Microstructures and mechanical properties of (TiBw+Ti5Si3)/TC11 composites fabricated by hot isostatic pressing and subjected to 2D forging

Yu Fu, Yongdong Xu, Yinyang Wang, Yu Bai, Hai Hao, Xiurong Zhu

Publisher page

Abstract

In this study, microstructures and mechanical properties of (TiBw+Ti 5Si 3 )/TC11 composites fabricated by hot isostatic pressing and 2D forging were investigated. A α + β titanium alloy TC11 (Ti-6.4Al-3.5Mo-1.4Zr-0.25Si) was used as a matrix material. The TiB 2 addition corresponding to 5.0 and 3.5 vol% of TiB w and the Si addition corresponding to 2.0, 4.0 and 6.0 vol% of Ti 5Si 3 were used as additives to the TC11 titanium alloy. TiB w and Ti 5Si 3 reinforced TC11 titanium matrix composites were fabricated by hot isostatic pressing and 2D forging in the α + β temperature field at T = 980 °C. The microstructure of the as-forged composites was composed of nanoscale Ti 5Si 3 particle within the β-phase and TiB w around TC11 matrix particle. The TiB w reinforcer tend to be distributed along the stretching deformation direction. Compared with the TC11 matrix alloy, the strength of the (2Ti 5Si 3 +5TiB w)/TC11 composite after 2D forging at room temperature increased by about 90 MPa due to the fine-grain strengthening of the α-phase, the precipitation strengthening of the nanoscale Ti 5Si 3 silicide, and the load transfer efficiency of TiB w. The main failure mechanism of the composites at room temperature is fracture of TiB w followed by ductile failure of the matrix. (2Ti 5Si 3 +5TiB w )/TC11 is thought as the optimal choice for engineering application, which UTS and El. at 600 °C are 851 MPa and 11%, respectively, and corresponding values of parameters at 750 °C are 385 MPa and 21%, respectively. Compared to the maximum service temperature 500 °C of TC11 alloy, the service temperature of (2Ti 5Si 3 +5TiB w)/TC11 composite can be improved by over 100 °C while retaining the similar tensile strength and elongation.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Additive Manufacturing Materials and Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Mechanical, wear and thermal behaviors of graphene reinforced titanium composites
2. Microstructure and tribological behavior of in situ synthesized (TiB+TiC)/Ti6Al4V (TiB/TiC=1/1) composites10.1016/j.triboint.2020.106177 ↗
3. Effect of TiB2 addition on the elevated temperature tribological behavior of spark plasma sintered Ti matrix composite10.1016/j.compositesb.2019.05.073 ↗
4. Influence of 2D forging processes and boron contents on the microstructures and mechanical properties of near α titanium alloys10.1016/j.intermet.2021.107181 ↗
5. Insights into wear behavior of (TiC+TiB)/TC4 composites against different counterface materials10.1088/2053-1591/ab4bac ↗
6. Strengthening and plasticity improvement mechanisms of titanium matrix composites with two-scale network microstructure10.1016/j.powtec.2019.09.008 ↗
7. In-situ Ti-6Al-4V/TiC composites synthesized by reactive spark plasma sintering: processing, microstructure, and dry sliding wear behavior
8. Hot isostatic pressing of in-situ TiB/Ti-6Al-4V composites with novel reinforcement architecture, enhanced hardness and elevated tribological properties10.1016/j.jallcom.2017.03.160 ↗
9. In-situ TiB/Ti-6Al-4V composites with a tailored architecture produced by hot isostatic pressing: microstructure evolution, enhanced tensile properties and strengthening mechanisms10.1016/j.compositesb.2019.01.080 ↗
10. Evaluation on tribological characteristics of (TiC+TiB)/Ti-6Al-4V composite in the range from 20°C to 600°C
11. Microstructure and mechanical properties of Ti6Al4V alloy modified and reinforced by in situ Ti5Si3/Ti composite ribbon inoculants10.3390/met7070267 ↗
12. In Situ reactions during direct laser deposition of Ti-B4C composites10.1016/j.scriptamat.2020.03.021 ↗
13. Constructing two-scale network microstructure with nano-Ti5Si3 for superhigh creep resistance10.1016/j.jmst.2019.04.001 ↗
14. Effects of first-scale TiBw on secondary-scale Ti5Si3 characteristics and mechanical properties of in-situ (Ti5Si3+TiBw)/Ti6Al4V composites10.1016/j.jallcom.2017.02.044 ↗
15. The tensile and fracture toughness properties of a (TiBw+TiCp)/Ti-3.5Al-5Mo-6V–3Cr-2Sn-0.5Fe composites after heat treatment10.1016/j.msea.2018.05.009 ↗
16. Network-strengthened Ti-6Al-4V/ (TiC+TiB) composites: powder metallurgy processing and enhanced tensile properties at elevated temperatures10.1007/s11661-019-05244-7 ↗
17. Relationships among reinforcement volume fraction, microstructure and tensile properties of (TiBw+TiCp)/Ti composites after (α+β) forging10.1016/j.msea.2017.06.061 ↗
18. Isothermal deformation and spheroidization mechanism of (TiB+La2O3)/Ti composites with different initial structures10.1016/j.matchar.2018.09.040 ↗
19. Multiscale architecture and superior high-temperature performance of discontinuously reinforced titanium matrix composites
20. Microstructure, mechanical properties and strengthening mechanisms of in-situ prepared (Ti5Si3+TiC0.67)/TC4 composites10.1016/j.jallcom.2019.04.056 ↗
21. Effect of multi-directional forging on the microstructure and mechanical properties of TiBw/TA15 composite with network architecture10.1016/j.matdes.2017.08.055 ↗
22. Precipitation behavior of silicide and synergetic strengthening mechanisms in TiB-reinforced high-temperature titanium matrix composites during multi-directional forging10.1016/j.jallcom.2021.159051 ↗
23. The influence of trace TiB and TiC on microstructure refinement and mechanical properties of in situ synthesized Ti matrix composite10.1016/j.compositesb.2012.01.075 ↗
24. High tensile-strength and ductile titanium matrix composites strengthened by TiB nanowires10.1016/j.scriptamat.2017.08.007 ↗
25. Microstructure and tensile properties of in situ (TiB+TiC)/Ti6242 (TiB:TiC=1:1) composites prepared by common casting technique10.1016/S0921-5093(01)00910-8 ↗
26. Strengthening behavior of in situ-synthesized (TiC-TiB)/Ti composites by powder metallurgy and hot extrusion10.1016/j.matdes.2016.01.092 ↗
27. Influence of (TiC+TiB) on the microstructure and tensile properties of Ti-B20 matrix alloy10.1016/j.jallcom.2014.12.056 ↗
28. Mechanical properties and strengthening effects of in situ (TiB+TiC)/Ti-1100 composite at elevated temperatures10.1016/j.msea.2015.12.071 ↗
29. Investigation on the microstructure, room and high temperature mechanical behaviors and strengthening mechanisms of the (TiB+TiC)/TC4 composites10.1016/j.jallcom.2017.08.017 ↗