Effects of TiB2 nanoparticles and ultrasonic vibration on the mechanical properties of an Mg-4Al-1.5Si alloy
Source abstract
Abstract
3 vol% TiB 2 nanoparticles were added to an Mg-4Al-1.5Si alloy through semi-solid stirring followed by ultrasonic vibration to refine coarse Mg 2Si phases. The effect of the added TiB 2 nanoparticles on the size and morphology of the Mg 2 Si phases as well as the mechanical properties of the magnesium alloy was investigated. The experimental results showed that under the synergistic action of ultrasonic vibration and heterogeneous nucleation of TiB 2 nanoparticles, the primary Mg 2 Si phases were not only refined from coarse dendritic to fine blocky shape but also uniformly dispersed. The morphology of the eutectic Mg 2 Si phases was transformed from coarse Chinese scripts to fine short strips. The Vickers-hardness, ultimate tensile strength, and yield strength of the obtained composites were increased by 101.8%, 69.8%, and 10.6%, respectively, compared with the matrix alloy, and the elongation was enhanced from 3.2% to 9.2% especially. The fracture mode was transformed from brittle fracture of the untreated Mg alloy to ductile fracture of the composites, indicating that the TiB 2 nanoparticles play an effective role in strengthening and toughening Mg-Al-Si alloys.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Study on solid-solution interaction and existing forms of alloying elements in Mg-Al-Zn-Gd alloy
2. Solute redistribution and mechanism of structure refinement of Mg-Al alloy during solidification under high pressure10.1016/j.jallcom.2022.164777 ↗
3. AZ91 alloy nanocomposites reinforced with Mg-coated graphene: phases distribution, interfacial microstructure, and property analysis10.1016/j.jallcom.2021.163484 ↗
4. Effect of Si content on microstructures, tensile properties, and creep properties in a cast Mg-6Al-0.4Mn-2Ca (wt%) alloy10.1016/j.msea.2020.139018 ↗
5. Formation of fine Mg2Si phase in Mg-Si alloy via solid-state sintering using high energy ball milling10.1016/j.jallcom.2019.153205 ↗
6. Effect of in situ Mg2Sip contents on microstructure and mechanical properties of Mg2Sip/AZ91D composites10.1007/s10853-020-05693-1 ↗
7. Effect of Sb doping on microstructure, mechanical and electronic properties of Mg2Si in Mg2Si/AZ91 composites by experimental investigation and first-principles calculation10.1016/j.jallcom.2022.163859 ↗
8. Revealing modification mechanism of Mg2Si in Sb modified Mg2Si/AZ91 composites and its effect on mechanical properties10.1016/j.jallcom.2020.156877 ↗
9. Effect of microalloying by Ca on the microstructure and mechanical properties of as-cast and wrought Mg-Mg2Si composites10.1016/j.msea.2021.141574 ↗
10. Synergetic modification effects on primary Mg2Si in Al-20Mg2Si alloy induced by the co-addition of beryllium and antimony10.1016/j.jallcom.2021.161477 ↗
11. Effect of complex modification of Ca and Sb on the microstructure and mechanical properties of hypoeutectic Al-11Mg2Si alloy10.1016/j.jallcom.2021.159304 ↗
12. Microstructure refinement and enhanced tensile properties of Al-11Mg2Si alloy modified by erbium10.1016/j.jallcom.2020.158421 ↗
13. Microstructural refinement and tensile properties enhancement of Al-10Mg2Si cast alloys by copper addition10.1016/j.jallcom.2021.163058 ↗
14. Structure and mechanical behavior of in situ developed Mg2Si phase in magnesium and aluminum alloys-a review10.1039/D0RA02744H ↗
15. Microstructures and mechanical performance of Mg-4Si-6Ni-xY in situ composite after extrusion process10.1080/02670836.2022.2027184 ↗
16. Kinetics of phase precipitation in Al-Mg-Si alloys subjected to equal-channel angular pressing during subsequent heating10.1016/j.jallcom.2021.160583 ↗
