Hard yet tough thermodynamics-driven nanostructured (AlCrNbSixTi)N multicomponent nitride hard coating
Source abstract
Abstract
Breaking the hardness-toughness trade-off has always been a critical issue for hard protective coatings. Rational materials design, which simultaneously incorporate multiple strengthening and toughening mechanisms, could provide pathways toward hard yet tough materials. In this study, (AlCrNbSi x Ti)N multicomponent nitride coatings with various Si content are fabricated via magnetron co-sputtering. Multi-dimensional strengthening and toughening mechanisms are found in thermodynamics-driven nanostructured (AlCrNbSi x Ti)N. Enhanced atomic packing, nanostructure formation, and microstructural modification originate from spinodal decomposition contribute to multiple strengthening and toughening mechanisms after Si incorporation. From atomic-level packing, spinodal-decomposed nanostructure, to microstructure, the evolutions are quantitatively characterized and correlated to mechanical properties. With the addition of 4.4 at% of Si, maximum hardness of 27.2 GPa is achieved while maintains high fracture toughness of 3.66±0.37MPa\sqrt{m}. On the other hand, the maximum fracture toughness is found for (AlCrNbSi 7.6 Ti)N and is attributed to the featureless microstructure, nanostructure formation and non-complete amorphization.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Boron and Carbon Nanomaterials Research · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. Toward hard yet tough ceramic coatings10.1016/j.surfcoat.2014.07.007 ↗
2. Toughening of hard nanostructural thin films: a critical review10.1016/j.surfcoat.2004.10.020 ↗
3. Hard yet tough nanocomposite coatings–present status and future trends10.1002/ppap.200600179 ↗
4. Supertoughening in B1 transition metal nitride alloys by increased valence electron concentration10.1016/j.actamat.2010.12.013 ↗
5. Electronic mechanism for toughness enhancement in Ti x M 1− x N (M= Mo and W)10.1103/PhysRevB.81.104107 ↗
6. Valence electron concentration as an indicator for mechanical properties in rocksalt structure nitrides, carbides and carbonitrides10.1016/j.actamat.2018.04.033 ↗
7. Microstructure and properties of spark plasma‐sintered ZrO2–ZrB2 nanoceramic composites10.1111/j.1551-2916.2006.01083.x ↗
8. Tuning hardness and fracture resistance of ZrN/Zr0. 63Al0. 37N nanoscale multilayers by stress-induced transformation toughening10.1016/j.actamat.2015.01.066 ↗
9. Effects of structure and interfaces on fracture toughness of CrN/AlN multilayer coatings10.1016/j.scriptamat.2013.01.039 ↗
10. Grain boundary design of thin films: using tilted brittle interfaces for multiple crack deflection toughening10.1016/j.actamat.2016.09.027 ↗
11. High temperature fracture toughness of ceramic coatings evaluated using micro-pillar splitting10.1016/j.scriptamat.2018.11.013 ↗
12. High temperature fracture toughness of single-layer CrAlN and CrAlSiN hard coatings10.1016/j.surfcoat.2021.126909 ↗
13. The influence of Ni concentration on the structure, mechanical and tribological properties of Ni–CrSiN coatings in seawater10.1016/j.jallcom.2019.152998 ↗
14. Fracture mechanisms in nanoscale layered hard thin films10.1016/S0040-6090(02)00944-6 ↗
15. Schier, Multilayer PVD coatings for wear protection10.1016/0257-8972(95)02555-3 ↗
16. Hard yet tough CrN/Si3N4 multilayer coatings deposited by the combined deep oscillation magnetron sputtering and pulsed dc magnetron sputtering10.1016/j.apsusc.2019.144168 ↗
17. On the spinodal nature of the phase segregation and formation of stable nanostructure in the Ti–Si–N system10.1016/j.msea.2006.03.017 ↗
