Unveiling the ductility enhancement mechanisms in AZ31 magnesium alloy achieved via shear strain-assisted twin orientation regulation

Pengbin Lu, Lifei Wang, Xiaohuan Pan, Guangsheng Huang, Qiang Zhang, Hua Zhang, Liuwei Zheng, Liwei Lu, Hongxia Wang, Shuyong Jiang, Kwang Seon Shin

Publisher page

Abstract

The ductility enhancement mechanisms were investigated in AZ31 magnesium alloy based on the newly proposed concept of shear strain-assisted twin orientation regulation (SATOR). The simple shear strain was imposed on pre-twinned samples with various strain levels to rotate the twin orientation. The results indicated that the fracture strain of SATORed samples with the greatest ductility improvement was ∼1.5 times higher than that of the original material. Overall shear-deformed samples generated a bimodal fine-grained structure. While the preferred texture of the as-received alloy was only deviated by ∼12° during shear deformation, the pre-twinned samples obtained a closed-45° shear texture. Furthermore, combining the simulation results of the visco-plastic self-consistent (VPSC) model, the improved ductility is mostly ascribed to the efficient regulation of initial twin orientation, the promoted basal slip activity, and bimodal fine-grained structure. The SATOR method has been proved to be a promising strategy for dramatically increasing ductility while also providing the reference required for texture control via twin orientation regulation in Mg alloys.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Mechanisms of extrusion-ratio dependent ultrafine-grain fabrication in AZ31 magnesium alloy by continuous squeeze casting-extrusion10.1016/j.jmatprotec.2022.117755 ↗
2. A review on recent advancements in biodegradable Mg-Ca alloys10.1016/j.jma.2022.08.002 ↗
3. Latest research advances on magnesium and magnesium alloys worldwide10.1016/j.jma.2020.02.003 ↗
4. Effects of cold and warm cross-rolling on microstructure and texture evolution of AZ31B magnesium alloy sheet10.1016/j.jma.2018.04.004 ↗
5. Microstructure, deformation, and property of wrought magnesium alloys10.1007/s11661-020-05974-z ↗
6. Improving the sheared edge in the blanking of commercial AZ31 sheet through texture modification10.1016/j.jmatprotec.2011.06.022 ↗
7. Calculation of Schmid factor in Mg alloys: Influence of stress state10.1016/j.scriptamat.2019.06.014 ↗
8. Compound role of tension twins and compression twins in microstructure and mechanical properties of Mg-Sn-Li rod10.1016/j.msea.2016.11.023 ↗
9. Improving the plastic homogeneity of a magnesium alloy by introducing high volume fraction of twins during ambient extrusion10.1016/j.jmatprotec.2019.116445 ↗
10. Microstructure, texture and mechanical properties evolution of pre-twinning Mg alloys sheets during large strain hot rolling10.1016/j.msea.2015.12.059 ↗
11. Texture control by {10-12} twinning to improve the formability of Mg alloys: a review10.1016/j.jmst.2019.03.045 ↗
12. Detwinning behavior of Mg–3Al–1Zn alloy at elevated temperatures10.1016/j.msea.2014.08.034 ↗
13. The effects of compressive pre-deformation on yield asymmetry in hot-extruded Mg–3Al–1Zn alloy10.1016/j.msea.2013.04.115 ↗
14. Influence of various initial microstructures on microstructure and mechanical property of ECAP processed Mg-8.4Li-3.58Al-0.36Si-0.05Ti-0.01B alloys
15. High strength and high ductility of Mg-10Gd-3Y alloy achieved by a novel extrusion-shearing process10.1016/j.jallcom.2022.167498 ↗
16. The evolution of microstructure and texture of AZ80 Mg alloy cup-shaped pieces processed by rotating backward extrusion10.1016/j.jma.2020.07.013 ↗
17. Achieving texture randomization and yield anisotropy reduction in rolled Mg-Zn-Y-Zr alloy by multidirectional impact forging10.1016/j.matchar.2022.112540 ↗
18. A comparative study on the microstructural features and mechanical properties of an Mg–Zn alloy processed by ECAP and SSE10.1016/j.msea.2022.143218 ↗
19. A modified die for equal channel angular pressing10.1016/j.jmatprotec.2008.07.022 ↗
20. Advances in ultrafine-grained materials10.1016/j.mattod.2013.03.004 ↗
21. Severe plastic deformation (SPD) of biodegradable magnesium alloys and composites: A review of developments and prospects10.1016/j.jma.2021.11.006 ↗
22. The influences of extrusion-shear process on microstructures evolution and mechanical properties of AZ31 magnesium alloy10.1016/j.jallcom.2016.10.234 ↗
23. Room-temperature equal channel angular extrusion of pure magnesium10.1016/j.actamat.2010.01.051 ↗
24. AZ31 magnesium alloy tube manufactured by composite forming technology including extruded-shear and bending based on finite element numerical simulation and experiments10.1007/s00170-021-07242-9 ↗
