journal article·2020-03

Effects of working pressure on structure and properties of Al-containing amorphous carbon films prepared by high-power impulse magnetron sputtering

Ya-Li Peng, Chao-Qian Guo, Song-Sheng Lin, Qian Shi, Chun-Bei Wei, Yi-Fan Su, Yi-Qian Wu, Peng Tang, Xia-Gao Zhu, Ming-Jiang Dai

Publisher page

Abstract

Abstract Al-containing amorphous carbon (a-C:Al) films were fabricated under different working pressures by high-power impulse magnetron sputtering. Morphologies, microstructure and chemical composition of a-C:Al films were characterized by scanning electron microscopy, atomic force microscope, X-ray photoelectron spectroscopy, transmission electron microscopy and Raman spectroscopy. Mechanical properties and tribological behavior of a-C:Al films were investigated by film stress tester, nano-indentation, scratch tester, ball-on-disk tribometer and 3D surface profiler. Results showed that atomic composition of Al in a-C:Al films was about 5%, independent of working pressure. The prepared films have smooth surfaces with Ra of 2.22 nm–5.89 nm. Typical amorphous structures could be observed in a-C:Al films and sp3 content could be governed by changing working pressures. Al existed as an oxide of aluminum in carbon matrix. There was a notable negative correlation between internal stress and sp3-C content. All samples manifested good adhesion strength to substrates with critical loads beyond 70 N. Wear rates were in 10−8 mm3 N−1 m−1 order of magnitude and had the same changing trend with H/E as working pressure rose from 0.3 Pa to 0.6 Pa. a-C:Al film prepared at 0.4 Pa has the best wear resistance with a wear rate of 4.38 × 10−8 mm3 N−1 m−1.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Study on failure mechanisms of DLC coated Ti6Al4V and CoCr under cyclic high combined contact stress10.1016/j.jallcom.2016.07.254 ↗
2. Optical properties of oxygen doped diamond-like carbon thin films10.1016/j.jallcom.2016.02.195 ↗
3. Electrical and mechanical properties of DLC coatings modified by plasma immersion ion implantation10.1016/j.jallcom.2006.02.108 ↗
4. Diamond-like amorphous carbon10.1016/S0927-796X(02)00005-0 ↗
5. Excellent adhered thick diamond-like carbon coatings by optimizing hetero-interfaces with sequential highly energetic Cr and C ion treatment10.1016/j.jallcom.2017.11.057 ↗
6. Corrosion resistance improvement of Mg alloy AZ31 by combining bilayer amorphous DLC:H/SiNx film with N+ ions implantation10.1016/j.jallcom.2018.05.217 ↗
7. Hard and adherent a-C:H gradient coatings by stress engineering10.1016/j.jallcom.2018.06.310 ↗
8. Diamond-like carbon nanocomposite films10.1063/1.1576909 ↗
9. Synthesis of diamondlike carbon films with superlow friction and wear properties10.1116/1.582459 ↗
10. Ti/Al co-doping induced residual stress reduction and bond structure evolution of amorphous carbon films: an experimental and ab initio study10.1016/j.carbon.2016.10.033 ↗
11. Tribo-pair dependence of friction and wear moisture sensitivity for aC: Si: Al carbon-based coating10.1016/j.jnoncrysol.2012.07.030 ↗
12. Effects of bias voltage on the microstructure and properties of Al-doped hydrogenated amorphous carbon films synthesized by a hybrid deposition technique10.1016/j.vacuum.2018.05.008 ↗
13. Deposition and properties of Al-containing diamond-like carbon films by a hybrid ion beam sources10.1016/j.jallcom.2011.01.132 ↗
14. Chemical structure and physical properties of diamond-like amorphous carbon films prepared by magnetron sputtering10.1557/JMR.1990.2543 ↗
15. 60years of DLC coatings: historical highlights and technical review of cathodic arc processes to synthesize various DLC types, and their evolution for industrial applications10.1016/j.surfcoat.2014.08.017 ↗
16. Structure and stress of Cu films prepared by high power pulsed magnetron sputtering10.1016/j.vacuum.2018.11.039 ↗
17. High power pulsed magnetron sputtering: a review on scientific and engineering state of the art10.1016/j.surfcoat.2009.11.013 ↗
18. Exploring the potential of high power impulse magnetron sputtering for growth of diamond-like carbon films10.1016/j.surfcoat.2011.11.032 ↗
19. Effects of Ar gas pressure on microstructure of DLC films deposited by high-power pulsed magnetron sputtering10.1016/j.vacuum.2012.07.004 ↗
20. Effects of gas pressure and r.f. power on the growth and properties of magnetron sputter deposited amorphous carbon thin films10.1016/S0925-9635(01)00544-1 ↗
21. The tension of metallic films deposited by electrolysis
22. Measurement of residual stress in DLC films prepared by plasma-based ion implantation and deposition10.1016/j.surfcoat.2004.04.010 ↗
