melting10.1016/j.matdes.2019.107775 ↗
31. Solute clustering and supersaturated solid solution of AlSi10Mg alloy fabricated by selective laser melting10.1016/j.heliyon.2019.e01186 ↗
32. Multiple precipitation pathways in an Al-7Si-0.6Mg alloy fabricated by selective laser melting10.1016/j.scriptamat.2018.09.045 ↗
33. Rapid solidification and non-equilibrium phase constitution in Laser Powder Bed Fusion (LPBF) of AlSi10Mg alloy: analysis of nano-precipitates, eutectic phases, and hardness evolution10.1007/s11661-019-05505-5 ↗
34. Contribution of Mg2Si precipitates to the strength of direct metal laser sintered AlSi10Mg10.1016/j.msea.2018.10.055 ↗
35. Low temperature annealing dedicated to AlSi10Mg selective laser melting products10.1016/j.jallcom.2016.12.019 ↗
36. Microstructural formation in hypereutectic Al-Mg2Si with extra Si10.1016/j.jallcom.2008.10.061 ↗
37. Eutectic reaction and microstructural characteristics of Al (Li)-Mg2Si alloys10.1023/A:1017525520066 ↗
38. Microstructural, mechanical and electrical characterization of directionally solidified Al-Si-Mg eutectic alloy10.1016/j.jallcom.2014.08.056 ↗
39. Solidification and precipitation behaviour of Al-Si-Mg casting alloys10.1023/A:1004801327556 ↗
40. Hot tearing behavior in double ternary eutectic alloy system: Al-Mg-Si alloys10.1007/s11661-020-06101-8 ↗
41. Observation and prediction of the hot tear susceptibility of ternary Al-Si-Mg alloys10.1007/s11661-012-1132-6 ↗
42. Influence of vanadium and niobium carbide particles on the mechanical, microstructural, and physical properties of AA6061 aluminum-based mono- and hybrid composite using FSP10.3390/coatings13010142 ↗
43. Microstructural evolution and strengthening mechanism of high-strength AlSi8.1Mg1.4 alloy produced by selective laser melting10.1016/j.matdes.2022.110674 ↗
44. Effect of heat treatment on the microstructure and mechanical properties of an Al-5Mg2Si-2Mg alloy processed by laser powder bed fusion10.1016/j.jallcom.2022.165944 ↗
45. Design high-strength Al–Mg–Si alloy fabricated by laser powder bed fusion: cracking suppression and strengthening mechanism10.1016/j.msea.2023.144591 ↗
46. A tailored AlSiMg alloy for laser powder bed fusion10.3390/met10040514 ↗
47. Additive manufacturing of a high strength Al-5Mg2Si-2Mg alloy: microstructure and mechanical properties10.1016/j.jmst.2021.02.048 ↗
48. Composition-dependent solidification cracking of aluminum-silicon alloys during laser powder bed fusion10.1016/j.actamat.2021.116698 ↗
49. Design of heat-resistant Al–Mg –Zn–Cu–Ni quinary alloy: controlling intermetallic phases and mechanical performance at elevated temperature10.1016/j.msea.2022.144055 ↗
50. CALPHAD-aided design for superior thermal stability and mechanical behavior in a TiZrHfNb refractory high-entropy alloy10.1016/j.actamat.2023.118728 ↗
51. Experimental validation of Scheil–Gulliver simulations for gradient path planning in additively manufactured functionally graded materials10.1016/j.mtla.2020.100689 ↗
52. The PANDAT software package and its applications10.1016/S0364-5916(02)00034-2 ↗
53. PANDAT software with PanEngine, PanOptimizer and PanPrecipitation for multi-component phase diagram calculation and materials property simulation10.1016/j.calphad.2008.08.004 ↗
54. Bemerkungen zur Schichtkristallbildung10.1515/ijmr-1942-340303 ↗
55. Solidification structures and properties of fusion welds10.1179/imr.1975.20.1.83 ↗
56. Effect of compositional variation on the microstructural evolution and the castability of Al–Mg–Si ternary alloys10.1007/s11661-021-06306-5 ↗
57. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
58. Microstructure of intermetallic-reinforced Al-based alloy composites fabricated using eutectic reactions in Al–Mg–Zn ternary system10.1016/j.intermet.2018.01.018 ↗
59. Geometrical effects on residual stress in selective laser melting
60. Determination of the effect of scan strategy on residual stress in laser powder bed fusion additive manufacturing
