Reactive self-consumption strategy to suppress SiO 2 phase transition-induced cracking
Source abstract
Abstract
The lifetime of Si bond coats in environmental barrier coatings (EBCs) is constrained by phase transition-induced cracking at the SiO₂ scale. In this study, reactive self-consumption and lattice solid solution strategies are employed to address this limitation via Si–Yb₄Al₂O₉ composite coatings. The formation of an Yb₂Si₂O₇ layer, through the consumption of the thermally grown SiO₂ scale and Yb₄Al₂O₉, reduces the SiO₂ thickness and significantly lowers the cracking driving force. Furthermore, the incorporation of Al into the SiO₂ lattice stabilizes high-temperature β-SiO₂, preventing phase transition-induced cracking. The proposed coating demonstrated an oxidation lifetime 20 times longer than that of pure Si at 1370 °C, highlighting its potential as an EBC bond coating.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Mineral Processing and Grinding · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. NP Padture. Advanced structural ceramics in aerospace propulsion. 2016, 15: 804-809.10.1038/nmat4687 ↗
2. JX Sun. A review on additive manufacturing of ceramic matrix composites. 2023, 138: 1-16.10.1016/j.jmst.2022.06.039 ↗
3. GH Zhang. Investigation on crystallization behavior between (Sc x Yb 1– x )O 1.5 and CMAS: A new insight in the effect of Sc substitution. 2024, 13: 789-799.10.26599/JAC.2024.9220898 ↗
4. ZF Zhao. High entropy pyrochlore (La 0.3Gd 0.3Ca 0.4) 2(Ti 0.2Zr 0.2Hf 0.2Nb 0.2Ta 0.2) 2O 7 ceramic with amorphous-like thermal conductivity for environmental/thermal barrier coating applications. 2025, 205: 315-326.10.1016/j.jmst.2024.02.089 ↗
5. BT Richards. Plasma spray deposition of tri-layer environmental barrier coatings. 2014, 34: 3069-3083.10.1016/j.jeurceramsoc.2014.04.027 ↗
6. KN Lee. Perspectives on environmental barrier coatings (EBCs) manufactured via air plasma spray (APS) on ceramic matrix composites (CMCs): A tutorial paper. 2021, 30: 40-58.10.1007/s11666-021-01168-0 ↗
7. LR Turcer. Towards multifunctional thermal environmental barrier coatings (TEBCs) based on rare-earth pyrosilicate solid-solution ceramics. 2018, 154: 111-117.10.1016/j.scriptamat.2018.05.032 ↗
8. B Kowalski. Thermally grown oxide in water vapor on coated and uncoated SiC. 2020, 103: 5978-5989.10.1111/jace.17295 ↗
9. K Kane. Evaluating steam oxidation kinetics of environmental barrier coatings. 2022, 105: 590-605.10.1111/jace.18093 ↗
10. L Dong. Realizing the excellent oxidation resistance of an environmental barrier coating through aluminum surface modification. 2024, 13: 976-986.10.26599/JAC.2024.9220911 ↗
11. PX Zhang. Xenotime-type high-entropy (Dy 1/7Ho 1/7Er 1/7Tm 1/7Yb 1/7Lu 1/7Y 1/7)PO 4: A promising thermal/environmental barrier coating material for SiC f/SiC ceramic matrix composites. 2023, 12: 1033-1045.10.26599/JAC.2023.9220736 ↗
12. BT Richards. Response of ytterbium disilicate–silicon environmental barrier coatings to thermal cycling in water vapor. 2016, 106: 1-14.10.1016/j.actamat.2015.12.053 ↗
13. BT Richards. Fracture mechanisms of ytterbium monosilicate environmental barrier coatings during cyclic thermal exposure. 2016, 103: 448-460.10.1016/j.actamat.2015.10.019 ↗
14. R Anton. Hafnia-doped silicon bond Coats manufactured by PVD for SiC/SiC CMCs. 2020, 183: 471-483.10.1016/j.actamat.2019.10.050 ↗
15. E Bakan. Oxidation kinetics of atmospheric plasma sprayed environmental barrier coatings. 2022, 42: 5122-5128.10.1016/j.jeurceramsoc.2022.05.003 ↗
16. L Chen. Promoting Yb 2Si 2O 7 environmental barrier coatings for service at 1425 °C. 2025, 45: 117200.10.1016/j.jeurceramsoc.2025.117200 ↗
17. L Chen. Suppressing the phase-transition-induced cracking of SiO 2 TGOs by lattice solid solution. 2023, 43: 3201-3215.10.1016/j.jeurceramsoc.2023.01.042 ↗
18. L Chen. Durable dual-state duplex Si–HfO 2 with excellent oxidation and cracking resistance. 2024, 13: 388-401.10.26599/JAC.2024.9220863 ↗
19. BJ Harder. Oxidation performance of Si–HfO 2 environmental barrier coating bond Coats deposited via plasma spray-physical vapor deposition. 2020, 384: 125311.10.1016/j.surfcoat.2019.125311 ↗
20. JC Luo. Silicon-based bond coatings for environmental barrier coatings: Present status and prospective. 2024, 21: 3771-3788.10.1111/ijac.14840 ↗