25. A twin size effect on thermally activated twin boundary migration in a Mg–3Al–1Zn alloy10.1016/j.msea.2015.05.070 ↗
26. The beneficial effect of AgIn addition on deformation behavior, microstructure and texture in Mg–Al–Zn alloy during single pass warm rolling10.1016/j.matdes.2015.05.029 ↗
27. Quasi in-situ EBSD analysis of twinning-detwinning and slip behaviors in textured AZ31 magnesium alloy subjected to compressive-tensile loading10.1016/j.jma.2021.08.025 ↗
28. Plasticity induced by twin lamellar structure in magnesium alloy10.1016/j.jmst.2013.10.017 ↗
29. Room temperature equal-channel angular pressing of a magnesium alloy10.1016/j.actamat.2013.01.063 ↗
30. Texture evolution in equal-channel angular extrusion10.1016/j.pmatsci.2009.01.001 ↗
31. Effect of subgrain and the associated DRX behaviour on the texture modification of Mg-6.63Zn-0.56Zr alloy during hot tensile deformation10.1016/j.msea.2021.141745 ↗
32. Reasonable utilization of {10-12} twin for optimizing microstructure and improving mechanical property in a Mg-Gd-Y alloy10.1016/j.matdes.2020.108600 ↗
33. Refining the microstructure and modifying the texture of the AZ80 alloy cylindrical tube by the rotating backward extrusion with different rotating revolutions10.1016/j.jallcom.2020.155442 ↗
34. Unveiling the planar deformation mechanisms for improved formability in pre-twinned AZ31 Mg alloy sheet at warm temperature10.1016/j.jallcom.2022.165495 ↗
35. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
36. Individual effect of recrystallisation nucleation sites on texture weakening in a magnesium alloy: Part 2- shear bands10.1016/j.actamat.2017.12.019 ↗
37. Unveiling the formation of basal texture variations based on twinning and dynamic recrystallization in AZ31 magnesium alloy during extrusion10.1016/j.actamat.2018.07.014 ↗
38. On the possibility to reduce ECAP deformation temperature in magnesium: Deformation behaviour, dynamic recrystallization and mechanical properties10.1016/j.msea.2021.141103 ↗
39. Correlation of plastic deformation and dynamic recrystallization in magnesium alloy ZK6010.1016/S1359-6454(01)00020-9 ↗
40. Influence of deformation twinning on static annealing of AZ31 Mg alloy10.1016/j.actamat.2013.06.037 ↗
41. Twinning-induced dynamic recrystallization in a magnesium alloy extruded at 450°C10.1016/j.scriptamat.2011.07.046 ↗
42. Microstructure, texture and mechanical properties of extruded AZ31 Mg alloy during small strain multi-directional forging with gradient cooling10.1016/j.jallcom.2022.164795 ↗
43. Influence of grain size and texture on the yield asymmetry of Mg-3Al-1Zn alloy10.1016/S1005-0302(11)60021-2 ↗
44. Ultra-Fine grained degradable magnesium for biomedical applications10.1016/S1875-5372(15)60001-7 ↗
45. Role of starting texture and deformation modes on low-temperature shear formability and shear localization of Mg–3Al–1Zn alloy10.1016/j.actamat.2014.12.006 ↗
46. The effect of twinning on dynamic recrystallization behavior of Mg-Gd-Y alloy during hot compression10.1016/j.jallcom.2019.06.279 ↗
47. Twin nucleation, twin growth and their effects on annealing strengths of Mg–Al–Zn–Mn sheets experienced different pre-compressive strains10.1016/j.jallcom.2019.152310 ↗
48. The microstructure evolution and mechanical anisotropy of extruded Mg-2Zn-0.4Ce-0.4Mn alloy tube during tension in different directions10.1016/j.jallcom.2021.159829 ↗
49. Research on deformation mechanism of AZ31 magnesium alloy sheet with non-basal texture during uniaxial tension at room temperature: a visco-plastic self-consistent analysis10.1016/j.jma.2020.12.008 ↗
50. Mechanical properties and deformation mechanism in Mg-Gd alloy laminate with dual-heterostructure grain size and texture10.1016/j.ijplas.2022.103371 ↗
51. A crystal plasticity model for hexagonal close packed (HCP) crystals including twinning and de-twinning mechanisms10.1016/j.ijplas.2013.02.016 ↗
52. Pre-strain effect on twinning and de-twinning behaviors of Mg-3Li alloy traced by quasi-in-situ EBSD10.1016/j.msea.2020.140069 ↗
53. Strain hardening due to {10-12} twinning in pure magnesium10.1080/14786430701881211 ↗
54. Characteristics of twin lamellar structure in magnesium alloy during room temperature dynamic plastic deformation10.1016/j.jmst.2013.08.003 ↗
55. Effect of severe shot peening on corrosion behavior of AZ31 and AZ91 magnesium alloys10.1016/j.jallcom.2018.08.141 ↗
56. Influence of grain size and texture on the yield strength of Mg alloys processed by severe plastic deformation10.1155/2014/356572 ↗