Abstract

In order to solve or suppress the problem of macro segregation of Fe phase of Cu-Fe alloy in the traditional casting process, we successfully prepared Cu-10Fe alloy prefabricated slabs with homogeneous and fine microstructure by spray deposition and achieved high strength Cu-10Fe alloy thin strips by subsequent cryorolling. Cryorolling was carried out at different reductions to investigate the relationship between microstructure evolution and mechanical properties. The results show that the spray deposited alloys have good plasticity and low temperature workability. As the reduction increased, the Fe phase becomes more fibrous and the average grain size of the alloy is refined to 0.35 μm. The {112}<111> texture was gradually transformed into a stabilized {110}<112> texture during cryorolling suggested that the low temperature suppressed cross-slip and improved the strength of the alloy. The mechanical properties of the alloys improved significantly after cryorolling is mainly attributed to the significant grain refinement, dislocation accumulation and the presence of ultrafine grains during the cryorolling process. The successful development of thin strips of Cu-Fe alloy with uniform distribution of Fe phase and high strength provides a new idea for the preparation of thin strips of immiscible alloys such as Cu-Fe alloy.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Attaining exceptional electrical conductivity in Cu-Fe composite by powder rolling strategy10.1016/j.scriptamat.2023.115302 ↗
2. Dramatically enhanced combination of ultimate tensile strength and electric conductivity of alloys via machine learning screening10.1016/j.actamat.2020.09.068 ↗
3. Composition design, phase transition and fabrication of copper alloys with high strength and electrical conductivity
4. Advances on high strength and high conductivity Cu-Ag materials
5. The roles of Hf element in optimizing strength, ductility and electrical conductivity of copper alloys10.1016/j.msea.2019.04.110 ↗
6. Microstructure and properties of high strength, high conductivity and magnetic Cu-10Fe-0.4Si alloy10.1016/j.msea.2021.142012 ↗
7. Microstructure and mechanical properties of a Cu-Fe-Nb alloy with a high product of the strength times the elongation
8. Managing mechanical and electrical properties of nanostructured Cu-Fe composite by aging treatment10.1016/j.matchar.2022.112600 ↗
9. Microstructure evolution and deformation behaviour of Cu-10 wt% Fe alloy during cold rolling10.1016/j.msea.2020.140379 ↗
10. Study on high-strength and high-conductivity Cu-Fe-P alloys10.1016/j.msea.2006.01.068 ↗
11. Microstructure and properties of Cu-Fe alloys fabricated via powder metallurgy and rolling10.1080/00325899.2021.1890403 ↗
12. Effect of composition and powder size on magnetic properties of rapidly solidified copper-iron alloys10.1016/j.jallcom.2018.01.245 ↗
13. Influence of minor Ag addition on the microstructure and properties of powder metallurgy Cu-10wt% Fe alloy10.1016/j.jallcom.2022.163983 ↗
14. Liquid immiscibility in copper-iron and copper-cobalt systems in the supercooled state10.1016/0001-6160(58)90061-0 ↗
15. Novel insight into evolution mechanism of second liquid-liquid phase separation in metastable immiscible Cu-Fe alloy10.1016/j.matdes.2018.06.044 ↗
16. Effect of Fe content on microstructure and mechanical properties of Cu-Fe-based composite coatings by laser induction hybrid rapid cladding10.1016/S1003-6326(16)64452-7 ↗
17. Effect of Zr addition on metastable liquid-liquid phase separation of Cu-Fe alloys10.1016/j.scriptamat.2021.114218 ↗
18. Microstructure and properties of Cu-10 wt% Fe alloy produced by double melt mixed casting and multistage thermomechanical treatment10.1016/j.jallcom.2019.153323 ↗
19. Effects of Fe content on microstructure and properties of Cu-Fe alloy10.1016/S1003-6326(21)65713-8 ↗
20. Study of microstructure evolution and properties of Cu-Fe microcomposites produced by a pre-alloyed powder method10.1016/j.matdes.2017.04.017 ↗
21. Microstructure and properties evolution of rolled powder metallurgy Cu-30Fe
22. Influence of Fe content on microstructure and performance of powder metallurgy Cu-Fe alloys, Trans. Nonferrous Metals Soc
23. Effect of lattice strain on the electrical conductivity of rapidly solidified copper-iron metastable alloys10.1016/j.jallcom.2017.10.180 ↗
24. Deformation behavior of heterogeneous lamellar Cu-Fe-P immiscible alloys with enhanced strength and ductility produced by laser powder bed fusion10.1016/j.jallcom.2023.172675 ↗
25. High-temperature oxidation behavior of Cu-Fe-based immiscible alloy produced by laser powder bed fusion
26. Achieving homogeneous Fe distribution and high strength in Cu-Fe composite consolidated by powder rolling10.1016/j.msea.2023.145563 ↗