21. M Ridley. Environmental barrier coatings on SiC without a siliconbond coating: Oxidation resistance, failure modes, and future improvements. 2024, 61: 800-810.10.1007/s43207-024-00386-w ↗
22. E Yilmaz. Constrained sintering and thermal ageing behaviour of electrophoretically deposited Yb 2Si 2O 7 environmental barrier coating. 2023, 43: 6427-6439.10.1016/j.jeurceramsoc.2023.06.025 ↗
23. HM Xiang. Crystal structure, mechanical and thermal properties of Yb 4Al 2O 9: A combination of experimental and theoretical investigations. 2017, 37: 2491-2499.10.1016/j.jeurceramsoc.2017.02.016 ↗
24. L Chen. Thermochemical stability of Yb 2Si 2O 7 environmental barrier coatings during thermal cycling and water vapor corrosion at 1350 °C. 2023, 32: 1811-1827.10.1007/s11666-023-01603-4 ↗
25. T Matsudaira. Mass transfer in polycrystalline ytterbium monosilicate under oxygen potential gradients at high temperatures. 2021, 41: 3150-3160.10.1016/j.jeurceramsoc.2020.07.045 ↗
26. L Chen. Improving oxidation resistance of Si coating by isolated-particle healing. 2022, 8: 9-17.10.1016/j.corcom.2022.03.006 ↗
27. DY Chen. Suspension HVOF sprayed ytterbium disilicate environmental barrier coatings. 2022, 31: 429-435.10.1007/s11666-022-01343-x ↗
28. BT Richards. Mechanisms of ytterbium monosilicate/mullite/silicon coating failure during thermal cycling in water vapor. 2015, 98: 4066-4075.10.1111/jace.13792 ↗
29. SW Yao. Conditions and mechanisms for the bonding of a molten ceramic droplet to a substrate after high-speed impact. 2016, 119: 9-25.10.1016/j.actamat.2016.07.057 ↗
30. S McCormack. The effect of porosity, mixed molecular/Knudsen diffusion, and a surface barrier layer on steam corrosion of Yb 2Si 2O 7. 2023, 219: 111238.10.1016/j.corsci.2023.111238 ↗
31. XR Lu. Plasma-sprayed Yb 3Al 5O 12 as a novel thermal barrier coating for gas turbine applications. 2024, 44: 5138-5153.10.1016/j.jeurceramsoc.2024.02.031 ↗
32. XF Wang. Mechanical properties and damage tolerance of bulk Yb 3Al 5O 12 ceramic. 2015, 31: 369-374.10.1016/j.jmst.2015.01.002 ↗
33. AH Paksoy. Influence of alumina addition on steam corrosion behaviour of ytterbium disilicates for environmental barrier coating applications. 2022, 207: 110555.10.1016/j.corsci.2022.110555 ↗
34. JA Deijkers. Failure mechanisms in model thermal and environmental barrier coating systems. 2022, 42: 5129-5144.10.1016/j.jeurceramsoc.2022.04.046 ↗
35. JA Deijkers. A duplex bond coat approach to environmental barrier coating systems. 2021, 217: 117167.10.1016/j.actamat.2021.117167 ↗
36. CH Chao. Stress-induced β→α-cristobalite phase transformation in (Na 2O+Al 2O 3)-codoped silica. 2002, 328: 267-276.10.1016/S0921-5093(01)01703-8 ↗
37. DE Damby. The α–β phase transition in volcanic cristobalite. 2014, 47: 1205-1215.10.1107/S160057671401070X ↗
38. X Wang. Influence of Yb 2Si 2O 7 doping concentration on mechanical properties and thermal conductivity of Yb 2SiO 5–Yb 2Si 2O 7 composite ceramics. 2021, 889: 161718.10.1016/j.jallcom.2021.161718 ↗
39. X Zhong. Microstructure and thermomechanical properties of atmospheric plasma-sprayed Yb 2O 3 coating. 2018, 27: 959-967.10.1007/s11666-018-0733-z ↗
40. YC Zhou. Theoretical investigation on mechanical and thermal properties of a promising thermal barrier material: Yb 3Al 5O 12. 2014, 30: 631-638.10.1016/j.jmst.2014.06.007 ↗
41. L Chen. Critical scale grain size for optimal lifetime of TBCs. 2022, 115: 241-250.10.1016/j.jmst.2021.12.007 ↗
42. KY Guo. Enhanced oxidation resistance in Ti 3AlC 2 via selective self-healing. 2024, 44: 116676.10.1016/j.jeurceramsoc.2024.116676 ↗
43. G Li. Oxidation resistance and thermal shock behavior of tri-layer Si/Si–Yb 2SiO 5/Yb 2SiO 5–SiC environmental barrier coatings at 1300 °C. 2023, 49: 13216-13226.10.1016/j.ceramint.2022.12.202 ↗
44. YL Wang. Failure behavior of SiC/SiC composites with Si/Yb 2SiO 5 and Si/mullite/Yb 2SiO 5 EBCs in wet oxygen at 1350 °C. 2024, 21: 358-369.10.1111/ijac.14491 ↗
45. WB Chen. Failure mechanisms of (Gd 0.9Yb 0.1) 2Zr 2O 7/Yb 2SiO 5/Si thermal/environmental barrier coatings during thermal exposure at 1300 °C/1400 °C. 2022, 42: 3297-3304.10.1016/j.jeurceramsoc.2022.02.023 ↗
46. Q Hu. Oxidation inhibition behaviors of environmental barrier coatings with a Si–Yb 2SiO 5 mixture layer for SiC f/SiC composites at 1300 °C. 2022, 438: 128421.10.1016/j.surfcoat.2022.128421 ↗