17. Synergistic effect of broken Mg2Si and sub-micron Mg17Al12 induced by EX-ECAP on the strength and ductility of deformed Mg-4Al-1Si-1Gd alloy10.1016/j.jmrt.2020.02.049 ↗
18. Microstructural homogeneity, mechanical properties, and wear behavior of in situ Mg2Si particles reinforced Al-matrix composites fabricated by hot rolling10.1016/j.jmrt.2019.12.020 ↗
19. The microstructure refinement and strength enhancement of Mg-Al-Si alloy subjected by alternating-frequency ultrasonic melt treatment
20. Effects of Bi modification and ultrasonic treatment on microstructure evolution and mechanical properties of AlMg5Si2Mn alloy
21. Variation of microstructure and mechanical properties of hybrid particulates reinforced Al-alloy matrix composites with ultrasonic treatment10.1016/j.jallcom.2019.03.074 ↗
22. M.L., H.X. Wang, W.L. Cheng, L.F. Wang, H.L. Wei Liang, Y.M. Liu, The creep behavior of Mg-9Al-1Si-1SiC composite at elevated temperature10.1016/j.jma.2019.06.004 ↗
23. Effect of in-situ TiB2 particles on microstructure and mechanical properties of Mg2Si/Al composites10.1016/j.jallcom.2018.10.301 ↗
24. Effects of modifying the hypoeutectic AlMg5Si2Mn alloy via addition of Al10Sr and/or Al5TiB
25. Microstructural improvement of eutectic Al + Mg2Si phases on Al-Zn-Si-Mg cast alloy with TiB2 particles additions10.3390/ma14112902 ↗
26. Cold spray additive manufacturing of metal matrix composites (MMCs) using a novel nano-TiB2-reinforced 7075Al powder10.1016/j.jallcom.2019.152962 ↗
27. An investigation on grain refinement mechanism of TiB2 particulate reinforced AZ91 composites and its effect on mechanical properties10.1016/j.jallcom.2018.11.253 ↗
28. Microstructure and tensile properties of magnesium matrix nanocomposite reinforced by high mass fraction of nano-sized particles including TiC and MgZn210.1016/j.jallcom.2019.153348 ↗
29. Effect of hybrid ultrasonic and mechanical stirring on the distribution of m‐SiCp in A356 alloy10.3390/met10050610 ↗
30. Fabrication and characterization two step stir casting with ultrasonic assisted novel AA7150-hBN nanocomposites10.1016/j.jallcom.2019.152464 ↗
31. Effect of ageing temperature on the corrosion behaviour of UHTC particulates reinforced magnesium composites fabricated through ultrasonic assisted squeeze casting process10.1016/j.jallcom.2020.158173 ↗
32. Investigation of macrosegregation for different dendritic arm spacing, casting temperature, and thermal boundary conditions in a direct-chill casting10.1007/s00339-020-03920-9 ↗
33. Grain refinement of magnesium alloys10.1007/s11661-005-0030-6 ↗
34. Distribution and motion behavior of desulfurizer particles in hot metal with mechanical stirring10.1016/j.powtec.2019.05.056 ↗
35. Effects of pouring temperature on microstructure and mechanical properties of the A356 aluminum alloy diecastings10.1590/1980-5373-mr-2019-0676 ↗
36. Tailoring the mechanical properties of hypereutectic in situ Al-Mg2Si composites via hybrid TiB2 reinforcement and hot extrusion10.1007/s43452-022-00416-6 ↗
37. Preparation and characterization of AZ91E/Al2O3 composites using hybrid mechanical and ultrasonic particle dispersion10.1016/j.msea.2021.141505 ↗
38. Enhancement of thermoelectric performance of Mg2Si via co-doping Sb and C by simultaneous tuning of electronic and thermal transport properties10.1016/j.jallcom.2021.161968 ↗
39. Influence of barium addition on the formation of primary Mg2Si crystals from Al-Mg-Si melts10.1016/j.jmrt.2021.01.051 ↗
40. Strengthening of the magnesium matrix composites hybrid reinforced by chemically oxidized carbon nanotubes and in situ Mg2Sip10.1016/j.jallcom.2020.157673 ↗
41. Microstructure evolution and mechanical properties of Mg-9Al-1Si-1SiC composites processed by multi-pass equal-channel angular pressing at various temperatures10.1007/s12613-020-2123-z ↗