journal article·2025-03-17Open access

Insights into long term glass corrosion mechanisms from the Ballidon experiment

C. L. Thorpe, A. J. Fisher, G. Manifold, S. Creasey-Gray, C. M. Jackson, B. Stone, C. L. Corkhill, C. Boothman, J. R. Lloyd, R. J. Hand

npj Materials Degradation· Volume 9· Issue 1

Abstract

Abstract At the Ballidon experiment, one of the longest running glass durability studies, modern and simulant archaeological glasses were buried in mildly alkaline, under-saturated, conditions for 52 years. Glass surfaces were analysed to determine the extent and mechanisms of alteration. Alteration layer chemistry was complex and included Ca from the surrounding limestone sediment and P from porewater resulting in Ca, Pb and Fe-phosphate rich phases interspersed with Si and Al rich regions. There was evidence for ongoing evolution of the alteration layer structure due to continued fluid ingress. Lamellae in the silica-rich regions approximately numbering the years of burial and indicating a possible link between their formation and seasonal climate cycling. Comparison of field samples with laboratory dissolution tests highlighted the impact of surface finish on initial alteration rate and the limitations of using alteration layer thickness to estimate the amount of glass that has dissolved.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Conservation Techniques and Studies · Building materials and conservation · Cultural Heritage Materials Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (74)

Show source-provided references
1. Fletcher, W. W. The chemical durability of glass. A burial experiment at Ballidon in Derbyshire. J. Glass Stud. 14, 149–151 (1972).
2. Hand, R. J. The Ballidon glass burial experiment – 35 years on. Glass Technol. 46, 237–242 (2005).
3. McLoughlin, S. D., Hand, R. J., Hyatt, N. C., Lee, W. E., Notingher, I. & McPhail, D. S. & Henderson, J. The long term corrosion of glasses: analytical results after 32 years of burial at Ballidon. Glass Technol. Eur. J. Glass Sci. Technol. Part A. 47, 59–67 (2006).
4. Verney-Carron, A. et al. Alteration of medieval stained glass windows in atmospheric medium: review and simplified alteration model. npj Mater. Degrad. 7, 49 (2023).10.1038/s41529-023-00367-0 ↗
5. Pandayil, J. T., Boetti, N. G. & Janner, D. Advancements in Biomedical Applications of Calcium Phosphate Glass and Glass-Based Devices—A Review. J. Funct. Biomater. 15, 79 (2024).10.3390/jfb15030079 ↗
6. Gin, S., Jollivet, P., Tribet, M., Peuget, S. & Schuller, S. Radionuclides containment in nuclear glasses: an overview. Radiochim. Acta 105, 927–959 (2017).10.1515/ract-2016-2658 ↗
7. Ojovan, M. I. & Yudintsev, S. V. Glass, ceramic, and glass-crystalline matrices for HLW immobilisation. Open Ceram. 14, 100355 (2023).10.1016/j.oceram.2023.100355 ↗
8. Gin, S., Delaye, J. M., Angeli, F. & Schulle, S. Aqueous alteration of silicate glass: state of knowledge and perspectives. Npj Mater. Degrad. 5, 42 (2021).10.1038/s41529-021-00190-5 ↗
9. Thorpe, C. L. et al. Forty years of durability assessment of nuclear waste glass by standard methods. npj Mater. Degrad. 5, 61 (2021).10.1038/s41529-021-00210-4 ↗
10. Zanini, R., Franceschin, G., Cattaruzza, E. & Traviglia, A. A review of glass corrosion: the unique contribution of studying ancient glass to validate glass alteration models. npj Mater. Degrad. 7, 38 (2023).10.1038/s41529-023-00355-4 ↗
11. Jewell, P. A. ed. 1963. The Experimental Earthwork on Overton Down. (British Association for the Advancement of Science, London, 1960). Wiltshire.
