Abstract

The cross accumulative roll bonding (CARB) combined with the heat treatment process was used to develop high-Zn Al-xZn alloys with 20 and 50 wt% Zn. The effect of the Zn content and fabrication process on the microstructural evolution, microhardness , tensile, and wear behaviors was investigated by using scanning electron microscopy (SEM) equipped with energy dispersive X-ray spectrometry (EDS), microhardness indentation, uniaxial tensile, and wear testing (pin-on-disk) at room temperature. The microstructure of the Al-20 wt% Zn alloy featured α-Al granular structures, whereas by Zn content increasing to 50 wt% the structure was α + η eutectoid structures with a fine distribution. The increase of the Zn element from 20 to 50 wt% was accompanied by a significant increase in tensile strength and also microhardness, but reduction in the elongation percentage of the Al–xZn alloys. Additionally, the wear resistance was improved as the Zn content was increased from 20 to 50 wt%. Finally, mechanical results confirmed that by increasing Zn content in the developed alloys the mechanical properties improved.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. New developments of high-zinc Al-Zn-Cu-Mn cast alloys10.1016/j.matpr.2018.10.410 ↗
2. Evolution of reinforcement distribution in Al–B4C composites during accumulative roll bonding10.1016/j.matdes.2011.02.063 ↗
3. Microstructure and mechanical properties of a high-Zn aluminum alloy prepared by melt spinning and extrusion10.1016/j.jallcom.2019.152990 ↗
4. Main directions of recent works on Al-Zn-based alloys for foundry engineering10.1007/s11665-019-04048-5 ↗
5. Characteristics and microstructure of newly designed Al-Zn-based alloys for the die-casting process10.1016/j.jallcom.2016.02.127 ↗
6. Microstructure and mechanical properties of a high-Zn aluminum alloy prepared by melt spinning and extrusion10.1016/j.jallcom.2019.152990 ↗
7. Effect of nickel additions on the mechanical and sliding wear properties of Al–40Zn–3Cu alloy10.1016/j.wear.2009.10.002 ↗
8. Effects of pressure and sliding speed on the friction and wear properties of Al–40Zn–3Cu–2Si alloy: A comparative study with SAE 65 bronze10.1016/j.msea.2008.06.008 ↗
9. Evaluation of microstructure, damping capacity and mechanical properties of Al-35Zn and Al-35Zn-0.5Sc alloys10.1016/j.jallcom.2017.12.234 ↗
10. Effects of Sc addition and rolling on the microstructure and mechanical properties of Al–35Zn alloys10.1016/j.msea.2017.07.042 ↗
11. Effect of copper content on the mechanical and sliding wear properties of monotectoid-based zinc-aluminium-copper alloys10.1016/S0301-679X(03)00113-0 ↗
12. R. Michalik, A. Tomaszewska, H. Woźnica, Influence of casting conditions and alloy additives on the Zn40Al2Cu alloy structure, {IOP} Conf. Ser. Mater. Sci. Eng. 22 (2011) 12010. https://doi.org/10.1088/1757–899x/22/1/012010.10.1088/1757-899X/22/1/012010 ↗
13. Dry sliding wear response of a modified zinc-based alloy10.2320/matertrans1989.38.197 ↗
14. Influence of heat treatment on the wear resistance of the ZnAl40Cu1.5Ti1.5 alloy10.1515/amm-2017-0017 ↗
15. Simultaneously increasing the ductility and strength of nanostructured alloys10.1002/adma.200600310 ↗
16. Recrystallization, precipitation, and resultant mechanical properties of rolled Al–Zn alloy after aging10.1016/j.msea.2016.01.079 ↗
17. Cu-(B4C)p metal matrix composites processed by accumulative roll-bonding10.1016/j.pnsc.2016.11.006 ↗
18. Processing of nanostructured metallic matrix composites by a modified accumulative roll bonding method with structural and mechanical considerations10.1007/s12613-012-0653-8 ↗
19. Strengthening mechanisms in ultrafine grained Al-Mg-Si alloy processed by hydrostatic extrusion – Influence of ageing temperature10.1016/j.msea.2016.05.109 ↗
20. Anisotropic compressive properties of iron subjected to single-pass equal-channel angular pressing10.1080/09500830600847095 ↗
21. Achieving large-area bulk ultrafine grained Cu via submerged multiple-pass friction stir processing10.1016/j.jmst.2013.09.021 ↗
22. Microstructure and mechanical properties of friction stir processed ultrafinegrained and nanostructured Cu-Al alloys
23. Nanostructured aluminium alloys produced by severe plastic deformation: new horizons in development10.1016/j.msea.2012.09.020 ↗
24. Strength, grain refinement and solute nanostructures of an Al–Mg–Si alloy (AA6060) processed by high-pressure torsion10.1016/j.actamat.2013.10.022 ↗
25. Formation of nanograined structure and decomposition of supersaturated solid solution during high pressure torsion of Al-Zn and Al-Mg alloys10.1016/j.actamat.2004.06.006 ↗
26. Softening by severe plastic deformation and hardening by annealing of aluminum–zinc alloy: Significance of elemental and spinodal decompositions10.1016/j.msea.2014.05.026 ↗
27. Ultrafine grained structures resulting from SPD-induced phase transformation in Al-Zn alloys10.1002/adem.201500151 ↗
28. Aluminum-matrix composites reinforced with E-glass fibers by cross accumulative roll bonding process10.1016/j.jallcom.2019.07.022 ↗
29. Structure, wear and corrosion characterizations of Al/20wt% Zn multilayered composites fabricated by cross-accumulative roll bonding10.1016/j.jmapro.2020.05.023 ↗
