Abstract The paper presents a study of various structural-phase states of the Fe-Mn-5Si alloy after severe plastic deformation by equal channel angular pressing and high-pressure torsion. Various physical and mechanical characteristics of the alloy were experimentally measured and analyzed in the austenitic coarse-grained, nanostructured grain-subgrain and twinned states, as well as in the predominantly martensitic and two-phase ultrafine-grained states. Indentation methods were used to find that severe plastic deformation increases the modulus of elasticity, the work of elastic deformation, and its elastic component, reducing the contact rigidity of the indenter with the deformed material and the work of plastic deformation. In this case, the alloy in the two-phase state after deformation has the lowest modulus of elasticity and work of plastic deformation at the highest work of elastic deformation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Shape Memory Alloy Transformations · Magnetic Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Zheng, Y.F., Gu, X.N., and Witte, F., Biodegradable metals, Materials Science and Engineering: R, 2014. vol. 77, pp. 1–34. https://doi.org/10.1016/j.mser.2014.01.00110.1016/j.mser.2014.01.001 ↗
2. Khan, A.R., Grewal, N.S., Zhou, C., Yuan, K., and Zhang, H.-J., Recent advances in biodegradable metals for implant applications: Exploring in vivo and in vitro responses, Results in Engineering, 2023, vol. 20, p. 101526. https://doi.org/10.1016/j.rineng.2023.10152610.1016/j.rineng.2023.101526 ↗
3. Heiden, M., Walker, E., and Stanciu, L., Magnesium, Iron and Zinc Alloys, the Trifecta of Bioresorbable Orthopaedic and Vascular Implantation - A Review, Journal of Biotechnology & Biomaterials, 2015, vol. 5, no. 2, pp. 1–9.
4. Muhammad Rabeeh, V.P. and Hanas, T. Progress in manufacturing and processing of degradable Fe‑based implants: a review, Progress in Biomaterials, 2022, vol. 11, no. 2, pp. 163–191. https://doi.org/10.1007/s40204-022-00189-410.1007/s40204-022-00189-4 ↗
5. Ridzwan, MIZ., Shuib, S., Hassan, A.Y., and Shokri, A.A., Mohammad Ibrahim, M.N. Problem of stress shielding and improvement to the hip implant designs: a review, Journal of Medical Science, 2007, vol. 7, no. 3, pp. 460–467. https://doi.org/10.3923/JMS.2007.460.46710.3923/JMS.2007.460.467 ↗
6. Edalati, K., Ahmed, A.Q., Akrami, S., et al., Severe plastic deformation for producing superfunctional ultrafine-grained and heterostructured materials: An interdisciplinary review, Journal of Alloys and Compounds, 2024, vol. 1002, no. 15, p. 174667. https://doi.org/10.1016/j.jallcom.2024.17466710.1016/j.jallcom.2024.174667 ↗
7. Edalati, K., Bachmaier, A., Beloshenko, V.A., Beygelzimer, Y., Blank, V.D., Botta, W.J., Bryła, K., Čížek, J., Divinski, S., Enikeev, N.A., Estrin, Y., Faraji, G., Figueiredo, R.B., Fuji, M., Furuta, T., Grosdidier, T., Gu-bicza, J., Hohenwarter, A., Horita, Z., Huot, J., Ikoma, Y., Janeček, M., Kawasaki, M., Krǎl, P., Kuramoto, S., Lang-don, T.G., Leiva, D.R., Levitas, V.I., Mazilkin, A., Mito, M., Miyamoto, H., Nishizaki, T., Pippan, R., Popov, V.V., Popova, E.N., Purcek, G., Renk, O., Révész, Á., Sauvage, X., Sklenicka, V., Skrotzki, W., Straumal, B.B., Suwas, S., Toth, L.S., Tsuji, N., Valiev, R.Z., Wilde, G., Zehet-bauer, M.J., and Zhu, X., Nanomaterials by severe plastic deformation: review of historical developments and recent advances, Materials Research Letters, 2022, vol. 10, no. 4, pp. 163–256.10.1080/21663831.2022.2029779 ↗
