Deformation and Fracture of Ti-6Al-4V/TiC Composites 3D Printed using Wire-Feed Electron Beam Additive Manufacturing under Uniaxial Tensile Stress

A. V. Panin, M. S. Kazachenok, А. R. Shugurov, G. M. Eremina, А. Yu. Smolin

Physical Mesomechanics· Volume 28· Issue 6
Publisher page

Abstract

Abstract The deformation and fracture patterns of Ti–6Al–4V/TiC composites 3D printed by wire-feed electron beam additive manufacturing using Ti–6Al–4V wire pre-electrospark alloyed with carbide-containing electrodes or by simultaneous melting of titanium wire and TiC powder are investigated. It is shown that Ti–6Al–4V/TiC composites obtained by both methods are characterized by the same microstructure and volume fraction of the carbide phase (~2%) but different sizes of TiC inclusions. It is found that the ductility of the Ti–6Al–4V/TiC composite obtained by electrospark alloying of the wire and containing TiC inclusions with a diameter of ~1 μm is significantly higher than that of the specimen 3D printed by simultaneous melting of titanium wire and TiC powder, in which the inclusion sizes vary within 15–30 μm. Different fracture characteristics of the investigated Ti–6Al–4V/TiC composites under uniaxial tensile stress were revealed. Three-dimensional modeling of elastic-plastic deformation and fracture of model Ti/TiC composites under mechanical loading is carried out using the method of movable cellular automata. The influence of the size and hardness of TiC particles, as well as the character of their distribution in the titanium matrix, on the regularities of crack initiation and propagation in the model composite is demonstrated. It is shown that the inhomogeneous distribution of large carbide inclusions in the titanium matrix is a key factor for crack initiation and propagation in the model composites.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Surface Treatment and Coatings · Electromagnetic Effects on Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Wang, J., Tang, L., Xue, Y., Zhao, Z., Ye, Z., Cao, W., Zhu, J., and Jiang, F., Microstructure and properties of (diamond + TiC) reinforced Ti6Al4V titanium matrix composites manufactured by directed energy deposition, J Journal of Materials Research and Technology, 2024, vol. 28, pp. 3110–3120. https://doi.org/10.1016/j.jmrt.2023.12.22710.1016/j.jmrt.2023.12.227 ↗
2. Fomin, V.M., Malikov, A.G., Golyshev, A.A., Bulina, N.V., Gulov, M.A., Vitoshkin, I.E., Brusentseva, T.A., Filippov, A.A., and Mishin, A.V., Structural-Phase State and Mechanical Properties of a Laser Cladding Titanium Matrix Composite Based on Ti64 Alloy and TiB2 Ceramics, Physical Mesomechanics, 2024, vol. 27, pp. 1–15. https://doi.org/10.1134/S102995992401001610.1134/S1029959924010016 ↗
3. Sánchez de Rojas Candela, C., Riquelme, A., Bonache, V., Rodrigo, P., and Rams, J., Ti6Al4V/SiC Metal Matrix Composites Additively Manufactured by Direct Laser Deposition, Metals and Materials International, 2022, vol. 28, pp. 3120–3144. https://doi.org/10.1007/s12540-022-01191-y10.1007/s12540-022-01191-y ↗
4. Hayat, M.D., Singh, H., He, Z., and Cao, P., Titanium metal matrix composites: An overview, Composites Part A: Applied Science and Manufacturing, 2019, vol. 121, pp. 418–438. https://doi.org/10.1016/j.compositesa.2019.04.00510.1016/j.compositesa.2019.04.005 ↗
5. Wang, Y., Zhu, M., Dong, L., Sun, G., Zhang, W., Xue, H., Fu, Y., Elmarakbi, A., and Zhang, Y., In-situ synthesized TiC/Ti-6Al-4V composites by elemental powder mixing and spark plasma sintering: Microstructural evolution and mechanical properties, Journal of Alloys and Compounds, 2023, vol. 947, p. 169557. https://doi.org/10.1016/j.jallcom.2023.16955710.1016/j.jallcom.2023.169557 ↗
6. Wang, L., Cai, X., Shi, B., Zhang, J., and Zhan, X., Direct energy deposition of TiC/Ti6Al4V graded materials and heat resistance improvement during the ablation process, Journal of Materials Research and Technology, 2024, vol. 33, pp. 8482–8490. https://doi.org/10.1016/j.jmrt.2024.11.17310.1016/j.jmrt.2024.11.173 ↗
7. Ma, Z.Y., Mishra, R.S., and Tjong, S.C., High-temperature creep behavior of TiC particulate reinforced Ti–6Al–4V alloy composite, Acta Materialia, 2002, vol. 50, no. 17, pp. 4293–4302. https://doi.org/10.1016/S1359-6454(02)00261-610.1016/S1359-6454(02)00261-6 ↗
