Effect of extrusion temperatures on the microstructures, mechanical properties and thermal properties of PM Al-20Si alloy
Source abstract
Abstract
Al-20Si alloy is fabricated by extruding pre-alloyed powder at different temperatures ranging from 350° to 550°C. Morphologies of the Si phase, mechanical properties and thermal properties of the alloy are influenced by extruding temperature. The alloy extruded at 350 °C mainly contains fine eutectic Si. Although its fine structure imparts high strength to the alloy, it is not stable in high-temperature CTE test and tends to agglomerate into large Si lumps due to Oswald ripening effect, therefore offsetting the restriction effect of Si on the thermal expansion of Al and thus increasing the CTE of the alloy. In contrast, the alloy extruded at 550 °C exhibits primary Si phase, which is large in size and more stable in the CTE test. Moreover, it has in-situ formed amorphous/δ * - Al 2O 3 at the grain boundaries which reduces the CTE of the alloy further. As a result, the alloy fabricated at 550 °C exhibits the best combination of thermal properties (i.e. TC 184.5 Wm −1K −1 and CTE 20.9 ×10 −6 K −1 at 400 ℃).
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Investigation of the influences of heat treatment on the microstructures and thermal properties of Al-20Si alloy fabricated by powder extrusion10.1016/j.matchar.2020.110522 ↗
2. The fabrication of functional gradient hypereutectic Al-Si composites by liquid-solid separation technology10.1016/j.jallcom.2018.05.204 ↗
3. Microstructural characterisation of spray formed Si-30Al for thermal management applications10.1016/j.scriptamat.2006.02.051 ↗
4. Preparation of Al-Si alloys by a rapid solidification and powder metallurgy route10.1016/j.matdes.2015.08.106 ↗
5. Effects of ultrasonic vibration on the iron-containing intermetallic compounds of high silicon aluminum alloy with 2% Fe10.1016/j.jallcom.2009.11.145 ↗
6. The influence of various Mg contents on the microstructures, mechanical properties and thermal expansion behaviors of P‑modified Al-50Si alloys
7. Al2O3 nanoparticles induced simultaneous refinement and modification of primary and eutectic Si particles in hypereutectic Al-20Si alloy10.1016/j.msea.2012.01.131 ↗
8. Jia · Mater. Des. · 2014 · 57 · 58510.1016/j.matdes.2013.12.066 ↗
9. Si phase modification on the elevated temperature mechanical properties of Al-Si hypereutectic alloys10.1016/j.msea.2019.01.119 ↗
10. Effect of high pressure solidification on tensile properties and strengthening mechanisms of Al-20Si10.1016/j.jallcom.2016.07.016 ↗
11. A new insight on induced-tribological behaviour of hypereutectic Al-Si alloys manufactured by selective laser melting10.1016/j.triboint.2019.04.035 ↗
12. Influence of Si content on thermal expansion characteristic of Al-Si alloys10.1080/02670836.2020.1732095 ↗
13. Influence of gating system parameters of die-cast molds on properties of Al-Si castings10.3390/ma14133755 ↗
14. Microstructure evolution and mechanical properties of Al-8wt% Si semi-solid billet fabricated by powder metallurgy liquid phase reaction sintering10.1016/j.msea.2020.140656 ↗
15. Microstructure and properties of Al-60wt%Si composites prepared by powder semi-solid squeeze10.1016/j.powtec.2018.11.011 ↗
16. High-Si reinforced Al matrix composites prepared by powder semi-solid squeeze10.1016/j.jallcom.2017.08.049 ↗
17. High-temperature mechanical properties and thermal cycling stability of Al-50Si alloy for electronic packaging10.1016/j.msea.2018.05.020 ↗
18. Effects of rare earth Er addition on microstructure and mechanical properties of hypereutectic Al-20% Si alloy10.1016/j.msea.2013.09.017 ↗
19. The role of strontium in modifying aluminium–silicon alloys10.1016/j.actamat.2012.03.031 ↗
20. Effect of yttrium addition on the microstructures and mechanical properties of hypereutectic Al-20Si alloy10.1016/j.msea.2018.03.015 ↗
21. Effect of minor scandium addition on the microstructure and properties of Al-50Si alloys for electronic packaging
22. Effect of hot extrusion on wear properties of Al-15 wt% Mg2Si in situ metal matrix composites10.1016/j.matdes.2013.07.084 ↗
23. Tribological characterization of Al7075-graphite composites fabricated by mechanical alloying and hot extrusion10.1016/j.matdes.2014.11.045 ↗
24. Effect of powder microstructure on the thermal and mechanical properties of hot extruded Al-CNT composite
25. Structural characterization of aluminum metastable phases in plasma sprayed deposits10.1016/0254-0584(90)90093-P ↗
26. On the thermal stability of ultrafine-grained Al stabilized by in-situ amorphous Al2O3 network10.1016/j.msea.2015.09.037 ↗
27. Influence of grain boundaries with dispersed nanoscale Al2O3 particles on the strength of Al for a wide range of homologous temperatures10.1016/j.jallcom.2018.09.164 ↗
28. Bulk nanostructured Al-Si alloy with remarkable improvement in strength and ductility10.1016/j.scriptamat.2021.113970 ↗
29. A selective laser melting and solution heat treatment refined Al-12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