27. A comparative study of metastable phase separation for undercooled liquid Fe35Cu65 alloy under natural and forced cooling conditions10.1016/j.jallcom.2022.167079 ↗
28. Development of a new class of high strength copper alloy using immiscibility route in Cu-Fe-Si system: evolution of hierarchical multi-scale microstructure10.1016/j.msea.2018.03.026 ↗
29. Microstructure and mechanical properties of multi-scale α-Fe reinforced Cu-Fe composite produced by vacuum suction casting10.1016/j.msea.2023.144603 ↗
30. Coordinated deformation behavior of Cu-10wt%FeC alloys through controlling structure morphology and distribution of Fe-C phases10.1016/j.jmrt.2022.12.020 ↗
31. High strength and high electrical conductivity in Cu-Fe alloys with nano and micro Fe particles10.1016/j.msea.2022.143948 ↗
32. Bulk nanostructured materials from severe plastic deformation10.1016/S0079-6425(99)00007-9 ↗
33. Structure of Cu deformed by high pressure torsion10.1016/j.actamat.2004.09.043 ↗
34. Evolution of microstructure and mechanical properties in Cu-14%Fe alloy during severe cold rolling10.1016/j.msea.2012.11.121 ↗
35. Thermal stability, microstructure evolution and grain growth kinetics of ultrafine grained Al 7075 alloy processed by cryogenic temperature extrusion machining10.1016/j.jallcom.2023.169900 ↗
36. Microstructural evolution in an Al-6061 alloy processed by high-pressure torsion10.1016/j.msea.2010.04.027 ↗
37. An alternative method for manufacturing high- strength CP Ti-SiC composites by accumulative roll bonding process10.1016/j.matdes.2014.03.040 ↗
38. Solid-state alloying of Al-Mg alloys by accumulative roll-bonding: microstructure and properties
39. High strength and toughness of Ti-6Al-4V sheets via cryorolling and short-period annealing10.1016/j.msea.2022.143766 ↗
40. Effect of annealing on microstructure and tensile properties of skew hot rolled Ti-6Al-3Nb-2Zr-1Mo alloy tube10.1016/j.msea.2019.138346 ↗
41. High tensile strength-ductility combination in cold multiaxial plane-strain forged and rolled nanostructured Titanium10.1016/j.mtla.2020.100698 ↗
42. High tensile ductility in a nanostructured metal10.1038/nature01133 ↗
43. Recent developments in flat rolling technologies
44. Enhancement in strength and ductility of Al-Mg-Si alloy by cryorolling followed by warm rolling10.1016/j.proeng.2013.11.027 ↗
45. Sandwich-like Cu/Al/Cu composites fabricated by cryorolling10.1002/adem.202000122 ↗
46. High strength and high electrical conductivity CuMg alloy prepared by cryorolling10.1016/S1003-6326(19)64968-X ↗
47. Optimization of the balance between high strength and high electrical conductivity in CuCrZr alloys through two-step cryorolling and aging10.1016/j.jallcom.2018.09.040 ↗
48. Effect of cryorolling on microstructure and property of high strength and high conductivity Cu-0.5wt%Cr alloy10.1016/S1003-6326(20)65393-6 ↗
49. Texture evolution and recrystallization behaviors of Cu-Ag alloys subjected to cryogenic rolling10.1016/S1003-6326(15)63921-8 ↗
50. Observations on the effect of a magnetic field on the annealing texture and microstructure evolution in zirconium10.1016/j.actamat.2010.02.027 ↗
51. Electroplasticity in the Al0.6CoCrFeNiMn high entropy alloy subjectedto electrically-assisted uniaxial tension10.1016/j.jmst.2022.11.031 ↗
52. Mechanism based strain gradient plasticity-I. Theory10.1016/S0022-5096(98)00103-3 ↗
53. Plastic strain partitioning in dual phase Al13CoCrFeNi high entropy alloy10.1016/j.msea.2018.02.044 ↗
54. Special rolling techniques for improvement of mechanical properties of ultrafine-grained metal sheets: a review10.1002/adem.201500369 ↗
55. Reinforcement size dependence of mechanical properties and strengthening mechanisms in diamond reinforced titanium metal matrix composites10.1016/j.compositesb.2018.12.014 ↗
56. Examination of inverse Hall-Petch relation in nanostructured aluminum alloys by ultra-severe plastic deformation10.1016/j.jmst.2021.01.096 ↗
57. Mechanical properties of Al-Mg-Si alloy sheets produced using asymmetric cryorolling and ageing treatment10.1016/j.msea.2013.01.048 ↗
58. Enhancing the comprehensive properties of as-cast Cu-Ni-Si alloys by continuous extrusion combined with subsequent thermomechanical treatment10.1016/j.matdes.2022.111033 ↗
59. Relationship and mechanism between double cold rolling-aging process, microstructure and properties of Cu-Ni-Si alloy prepared by two-phase zone continuous casting10.1016/j.msea.2020.140148 ↗
60. Effects of cryogenic treatment on microstructure and mechanical properties of AZ31 magnesium alloy rolled at different paths
61. Effect of cold rolling on microstructure and mechanical properties of a Cu-Zn-Sn-Ni-Co-Si alloy for interconnecting devices
62. Homogeneous Cu-Fe supersaturated solid solutions prepared by severe plastic deformation10.1080/14786430903313682 ↗