8. Estrin, Y. and Vinogradov, A., Extreme grain refinement by severe plastic deformation: A wealth of challenging science, Acta Materialia, 2013, vol. 61, pp. 782–817. https://doi.org/10.1016/j.actamat.2012.10.03810.1016/j.actamat.2012.10.038 ↗
9. Andrievski, R.A. and Glezer, A.M, Strength of nanostructures, Physics-Uspekhi, 2009, vol. 52, no. 4, pp. 315–334. https://doi.org/10.3367/UFNE.0179.200904A.033710.3367/UFNE.0179.200904A.0337 ↗
10. Valiev, R.Z. and Langdon, T.G., Principles of equal-channel angular pressing as a processing tool for grain refinement, Progress in Materials Science, 2006, vol. 51, no. 7, pp. 881–981. https://doi.org/10.1016/j.pmatsci.2006.02.00310.1016/j.pmatsci.2006.02.003 ↗
11. Valiev, R.Z., Islamgaliev, R.K., and Alexandrov, I.V., Bulk nanostructured materials from severe plastic deformation, Progress in Materials Science, 2000, vol. 45, pp. 103–189. https://doi.org/10.1016/S0079-6425(99)00007-910.1016/S0079-6425(99)00007-9 ↗
12. Gleiter, H., Nanostructured materials: basic concepts and microstructure, Nanostructured Materials, 1992, vol. 1, pp. 1–18. https://doi.org/10.1016/S1359-6454(99)00285-210.1016/S1359-6454(99)00285-2 ↗
13. Rybalchenko, O., Anisimova, N., Martynenko, N., Rybalchenko, G., Kiselevskiy, M., Tabachkova, N., Shchetinin, I., Raab, A., and Dobatkin, S., Structure Optimization of a Fe–Mn–Pd Alloy by Equal-Channel Angular Pressing for Biomedical Use, Materials, 2023, vol. 16, no. 1, p. 45. https://doi.org/10.3390/ma1601004510.3390/ma16010045 ↗
14. Rybalchenko, O.V., Anisimova, N.Yu., Kiselevsky, M.V., Rybalchenko, G.V., Martynenko, N.S., Bochvar, N.R., Tabachkova, N.Yu., Shchetinin, I.V., Shibaeva, T.V., Konushkin, S.V., Tokar, A.A., Raab, A.G., and Dobatkin, S.V., Effect of equal-channel angular pressing on structure and properties of Fe-Mn-C alloys for biomedical applications, Materials Today Communications, 2022, vol. 30, p. 103048. https://doi.org/10.1016/j.mtcomm.2021.10304810.1016/j.mtcomm.2021.103048 ↗
15. Rybalchenko, O., Anisimova, N., Martynenko, N., Rybalchenko, G., Belyakov, A., Shchetinin, I., Lukyanova, E., Chernogorova, O., Raab, A., Pashintseva, N., Kornyushenkov, E., Babaeva, G., Sokolova, D., Kiselevskiy, M., and Dobatkin, S., Biocompatibility and Biodegradation in vitro and in vivo of Fe-Mn-5Si Alloy Strengthened by Equal Channel Angular Pressing, Applied Sciences, 2023, vol. 13, no. 17, p. 9628. https://doi.org/10.3390/app1317962810.3390/app13179628 ↗
16. González-Masís, J., Cubero-Sesin, J.M., Campos-Quirós, A., and Edalati, K., Synthesis of biocompatible high-entropy alloy TiNbZrTaHf by high-pressure torsion, Materials Science and Engineering: A, 2021, vol. 825, p. 141869. https://doi.org/10.1016/j.msea.2021.14186910.1016/j.msea.2021.141869 ↗
17. Maity, T., Balcı, Ö., Gammer, C., Ivanov, E., Eckert, J., and Prashanth, K.G., High pressure torsion induced lowering of Young's modulus in high strength TNZT alloy for bio-implant applications, Journal of the Mechanical Behavior of Biomedical Materials, 2020, vol. 108, p. 103839. https://doi.org/10.1016/j.jmbbm.2020.10383910.1016/j.jmbbm.2020.103839 ↗
18. Kardashev, B.K., Narykova, M.V., Betekhtin, V.I., and Kadomtsev, A.G., Evolution of Elastic Properties of Ti and Its Alloys due to Severe Plastic Deformation, Physical Mesomechanics, 2020, vol. 23, pp. 193–198. https://doi.org/10.1134/S102995992003002910.1134/S1029959920030029 ↗