12. Jewell, P. A. & Dimbleby, G. W. The Experimental Earthwork on Overton Down, Wiltshire, England: the first four years. Proc. Prehist. Soc. 32, 313–342 (1966).10.1017/S0079497X00014420 ↗
13. Evans, J. & Limbrey, S. The Experimental Earthwork on Morden Bog, Wareham, Dorset, England: 1963 to 1972: Report of the Experimental Earthworks Committee of the British Association for the Advancement of Science. Proc. Prehist. Soc. 40, 170–202 (1974).10.1017/S0079497X00011385 ↗
14. Bell, M., Fowler, P. J., & Hillson, S. W. The experimental earthwork project: 1960-1992. (CBA Research Report No 100). York Council Brit. Archaeol. 71, 1098–1099 (1996).10.1017/S0003598X00086154 ↗
15. Lawson, T., Hopkins, D. W., Chudek, J. A., Janaway, R. C. & Bell, M. G. The experimental Earthwork at Wareham, Dorset after 33 Years: 3. Interaction of Soil Organisms with Buried Materials. J. Archaeol. Sci. 27, 273–285 (2000).10.1006/jasc.1999.0462 ↗
16. Newton, R. G. A summary of the progress of the Ballidon glass burial experiment. Glass Technol. 22, 42–45 (1981).
17. Newton, R. G. The Ballidon glass burial experiment. Glass Technol. 26, 293 (1985).
18. Newton, R. G. More results from the Ballidon glass burial experiment. Glass Technol. 29, 106–107 (1988).
19. Newton, R. G. The future of the Ballidon glass burial experiment. Glass Technol. 33, 179–180 (1992).
20. ASTM C1926-23, Standard Test Method for Measurement of Glass Dissolution Rate Using Stirred Dilute Reactor Conditions on Monolithic Samples. https://doi.org/10.1520/C1926-23 (2023).10.1520/C1926-23 ↗
21. Schulz, R. L. et al. Surface analyses of SRS glasses buried in limestone for up to 5 years. Ceram. Trans. 61, 569–576 (1995).
22. Wicks, G. G. US field testing programs and results. J. Nucl. Mater. 298, 78–85 (2001).10.1016/S0022-3115(01)00617-1 ↗
23. Namboodri, C. G. Jr. et al. Surface analyses of SRS waste glass buried for up to two years in limestone in the United Kingdom. Ceram. Trans. 23, 653–662 (1991).
24. Tanguy, M., Dixon, H., Prosdocimi, I., Morris, D. G. & Keller, V. D. J. Gridded estimates of daily and monthly areal rainfall for the United Kingdom (1890-2019) [CEH-GEAR]. NERC EDS Environmental Information Data Centre. https://doi.org/10.5285/dbf13dd5-90cd-457a-a986-f2f9dd97e93c (2021)10.5285/dbf13dd5-90cd-457a-a986-f2f9dd97e93c ↗
25. Khamis, D., Smith, R., Fry, M. & Evans, J. Modelled daily soil moisture and soil temperature at 1km resolution across the UK mainland, 1965-2018. NERC EDS Environmental Information Data Centre. (Dataset). https://doi.org/10.5285/5100e84a-6af9-419b-b4b6-4a5df13b1aec (2024).10.5285/5100e84a-6af9-419b-b4b6-4a5df13b1aec ↗
26. Met Office, Hollis, D., McCarthy, M., Kendon, M. & Legg, T. HadUK-Grid Gridded Climate Observations on a 60km grid over the UK, v1.2.0.ceda (1836-2022). NERC EDS Centre for Environmental Data Analysis, 30 August 2023. https://doi.org/10.5285/22df6602b5064b1686dda7e9455f86fc (2023).10.5285/22df6602b5064b1686dda7e9455f86fc ↗
27. Ojovan, M. On alteration layer renewal stage of nuclear waste glass corrosion. MRS Adv. 5, 111–120 (2020).10.1557/adv.2020.36 ↗
28. Singh, S., Elumalai, S. P. & Pal, A. K. Rain pH estimation based on the particulate matter pollutants and wet deposition study. Sci. Total Environ. 563, 293–301 (2016).10.1016/j.scitotenv.2016.04.066 ↗
29. Ojovan, M. I. & Lee, W. E. About U-shaped glass corrosion rate/pH curves for vitreous nuclear wasteforms. Inn. Corr. Mat. Sci. 7, 30–37 (2017).
