Abstract

Abstract We have studied the structural changes of Ti 24 Cr 36 V 40 alloy prepared by arc-melting using positron annihilation spectroscopy and X-ray diffraction (XRD) as functions of the number of hydrogen pressure swing cycles and degassing temperature. As the hydrogen storage capacity decreased with the number of pressure swing cycles, both positron lifetime and XRD peak width increased. Upon hydriding, the crystal structure changed from bcc to bct with increased lattice constants. The increase in positron lifetime is due to the volume expansion caused by hydride formation. After degassing at 500 °C, the hydrogen storage capacity recovered to 95% of the initial level, and the XRD peak width and the lattice constants nearly completely returned to their initial values. However, the positron lifetime was still longer than the initial level suggesting the survival of dislocations. The degradation of hydrogen storage capacity is probably caused by both hydride formation and the generation of dislocations.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Muon and positron interactions and applications · Hydrogen Storage and Materials · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Mori · Int. J. Hydrogen Energy · 2009 · 34 · 456910.1016/j.ijhydene.2008.07.115 ↗
2. Kabutomori · J. Alloys Compd. · 1995 · 231 · 52810.1016/0925-8388(95)01859-X ↗
3. Akiba · Intermetallics · 1998 · 6 · 46110.1016/S0966-9795(97)00088-5 ↗
4. Cho · J. Alloys Compd. · 1999 · 288 · 29410.1016/S0925-8388(99)00096-1 ↗
5. Tominaga · Mater. Trans. JIM · 1999 · 40 · 87110.2320/matertrans1989.40.871 ↗
6. Itoh · J. Alloys Compd. · 2005 · 404–406 · 41710.1016/j.jallcom.2004.12.175 ↗
7. Huang · Mater. Chem. Phys. · 2005 · 93 · 54410.1016/j.matchemphys.2005.04.004 ↗
8. Huang · Intermetallics · 2007 · 15 · 59310.1016/j.intermet.2006.10.035 ↗
9. Arashima · J. Jpn. Inst. Met. · 2006 · 70 · 70910.2320/jinstmet.70.709 ↗
10. Arashima · J. Alloys Compd. · 2003 · 356–357 · 40510.1016/S0925-8388(03)00363-3 ↗
11. Washio · J. Jpn. Inst. Met. · 2007 · 71 · 52210.2320/jinstmet.71.522 ↗
12. Singh · Int. J. Hydrogen Energy · 2007 · 32 · 496110.1016/j.ijhydene.2007.07.010 ↗
13. Santos · J. Metastable Nanocryst. Mater. · 2004 · 20–21 · 29110.4028/www.scientific.net/JMNM.20-21.291 ↗
14. Ho · J. Alloys Compd. · 1993 · 202 · 2310.1016/0925-8388(93)90511-K ↗
15. Mazzolai · J. Alloys Compd. · 2008 · 466 · 13310.1016/j.jallcom.2007.11.040 ↗
16. Fukai · Jpn. J. Appl. Phys. · 1993 · 32 · L125610.1143/JJAP.32.L1256 ↗
17. Shirai · J. Alloys Compd. · 2002 · 330–332 · 12510.1016/S0925-8388(01)01635-8 ↗
18. Mizuno · J. Alloys Compd. · 2003 · 356–357 · 18610.1016/S0925-8388(02)01229-X ↗
19. Čížek · Phys. Rev. B · 2004 · 69 · 22410610.1103/PhysRevB.69.224106 ↗
20. Čížek · J. Alloys Compd. · 2007 · 446–447 · 47910.1016/j.jallcom.2006.11.105 ↗
21. P. Kirkegaard, N.J. Pederson, M. Eldrup, PATFIT-88, Riso-M-2704 (1989).
22. Puska · Rev. Mod. Phys. · 1994 · 66 · 84110.1103/RevModPhys.66.841 ↗
23. Borónski · Phys. Rev. B · 1986 · 34 · 382010.1103/PhysRevB.34.3820 ↗
24. Nakamura · J. Alloys Compd. · 2001 · 316 · 28410.1016/S0925-8388(00)01503-6 ↗
25. Kubo · 2004
26. Blöchl · Phys. Rev. B · 1994 · 50 · 1795310.1103/PhysRevB.50.17953 ↗
27. Gonze · Comput. Mater. Sci. · 2002 · 25 · 47810.1016/S0927-0256(02)00325-7 ↗
28. Holzwarth · Comput. Phys. Commun. · 2001 · 135 · 32910.1016/S0010-4655(00)00244-7 ↗
29. Clementi · At. Data Nucl. Data Tables · 1974 · 14 · 17710.1016/S0092-640X(74)80016-1 ↗
30. Shirai · Mater. Sci. Forum · 1992 · 105–110 · 122510.4028/www.scientific.net/MSF.105-110.1225 ↗
31. Kamimura · Phys. Rev. B · 1995 · 52 · 87910.1103/PhysRevB.52.879 ↗