journal article·2022-05

The microstructure and radiation resistance of fine-grained W-0.3 wt%Y2O3 prepared by nano in-situ composite exposed to low-energy and high‑flux helium plasma

Yongqi Lv, Siqi Zhao, Yong Han, Huichao Cheng, Zongbiao Ye, Hongbo Zhang, Yuanchun Huang, Jinglian Fan

Publisher page

Abstract

Tungsten is facing extremely harsh irradiation environmental challenges as plasma-facing materials. In this work, W-0.3 wt%Y 2O 3 composites fabricated by nano in-situ composite method were subjected to He plasma irradiation with 60–80 eV and 2.88 × 10 22–2.3 × 10 26 m −2. The microstructure, morphology, and phase evolution on the surface before and after irradiation were systematically investigated. Besides, the damage behavior and mechanism were initially analyzed. Results show that the nano-scaled Y 2O 3 with the size of 40–350 nm dispersed uniformly at the grain boundary and within grains of matrix, and part of it formed orientation relationship of [ 1 ̅ 11 ] ( 1 ̅ 1 ̅ 0) W (bcc) // [011] (400) Y 2O 3 (bcc) with W to significantly improve the phase interface. Surprisingly, there is a semi-coherent relationship between W matrix and Y 2O 3 phase. Simultaneously, the fine-grained W-0.3Y 2O 3 composites reveals excellent resistance to He plasma irradiation. As the irradiation dose increases, the surface morphology evolves from smooth to roughening, micro-bulges, rod-shaped and swelling, however, no nano-fuzz are observed when the irradiation dose was up to 2.3 × 10 26 m −2 . Besides, the chemical constitution and phase composition on surface is unchanged. Moreover, the dislocation lines, loops and rafts are observed by TEM on the surface layer, but no He bubble is formed. The high irradiation resistance may be attributed to the formation channels to release He, which can provide a strategy and idea for designing anti-irradiation W materials.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. On helium cluster dynamics in tungsten plasma facing components of fusion devices10.1088/0029-5515/54/7/073019 ↗
2. Characterization of He plasma irradiated bulk tungsten: a comparison with the in-situ TEM technique10.1016/j.fusengdes.2018.11.024 ↗
3. Unprecedented irradiation resistance of nanocrystalline tungsten with equiaxed nanocrystalline grains to dislocation loop accumulation10.1016/j.actamat.2018.11.024 ↗
4. Mechanical properties of Y2O3-doped W-Ti alloys10.1016/j.jnucmat.2010.07.016 ↗
5. Mechanical properties of W-Ti alloys from first-principles calculations10.1016/j.fusengdes.2016.03.028 ↗
6. Effect of sputtering on self-damaged recrystallized W mirror specimens10.1016/j.jnucmat.2012.12.007 ↗
7. Effect of Y2O3 particles on the He plasma irradiation damage of W-2%Y2O3 composite prepared by wet chemical method10.1016/j.mtla.2019.100268 ↗
8. Effects of helium on mechanical properties of tungsten for fusion applications10.1016/j.nme.2018.04.003 ↗
9. Nanostructured laminar tungsten alloy with improved ductility by surface mechanical attrition treatment10.1038/s41598-017-01458-0 ↗
10. Preparation of ultra-fine grain W-Y2O3 alloy by an improved wet chemical method and two-step spark plasma sintering10.1016/j.jallcom.2016.11.364 ↗
11. Effect of grain size on the behavior of hydrogen/helium retention in tungsten: a cluster dynamics modeling10.1088/1741-4326/aa7640 ↗
12. X.M. Bai, A.F. Voter, R.G. Hoagland, M. Nastasi, B.P. Uberuaga, Efficient annealing of radiation damage near grain boundaries via interstitial emission, Science, 327(5973), pp. 1631–1634.10.1126/science.1183723 ↗
13. Basic characterization of oxide dispersion strengthened fine-grained tungsten based materials fabricated by mechanical alloying and spark plasma sintering10.1016/j.jnucmat.2011.11.039 ↗
14. Nanostructured yttria dispersion-strengthened tungsten synthesized by sol-gel method10.1016/j.jallcom.2015.10.059 ↗
15. Grain size threshold for enhanced irradiation resistance in nanocrystalline and ultrafine tungsten10.1080/21663831.2017.1292326 ↗
16. W-Y2O3 composite nano-powders prepared by freeze-drying method and its sintering characteristics10.1016/j.jallcom.2019.07.214 ↗
17. Surface damage evolution during transient thermal shock of W-2%volY2O3 composite material in different surfaces10.1016/j.fusengdes.2019.01.010 ↗