30. Backhouse, D. J. et al. Corrosion of the International Simple Glass under acidic to hyperalkaline conditions. npj Mater. Degrad. 2, 29 (2018).10.1038/s41529-018-0050-5 ↗
31. Strachan, D. Glass dissolution as a function of pH and its implications for understanding mechanisms and future experiments. Geochim. Cosmochim. Acta 219, 111–123 (2017).10.1016/j.gca.2017.09.008 ↗
32. Inagaki, Y., Kikunaga, T., Idemitsu, K. & Arima, T. Initial dissolution rate of the international simple glass as a function of pH and temperature measured using microchannel flow‐through test method. Int. J. Appl. Glass Sci. 4, 317–327 (2013).10.1111/ijag.12043 ↗
33. Sessegolo, L. et al. Alteration rate of medieval potash-lime silicate glass as a function of pH and temperature: A low pH-dependent dissolution. Chem. Geol. 550, 119704 (2020).10.1016/j.chemgeo.2020.119704 ↗
34. Zavarzina, D. G. et al. Geoalkalibacter ferrihydriticus gen. nov. sp. nov., the first alkaliphilic representative of the family Geobacteraceae, isolated from a soda lake. Microbiol 75, 673–682 (2006).10.1134/S0026261706060099 ↗
35. Falagán, C. & Johnson, D. B. Acidibacter ferrireducens gen. nov., sp. nov.: an acidophilic ferric iron-reducing gammaproteobacterium. Extremophiles 18, 1067–1073 (2014).10.1007/s00792-014-0684-3 ↗
36. Lloyd, J. R. Microbial reduction of metals and radionuclides. FEMS Microbiol. Rev. 27, 411–425 (2003).10.1016/S0168-6445(03)00044-5 ↗
37. Villemur, R., Lanthier, M., Beaudet, R. & Lépine, F. The Desulfitobacterium genus. FEMS Microbiol. Rev. 30, 706–733 (2006).10.1111/j.1574-6976.2006.00029.x ↗
38. Casar, C. P., Momper, L. M., Kruger, B. R. & Osburn, M. R. Iron-Fueled Life in the Continental Subsurface: Deep Mine Microbial Observatory, South Dakota, USA. Appl. Environ. Microbiol. 87, e0083221 (2021).10.1128/AEM.00832-21 ↗
39. Tang, R. et al. Three Fe(III)-reducing and nitrogen-fixing bacteria, Anaeromyxobacter terrae sp. nov., Anaeromyxobacter oryzisoli sp. nov. and Anaeromyxobacter soli sp. nov., isolated from paddy soil. Int. J. Syst. Evol. Microbiol. 72, 2 (2024).
