journal article·2020-01

Effects of multi-stage aging treatments on the precipitation behavior and properties of 7136 aluminum alloy

Yingchen Wang, Maowen Liu, Wenlong Xiao, Weitao Zhao, Chaoli Ma

Publisher page

Abstract

Abstract The solutionized 7136 Al alloy was heat treated by one-step aging, two-step aging, retrogression and re-aging (RRA) and RRA plus further aging treatment, respectively. The influences of different aging treatments on the precipitation behavior, electrical conductivity and tensile properties were investigated. The results showed that one-step aging treatment forms continuous grain boundary precipitates (GBPs), coherent Guinier-Preston (GP) zone and semi-coherent η’ grain interior precipitates (GIPs). By two-step aging treatment, the GIPs are coarsened and partly transformed into incoherent η phase, which result in a reduction of strength but an enhancement of ductility and electrical conductivity. RRA treatment makes the GBPs to be discontinuous and forms precipitates free zone (PFZ) near grain boundary. The RRA alloy shows similar strength but higher electrical conductivity in comparison with one-step aging. When the RRA alloy further aged at 160 °C, the strength keeps almost constant until 10 h, while the electrical conductivity is increased with increasing aging time. The PFZ is widened and the GIPs become coarser by further aging at high temperature. By contrast, the PFZ is eliminated, accompanying with the formation of GP(II) as further aged at low temperature of 70 °C, therefore a higher strength and lower electrical conductivity are obtained.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Light alloys: metallurgy of the light metals
2. Chakrabarti · 2002
3. Calorimetric studies of 7000 series aluminum alloys: II. Comparison of 7075, 7050 and RX720 alloys10.1007/BF02667404 ↗
4. Alloy · 2016
5. Al-Zr (aluminum-zirconium)10.1007/BF02667824 ↗
6. Enhanced plasticity and corrosion resistance of high strength Al-Zn-Mg-Cu alloy processed by an improved thermomechanical processing10.1016/j.jallcom.2017.05.047 ↗
7. Microstructural evolution of ultra-high strength Al-Zn-Cu-Mg-Zr alloy containing Sc during homogenization10.1016/S1003-6326(11)60984-9 ↗
8. 2008
9. 2016
10. Improved solution treatment for an as-rolled Al–Zn–Mg–Cu alloy. Part I. Characterisation of constituent particles and overheating10.1016/j.msea.2011.11.065 ↗
11. Effect of homogenization and aging treatment on mechanical properties and stress-corrosion cracking of 7050 alloys10.1007/s11661-007-9200-z ↗
12. An improved thermo-mechanical treatment of high-strength Al–Zn–Mg–Cu alloy for effective grain refinement and ductility modification10.1016/j.jmatprotec.2016.08.027 ↗
13. On the nature of T(Al2Mg3Zn3) and S(Al2CuMg) phases present in as-cast and annealed 7055 aluminum alloy10.1016/j.msea.2004.09.013 ↗
14. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
15. Microstructural study of a high-strength stress-corrosion resistant 7075 aluminium alloy10.1007/BF00644656 ↗
16. Microchemical analysis of precipitate free zones in 7075-A1 in the T6, T7 and RRA tempers10.1016/0956-7151(91)90127-M ↗
17. Gheorghe · 2007
18. Rene · 2007
19. Burford · 2013
20. Effects of tool design and friction stir welding parameters on weld morphology in aluminum alloys
21. Influence of equal-channel angular pressing on precipitation in an Al–Zn–Mg–Cu alloy10.1016/j.actamat.2009.03.017 ↗
22. Microstructure and mechanical properties of friction stir welded 7136–T76 aluminium alloy10.1179/026708309X12584564052175 ↗
23. Effect of Zr on recrystallization in a directionally solidified AA705010.1016/j.msea.2017.06.026 ↗
24. Effect of compositional variations on characteristics of coarse intermetallic particles in overaged 7000 aluminium alloys10.1179/026708301101509449 ↗
25. Microstructural evolution in aluminium alloy 7050 during processing10.1016/j.msea.2004.05.006 ↗
26. Tailored Mg and Cu contents affecting the microstructures and mechanical properties of high-strength Al–Zn–Mg–Cu alloys10.1016/j.msea.2016.01.039 ↗
27. Precipitation in an Al-Zn-Mg-Cu alloy during isothermal aging: atomic-scale HAADF-STEM investigation10.1016/j.msea.2017.03.032 ↗
28. Correlations between stress corrosion cracking susceptibility and grain boundary microstructures for an Al–Zn–Mg alloy10.1016/j.corsci.2013.07.032 ↗
29. Effect of heat treatments on the tensile strength and SCC-resistance of AA7050 in an alkaline saline solution10.1016/j.corsci.2005.11.009 ↗
30. GP-zones in Al–Zn–Mg alloys and their role in artificial aging10.1016/S1359-6454(01)00251-8 ↗
31. Precipitation kinetics in warm forming of AW-7020 alloy10.1016/j.msea.2012.10.031 ↗
32. Differential scanning calorimetry and electron diffraction investigation on low-temperature aging in Al-Zn-Mg alloys10.1007/s11661-000-0269-x ↗
33. Early-stage precipitation in Al–Zn–Mg–Cu alloy (7050)10.1016/j.actamat.2004.06.025 ↗
34. Point defect interactions with Guinier-Preston zones in Al-Cu based alloys: vacancy mediated GPZ to θ′-phase transformation10.1016/j.scriptamat.2019.02.024 ↗