8. Zheng, Y., Yan, X., Qiao, G., Tang, Y., Geng, Y., Shao, Z., and Bai, Q., Enhanced wear resistance of TiC/Ti6Al4V composites through changing TiC morphologies in laser direct energy deposition, Additive Manufacturing, 2024, vol. 84, p. 104134. https://doi.org/10.1016/j.addma.2024.10413410.1016/j.addma.2024.104134 ↗
9. Falodun, O.E., Obadele, B.A., Oke, S.R., and Okoro, A.M., Titanium-based matrix composites reinforced with particulate, microstructure, and mechanical properties using spark plasma sintering technique: a review, International Journal of Advanced Manufacturing Technology, 2019, vol. 102, pp. 1689–1701. https://doi.org/10.1007/s00170-018-03281-x10.1007/s00170-018-03281-x ↗
10. Ou, Y., Ma, Z., Guo, S., Zhou, Q., and Wang, K., Microstructure Evolution and Mechanical Properties of TiC/Ti6Al4V Composites Formed by Selective Laser Melting, Journal of Materials Engineering and Performance, 2023, pp. 1–21. https://doi.org/10.1007/s11665-024-10548-w10.1007/s11665-024-10548-w ↗
11. Fang, J., Tan, Y., Tai, V. Janasekaran, S., Kee, C., Wang, D., and Yang, Y., Selective laser melting of titanium matrix composites: An in-depth analysis of materials, microstructures, defects, and mechanical properties, Heliyon, 2024, vol. 10, p. e40200. https://doi.org/10.1016/j.heliyon.2024.e4020010.1016/j.heliyon.2024.e40200 ↗
12. Yang, Y., Zhang, J., and Wei, W., Microstructure and mechanical properties of TiC/Ti6Al4V nanocomposites fabricated by gas–liquid reaction laser powder bed fusion, Materials Science and Engineering: A, 2023, vol. 829, p. 144829. https://doi.org/10.1016/j.msea.2023.14482910.1016/j.msea.2023.144829 ↗
13. Li, L, Wang, J, Lin, P, and Liu, H., Microstructure and mechanical properties of functionally graded TiCp/Ti6Al4V composite fabricated by laser melting deposition, Ceramics International, 2017, vol. 43, pp. 16638–16651. https://doi.org/10.1016/j.ceramint.2017.09.05410.1016/j.ceramint.2017.09.054 ↗
14. Yu, C., Liu, X., Li, Y., Song, C., Ma, G., Niu, F., and Wu, D., Investigations of the microstructure and performance of TiCp/Ti6Al4V composites prepared by directed laser deposition, International Journal of Mechanical Sciences, 2021, vol. 205, p. 106595. https://doi.org/10.1016/j.ijmecsci.2021.10659510.1016/j.ijmecsci.2021.106595 ↗
15. Wang, J., Li, L., Lin, P., and Wang, J., Effect of TiC particle size on the microstructure and tensile properties of TiCp/Ti6Al4V composites fabricated by laser melting deposition, Optics and Laser Technology, 2018, vol. 105, pp. 195–206. https://doi.org/10.1016/j.optlastec.2018.03.00910.1016/j.optlastec.2018.03.009 ↗
16. Hua, Z., Xiong, L., Zhang, M., Wang, C., Mi, G., and Jiang, P., Microstructure evolution and tribological properties of (TiB+TiC)/Ti–6Al–4V composites fabricated via in situ laser-directed energy deposition of wire and powders in an underwater environment, Composites Part B: Engineering, 2023, vol. 263, p. 110817. https://doi.org/10.1016/j.compositesb.2023.11081710.1016/j.compositesb.2023.110817 ↗
17. Panin, A.V., Kazachenok, M.S., Sinyakova, E.A., Builuk, A.O., Martynov, S.A., Panin, S.V., and Berto, F., Enhancing mechanical properties of wire-based EBAM Ti–6Al–4V parts by adding TiC powders, Material Design and Processing Communications, 2021, vol. 3, pp. 136–141. https://doi.org/10.1002/mdp2.13610.1002/mdp2.136 ↗
18. Wang, Z., Bai, X., Que, M., and Zhou, X., Wire arc additive manufacturing of network microstructure (TiB+TiC)/Ti6Al4V composites using flux-cored wires, Ceramics International, 2023, vol. 49, no. 3, pp. 4168–4176. https://doi.org/10.1016/j.ceramint.2022.09.29910.1016/j.ceramint.2022.09.299 ↗
19. Panin, A.V., Kazachenok, M.S., Lobova, T.A., Pribytkov, G.A., Panina, A.A., and Martynov, S.A., Microstructure and phase composition of 3D printed titanium metal matrix сomposites based on Ti–Al–V–Fe system and reinforced with TiC particles, Russian Physics Journal, 2024, vol. 67, pp. 1400–1407. https://doi.org/10.1007/s11182-024-03260-810.1007/s11182-024-03260-8 ↗
