journal article·2020-11

A study of the preparation and properties of dense binderless titanium carbonitride-based ceramics

Xiyue Kang, Yuehui He, Nan Lin, Meimei Zhang, Yan Yan, Jianhua Huang

Publisher page

Abstract

Abstract In this study, the surface oxidation phenomenon of raw powders in the preparation of binderless titanium carbonitride-based ceramics was investigated, which might hinder the densification process. In order to reduce the oxidation and strengthen mutual diffusion, the micrometer-sized powder mixtures of Ti(C,N) and carbides additives, pre-alloyed (Ti,W,Mo,Ta)(C,N) solid solution powders were used. The utilization of solid solution raw powders can reduce the oxidation and promote densification effectively. In this way, the binderless ceramics with high relative density and great mechanical properties were fabricated. The hardness, transverse rapture strength and fracture toughness of materials prepared by solid solution powders were 2030 HV, 1280 MPa and 7.8 MPa m1/2, respectively. Moreover, the obtained binderless titanium carbonitride-based ceramics were found with low friction coefficient, excellent wear and oxidation resistance. The great oxidation resistance was attributed to the formation of rutile-type oxidation products facilitated by the existence of other metal elements in the ceramics.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Design and fabrication of gradient cermet composite cutting tool, and its cutting performance10.1016/j.jallcom.2017.10.187 ↗
2. Microstructure and mechanical properties of Ti(C,N) based cermets reinforced with different ceramic particles processed by spark plasma sintering10.1016/j.ceramint.2017.05.103 ↗
3. Effects of boron addition on the microstructure and mechanical properties of (Ti,Ta)(C,N)-Co based cermets10.3390/met9070787 ↗
4. Enhanced mechanical properties and high temperature oxidation resistance of Ti(C,N)-based cermets containing Zr10.1016/j.jallcom.2019.02.266 ↗
5. Development of Ti(C,N)-based cermets with (Co,Fe,Ni)-based high entropy alloys as binder phase10.1016/j.jallcom.2019.152218 ↗
6. Effect of ultra-fine powders on the microstructure of Ti(C,N)–WC–Ni cermets10.1016/j.actamat.2003.11.021 ↗
7. Microstructure and performance of a cermet material heat-treated in nitrogen10.1016/S1359-6454(00)00212-3 ↗
8. formation of core/rim structures in Ti(C,N)-WC-Ni cermets via a dissolution and precipitation process10.1111/j.1151-2916.2000.tb01415.x ↗
9. Ti(C,N)-based cermets: critical review of achievements and recent developments10.4028/b-FFWx1i ↗
10. Effects of sintering temperature and nano Ti(C,N) on the microstructure and mechanical properties of Ti (C, N) cermets cutting tool materials with low Ni-Co10.1016/j.msea.2017.08.033 ↗
11. Resistance of a binderless cemented carbide to abrasion and particle erosion
12. Ultrafine particle binderless cemented carbide10.1016/0026-0657(92)91549-Y ↗
13. Non-isothermal kinetic of oxidation of tungsten carbide10.1007/s10973-006-8036-x ↗
14. Kinetics of WC-Co oxidation accompanied by swelling10.1007/BF00351615 ↗
15. Spark-plasma-sintering (SPS) of nanostructured titanium carbonitride powders10.1016/j.jeurceramsoc.2004.06.008 ↗
16. Advances in modern nitrogen-containing hardmetals and cermets10.1016/S0263-4368(00)00016-0 ↗
17. High-frequency induction heated sintering of High-energy ball milled TiC0.5N0.5 powders and mechanical properties of the sintered products10.1016/j.ceramint.2012.06.068 ↗
18. Spark plasma sintering of TiCN nanopowders in non-linear heating and loading regimes10.1016/j.jeurceramsoc.2010.11.030 ↗
19. Fabrication of titanium carbonitride based cermets by microwave and spark plasma sintering
20. Microstructure evolution and phase transformation during spark plasma sintering of Ti(C,N)-based cermets10.1016/j.ijrmhm.2007.08.001 ↗
21. Densification and mechanical properties of TiC by SPS-effects of holding time, sintering temperature and pressure condition10.1016/j.jeurceramsoc.2012.04.017 ↗