23. Evaluation of Stoney equation for determining the internal stress of DLC thin films using an optical profiler10.1016/j.surfcoat.2016.07.098 ↗
24. Diamond like carbon films deposited by HiPIMS using oscillatory voltage pulses10.1016/j.surfcoat.2014.06.061 ↗
25. Barin · 2008
26. Synthesis of ultra-smooth and ultra-low friction DLC based nanocomposite films on rough substrates10.1016/j.tsf.2010.08.094 ↗
27. Microstructure, mechanical and tribological properties of Si and Al co-doped hydrogenated amorphous carbon films deposited at various bias voltages10.1016/j.surfcoat.2012.04.006 ↗
28. Fullerton · 1994
29. Effect of substrate temperature on properties of diamond-like films deposited by combined DC impulse vacuum-arc method10.1016/j.surfcoat.2013.10.023 ↗
30. Diamond like carbon coatings deposited by microwave plasma CVD: XPS and ellipsometric studies10.1007/s12034-007-0084-8 ↗
31. The preparation and mechanical properties of Al-containing a-C : H thin films10.1088/0022-3727/40/21/039 ↗
32. Catalytic carbide formation at aluminium-carbon interfaces10.1007/BF00720185 ↗
33. Structural properties of hydrogenated Al-doped diamond-like carbon films fabricated by a hybrid plasma system10.1016/j.diamond.2018.06.012 ↗
34. Influence of bias voltage on microstructure and properties of Al-containing diamond-like carbon films deposited by a hybrid ion beam system10.1016/j.surfcoat.2012.03.076 ↗
35. Interface architecture for superthick carbon-based films toward low internal stress and ultrahigh load-bearing capacity10.1021/am400778p ↗
36. Determination of bonding in diamond-like carbon by Raman spectroscopy10.1016/S0925-9635(01)00730-0 ↗
37. Raman ‘‘fingerprinting’’of amorphous carbon films10.1063/1.357385 ↗
38. Characterization of diamond-like carbon films by SEM, XRD and Raman spectroscopy10.1016/j.apsusc.2010.04.025 ↗
39. Raman spectroscopy on amorphous carbon films10.1063/1.362745 ↗
40. Resonant Raman spectroscopy of disordered, amorphous, and diamondlike carbon10.1103/PhysRevB.64.075414 ↗
41. Substantiation of subplantation model for diamond-like film growth by atomic-force microscopy10.1103/PhysRevLett.72.2753 ↗
42. Deposition mechanisms for promoting sp3 bonding in diamond-like carbon10.1016/0925-9635(93)90262-Z ↗
43. Structural properties and growth evolution of diamond-like carbon films with different incident energies: a molecular dynamics study10.1016/j.apsusc.2013.02.108 ↗
44. Hard carbon nanocomposite films with low stress10.1016/S0925-9635(00)00429-5 ↗
45. Stress-induced formation of high-density amorphous carbon thin films10.1063/1.366469 ↗
46. Compressive-stress-induced formation of thin-film tetrahedral amorphous carbon10.1103/PhysRevLett.67.773 ↗
47. Is stress necessary to stabilise sp3 bonding in diamond-like carbon?10.1016/S0925-9635(01)00705-1 ↗
48. Adhesion and composite micro-hardness of DLC and Si-DLC films deposited on nitrile rubber10.1016/j.surfcoat.2012.05.079 ↗
49. Hard and sp2-rich amorphous carbon structure formed by ion beam irradiation of fullerene, aC and polymeric aC: H films10.1016/j.diamond.2004.04.006 ↗
50. Requirements of ultrathin carbon coatings for magnetic storage technology10.1016/S0301-679X(02)00216-5 ↗
51. Preparation of various DLC films by T-shaped filtered arc deposition and the effect of heat treatment on film properties10.1016/j.vacuum.2008.04.016 ↗
52. The microstructure, mechanical and friction properties of protective diamond like carbon films on magnesium alloy10.1016/j.apsusc.2011.10.031 ↗
53. A first-principles study on the bond characteristics in carbon containing Mo, Ag, or Al impurity atoms10.1016/j.carbon.2007.11.005 ↗
54. Ceramic TiC/a:C protective nanocomposite coatings: structure and composition versus mechanical properties and tribology10.1016/j.ceramint.2016.04.164 ↗
55. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
56. Mechanical properties of nanostructured copper-hydrogenated amorphous carbon composite films studied by nanoindentation10.1016/j.surfcoat.2003.10.117 ↗
57. A study of the wear mechanism of diamond-like carbon films10.1016/0257-8972(95)02623-1 ↗
58. Study on structure, mechanical and tribological properties of iron incorporated diamond-like carbon films10.1016/j.jnoncrysol.2016.10.018 ↗
59. The role of hydrogen in tribological properties of diamond-like carbon films10.1016/S0257-8972(01)01417-7 ↗
60. Tribological response and characterization of Mo–W doped DLC coating10.1016/j.wear.2016.11.036 ↗
61. Friction and wear of hydrogenated and hydrogen-free diamond-like carbon films: relative humidity dependent character10.1016/j.apsusc.2017.05.210 ↗
62. Influence of surface passivation on the friction and wear behavior of ultrananocrystalline diamond and tetrahedral amorphous carbon thin films10.1103/PhysRevB.85.155448 ↗