journal article·2012-10-01

Influence of Machine Setting and Wood Parameters on Crack Formation in Scots Pine Joints Produced by Linear Friction Welding

Mojgan Vaziri, Owe Lindgren, Antonio Pizzi

Publisher page

Abstract

Abstract Previous investigations on linear welded woods have shown that the connections are not sufficiently resistant to water for use in outdoor conditions. Therefore, they are utilized mainly for non-structural use, with only short time exposure to varying humidity. Influences of some welding and wood parameters such as welding pressure, welding time and heartwood or sapwood on crack formation in the weldline of Scots pine (Pinus sylvestris) were investigated. Axial samples measuring 200 mm × 20 mm × 20 mm from Scots pine were welded, placed vertically in 5-mm-deep tap water and were taken out of the water one at a time after each 10 min of water absorption. Then they were scanned and put back into water until the first crack appeared in the weldline. An X-ray Computer Tomography (CT-) scanner was used to monitor water movement and density change in the weldlines during water absorption–desorption. CT-scanning enabled to detect the cracks as they formed in the weldline and could be used in wood welding studies. Data evaluation showed that all the three studied parameters had significant effects on crack formation and that crack occurrence could be postponed by using heartwood samples with 1.3 MPa welding pressure and 1.5 s welding time. Keywords: Linear weldingtomographywater resistancewelding parameterscrack time Acknowledgements This research was supported by the Luleå University of Technology (LTU) in Sweden and ENSTIB-LERMAB, Université Henri Poincaré, Epinal, France.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Tree Root and Stability Studies · Wood and Agarwood Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

a Department of Wood Science and Technology , Luleå University of Technology , Forskargatan 1, 931 87, Skellefteå , Sweden

b ENSTIB-LERMAB, Université Henri Poincaré , Nancy 1, 27 rue Philippe Séguin, BP 1041, 88051 Épinal Cedex 9, France

References (11)

Show source-provided references
1. Stamm B. · Holz Roh Werkstoff · 2005 · 63 · 38810.1007/s00107-005-0002-y ↗
2. Mansouri H.R. · J. Adhesion Sci. Technol. · 2009 · 23 · 6310.1163/156856108X335595 ↗
3. 10.1163/016942410X50109810.1163/016942410X501098 ↗
4. Lindgren O. · Wood Sci. Technol. · 1991 · 25 · 425
5. O. Lindgren, Medical CT-canners for non-destructive wood density and moisture content measurements, Doctoral Thesis, Lulea University of Technology, Sweden (1992).
6. Montgomery D.C. · 2005
7. Stamm B. · Holz Roh Werkstoff · 2005 · 63 · 31310.1007/s00107-005-0007-6 ↗
8. Gfeller B. · Holz-forschung · 2004 · 58 · 45
9. Siau J.F. · 198410.1007/978-3-642-69213-0 ↗
10. Back E.L. · 2000
11. Rydell Å. · Holzforschung · 2005 · 59 · 18310.1515/HF.2005.029 ↗