journal article·2023-09

Effect of strain-induced melt activation process and thixoforming on microstructure and mechanical properties of 319 aluminum alloy

Z. Delbari Ragheb, S.G. Shabestari, Y. Najafi

Publisher page

Abstract

The effect of the thixoforming process on the microstructure and mechanical properties of modified and grain refined 319 aluminum alloy has been investigated. The strain-induced melt activated (SIMA) process has been applied to achieve proper microstructure for semi-solid processing. As-cast 319 aluminum parts have a dendritic microstructure and mostly contain defects such as porosity and shrinkage. The semi-solid treatment process eliminates these defects and is used to obtain a spherical structure with enhanced mechanical properties. Image analysis of the semi-solid treated specimens showed that the best sample had the highest amount of α-Al particle sphericity (0.88) and the lowest average equivalent diameter of α-Al phases (56 µm) under the conditions of 30% of the hot pre-deformation at 560 °C and isothermal holding time of 30 min. The specimens were thixoformed after the SIMA process to generate near-net-shape pieces. The thixoforming process enhanced the hardness of 319 aluminum alloy from 78.1 ± 1.91 HB to 115.6 ± 1.73 HB. Based on the tensile test results, the thixoforming process raised the ultimate tensile strength, yield strength, elongation, and toughness by 30%, 69%, 180.5%, and 189%, respectively, compared to the as-cast state.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Cluster-assisted nucleation of silicon phase in hypoeutectic Al-Si alloy with further inoculation10.1016/j.actamat.2014.01.061 ↗
2. Analysis of the solidification characteristics of a 319 type Al alloy using in-situ neutron diffraction10.1016/j.jallcom.2016.11.175 ↗
3. Enhanced mechanical properties of Al-Si–Cu–Mg(-Fe) alloys by a deformation-semisolid extrusion process10.1016/j.msea.2021.141667 ↗
4. Novel high strength Al-10.5Si-3.4Cu-0.2Mg alloy produced through two-stage solution heat treatment10.1016/S1003-6326(21)65520-6 ↗
5. Microstructure and mechanical properties of thixoformed A319 aluminum alloy10.1016/j.matdes.2014.07.014 ↗
6. Mechanical properties and microstructures of a modified Al-Si-Cu alloy prepared by thixoforming process for automotive connecting rods10.1016/j.jmrt.2020.12.085 ↗
7. Effects of solution heat treatment time on the as-quenched microstructure, hardness and electrical conductivity of B319 aluminum alloy10.1016/j.jallcom.2020.155577 ↗
8. The combined effects of Sr additions and heat treatment on the microstructure and mechanical properties of high-pressure die-cast A383 alloy10.1016/j.msea.2019.04.042 ↗
9. Effect of P and Sr complex modification on Si phase in hypereutectic Al–30Si alloys10.1016/j.matdes.2012.12.054 ↗
10. Effect of Al-5Ti-1B and Zr grain refiners on the solidification characteristics and microstructure of Al-6Mg alloy studied through thermal analysis10.1016/j.tca.2022.179200 ↗
11. Evolution of secondary phase particles during deformation of Al-5Ti-1B master alloy and their effect on α-Al grain refinement10.1016/j.jmst.2018.04.018 ↗
12. Grain size prediction and investigation of 7055 aluminum alloy inoculated by Al-5Ti-1B master alloy10.1016/j.jallcom.2019.153504 ↗
13. The influence of Al-10Sr or/and Al-5Ti-1B on microstructure and mechanical properties of Al-12Si-4Cu-2Ni-0.8 Mg alloys10.1016/j.jallcom.2019.151856 ↗
14. Microstructural evolution during semisolid processing of Al-Si-Cu alloy with different Mg contents10.1016/S1003-6326(17)60169-9 ↗
15. Microstructure and properties of semi-solid aluminum alloys: a literature review10.3390/met8030181 ↗
16. The effects of Mg addition on the microstructure and mechanical properties of thixoformed Al-5% Si-Cu alloys10.1016/j.jallcom.2014.09.152 ↗
17. Evaluation of the microstructure and dry sliding wear behaviour of thixoformed A319 aluminum alloy10.1016/j.matdes.2015.03.057 ↗
18. Microstructure evolution and semi-solid deformation behavior of an A356 aluminum alloy processed by strain induced melt activated method10.1016/j.matdes.2012.10.041 ↗
19. Effects of SIMA (Strain Induced Melt Activation) on microstructure and electrochemical behavior of Al-Zn-In sacrificial anodes10.1016/j.jallcom.2017.09.316 ↗
20. Effect of semi-solid forming on the microstructure and mechanical properties of the iron containing Al-Si alloys10.1016/j.jallcom.2011.05.052 ↗
21. The effect of deformation ratio and heat treatment time on the microstructure and mechanical properties of A356 aluminium alloy during SIMA process
22. Effect of thixoforming and precipitation hardening on microstructure and mechanical properties of Al-10.5Si-3Cu-0.2Mg alloy produced by strain induced melt activation process10.1016/j.jmrt.2021.10.086 ↗
23. Thermomechanical Processing of metal feedstock for semisolid forming: a review10.1007/s11663-018-1387-4 ↗
24. N.H. Husain, A.H. Ahmad, M.M. Rashidi, An overview of thixoforming process, in IOP Conference Series: Mater. Sci. Eng, 2017, vol. 257, p. 12053, DOI: 10.1088/1757–899X/257/1/012053.10.1088/1757-899X/257/1/012053 ↗
25. Microstructural evolution and mechanical properties of thixoformed A319 alloys containing variable amounts of magnesium10.1016/S1003-6326(16)64321-2 ↗
26. Assessment of the microstructure and solidification characteristics of al–20% Mg2Si composite under melt superheating treatment using thermal analysis
27. Assessment of modification and formation of intermetallic compounds in aluminum alloy using thermal analysis10.1016/j.msea.2007.05.022 ↗
28. Effect of isothermal process parameters on semi-solid microstructure of chip-based Al-Cu-Mn-Ti alloy prepared by SIMA method10.1142/S0217984920503856 ↗
29. Effect of plastic deformation and semisolid forming on iron–manganese rich intermetallics in Al–8Si–3Cu–4Fe–2Mn alloy10.1016/j.jallcom.2010.08.043 ↗
30. Microstructural evolution, dislocation density and tensile properties of Al–6.5Si–2.1Cu–0.35Mg alloy produced by different casting processes10.1016/j.jmst.2021.02.074 ↗