18. The formation and role of interfaces in superhard nc-MenN/a-Si3N4 nanocomposites10.1016/j.surfcoat.2006.08.112 ↗
19. Composition, nanostructure and origin of the ultrahardness in nc-TiN/a-Si3N4/a-and nc-TiSi2 nanocomposites with HV= 80 to≥ 105 GPa10.1016/S0257-8972(00)00957-9 ↗
20. The search for novel, superhard materials10.1116/1.581977 ↗
21. Understanding why the thinnest SiN x interface in transition-metal nitrides is stronger than the ideal bulk crystal10.1103/PhysRevB.81.245418 ↗
22. Nanostructured high‐entropy alloys with multiple principal elements: novel alloy design concepts and outcomes10.1002/adem.200300567 ↗
23. Microstructural development in equiatomic multicomponent alloys10.1016/j.msea.2003.10.257 ↗
24. Microstructure, physical and chemical properties of nanostructured (Ti–Hf–Zr–V–Nb) N coatings under different deposition conditions10.1016/j.matchemphys.2014.06.062 ↗
25. Structure and properties of two Al–Cr–Nb–Si–Ti high-entropy nitride coatings10.1016/j.surfcoat.2013.01.036 ↗
26. Combinatorial synthesis of reactively co-sputtered high entropy nitride (HfNbTiVZr) N coatings: microstructure and mechanical properties10.1016/j.surfcoat.2022.128564 ↗
27. Effects of silicon content on the structure and mechanical properties of (AlCrTaTiZr)–Six–N coatings by reactive RF magnetron sputtering10.1088/0022-3727/44/20/205405 ↗
28. Structure and properties of duodenary (TiVCrZrNbMoHfTaWAlSi) N coatings by reactive magnetron sputtering10.1016/j.matchemphys.2018.08.068 ↗
29. Oxidation behavior of Al-Cr-Nb-Si-Zr high entropy nitride thin films at 850° C10.1016/j.corsci.2021.109467 ↗
30. Superior oxidation resistance of (Al0. 34Cr0. 22Nb0. 11Si0. 11Ti0. 22) 50N50 high-entropy nitride10.1149/2.028311jes ↗
31. Mechanical properties and thermal stability of reactively sputtered multi-principal-metal Hf-Ta-Ti-V-Zr nitrides10.1016/j.surfcoat.2020.125674 ↗
32. Inhibition of grain coarsening up to 1000C in (AlCrNbSiTiV) N superhard coatings10.1016/j.scriptamat.2009.09.015 ↗
33. Lattice distortion or cocktail effect dominates the performance of Tantalum-based high-entropy nitride coatings10.1016/j.apsusc.2021.151894 ↗
34. Effects of nitrogen content on structure and mechanical properties of multi-element (AlCrNbSiTiV) N coating10.1016/j.surfcoat.2009.01.016 ↗
35. Improvement of high entropy alloy nitride coatings (AlCrNbSiTiMo) N on mechanical and high temperature tribological properties by tuning substrate bias10.1016/j.surfcoat.2020.126247 ↗
36. Improving the hardness of high entropy nitride (Cr0. 35Al0. 25Nb0. 12Si0. 08V0. 20) N coatings via tuning substrate temperature and bias for anti-wear applications10.1016/j.surfcoat.2020.126417 ↗
37. Effects of silicon content on the structure and properties of (AlCrMoTaTi) N coatings by reactive magnetron sputtering10.1016/j.jallcom.2014.07.095 ↗
38. Structure and mechanical properties of multi-principal-element (AlCrNbSiTi) N hard coating10.1016/j.surfcoat.2022.128113 ↗
39. Surface studies of solids by total reflection of X-rays10.1103/PhysRev.95.359 ↗
40. X-ray interactions: photoabsorption, scattering, transmission, and reflection at E = 50-30,000 eV, Z = 1-9210.1006/adnd.1993.1013 ↗
41. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
42. Structural and elastic properties of cubic and hexagonal TiN and AlN from first-principles calculations10.1016/j.commatsci.2010.03.014 ↗
43. Structural, electronic and mechanical properties of CrN: A first principles study10.1142/S0217984915500098 ↗
44. Elastic properties and electronic structures of 4d-and 5d-transition metal mononitrides10.1016/j.jallcom.2010.03.176 ↗
45. Phase stability, chemical bonding and mechanical properties of titanium nitrides: a first-principles study10.1039/C5CP00156K ↗
