In situ absorption synchrotron measurements, predictive modeling, microstructural analysis, and scanning probe measurements of laser melted Ti-6Al-4V single tracks for additive manufacturing applications

Nicholas Derimow, Edwin J. Schwalbach, Jake T. Benzing, Jason P. Killgore, Alexandra B. Artusio-Glimpse, Nikolas Hrabe, Brian J. Simonds

Publisher page

Abstract

In this work, the fundamental processing-structure-property (PSP) relationships that govern laser-based additive manufacturing were investigated with the Ti-6Al-4V alloy. X-ray synchrotron imaging carried out in conjunction with in-situ integrating sphere radiometry enabled real-time energy absorption measurements for a range of melting conditions that varied laser power and velocity. A thermal conduction model that incorporated the in-situ absorption data and final melt pool geometry was used to predict the thermal histories and diffusion distances along the heat-affected zone (HAZ) in the Ti-6Al-4V alloy to provide insight into the solid-state phase transformations that occurred in the unmelted regions adjacent to the melt pool. Resulting microstructural features were quantified using scanning electron microscopy techniques to elucidate changes in solidification behavior. Significant changes to α/ β -Ti phase fractions were measured in the unmelted HAZ, across all test cases. Nanoindentation and scanning probe microscopy revealed differences in the hardness, modulus, and Volta potential across the resolidified melt pool, HAZ, and wrought base material. These measurements and simulations can be used to predict how processing changes lead to differences in the as-built performance of titanium parts that are used in aerospace and biomedical applications. This work demonstrates the utility of coupling in-situ absorption data with a conduction-only high speed model, which leads reasonable agreement with the synchrotron imaging measurements and microstructural transformations observed herein.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Additive manufacturing of metallic components - process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. Findings from the NIST/ASTM Workshop on Mechanical Behavior of Additive Manufacturing Components
3. Additive manufacturing of medical instruments: a state-of-the-art review
4. Ultrafast X-ray imaging of laser-metal additive manufacturing processes10.1107/S1600577518009554 ↗
5. Real-time monitoring of laser powder bed fusion process using high-speed X-ray imaging and diffraction
6. In situ X-ray imaging of defect and molten pool dynamics in laser additive manufacturing10.1038/s41467-018-03734-7 ↗
7. High-speed synchrotron X-ray imaging of laser powder bed fusion process10.1080/08940886.2019.1582280 ↗
8. In situ synchrotron X-ray imaging of 4140 steel laser powder bed fusion10.1016/j.mtla.2019.100306 ↗
9. Correlative synchrotron X-ray imaging and diffraction of directed energy deposition additive manufacturing10.1016/j.actamat.2021.116777 ↗
10. Keyhole threshold and morphology in laser melting revealed by ultrahigh-speed x-ray imaging10.1126/science.aav4687 ↗
11. in-situ Synchrotron imaging of keyhole mode multi-layer laser powder bed fusion additive manufacturing
12. revealing transient powder-gas interaction in laser powder bed fusion process through multi-physics modeling and high-speed synchrotron x-ray imaging
13. Pressure dependence of the laser-metal interaction under laser powder bed fusion conditions probed by in situ X-ray imaging
14. Critical instability at moving keyhole tip generates porosity in laser melting10.1126/science.abd1587 ↗
15. The causal relationship between melt pool geometry and energy absorption measured in real time during laser-based manufacturing
16. Time-resolved absorptance and melt pool dynamics during intense laser irradiation of a metal10.1103/PhysRevApplied.10.044061 ↗
17. onset of periodic oscillations as a precursor of a transition to pore-generating turbulence in laser melting
18. high speed synchrotron X-ray diffraction experiments resolve microstructure and phase transformation in laser processed Ti-6Al-4V10.1080/21663831.2021.1966537 ↗
19. Application of synchrotron x-ray imaging and diffraction in additive manufacturing: a review
20. NIST SRM 654b, Standard Reference Material (SRM) 654b, Titanium Alloy, 6Al-4V, National Institute of Standards and Technology, 2013.
21. simultaneous high-speed x-ray transmission imaging and absolute dynamic absorptance measurements during high-power laser-metal processing10.1016/j.procir.2020.09.135 ↗
22. A discrete source model of powder bed fusion additive manufacturing thermal history
23. A critical assessment of the effect of indentation spacing on the measurement of hardness and modulus using instrumented indentation testing
24. D. Hurley, J. Killgore, Dynamic Contact AFM Methods for Nanomechanical Properties, in: D. G. Yablon (Ed.), Scanning Probe Microscopy in Industrial Applications, Wiley, 2013, Ch. Dynamic Co, 115–149.10.1002/9781118723111.ch5.10.1002/9781118723111.ch5 ↗
25. kelvin probe force microscopy and its application10.1016/j.surfrep.2010.10.001 ↗
26. Dual-frequency resonance-tracking atomic force microscopy10.1088/0957-4484/18/47/475504 ↗
27. Atomic number and crystallographic contrast images with the SEM: a review of backscattered electron techniques10.1180/minmag.1987.051.359.02 ↗
28. Fiji: An open-source platform for biological-image analysis10.1038/nmeth.2019 ↗
29. Anomalous diffusion of Aluminum in β -Titanium10.1007/BF02665465 ↗
30. Leyens · 2003
31. Rapid solidification processing of titanium alloys10.1007/BF03338360 ↗
32. Influence of laser heat input on weld zone width and fatigue performance of Ti-6Al-4V sheet10.1016/j.mseb.2020.114699 ↗
33. Temperature-gradient induced microstructure evolution in heat-affected zone of electron beam welded Ti-6Al-4V titanium alloy10.1016/j.jmst.2019.04.004 ↗
34. Effect of temperature and cooling rates on the α.β morphology of Ti-6Al-4V alloy10.1016/j.prostr.2019.07.056 ↗
35. Development of computational framework for titanium alloy phase transformation prediction in laser powder-bed fusion additive manufacturing10.1016/j.mtla.2020.100934 ↗
36. Kuo · 2003
37. Surface tension of liquid Ti with adsorbed oxygen and its prediction10.1016/j.molliq.2019.111226 ↗
38. On capturing the grain-scale elastic and plastic anisotropy of alpha-Ti with spherical nanoindentation and electron back-scattered diffraction10.1016/j.actamat.2016.06.053 ↗
39. Evolution of microstructure and residual stress in hot rolled Ti-6Al-4V plates subjected to different heat treatment conditions
40. Impact of grain orientation and phase on Volta potential differences in an additively manufactured titanium alloy10.1063/5.0038114 ↗
41. Hot isostatic pressing (HIP) to achieve isotropic microstructure and retain as-built strength in an additive manufacturing titanium alloy (Ti-6Al-4V)10.1016/j.matlet.2019.126690 ↗