journal article·2024-05

Defect-based fatigue crack nucleation and strength evaluation of additively manufactured TiC/Ti6Al4V titanium matrix composite at different temperatures

Cheng Li, Wei Li, Chuanwen Sun, Muhammad Imran Lashari

Publisher page

Abstract

In mechanical applications, defect-based fatigue cracking is a significant strength-limiting failure mode of additively manufactured composites that is not yet fully understood in the service environment. In this paper, axial loading tests were carried out at 25 ℃ and 450 ℃, and then the effects of temperature on the long-life fatigue properties of the TiC-reinforced Ti6Al4V composite fabricated by Laser Powder Bed Fusion (LPBF) were investigated by combining the techniques of electron backscatter diffraction, X-ray computed tomography, and 3D morphological reconstruction. With the increase in temperature, the fatigue strength of the LPBF TiC/Ti6Al4V composite decreases significantly. The main causes of the interior failure at both temperatures are the inhomogeneous hardening zone (IHZ) formed by TiC agglomeration and the pore defect generated during the manufacturing process. The presence of brittle IHZ and pores causes stress concentration, which leads to crack nucleation. When a crack reaches the specimen surface, the combined effects of temperature and oxygen accelerate the ensuing crack propagation at high temperature. Based on the temperature effect, material properties, and the statistical distribution of defects, a model has been developed to predict the P-S-N curves at both temperatures. This model performed well in estimating the fatigue strength at 10 9 cycles. These findings provide new insights into the defect-related fatigue failure mechanisms and strength evaluation of the LPBF TiC/Ti6Al4V composite at different temperatures.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Recent developments and opportunities in additive manufacturing of titanium-based matrix composites: A review10.1016/j.ijmachtools.2018.06.003 ↗
2. Effects of heat accumulation on microstructure and mechanical properties of Ti6Al4V alloy deposited by wire arc additive manufacturing
3. Titanium Metal Matrix Composites: An Overview10.1016/j.compositesa.2019.04.005 ↗
4. Machinability of titanium alloys (Ti6Al4V and Ti555.3)10.1016/j.jmatprotec.2008.06.020 ↗
5. Complexion-mediated martensitic phase transformation in Titanium10.1038/ncomms14210 ↗
6. On the microstructure, mechanical properties and wear resistance of an additively manufactured Ti64/metallic glass composite
7. Microstructure and properties of functionally graded materials Ti6Al4V/TiC fabricated by direct laser deposition10.1108/RPJ-12-2016-0215 ↗
8. Graphene-TiC hybrid reinforced titanium matrix composites with 3D network architecture: Fabrication, microstructure and mechanical properties10.1016/j.jallcom.2020.157777 ↗
9. Fabrication and mechanical properties of in situ TiC/Ti metal matrix composites10.1016/j.jallcom.2010.12.086 ↗
10. High Temperature Mechanical Properties of Aeronautical TC4 Titanium Alloy, Hot
11. Deformation behavior and softening mechanism of TiB reinforced near-α titanium matrix composite during hot compression10.1016/j.jmrt.2020.09.030 ↗
12. High-mass-proportion TiCp/Ti6Al4V titanium matrix composites prepared by directed energy deposition
13. Effect of composition and sintering temperature on mechanical properties of ZrO2 particulate-reinforced titanium-matrix composite10.1016/S1003-6326(11)61397-6 ↗
14. Production and mechanical properties of nano SiC particle reinforced Ti-6Al-4V matrix composite10.1016/S1003-6326(17)60009-8 ↗
15. Influence of matrix characteristics on tensile properties of in situ synthesized TiC/TA15 composite10.1016/j.msea.2012.05.092 ↗
16. The influences of melting degree of TiC reinforcements on microstructure and mechanical properties of laser direct deposited Ti6Al4V-TiC composites10.1016/j.matdes.2017.09.063 ↗
17. Preparation and Mechanical Properties of Particulate-Reinforced Powder Metallurgy Titanium Matrix Composites10.1007/s11661-007-9329-9 ↗
18. Microstructure and mechanical properties of TiC/Ti–6Al–4V composites processed by in situ casting route10.1179/026708310X12699498462922 ↗
19. Influence of spark plasma sintering and subsequent hot rolling on microstructure and flexural behavior of in-situ TiB and TiC reinforced Ti6Al4V composite10.1016/j.msea.2014.11.036 ↗
20. On the current research progress of metallic materials fabricated by laser powder bed fusion process: a review10.1016/j.jmrt.2022.07.085 ↗