19. Pillmeier, S., Pippan, R., Eckert, J., and Hohenwarter, A., Fatigue crack growth behavior of a nanocrystalline low Young's modulus β-type Ti–Nb alloy, Materials Science and Engineering: A, 2023, vol. 871, p. 144868. https://doi.org/10.1016/j.msea.2023.14486810.1016/j.msea.2023.144868 ↗
20. Jiang, H., Liu, H., Xing, H., Tang, J., and Lu, Z., Microstructure evolution and corrosion behavior of metastable β Ti-18.4Nb–5Zr alloy with low modulus after thermomechanical treatment, Materials Chemistry and Physics, 2025, vol. 332, p. 130216. https://doi.org/10.1016/j.matchemphys.2024.13021610.1016/j.matchemphys.2024.130216 ↗
21. Kluy, L., Klinge, L., Spiegel, C., Siemers, C., and Groche, P., Design of thermomechanical processes for tailored microstructures: Methodology and application to nanocrystalline titanium alloy Ti-13Nb-13Zr (NanoTNZ), Manufacturing Letters, 2024, vol. 41, pp. 421–428. https://doi.org/10.1016/j.mfglet.2024.09.05010.1016/j.mfglet.2024.09.050 ↗
22. Prokoshkin, S., Pustov, Y., Zhukova, Y., Kadirov, P., Dubinskiy, S., Sheremetyev, V., and Karavaeva, M., Effect of Thermomechanical Treatment on Functional Properties of Biodegradable Fe-30Mn-5Si Shape Memory Alloy, Metallurgical and Materials Transactions A, 2021, vol. 52, pp. 2024–2032. https://doi.org/10.1007/s11661-021-06217-510.1007/s11661-021-06217-5 ↗
23. Kadirov, P., Sheremetyev, V., Pustov, Y., Karavaeva, M., Zhukova, Y., Cheverikin, V., Galkin, S., and Prokoshkin, S., Effect of combined thermomechanical treatment on structure, mechanical properties, electrochemical behavior and functional corrosion fatigue of biodegradable Fe-30Mn-5Si alloy, Journal of Alloys and Compounds, 2024, vol. 1008, p. 176635. https://doi.org/10.1016/j.jallcom.2024.17663510.1016/j.jallcom.2024.176635 ↗
24. Feng, Y.P., Blanquer, A., Fornell, J., Zhang, H., Solsona, P., Baró, M.D., Suriñach, S., Ibáñez, E., García-Lecina, E., Wei, X., Li, R., Barrios, L., Pellicer, E., Nogués, C., and Sort, J., Novel Fe-Mn-Si-Pd alloys: insights into mechanical, magnetic, corrosion resistance and biocompatibility performances, Journal of Materials Chemistry B, 2016, vol. 4, pp. 6402–6412. https://doi.org/10.1039/c6tb01951j10.1039/c6tb01951j ↗
25. Allain, S., Chateau, J.-P., Bouaziz, O., Migot, S., and Guelton, N., Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe–Mn–C alloys, Materials Science and Engineering: A, 2004, vols. 387–389, pp. 158–162. https://doi.org/10.1016/j.msea.2004.01.05910.1016/j.msea.2004.01.059 ↗
26. Grässel, O., Krüger, L., Frommeyer, G., and Meyer, L.W., High strength Fe–Mn–(Al, Si) TRIP/TWIP steels development — properties — application, International Journal of Plasticity, 2000, vol. 16, pp. 1391–1409. https://doi.org/10.1016/S0749-6419(00)00015-210.1016/S0749-6419(00)00015-2 ↗
27. Tian, X. and Zhang, Y.S., Effect of Si content on the stacking fault energy in γ-Fe–Mn–Si–C alloys: Part I. X-ray diffraction line profile analysis, Materials Science and Engineering: A, 2009, vol. 516, pp. 73–77. https://doi.org/10.1016/j.msea.2009.02.03210.1016/j.msea.2009.02.032 ↗
28. GOST R 8748-2011 (ISO 14577-1:2002) (State Standard) Metals and Alloys. Measurement of Hardness and Other Material Parameters by Instrumented Indentation, 2011.
29. Oliver, W.C. and Pharr, G.M., An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments, Journal of Materials Research, 1992, vol. 7, no. 6, pp. 1564–1583.10.1557/JMR.1992.1564 ↗
30. GOST 25142-82 (State Standard) Surface Roughness. Terms and Definitions, 1982.
31. ISO 25178-1:2016 Geometrical product specifications (GPS) — Surface texture: Areal — Part 1: Indication of surface texture, 2016.