40. Mansfield, J. T., Thorpe, C. L., Corkhill, C. L., Harrison, M. T. & Hand, R. J. Localised extended (“vermiform”) features formed during glass dissolution. J. Non Cryst. Solids 608, 122230 (2023).10.1016/j.jnoncrysol.2023.122230 ↗
41. Michelin, A. et al. Silicate Glass Alteration Enhanced by Iron: Origin and Long-Term Implications. Environ. Sci. Technol. 47, 750–756 (2012).10.1021/es304057y ↗
42. Burger, E. et al. Impact of iron on nuclear glass alteration in geological repository conditions: A multiscale approach. Appl. Geochem. 31, 159–170 (2013).10.1016/j.apgeochem.2012.12.016 ↗
43. Wang, K. et al. Formation and evolution of secondary phases and surface altered layers during borosilicate glass corrosion in pore water. npj Mater. Degrad. 8, 26 (2024).10.1038/s41529-024-00444-y ↗
44. Pèlegrin, E., Calas, G., Ildefonse, P., Jollivet, P. & Galoisy, L. Structural evolution of glass surface during alteration: application to nuclear waste glasses. J. NonCryst. Solids 356, 2497–2508 (2010).10.1016/j.jnoncrysol.2010.02.022 ↗
45. Schalm, O. & Anaf, W. Laminated altered layers in historical glass: density variations of silica nanoparticle random packings as explanation for the observed lamellae. J. Non Cryst. Solids 442, 1–16 (2016).10.1016/j.jnoncrysol.2016.03.019 ↗
46. Lenting, C. et al. Towards a unifying mechanistic model for silicate glass corrosion. npj Mater. Degrad. 2, 28 (2018).10.1038/s41529-018-0048-z ↗
47. Schalm, O., Nuyts, G. & Janssens, K. Some critical observations about the degradation of glass: The formation of lamellae explained. J. Non Crystalline Solids 569, 120984 (2021).10.1016/j.jnoncrysol.2021.120984 ↗
48. Cox, G. A. & Ford, B. A. The long-term corrosion of glass by ground-water. J. Mater. Sci. 28, 5637–5647 (1993).10.1007/BF00367840 ↗
49. Dussossoy, J. L., Dubois, C., Vernaz, E. & Chambaudet, A. Effect of Surface Finish on Nuclear Glass Dissolution Rate. MRS Online Proc. Libr. 257, 109–115 (1991).10.1557/PROC-257-109 ↗
50. Jackson, C. M., Greenfield, D. & Howie, L. A. An assessment of compositional and morphological changes in model archaeological glasses in an acid burial matrix. Archaeometry 54, 489–507 (2012).10.1111/j.1475-4754.2011.00632.x ↗
51. Strachan, D. et al. On the dissolution of a borosilicate glass with the use of isotopic tracing–Insights into the mechanism for the long-term dissolution rate. Geochim. Cosmochim. Acta 318, 213–229 (2022).10.1016/j.gca.2021.12.004 ↗
52. Corkhill, C. L. et al. Surface interfacial analysis of simulant high level nuclear waste glass dissolved in synthetic cement solutions. npj Mater. Degrad. 6, 67 (2022).10.1038/s41529-022-00279-5 ↗
53. Verney-Carron, A., Gin, S. & Libourel, G. A fractured roman glass block altered for 1800 years in seawater: analogy with nuclear waste glass in a deep geological repository. Geochem. Cosmochim. Acta 72, 5372e5385 (2008).10.1016/j.gca.2008.08.018 ↗
54. Lombardo, T. et al. Characterisation of complex alteration layers in medieval glasses. Corr. Sci. 72, 10–19 (2013).10.1016/j.corsci.2013.02.004 ↗
55. Sterpenich, J. Crystal-chemistry of alteration products of vitrified wastes: implications on the retention of polluting elements. Waste Manag. 28, 120–132 (2008).10.1016/j.wasman.2006.11.004 ↗
56. Henisch, H. K. Crystals in gels and Liesegang rings. (Cambridge University Press, 1988).10.1017/CBO9780511525223 ↗
57. Doménech-Carbó, M.-T., Doménech-Carbó, A., Osete-Cortina, L. & Saurí-Peris, M.-C. A study on corrosion processes of archaeological glass from the Valencian region (Spain) and its consolidation treatment. Microchimica Acta 154, 123–142 (2006).10.1007/s00604-005-0472-y ↗
58. Gulmini, M., Pace, M., Ivaldi, G., Negro Ponzi, M. & Mirti, P. Morphological and chemical characterization of weathering products on buried Sasanian glass from central Iraq. J. Non Cryst. Solids 355, 1631–1621 (2009).10.1016/j.jnoncrysol.2009.05.056 ↗
59. Pierce, E. et al. Experimental determination of the effect of the ratio of B/Al on glass dissolution along the nepheline (NaAlSiO4)–malinkoite (NaBSiO4) join. Geochim. Cosmochim. Acta 74, 2634–2654 (2010).10.1016/j.gca.2009.09.006 ↗
60. Chinnam, R., Fossati, P. & Lee, W. Degradation of partially immersed glass: A new perspective. J. Nucl. Mater. 503, 56–65 (2018).10.1016/j.jnucmat.2018.02.040 ↗
61. Iler, R. K. The Chemistry of Silica: Solubility, Polymerization, Colloid and Surface Properties, and Biochemistry. (John Wiley and Sons Ltd., New York, 1979).
