journal article·2021-03

Very High Cycle Fatigue Failure of Near β Titanium Alloy

E. V. Naydenkin, A. P. Soldatenkov, I. P. Mishin, V. A. Oborin, A. A. Shanyavskiy

Physical Mesomechanics· Volume 24· Issue 3
Publisher page

Abstract

Fracture behavior of VT22 near β titanium alloy produced by radial shear rolling and subsequent aging was studied in very high cycle fatigue tests with ultrasonic vibration frequency. This type of processing was shown to significantly increase the static and fatigue strengths of the alloy. According to fractographic analysis, the transition from very high cycle to high cycle fatigue failure occurs in the stress amplitude range of 850–900 MPa, which is almost two times higher than the fatigue limit of the conventionally produced VT22 titanium alloy. It was found that fatigue crack initiation in the very high cycle fatigue region is associated with the formation of a fracture facet inclined at an angle of less than 90° to the specimen axis. The facet exhibits a higher local concentration of interstitial impurities (carbon and oxygen) compared to the chemical composition of the surrounding material, which is due to diffusion mass transfer from the adjacent regions to the zone of highest compressive-tensile stresses.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Microstructure and mechanical properties · High-Velocity Impact and Material Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Speckmann, H. and Roesner, H., Structural Health Monitoring: A Contribution to the Intelligent Aircraft Structure, in Proceedings of ECNDT 2006, Berlin, 2006.
2. Shanyavskii, A.A. and Artamonov, M.A., Effect of Laser Irradiation on Fatigue Fracture of Alloy 2024-Т351, Fiz. Mezomekh., 2007, vol. 10, no. 4, pp. 87–95. https://doi.org/10.24411/1683-805X-2007-0002010.24411/1683-805X-2007-00020 ↗
3. Shanyavskiy, A.A., The Effects of Loading Waveform and Microstructure on the Fatigue Response of Ti-6Al-2Sn-4Zn-2Mo Alloy, Fatigue Fract. Eng. Mater. Struct., 2005, vol. 28(1–2), pp. 195–204.10.1111/j.1460-2695.2004.00844.x ↗
4. Meyers, M.A., Mishra, A., and Benson, D.J., Mechanical Properties of Nanocrystalline Materials, Prog. Mater. Sci., 2006, vol. 51, pp. 427–556.10.1016/j.pmatsci.2005.08.003 ↗
5. Ovid’ko, I.A., Valiev, R.Z., and Zhu, Y.T., Review on Superior Strength and Enhanced Ductility of Metallic Nanomaterials, Prog. Mater. Sci., 2018, vol. 94, pp. 462–540.10.1016/j.pmatsci.2018.02.002 ↗
6. Naydenkin, E.V., Ratochka, I.V., Mishin, I.P., Lykova, O.N., and Varlamova, N.V., The Effect of Interfaces on Mechanical and Superplastic Properties of Titanium Alloys, J. Mater. Sci., 2017, vol. 52(8), pp. 4164–4171.10.1007/s10853-016-0508-1 ↗
7. Höppel, H.W., Kautz, M., Xu, C., Murashkin, M., Langdon, T.G., Valiev, R.Z., and Mughrabi, H., An Overview: Fatigue Behavior of Ultra-Fine Grained Metals and Alloys, Int. J. Fatigue, 2006, vol. 28, pp. 1001–1010.10.1016/j.ijfatigue.2005.08.014 ↗
8. Kim, W.J., Yyun, C.Y., and Kim, H.K., Fatigue Strength of Ultrafine-Grained Pure Ti after Severe Plastic Deformation, Scripta Mater., 2006, vol. 54, pp. 1745–1750.10.1016/j.scriptamat.2006.01.042 ↗
9. Saitova, L.R., Höppel, H.W., Göken, M., Semenova, I.P., and Valiev, R.Z., Cyclic Deformation Behaviour and Fatigue Lives of Ultrafine-Grained Ti-6Al-4V ELI Alloy for Medical Use, Int. J. Fatigue, 2009, vol. 31, pp. 322–331.10.1016/j.ijfatigue.2008.08.007 ↗
10. Naydenkin, E.V., Ratochka, I.V., Mishin, I.P., and Lykova, O.N., Evolution of the Structural-Phase State of a VT22 Titanium Alloy during Radial Shear Rolling and Subsequent Aging, Russ. Phys. J., 2015, vol. 58, pp. 1068–1073.10.1007/s11182-015-0613-7 ↗
11. Sheremetyev, V., Kudryashova, A., Cheverikin, V., Korotitskiy, A., Galkin, S., Prokoshkin, S., and Brailovski, V., Hot Radial Shear Rolling and Rotary Forging of Metastable Beta Ti-18Zr14Nb (at. %) Alloy for Bone Implants: Microstructure, Texture and Functional Properties, J. Alloy. Comp., 2019, vol. 800, pp. 320–326.10.1016/j.jallcom.2019.06.041 ↗
12. Dobatkin, S., Galkin, S., Estrin, Y., Serebryany, V., Diez, M., Martynenko, N., Lukyanova, E., and Perezhogin, V., Grain Refinement, Texture, and Mechanical Properties of a Magnesium Alloy after Radial-Shear Rolling, J. Alloy. Comp., 2019, vol. 774, pp. 969–979.10.1016/j.jallcom.2018.09.065 ↗