20. Li, N., He, D., Liu, D., Ma, L., He, C., Xu, Y., and Yu, J., In-situ TiB reinforced titanium matrix composite coatings prepared by laser cladding: Effect of TiB2 content on microstructure, hardness and wear properties, Journal of Alloys and Compounds, 2025, vol. 1010, p. 178215. https://doi.org/10.1016/j.jallcom.2024.17821510.1016/j.jallcom.2024.178215 ↗
21. Panin, A., Martynov, S., Kazachenok, M., Kazantseva, L., Bakulin, A., Kulkova, S., Perevalova, O., and Sklyarova, E., Effects of Water Cooling on the Microstructure of Electron Beam Additive-Manufactured Ti–6Al–4V, Metals, 2021, vol. 11, p. 1742. https://doi.org/10.3390/met1111174210.3390/met11111742 ↗
22. Panin, A.V., Syrtanov, M.S., Lobova, T.A., Perevalova, O.B., and Kazachenok, M.S., In Situ High-Temperature Synchrotron X-Ray Studies of the Microstructure and Phase Composition of Additively Manufactured Metal-Matrix Composite Ti–6Al–4V/TiC, 2025, vol. 19, no. 4, pp. 980-988. https://doi.org/10.1134/S102745102570140X10.1134/S102745102570140X ↗
23. Aniszewska, D. and Rybaczuk, M., Mechanical properties of silica aerogels modelled by movable cellular automata simulations. Materials Today Communications, 2021, vol. 27, p. 102432. https://doi.org/10.1016/j.mtcomm.2021.10243210.1016/j.mtcomm.2021.102432 ↗
24. Shilko, E.V. and Grigoriev, A.S., Understanding the properties of the cohesive zone in dynamic shear fracture, Engineering Fracture Mechanics, 2025, vol. 315, p. 110780. https://doi.org/10.1016/j.engfracmech.2024.11078010.1016/j.engfracmech.2024.110780 ↗
25. Zhao, M., Liu, F., Fu, G., Zhang, D. Z., Zhang, T., and Zhou, H., Improved Mechanical Properties and Energy Absorption of BCC Lattice Structures with Triply Periodic Minimal Surfaces Fabricated by SLM, Materials, 2018, vol. 11 p. 2411. https://doi.org/10.3390/ma1112241110.3390/ma11122411 ↗
26. Omoniyi, P.O., Akinlabi, E.T., and Mahamood, R.M., Heat Treatments of Ti6Al4V Alloys for Industrial Applications: An Overview, IOP Conf. Series: Materials Science and Engineering, 2021, vol. 1107, p. 012094. https://doi.org/10.1088/1757-899X/1107/1/01209410.1088/1757-899X/1107/1/012094 ↗
27. Milman, Y.V., Galanov, B.A., and Chugunova, S.I., Plasticity characteristic obtained through hardness measurement, Acta metallurgica et materialia, 1993, vol. 41, no. 9, pp. 2523–2532. https://doi.org/10.1016/0956-7151(93)90122-910.1016/0956-7151(93)90122-9 ↗
28. Golovin, Yu.I., Nanoindentation and Its Capabilities¸ Mashinostroenie, Moscow, 2009.
29. Fan, M., Yi, D.K., and Xiao, Z.M., A Zener–Stroh crack in fiber-reinforced composites with generalized Irwin plastic zone correction, International Journal of Mechanical Sciences, 2014, vol. 82, pp. 81–89. https://doi.org/10.1016/j.ijmecsci.2014.03.00810.1016/j.ijmecsci.2014.03.008 ↗
30. Chen, J., Magdy, M., Cao, T., Hu, Y., Cheng, C., and Zhao, J., Analysis of stress state and crack initiation time around hard-brittle particles in nickel-based alloys by interface model, Materials Today Communications, 2024, vol. 38, p. 108462. https://doi.org/10.1016/j.mtcomm.2024.10846210.1016/j.mtcomm.2024.108462 ↗
31. Panin, A.V., Kazachenok, M.S., Dmitriev, A.I., Nikonov, A.Yu., Perevalova, O.B., Kazancheva, L.A., Sinyakova, E.A., and Martynov, S.A., The effect of ultrasonic impact treatment on deformation and fracture of electron beam additive manufactured Ti–6Al–4V under uniaxial tension, Materials Science and Engineering: A, 2022, vol. 832, p. 142458. https://doi.org/10.1016/j.msea.2021.14245810.1016/j.msea.2021.142458 ↗
32. Henry, H., Pinning of crack fronts by hard and soft inclusions: A phase field study, Physical Review E, 2024, vol. 109, p. 025002. https://doi.org/10.1103/PhysRevE.109.02500210.1103/PhysRevE.109.025002 ↗
33. Ganesh, K.V., Islam, Md R.I., and Patra, P.K., Numerical modeling of interfacial cracking with soft and hard inclusions, Engineering Analysis with Boundary Elements, 2023, vol. 156, pp. 293–298. https://doi.org/10.1016/j.enganabound.2023.08.00910.1016/j.enganabound.2023.08.009 ↗
34. Ahmadian, P. and Taghizadeh, M., The effect of non-metallic inclusion size and orientation on tensile properties of stainless steel (simulation and experiment), Metallurgical and Materials Engineering, 2020, vol. 26, no. 1, pp. 43–55. https://doi.org/10.30544/47110.30544/471 ↗