journal article·2018-09-17

Residual static strength and the fracture initiation path in adhesively bonded joints weakened with interfacial edge pre-crack

A. Akhavan-Safar, M. R. Ayatollahi, S. Rastegar, L. F. M. da Silva

Publisher page

Abstract

This paper deals with the application of fracture mechanics approaches for predicting the residual static strength and the crack kinking angle of adhesively bonded joints containing interfacial edge pre-cracks. The interfacial cracks are created due to different factors such as inappropriate surface preparation which cause a significant reduction of the joint strength. To investigate the residual strength of interfacial cracked adhesive joints and predict the crack kinking angle, three different approaches including the maximum tangential stress (MTS), the minimum strain energy density (SED) and the maximum tangential strain energy density (MTSED) were assessed. To this end, single lap joints (SLJs) containing a brittle adhesive material and with different pre-crack sizes and various substrate thicknesses were manufactured and tested. The results were also verified by applying fracture mechanics approaches on previously published experimental data. According to the results, it was concluded that in mode II dominant cases, the predictions of kinking angle using the MTS method was in good agreement with the experimental observations, while in mode I dominant cases the mentioned approach provided poor predictions. It was also found that the SED criterion could be a precise model for predicting the crack extension angle in mode I dominant conditions. The results also showed that the MTS criterion predicts the residual static strength of interfacial cracked adhesive joints very well.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Mechanical Behavior of Composites · Fatigue and fracture mechanics · Structural Load-Bearing Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Fatigue and Fracture Research Laboratory, Center of Excellence in Experimental Solid Mechanics and Dynamics, School of Mechanical Engineering, Iran University of Science and Technology, Tehran, Iran

Departamento de Engenharia Mecanica, Faculdade de Engenharia daUniversidade do Porto, Porto, Portugal

References (54)

Show source-provided references
1. Khoramishad H · Proc Inst Mech Eng L J Mater Design Appl · 2017 · 231 · 237
2. Akhavan-Safar A · J Adhes Sci Technol · 2017 · 1
3. 10.1080/15376494.2011.64605510.1080/15376494.2011.646055 ↗
4. 10.1016/j.tafmec.2015.07.01310.1016/j.tafmec.2015.07.013 ↗
5. 10.1080/1537649090355665910.1080/15376490903556659 ↗
6. 10.1016/j.ijsolstr.2017.01.02210.1016/j.ijsolstr.2017.01.022 ↗
7. Náhlík L · Engin Mech · 2008 · 15 · 99
8. Wells A · British Welding J · 1963 · 10 · 563
9. 10.1007/BF0056129110.1007/BF00561291 ↗
10. 10.1016/0013-7944(71)90023-310.1016/0013-7944(71)90023-3 ↗
11. 10.1007/BF0001720210.1007/BF00017202 ↗
12. Kim Y-J · J Mech Sci Technol · 2001 · 15 · 1079
13. 10.1080/14786435.2011.58637410.1080/14786435.2011.586374 ↗
14. 10.1016/j.optlaseng.2012.01.02610.1016/j.optlaseng.2012.01.026 ↗
15. Chai H · Int J Frac · 1993 · 60 · 31110.1007/BF00034739 ↗
16. 10.1016/S0022-5096(99)00052-610.1016/S0022-5096(99)00052-6 ↗
17. 10.1016/S0013-7944(01)00110-210.1016/S0013-7944(01)00110-2 ↗
18. 10.1016/j.engfracmech.2003.12.00310.1016/j.engfracmech.2003.12.003 ↗
19. 10.1080/1537649080254055610.1080/15376490802540556 ↗
20. 10.1016/j.ijsolstr.2005.06.06410.1016/j.ijsolstr.2005.06.064 ↗
21. 10.1016/0020-7683(89)90021-810.1016/0020-7683(89)90021-8 ↗
22. 10.1016/S0020-7683(01)00006-310.1016/S0020-7683(01)00006-3 ↗
23. 10.1016/0020-7683(91)90069-R10.1016/0020-7683(91)90069-R ↗
24. 10.1016/0013-7944(77)90013-310.1016/0013-7944(77)90013-3 ↗
25. Xie D · Com Modeling Engin Sci · 2004 · 6 · 515
26. 10.1016/B978-0-08-021792-5.50010-010.1016/B978-0-08-021792-5.50010-0 ↗
27. 10.1016/j.engfracmech.2005.03.00810.1016/j.engfracmech.2005.03.008 ↗
28. Malyshev B · Int. J. Frac · 1965 · 1 · 11410.1007/BF00186749 ↗
29. 10.1115/1.317366810.1115/1.3173668 ↗
30. 10.1115/1.317607810.1115/1.3176078 ↗
31. 10.1016/0167-6636(89)90020-310.1016/0167-6636(89)90020-3 ↗
32. 10.1016/0013-7944(92)90150-D10.1016/0013-7944(92)90150-D ↗
33. 10.1243/030932405X1603410.1243/030932405X16034 ↗
34. 10.1115/1.362581610.1115/1.3625816 ↗
35. 10.1007/s00466-009-0422-310.1007/s00466-009-0422-3 ↗
36. 10.1016/S0020-7683(97)00132-710.1016/S0020-7683(97)00132-7 ↗
37. 10.1115/1.317617010.1115/1.3176170 ↗
38. 10.1115/1.365689710.1115/1.3656897 ↗
39. 10.1016/j.engfracmech.2010.03.00910.1016/j.engfracmech.2010.03.009 ↗
40. 10.1016/j.engfracmech.2007.04.00710.1016/j.engfracmech.2007.04.007 ↗
41. Kinloch AJ · 1981
42. 10.1080/0021846810807118910.1080/00218468108071189 ↗
43. 10.1016/0032-3861(83)90071-X10.1016/0032-3861(83)90071-X ↗
44. Kinloch AJ · 1983
45. 10.1016/j.engfracmech.2004.07.00110.1016/j.engfracmech.2004.07.001 ↗
46. Spaggiari A · Proc Inst Mech Eng L J Mater Design Appl · 2016 · 230 · 735
47. Da Silva LFM · 2008
48. 10.1016/j.tafmec.2015.07.01310.1016/j.tafmec.2015.07.013 ↗
49. Sih G · 1973 · 21
50. 10.1016/0013-7944(74)90033-210.1016/0013-7944(74)90033-2 ↗
51. 10.1016/j.tafmec.2015.09.00410.1016/j.tafmec.2015.09.004 ↗
52. 10.1016/0013-7944(91)90057-810.1016/0013-7944(91)90057-8 ↗
53. 10.1016/j.ijadhadh.2006.09.00710.1016/j.ijadhadh.2006.09.007 ↗
54. 10.1080/00218464.2017.132965610.1080/00218464.2017.1329656 ↗