61. Laser powder bed fusion of Ti-6Al-4V parts: thermal modeling and mechanical implications10.1016/j.ijmachtools.2017.04.007 ↗
62. On the limitations of volumetric energy density as a design parameter for selective laser melting10.1016/j.matdes.2016.10.037 ↗
63. Design of laser parameters for selectively laser melted maraging steel based on deposited energy density
64. Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments10.1016/j.msea.2017.08.029 ↗
65. Solidification pattern, microstructure and texture development in Laser Powder Bed Fusion (LPBF) of Al10SiMg alloy10.1016/j.matchar.2018.08.025 ↗
66. Effects of the grain shape and crystallographic texture on the grain-scale mechanical behavior of additively manufactured aluminum alloys
67. Design of Al–Fe–Mn alloy for both high-temperature strength and sufficient processability of laser powder bed fusion
68. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
69. Rapid solidification: selective laser melting of AlSi10Mg10.1007/s11837-015-1763-3 ↗
70. Effect of low-temperature annealing on electrical resistivity and mechanical properties of laser-powder bed fused AlSi10Mg alloy10.1016/j.msea.2023.144876 ↗
71. Enhancement in strength and ductility of laser powder bed fused Al–12Si alloy by introducing nanoscale precipitates
72. Selective laser melted Al-7Si-0.6Mg alloy with in-situ precipitation via platform heating for residual strain removal10.1016/j.matdes.2019.108005 ↗
73. Investigation of the influences of ternary Mg addition on the solidification microstructure and mechanical properties of as-cast Al–10Si alloys10.1016/j.msea.2020.140247 ↗
74. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
75. Review on residual stress in selective laser melting additive manufacturing of alloy parts10.1016/j.optlastec.2020.106283 ↗
76. Processability and cracking behaviour of novel high-alloyed tool steels processed by Laser Powder Bed Fusion10.1016/j.jmatprotec.2021.117435 ↗
77. Defects in a laser powder bed fused tool steel10.1002/adem.202000833 ↗
78. Microstructure, mechanical, and tribological properties of M3:2 high-speed steel processed by selective laser melting, hot-isostatic pressing, and casting
79. Study on the microstructure, mechanical property and residual stress of SLM Inconel-718 alloy manufactured by differing island scanning strategy10.1016/j.optlastec.2015.07.009 ↗
80. Processability and optimization of laser parameters for densification of hypereutectic Al–Fe binary alloy manufactured by laser powder bed fusion10.3390/cryst11030320 ↗
81. Microstructural formation and characterization mechanisms of selective laser melted Al–Si–Mg alloys with increasing magnesium content10.1016/j.msea.2019.02.015 ↗
82. The fracture toughness of Mg2Si determined by 3-point bending and the indentation microcracking method10.1515/ijmr-2003-0240 ↗
83. Orientation dependence of fracture toughness and its relation to surface energy in Si crystals10.2320/jinstmet.68.787 ↗
84. Phase field simulation of powder bed-based additive manufacturing10.1016/j.actamat.2017.11.033 ↗
85. Prediction of microstructure in laser powder bed fusion process10.1016/j.actamat.2016.11.018 ↗
86. 3D phase-field computations of microsegregation in nodular cast iron compared to experimental data and Calphad-based Scheil-prediction10.1016/j.mtla.2019.100538 ↗
87. Modeling of binary alloy solidification under conditions representative of additive manufacturing10.1016/j.commatsci.2018.04.004 ↗
88. Modeling of solidification microstructure evolution in laser powder bed fusion fabricated 316L stainless steel using combined computational fluid dynamics and cellular automata
89. Cellular automaton simulation of three-dimensional dendrite growth in Al-7Si-Mg ternary aluminum alloys10.1016/j.commatsci.2015.04.035 ↗
90. Understanding the effect of laser scan strategy on residual stress in selective laser melting through thermo-mechanical simulation
91. Synergic strategies to improve the PBF-LB\M processability of a cracking-sensitive alloy10.1016/j.matdes.2022.111396 ↗