22. Sintering of binderless TiN and TiCN-based cermet for toughness applications: processing techniques and mechanical properties: a review10.1016/j.ceramint.2019.07.191 ↗
23. NATO science series II: mathematics, physics and chemistry
24. Zgalat-Lozynskyy · 2001 · 161
25. Baraton · 2001
26. Consolidation of binderless WC–TiC by high frequency induction heating sintering10.1016/j.ijrmhm.2007.01.006 ↗
27. Investigation of binderless WC–TiC–Cr3C2 hard materials prepared by spark plasma sintering (SPS)10.1016/j.ijrmhm.2012.12.002 ↗
28. Influence of Mo2C and TaC additions on the microstructure and mechanical properties of Ti (C, N)-based cermets10.1016/j.ceramint.2015.10.168 ↗
29. Bulk ultrafine binderless WC prepared by spark plasma sintering10.1016/j.scriptamat.2005.10.014 ↗
30. Ti (C, N)-based cermets with strengthened interfaces: roles of secondary cubic carbides10.1111/jace.16893 ↗
31. Zhang · 2018 · 9
32. Huang · 2018 · 43
33. Oshida · 2010
34. Surface chemistry of transition metal carbides10.1021/cr0204606 ↗
35. Physicochemical properties of titanium oxynitrides and carbonitrides
36. Solid solution extent of WC and TaC in Ti (C, N) as revealed by lattice parameter increase10.1016/0263-4368(93)90022-8 ↗
37. AES, EELS and XPS characterization of Ti (C,N,O) films prepared by PLD using a Ti target in N2, CH4, O2 and CO as reactive gases10.1016/j.apsusc.2004.03.212 ↗
38. The quantitative analysis of surfaces by XPS: a review10.1002/sia.740020607 ↗
39. NIST-JANAF thermochemical tables
40. An update on the thermodynamics of Ta2O510.1016/j.jct.2008.12.006 ↗
41. Oxidation of TiC at low temperatures10.1007/BF01107214 ↗
42. Oxidation of tungsten carbide powders in air10.1016/j.ijrmhm.2013.05.001 ↗
43. The effect of WC, Mo2C, TaC content on the microstructure and properties of ultra-fine TiC0.7N0.3 cermet10.1016/j.matdes.2006.03.005 ↗
44. Effect of WC content on the microstructure and mechanical properties of (Ti, W)(C, N)–Co cermets10.1016/j.ijrmhm.2007.01.003 ↗
45. Study on the formation of core–rim structure in Ti(C,N)-based cermets10.1016/j.ijrmhm.2012.03.012 ↗
46. Effects of Y2O3 on the densification and fracture toughness of SPS-sintered TiC
47. Effect of SPS process sintering on the microstructure and mechanical properties of nanocrystalline TiC for tools application10.1016/j.ijrmhm.2011.06.013 ↗
48. Rapidly sintering nanosized SiC particle reinforced TiC composites by the spark plasma sintering (SPS) technique10.1023/B:JMSC.0000034145.54280.53 ↗
49. Comparisons of grain size-density trajectory during microwave and conventional sintering of titanium nitride10.1016/j.jallcom.2013.07.159 ↗
50. The effect of ball milling on the mechanical properties of TiN consolidated by pulsed current activated sintering10.1016/j.jallcom.2013.05.060 ↗
51. Spark plasma sintering of titanium nitride in nitrogen: does it affect the sinterability and the mechanical properties?10.1016/j.jeurceramsoc.2017.12.029 ↗
52. Valence-electron structure and properties of main phases in Ti(C, N)-based cermets10.1016/j.matchemphys.2003.07.008 ↗
53. Effects of the ratio of hardness to Young's modulus on the friction and wear behavior of bilayer coatings10.1063/1.1811377 ↗
54. Young modulus dependence of nanoscopic friction coefficient in hard coatings10.1063/1.1609234 ↗
55. Effect of Young's modulus and surface roughness on the inter-particle friction of granular materials10.3390/ma11020217 ↗
56. Influence of WO3 additive on crystallite structural transformation of TiO2 powders10.1016/S1875-5372(10)60099-9 ↗
57. Surface and subsurface oxygen vacancies in anatase TiO2 and differences with rutile10.1103/PhysRevB.79.092101 ↗
58. Influence of nitrogen doping on the defect formation and surface properties of TiO2 rutile and anatase
59. Review of the anatase to rutile phase transformation10.1007/s10853-010-5113-0 ↗
60. Anatase crystal growth and phase transformation to rutile in high-area TiO2, MoO3–TiO2 and other TiO2-supported oxide catalytic systems10.1039/JM9950501245 ↗