30. T.B. Massalski, Massalski T.B.-Binary alloy phase diagrams. V2, 1986, 1129.
31. Precipitation behavior and mechanical properties of Al–Zn–Mg alloy with high Zn concentration10.1016/j.jallcom.2020.154005 ↗
32. Characteristics and microstructure of newly designed Al–Zn-based alloys for the die-casting process10.1016/j.jallcom.2016.02.127 ↗
33. Effects of high Zn content on the microstructure and mechanical properties of Al–Zn–Cu gravity-cast alloys10.1016/j.msea.2016.09.022 ↗
34. Microstructure and phase composition of Al-Zn alloys10.1166/jamr.2013.1168 ↗
35. Effects of combined additions of Mn and Zr on dispersoid formation and recrystallization behavior in Al-Zn-Mg alloys10.1007/s11661-019-05368-w ↗
36. Structural changes in aluminum alloys upon severe plastic deformation10.1134/S1063783407050113 ↗
37. Effects of Sc addition and rolling on the microstructure and mechanical properties of Al–35Zn alloys10.1016/j.msea.2017.07.042 ↗
38. Evaluation of microstructure and mechanical properties of Al–Zn alloy during rolling10.1016/j.msea.2015.12.073 ↗
39. Squeeze-cast Al-xZn-3Cu alloys exhibiting high strength, ductility, and wear resistance10.1016/j.msea.2017.02.103 ↗
40. Microstructure and mechanical properties of TiB-containing Al–Zn binary alloys10.1016/j.jmst.2016.04.016 ↗
41. Microstructural evolution and mechanical properties of Al-40 wt%Zn alloy processed by equal-channel angular extrusion10.1016/j.jmatprotec.2008.05.043 ↗
42. Effect of strengthening mechanisms on cold workability and instantaneous strain hardening behavior during grain refinement of AA 6061–10 wt% TiO 2 composite prepared by mechanical alloying10.1016/j.jallcom.2010.07.168 ↗
43. Microstructure and strengthening mechanisms in cold-drawn pearlitic steel wire10.1016/j.actamat.2011.02.017 ↗
44. Strengthening mechanisms on (Cu–10Zn)100−x–x wt% Al2O3 (x = 0, 3, 6, 9 and 12) nanocomposites prepared by mechanical alloying and vacuum hot pressing: influence of reinforcement content10.1007/s12666-017-1054-5 ↗
45. Microstructural evolutions and enhanced mechanical performance of novel Al-Zn die-casting alloys processed by squeezing and hot extrusion10.1016/j.jmatprotec.2021.117063 ↗
46. Effect of grain refinement on tensile properties of cast zinc alloys10.1007/s11661-015-3229-1 ↗
47. The enhanced microhardness in a rapidly solidified Al alloy10.1016/j.msea.2017.03.052 ↗
48. Strength prediction of multi-layered copper-based composites fabricated by accumulative roll bonding10.1016/S1003-6326(21)65611-X ↗
49. Microstructural evolutions and enhanced mechanical performance of novel Al-Zn die-casting alloys processed by squeezing and hot extrusion10.1016/j.jmatprotec.2021.117063 ↗
50. Effect of Zn content on the dynamic softening of Al–Zn–Mg–Cu alloys during hot compression deformation10.1016/j.vacuum.2020.109941 ↗
51. Grain boundary wetting by a solid phase; microstructural development in a Zn–5 wt% Al alloy10.1016/j.actamat.2004.06.011 ↗
52. Microstructural evolution and mechanical strengthening mechanism of the high pressure heat treatment (HPHT) on Al-Mg alloy10.1016/j.jallcom.2016.09.108 ↗
53. Influence of deformation substructure on flow and fracture of fully pearlitic steel10.1016/0001-6160(88)90008-9 ↗
54. Effect of ferrite-pearlite microstructure on structural steel properties10.1007/s11015-012-9619-3 ↗
55. Analysis of strengthening mechanisms in an artificially aged ultrafine grain 6061 aluminum alloy
56. Microstructure and mechanical properties of SiCnp/Al6082 aluminum matrix composites prepared by squeeze casting combined with stir casting10.1016/j.jmatprotec.2020.116699 ↗
57. On the yield and flow stress of lamellar pearlite
58. The effect of interlamellar spacing on strength of pearlite in annealed eutectoid and hypoeutectoid plain carbon steels10.1016/0956-7151(91)90002-I ↗
59. Effect of cooling rate and austenite deformation on hardness and microstructure of 960MPa high strength steel10.1515/secm-2020-0045 ↗
60. Composition and process parameter dependence of yield strength in laser powder bed fusion alloys10.1016/j.matdes.2020.109024 ↗
61. Effects of zinc content on strength and wear performance of Al−12Si−3Cu based alloy10.1016/S1003-6326(19)65154-X ↗
62. Influence of Zn content on the microstructure and mechanical performance of ultrafine-grained Al–Zn alloys processed by high-pressure torsion10.1016/j.matlet.2016.09.114 ↗
63. A new type of wear-resistant material: pseudo-elastic TiNi alloy10.1016/S0043-1648(98)00269-5 ↗
64. Enhancing wear rate of high-density polyethylene (HDPE) by adding ceramic particles to propose an option for artificial hip joint liner10.1088/1757-899X/561/1/012071 ↗