46. Young’s modulus of silicon nitride used in scanning force microscope cantilevers10.1063/1.1638886 ↗
47. Mechanical properties of thin films10.1007/BF02666659 ↗
48. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
49. Toughness evaluation of hard coatings and thin films10.1016/j.tsf.2011.09.036 ↗
50. Measurement of mechanical properties by ultra-low load indentation10.1016/S0921-5093(98)00724-2 ↗
51. D. Broek, Elementary engineering fracture mechanics, Springer Science & Business Media, 1982.10.1007/978-94-009-4333-9 ↗
52. Cohesive interface simulations of indentation cracking as a fracture toughness measurement method for brittle materials10.1016/j.actamat.2012.07.011 ↗
53. Determination of crystallite size with the X‐Ray spectrometer10.1063/1.1699612 ↗
54. Influence of Fe (Cr) miscibility on thin film grain size and stress10.1016/j.tsf.2016.05.024 ↗
55. Structural and mechanical properties of titanium–aluminium–nitride films deposited by reactive close-field unbalanced magnetron sputtering10.1016/j.surfcoat.2003.12.011 ↗
56. Influence of Al and Si content on structure and mechanical properties of arc evaporated Al–Cr–Si–N thin films10.1016/j.tsf.2013.03.017 ↗
57. Oxidation behavior of Si-doped nanocomposite CrAlSiN coatings10.1016/j.surfcoat.2010.08.156 ↗
58. Microstructural control of Cr–Si–N films by a hybrid arc ion plating and magnetron sputtering process10.1016/j.actamat.2009.07.001 ↗
59. The microstructure of sputter‐deposited coatings10.1116/1.573628 ↗
60. Influence of apparatus geometry and deposition conditions on the structure and topography of thick sputtered coatings10.1116/1.1312732 ↗
61. A structure zone diagram including plasma-based deposition and ion etching10.1016/j.tsf.2009.10.145 ↗
62. Fast Fourier Transform and autocorrelation function for the analysis of complex mass spectra10.1016/j.ijms.2013.01.003 ↗
63. J. Odqvist, J. Zhou, W. Xiong, P. Hedström, M. Thuvander, M. Selleby, J. Ågren, 3D analysis of phase separation in ferritic stainless steels, in: Proceedings of the 1st International Conference on 3D Materials Science, Springer, 2012, pp. 221–226.10.1007/978-3-319-48762-5_34 ↗
64. J.P. Davim, Tribology for engineers: A practical guide, Elsevier, 2011.10.1533/9780857091444 ↗
65. Characterizing topography of EDM generated surface by time series and autocorrelation function10.1016/j.triboint.2017.02.016 ↗
66. Size effect of thermal expansion and thermal/intrinsic stresses in nanostructured thin films: experiment and model10.1016/j.actamat.2011.07.018 ↗
67. Residual stresses in nitride hard coatings prepared by magnetron sputtering and arc evaporation10.1016/0257-8972(95)08235-2 ↗
68. The issue of the reproducibility of deposition of superhard nanocomposites with hardness of≥ 50 GPa10.1016/j.surfcoat.2004.11.023 ↗
69. Residual stresses in PVD hard coatings10.1016/0257-8972(95)02581-2 ↗
70. The effect of substrate temperature and biasing on the mechanical properties and structure of sputtered titanium nitride thin films10.1016/S0257-8972(99)00606-4 ↗
71. T. Tsui, G. Pharr, W. Oliver, C. Bhatia, R. White, S. Anders, A. Anders, I. Brown, Nanoindentation and nanoscratching of hard carbon coatings for magnetic disks, MRS Online Proceedings Library (OPL), 383 (1995).10.1557/PROC-383-447 ↗
72. K.L. Johnson, K.L. Johnson, Contact mechanics, Cambridge university press, 1987.
73. Densification and mechanical properties of B4C with Al2O3 as a sintering aid10.1111/j.1151-2916.2000.tb01647.x ↗
74. Hindered crack propagation in materials with periodically varying Young's modulus—lessons from biological materials10.1002/adma.200602394 ↗
75. Improvements of strength and fracture resistance by spatial material property variations10.1016/j.actamat.2014.01.034 ↗