UV LED ageing of polymers for PV cell encapsulation
Source abstract
Abstract
Encapsulation polymers in terrestrial solar modules degrade due to ultraviolet radiation from the sun. To assess a polymer’s durability under UV light, accelerated aging tests can be conducted. A new LEDs device allows us to investigate the effects of temperature, irradiation, and UV source spectrum on the photooxidation mechanism and kinetics of two polyethylene-based commercial encapsulants, differentiated by the presence or absence of UV absorbers. The photooxidation rate of the polymer matrix increases as the temperature and irradiance increase between 62 and 82 °C, and 12 and 28 W.m −2 , respectively. In the last case, the photooxidation rate is not proportional to the number of photons. Finally, we observed different distributions of degradation products under UVB radiation at 305 nm compared to those under UVA radiation at 365 nm. UVB photons enable Norrish reactions that are not possible with UVA alone. Special care is needed to maintain a balance between UVA and UVB photons to ensure representative durability tests. With a few adjustments to their emission spectrum, UV LED devices appear to be good candidates for accelerated aging of encapsulation polymers.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Photovoltaic Systems and Sustainability · Photovoltaic System Optimization Techniques · solar cell performance optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. National Renewable Energy Laboratory (NREL). Best research-cell efficiency chart. nrel.gov, 2021, [Online]. Available: https://www.nrel.gov/pv/cell-efficiency.html. Accessed 04 Aug 2021.
2. Jean, J., Woodhouse, M. & Bulović, V. Accelerating photovoltaic market entry with module replacement. Joule 3, 2824–2841 (2019).10.1016/j.joule.2019.08.012 ↗
3. De Oliveira, M. C. C., Diniz, A. S. A. C., Viana, M. M. & Lins, VdeF. C. The causes and effects of degradation of encapsulant ethylene vinyl acetate copolymer (EVA) in crystalline silicon photovoltaic modules: a review. Renew. Sustain. Energy Rev. 81, 2299–2317 (2018).10.1016/j.rser.2017.06.039 ↗
4. Measurement procedures for materials used in photovoltaic modules-Part 7.2: Environmental exposures-Accelerated weathering tests of polymeric materials. IEC 62788-7-2 standard, 2017.
5. Peike, C., Hädrivh, I., Weiß, K.-A. & Dürr, I. Overview of PV module encapsulation materials. Photovolt. Int. 19, 85–92 (2013).
6. Partridge, R. H. Near ultraviolet absorption spectrum of polyethylene. J. Chem. Phys. 45, 1679–1684 (1966).10.1063/1.1727814 ↗
7. Gardette, M. et al. Photo- and thermal oxidation of polyethylene: comparison of mechanisms and influence of unsaturation content. Polym. Degrad. Stab. 98, 2383–2390 (2013).10.1016/j.polymdegradstab.2013.07.017 ↗
8. Bigger, S. W., Scheirs, J. & Delatycki, O. Effect of light intensity on the photooxidation kinetics of high-density polyethylene. J. Polym. Sci. Part A Polym. Chem. 30, 2277–2280 (1992).10.1002/pola.1992.080301025 ↗
9. Bigger, S. W. & Delatycki, O. Effects of temperature and the partial pressure of oxygen on the rate of photooxidation of polyethylene. Polymer 29, 1277–1281 (1988).10.1016/0032-3861(88)90056-0 ↗
10. Therias, S., Rapp, G., Masson, C. & Gardette, J.-L. Limits of UV-light acceleration on the photooxidation of low-density polyethylene. Polym. Degrad. Stab. 183, 109443 (2021).10.1016/j.polymdegradstab.2020.109443 ↗
11. Mazeau, E. et al. Influence of irradiance on the photooxidation of HALS stabilized low-density polyethylene. Polym. Degrad. Stab. 216, 110478 (2023).10.1016/j.polymdegradstab.2023.110478 ↗
12. Fairbrother, A. et al. Temperature and light intensity effects on photodegradation of high-density polyethylene. Polym. Degrad. Stab. 165, 153–160 (2019).10.1016/j.polymdegradstab.2019.05.002 ↗
13. Arrhenius, S. Über die Reaktionsgeschwindigkeit bei der Inversion von Rohrzucker durch Säuren. Z. Phys. Chem. 4U, 226–248 (1889).10.1515/zpch-1889-0416 ↗
14. Martin, J. W., Chin, J. W. & Nguyen, T. Reciprocity law experiments in polymeric photodegradation: a critical review. Prog. Org. Coat. 47, 292–311 (2003).10.1016/j.porgcoat.2003.08.002 ↗
15. Glikman, J.-F., Arnaud, R., Lemaire, J. & Seneira, H. Photo-oxydation et photolyse de copolymères d’éthylène et d’acétate de vinyle à courte et grandes longueurs d’onde. Die Makromol. Chem. 188, 987–1004 (1987).10.1002/macp.1987.021880505 ↗
16. Heidrich, R. et al. UV lamp spectral effects on the aging behavior of encapsulants for photovoltaic modules. Sol. Energy Mater. Sol. Cells 266, 112674 (2024).10.1016/j.solmat.2023.112674 ↗
17. Bourgogne, D., Therias, S. & Gardette, J.-L. Wavelength effect on polymer photooxidation under LED weathering conditions. Polym. Degrad. Stab. 202, 110021 (2022).10.1016/j.polymdegradstab.2022.110021 ↗
18. Pickett, J. E. Review and kinetics analysis of the photodegradation of UV absorbers. Macromol. Symposia 115, 127–141 (1997).10.1002/masy.19971150109 ↗
19. Cruz-Pinto, J. J. C., Carvalho, M. E. S. & Ferreira, J. F. A. The kinetics and mechanism of polyethylene photo-oxidation. Die Angew. Makromol. Chem. 3872, 133–133 (1994).
20. Corrales, T., Catalina, F., Peinado, C., Allen, N. S. & Fontan, E. Photooxidative and thermal degradation of polyethylenes: interrelationship by chemiluminescence, thermal gravimetric analysis and FTIR data. J. Photochem. Photobiol. A: Chem. 147, 213–224 (2002).10.1016/S1010-6030(01)00629-3 ↗
21. Pinochet, N., Couderc, R. & Therias, S. Solar cell UV-induced degradation of module discolouration: between the devil and the deep yellow sea. Prog. Photovolt. Res. Appl. 31, 1091–1100 (2023).10.1002/pip.3725 ↗
22. Heidrich, R., Lüdemann, M., Mordvinkin, A. & Gottschalg, R. Diffusion of UV additives in ethylene-vinyl acetate copolymer encapsulants and the impact on polymer reliability. IEEE J. Photovolt. 14, 131–139 (2024).10.1109/JPHOTOV.2023.3333198 ↗
23. Tidjani, A. Comparison of formation of oxidation products during photo-oxidation of linear low density polyethylene under different natural and accelerated weathering conditions. Polym. Degrad. Stab. 68, 465–469 (2000).10.1016/S0141-3910(00)00039-2 ↗
24. Martinez, R. D., Buitrago, A. A., Howell, N. W., Hearn, C. H. & Joens, J. A. The near U.V. absorption spectra of several aliphatic aldehydes and ketones at 300 K. Atmos. Environ. Part A. Gen. Top. 26, 785–792 (1992).10.1016/0960-1686(92)90238-G ↗
25. Vittoria, V. Influence of the crystallinity on the transport properties of polyethylene. J. Mater. Sci. 30, 3954–3958 (1995).10.1007/BF01153962 ↗
26. Pinochet N., Couderc R., Therias S. Enceinte de photo-vieillissement à multi-irradiance. Patent FR2113280 (2021).