18. Surface damage during transient thermal load of 50% thickness reduced W-2% (Vol.) Y2O3 sheet with different recrystallization volume fraction10.1016/j.ijrmhm.2020.105197 ↗
19. Densification and microstructure evolution of W-TiC-Y2O3 during spark plasma sintering10.1016/j.ijrmhm.2018.11.014 ↗
20. The influence of modification route on the properties of W-0.3 wt%Y2O3 powder and alloy prepared by nano-in-situ composite method10.1016/j.jallcom.2018.09.163 ↗
21. Nano-in-situ-composite ultrafine-grained W-Y2O3 materials: microstructure, mechanical properties and high heat load performances10.1016/j.jallcom.2020.157366 ↗
22. Effect of tungsten crystallographic orientation on He-ion-induced surface morphology changes10.1016/j.actamat.2013.09.045 ↗
23. Sintering densification behavior and kinetic mechanism of nano-tungsten powder prepared by sol-spray drying10.1007/s42864-020-00069-z ↗
24. Characterization of high flux magnetized helium plasma in SCU-PSI linear device10.1088/2058-6272/aa936e ↗
25. Compatibility between high-flux helium plasma irradiated molybdenum and liquid lithium10.1016/j.jnucmat.2018.04.038 ↗
26. Pressureless two-step sintering of ultrafine-grained tungsten10.1016/j.actamat.2020.01.001 ↗
27. Towards pressureless sintering of nanocrystalline tungsten10.1016/j.actamat.2021.117344 ↗
28. Microstructure and texture evolution in warm-rolled fine-grained tungsten10.1016/j.ijrmhm.2021.105690 ↗
29. The simultaneous improvements of strength and ductility in W-Y2O3 alloy obtained via an alkaline hydrothermal method and subsequent low temperature sintering10.1016/j.msea.2020.139329 ↗
30. Enhancing interface doping in graphene-metal hybrid devices using H2 plasma clean10.1016/j.apsusc.2020.148046 ↗
31. Nanochannel structures in W enhance radiation tolerance10.1016/j.actamat.2018.04.048 ↗
32. Grain orientations and grain boundaries in tungsten nonotendril fuzz grown under divertor-like conditions10.1016/j.scriptamat.2016.09.018 ↗
33. Surface damages of polycrystalline Wand La2O3-doped W induced by high-flux He plasma irradiation10.1016/j.jnucmat.2018.01.047 ↗
34. Effect of Ta addition on the fuzz formation of additively manufactured W-based materials10.1088/1741-4326/ab8a69 ↗
35. Impact of neutron irradiation on the strength and ductility of pure and ZrC reinforced tungsten grades10.1016/j.jnucmat.2020.152226 ↗
36. Effects of low energy and high flux Helium/Hydrogen plasma irradiation on tungsten as plasma facing material10.1088/1009-0630/7/3/010 ↗
37. Flux and fluence dependent helium plasma-materials interaction in hot-rolled and recrystallized tungsten10.1016/j.jnucmat.2018.07.048 ↗
38. Investigation of hydrogen bubbles behavior in tungsten by high-flux hydrogen implantation10.1016/j.jnucmat.2018.03.004 ↗
39. Low energy He plasma irradiation induced nanostructure formation on tungsten surface10.1016/j.jnucmat.2017.02.029 ↗
40. Formation process of tungsten nanostructure by the exposure to helium plasma under fusion relevant plasma conditions10.1088/0029-5515/49/9/095005 ↗
41. Effect of starting microstructure on helium plasma-materials interaction in tungsten10.1016/j.actamat.2016.11.042 ↗
42. Effect of Ta addition on the fuzz formation of additively manufactured W-based materials10.1088/1741-4326/ab8a69 ↗
43. Irradiation hardening induced by blistering in tungsten due to low-energy high flux hydrogen plasma exposure10.1016/j.jnucmat.2019.05.004 ↗
44. Morphologies of tungsten nanotendrils grown under helium exposure10.1038/srep42315 ↗
45. Effect of Y2O3 particles on the helium ion irradiation damage of W-2%Y2O3 composite prepared by wet chemical method10.1016/j.mtla.2019.100268 ↗
46. Repair behavior of He+-irradiated W-Y2O3 composites after different temperature-isochronal annealing experiments10.1016/j.nimb.2017.11.013 ↗
47. Combined effect of laser thermal shock and helium ion irradiation on W-Y2O3 composites10.1016/j.fusengdes.2019.01.134 ↗
48. Pearson · 2013
49. The effect of low energy He plasma irradiation on tungsten-tantalum (W-Ta) alloys under fusion relevant conditions10.1016/j.jnucmat.2017.05.009 ↗
50. Defect distribution in ion-irradiated pure tungsten at different temperatures10.1016/j.jnucmat.2016.08.029 ↗