62. Icopini, G. A., Brantley, S. L. & Heaney, P. J. Kinetics of silica oligomerization and nanocolloid formation as a function of pH and ionic strength at 25 °C. Geochim. Cosmochim. Acta 69, 293–303 (2005).10.1016/j.gca.2004.06.038 ↗
63. Viollier, E., Inglett, P. W., Hunter, K., Roychoudhury, A. N. & Van Cappellen, P. The ferrozine method revisited: Fe(II)/Fe(III) determination in natural waters. Appl. Geochem. 15, 785–790 (2000).10.1016/S0883-2927(99)00097-9 ↗
64. Plymale, A. E., et al. Niche Partitioning of Microbial Communities at an Ancient Vitrified Hillfort: Implications for Vitrified Radioactive Waste Disposal. Geomicrobiol. J. 38, 36–56 (2021).10.1080/01490451.2020.1807658 ↗
65. Caporaso, J. G., Lauber, C. L., Walters, W. A., Berg-Lyons, D. & Lozupone, C. A. Global patterns of 16S rRNA diversity at a depth of millions of sequences per sample. Proc. Natl Acad. Sci. 108, 4516–4522 (2011).10.1073/pnas.1000080107 ↗
66. Caporaso, J. G. et al. Ultra-high-throughput microbial community analysis on the Illumina HiSeq and MiSeq platforms. ISME J. 6, 1621–1624 (2012).10.1038/ismej.2012.8 ↗
67. Kozich, J. J., Westcott, S. L., Baxter, N. T., Highlander, S. K. & Schloss, P. D. Development of a Dual-Index Sequencing Strategy and Curation Pipeline for Analyzing Amplicon Sequence Data on the MiSeq Illumina Sequencing Platform. Appl. Environ. Microbiol. 79, 5112–5120 (2013).10.1128/AEM.01043-13 ↗
68. Bolyen, E. et al. Reproducible, interactive, scalable and extensible microbiome data science using QIIME 2. Nat. Biotechnol. 37, 852–857 (2019).10.1038/s41587-019-0209-9 ↗
69. McDonald, D. et al. The biological observation matrix (BIOM) format or: how I learned to stop worrying and love the ome-ome. Gigascience 1, 7 (2012).10.1186/2047-217X-1-7 ↗
70. Bokulich, N. A. et al. Optimizing taxonomic classification of marker-gene amplicon sequences with QIIME 2’s q2-feature-classifier plugin. Microbiome 6, 90 (2018).10.1186/s40168-018-0470-z ↗
71. Pedregosa, F. et al. Scikit-learn: Machine Learning in Python. J. Mach. Learn. Res. 12, 2825–2830 (2011).
72. Quast, C. et al. The SILVA ribosomal RNA gene database project: improved data processing and web-based tools. Nucl. Acids Res. 41, D590–D596 (2013).10.1093/nar/gks1219 ↗
73. Holden, E. W. Excavations at the deserted medieval village of Hangleton: Part I, Sussex Archaeol. Collect 101, 54–181 (1963).
74. McLoughlin, S. D. The characterisation of archaeological glasses using advanced analytical techniques. PhD thesis (Imperial College, University of London, 2003).