13. Sheremetyev, V., Kudryashova, A., Dubinskiy, S., Galkin, S., Prokoshkin, S., and Brailovski, V., Structure and Functional Properties of Metastable Beta Ti-18Zr-14Nb (at. %) Alloy for Biomedical Applications Subjected to Radial Shear Rolling and Thermomechanical Treatment, J. Alloy. Comp., 2018, vol. 737, pp. 678–683.10.1016/j.jallcom.2017.12.119 ↗
14. Ilyin, A.A., Kolachev, B.A., and Polkin, I.S., Titanium Alloys. Composition, Structure, and Properties: A Book of Reference, Moscow: VILS-MATI, 2009.
15. Moiseyev, V.N., Titanium Alloys. Russian Aircraft and Aerospace Applications, New York: CRC Press, 2005.10.1201/9781420037678 ↗
16. Beirow, B., Kühhorn, A., Figaschewsky, F., Hönisch, P., Giersch, T., and Schrape, S., Model Update and Validation of a Mistuned High-Pressure Compressor Blisk, Aeronaut. J., 2019, vol. 123(1260), pp. 230–247. https://doi.org/10.1017/aer.2018.14910.1017/aer.2018.149 ↗
17. Kaibyshev, O.A., Patent 2 450 883 C1 RU, A Method of Manufacturing a Blisk (Variants) and a Die for Implementation Thereof, Byull. Izobret., 2012, no. 14.
18. Shanyavskiy, A.A. and Soldatenkov, A.P., Scales of Metal Fatigue Limit, Phys. Mesomech., 2020, vol. 23, no. 2, pp. 120–127. https://doi.org/10.1134/S102995992002003410.1134/S1029959920020034 ↗
19. Aircraft Materials: A Book of Reference, Tumanov, A.T., Ed., Moscow: VIAM, 1975.
20. Nikitin, A.D., Palin-Luc, T., Shanyavskiy, A.A., and Bathias, C., Crack Path in Aeronautical Titanium Alloy under Ultrasonic Torsion Loading, Fratt. Integr. Struttur., 2016, vol. 35, pp. 213–222. https://doi.org/10.3221/IGF-ESIS.35.2510.3221/IGF-ESIS.35.25 ↗
21. Nikitin, A.D., Palin-Luc, T., and Shanyavskiy, A.A., Crack Initiation in VHCF Regime on Forged Titanium Alloy under Tensile and Torsion Loading Modes, Int. J. Fatigue, 2016, vol. 93, pp. 318–325.10.1016/j.ijfatigue.2016.05.030 ↗
22. Nikitin, A.D., Palin-Luc, T., and Shanyavskiy, A.A., Fatigue Crack Initiation and Growth on an Extruded Titanium Alloy in Gigacycle Regime: Comparison Between Tension and Torsion Loadings, Proc. Struct. Integr., 2016, vol. 2, pp. 1125–1132. https://doi.org/10.1016/j.prostr.2016.06.14410.1016/j.prostr.2016.06.144 ↗
23. Naydenkin, E.V., Mishin, I.P., Ratochka, I.V., Lykova, O.N., and Zabudchenko, O.V., The Effect of Alpha-Case Formation on Plastic Deformation and Fracture of Near Titanium Alloy, Mater. Sci. Eng. A, 2020, vol. 769, p. 138495.10.1016/j.msea.2019.138495 ↗
24. Naydenkin, E.V., Mishin, I.P., Ratochka, I.V., Oborin, V.A., Bannikov, M.V., Bilalov, D.A., and Naydenkin, K.E., Fatigue and Fracture Behavior of Ultrafine-Grained Near Titanium Alloy Produced by Radial Shear Rolling and Subsequent Aging, Mater. Sci. Eng. A, 2021, vol. 810, p. 140968. https://doi.org/10.1016/j.msea.2021.14096810.1016/j.msea.2021.140968 ↗
25. Murakami, Y., Metal Fatigue Effects of Small Defects and Nonmetallic Inclusions, Elsevier Ltd., 2002.
26. Shanyavskiy, A.A., Modeling of Fatigue Fracture of Metals. Synergetics in Aviation, Ufa: Monograph, 2007.
27. Panin, V.E., Pochivalov, Yu.I., Moiseenko, D.D., Maksimov, P.V., and Bikineev, G.Sh., Tribological Contact in Friction Pairs as a Hierarchically Organized Multilevel System, Fiz. Mezomekh., 2010, vol. 13, no. 6, pp. 27–34. https://doi.org/10.24411/1683-805X-2010-0007410.24411/1683-805X-2010-00074 ↗
28. Shaniavski, A.A., Rotational Instability of Mesoscale Deformation and Fracture of Metals in Fatigue Crack Propagation. I. Plastic Deformation at the Crack Tip, Phys. Mesomech., 2001, vol. 4, no. 1, p. 67. https://doi.org/10.24411/1683-805X-2001-0005410.24411/1683-805X-2001-00054 ↗
29. Shanyavskiy, A.A., Banov, M.D., and Zakharova, T.P., Principles of Physical Mesomechanics of Nanostructural Fatigue of Metals. I. Model of Subsurface Fatigue Crack Nucleation in VT3-1 Titanium Alloy, Phys. Mesomech., 2010, vol. 13, no. 3–4, pp. 133–142. https://doi.org/10.24411/1683-805X-2010-0007110.24411/1683-805X-2010-00071 ↗
30. Pan, X., Xu, S., Qian, G., Nikitin, A., Shanyavskiy, A., Palin-Luc, T., and Hong, Y., The Mechanism of Internal Fatigue-Crack Initiation and Early Growth in a Titanium Alloy with Lamellar and Equiaxed Microstructure, Mater. Sci. Eng. A, 2020, vol. 798, p. 140110.10.1016/j.msea.2020.140110 ↗
31. Gorsky, W.S., Theory of Elastic Affereffect in Unordered Mixed Crystals, Phys. Zeitschr. Sowjet, 1935, vol. 8, pp. 457–471.