21. Additive Manufacturing Techniques in Manufacturing -An Overview10.1016/j.matpr.2017.11.642 ↗
22. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
23. Microstructural characterization and comparison of Ti-6Al-4V manufactured with different additive manufacturing processes10.1016/j.matchar.2018.02.003 ↗
24. Selective Laser Melting of in-situ TiC/Ti5Si3 composites with novel reinforcement architecture and elevated performance10.1016/j.surfcoat.2010.11.051 ↗
25. Microstructural Evolution, Mechanical and Tribological Properties of TiC/Ti6Al4V Composites with Unique Microstructure Prepared by SLM10.1016/j.msea.2021.141187 ↗
26. In situ transformations during SLM of an ultra-strong TiC reinforced Ti composite10.1038/s41598-020-67434-3 ↗
27. Heat treatment possibilities for an in situ βTi-TiC composite made by laser powder bed fusion
28. Microstructure and high temperature-mechanical properties of TiC/graphene/Ti6Al4V composite formed by laser powder bed fusion10.3390/met13010163 ↗
29. Laser powder bed fusion additive manufacturing, microstructure evolution, and mechanical performance of carbon nanotube-decorated titanium alloy powders10.1016/j.powtec.2020.12.066 ↗
30. Faceted crack induced failure behavior and micro-crack growth based strength evaluation of titanium alloys under very high cycle fatigue10.1016/j.ijfatigue.2019.105369 ↗
31. In Situ Scanning Electron Microscopy Observations of Tensile Deformation in a Boron-Modified Ti-6Al-4V Alloy10.1016/j.scriptamat.2006.05.008 ↗
32. Enhanced Fatigue Crack Growth Resistance at Elevated Temperature in TiC/Ti-6Al-4V Composite
33. Thermomechanical Properties of P/M β Titanium Metal Matrix Composite10.1016/S0921-5093(97)00813-7 ↗
34. Prediction of fatigue limit in additively manufactured Ti-6Al-4V alloy at elevated temperature10.1016/j.ijfatigue.2019.04.025 ↗
35. Tensile and very high cycle fatigue behaviors of a compressor blade titanium alloy at room and high temperatures10.1016/j.msea.2021.141049 ↗
36. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
37. Grain morphology evolution behavior of titanium alloy components during laser melting deposition additive manufacturing10.1016/j.jallcom.2015.01.256 ↗
38. Fracture and Fatigue in Additively Manufactured Metals10.1016/j.actamat.2021.117240 ↗
39. Defects in Additive Manufactured Metals and Their Effect on Fatigue Performance: A State-of-the-Art Review
40. Additive manufacturing of Ti6Al4V alloy: A review10.1016/j.matdes.2018.107552 ↗
41. 3D quantitative analysis of graphite morphology in high strength cast iron by high-energy X-ray tomography10.1016/j.scriptamat.2015.03.017 ↗
42. Analysis of the mechanism of Superlong fatigue failure by optical microscope and SEM/AFM observations
43. Subsurface facets-induced crack nucleation behavior and microstructure-based strength evaluation of titanium alloys in ultra-long life regime10.1016/j.msea.2019.138055 ↗
44. Quantitative evaluation of effects of non-metallic inclusions on fatigue strength of high strength steels. I: Basic fatigue mechanism and evaluation of correlation between the fatigue fracture stress and the size and location of non-metallic inclusions10.1016/0142-1123(89)90054-6 ↗
45. Factors influencing the mechanism of superlong fatigue failure in steels10.1046/j.1460-2695.1999.00187.x ↗
46. An unusual fatigue phenomenon: duality of the S-N fatigue curve in the beta-titanium alloy Ti-10V–2Fe-3Al10.1016/S1359-6462(02)00565-1 ↗
47. Refined microstructure and enhanced wear resistance of titanium matrix composites produced by selective laser melting10.1016/j.optlastec.2020.106644 ↗
48. The Behavior of Crack Initiation and Early Growth in High-Cycle and Very-High-Cycle Fatigue Regimes for a Titanium Alloy10.1016/j.ijfatigue.2018.03.021 ↗
49. Effects of stress ratio on high-cycle and very-high-cycle fatigue behavior of a Ti–6Al–4V alloy
50. Microstructure based cracking behavior and life assessment of titanium alloy under very-high-cycle fatigue with elevated temperatures10.1016/j.ijfatigue.2022.106914 ↗
51. S-N curves in the very-high-cycle fatigue regime: Statistical modeling based on the hydrogen embrittlement consideration10.1111/ffe.12431 ↗
52. Gigacycle fatigue of ferrous alloys10.1046/j.1460-2695.1999.t01-1-00185.x ↗
53. Prediction of the S–N curves of high-strength steels in the very high cycle fatigue regime10.1016/j.ijfatigue.2010.02.006 ↗
54. Dominant factors for very-high-cycle fatigue of high-strength steels and a new design method for components10.1111/ffe.12331 ↗