A comparative review of the aqueous corrosion of glasses, crystalline ceramics, and metals
Source abstract
Abstract
Abstract All materials can suffer from environmental degradation; the rate and extent of degradation depend on the details of the material composition and structure as well as the environment. The corrosion of silicate glasses, crystalline ceramics, and metals, particularly as related to nuclear waste forms, has received a lot of attention. The corrosion phenomena and mechanisms of these materials are different, but also have many similarities. This review compares and contrasts the mechanisms of environmental degradation of glass, crystalline ceramics, and metals, with the goal of identifying commonalities that can seed synergistic activities and advance the current knowledge in each area.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Nuclear materials and radiation effects · Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Frankel, G. S., Vienna, J. & Lian, J. WastePD, an innovative center on materials degradation. npj Mater. Degrad. 1, 5 (2017).10.1038/s41529-017-0002-5 ↗
2. Vienna, J. D., Ryan, J. V., Gin, S. & Inagaki, Y. Current understanding and remaining challenges in modeling long-term degradation of borosilicate nuclear waste glasses. Int. J. Appl. Glass Sci. 4, 283–294 (2013).10.1111/ijag.12050 ↗
3. Jantzen, C. M., Brown, K. G. & Pickett, J. B. Durable glass for thousands of years. Int. J. Appl. Glass Sci. 25, 38–62 (2010).10.1111/j.2041-1294.2010.00007.x ↗
4. Gin, S. Open scientific questions about nuclear glass corrosion. Procedia Mater. Sci. 7, 163–171 (2014).10.1016/j.mspro.2014.10.022 ↗
5. Fournier, M. et al. Glass dissolution rate measurement and calculation revisited. J. Nucl. Mater. 476, 140–154 (2016).10.1016/j.jnucmat.2016.04.028 ↗
6. Gin, S. et al. An international initiative on long-term behavior of high-level nuclear waste glass. Mater. Today 16, 243–248 (2013).10.1016/j.mattod.2013.06.008 ↗
7. Inagaki, K., Furuya, H., Idemitsu, K. & Arima, T. Review of waste glass corrosion and associated radionuclide release as a part of safety assessment of entire disposal system. Prog. Nucl. Energ. 32, 501–508 (1998).10.1016/S0149-1970(97)00060-7 ↗
8. Bunker, B. C. Molecular mechanisms for corrosion of silica and silicate glasses. Non-Cryst. Solids 179, 300–308 (1994).10.1016/0022-3093(94)90708-0 ↗
9. Van Iseghem, P. et al. in Ceramic Transactions Vol. 207 (eds Cosi, A. & Ohji, T.) 115–126 (American Ceramic Society, Westerville, OH, 2009).
10. Grambow, B. Nuclear waste glasses - How durable? Elements 2, 357–364 (2006).10.2113/gselements.2.6.357 ↗
11. Parruzot, B. Altération des verres basaltiques dans des environnements confinés: analogie avec le stockage géologique des verres nucléaires [Basaltic glass alteration in confined environment: analogy to nuclear waste glass geological repository]. PhD thesis, Univ. Montpellier, (2014).
12. Verney-Carron, A., Gin, S. & Libourel, G. Archaeological analogs and the future of nuclear waste glass. J. Nucl. Mater. 406, 365–370 (2010).10.1016/j.jnucmat.2010.09.028 ↗
13. Ferrand, K., Liu, S. & Lemmens, K. The effect of Ordinary Portland Cement on nuclear waste glass dissolution. Procedia Mat. Sci. 7, 223–229 (2014).10.1016/j.mspro.2014.10.029 ↗
14. Maeda, T., Ohmori, H., Mitsui, S. & Banba, T. Corrosion behavior of simulated HLW glass in the presence of magnesium ion. Int. J. Corros. 2011, 796457 (2011).10.1155/2011/796457 ↗
15. Debure, M., Frugier, P., De Windt, L. & Gin, S. Borosilicate glass alteration driven by magnesium carbonates. J. Nucl. Mater. 420, 347–361 (2012).10.1016/j.jnucmat.2011.09.032 ↗
16. Debure, M., De Windt, L., Frugier, P. & Gin, S. HLW glass dissolution in the presence of magnesium carbonate: diffusion cell experiment and coupled modeling of diffusion and geochemical interactions. J. Nucl. Mater. 443, 507–521 (2013).10.1016/j.jnucmat.2013.07.068 ↗
17. Debure, M., De Windt, L., Frugier, P., Gin, S. & Vieillard, P. Mineralogy and thermodynamic properties of magnesium phyllosilicates formed during the alteration of a simplified nuclear glass. J. Nucl. Mater. 475, 255–265 (2016).10.1016/j.jnucmat.2016.04.008 ↗
18. Michelin, A. et al. Silicate glass alteration enhanced by iron: origin and long-term implications. Environ. Sci. Technol. 47, 750–756 (2013).10.1021/es304057y ↗
19. Rebiscoul, D. et al. Reactive transport processes occurring during nuclear glass alteration in presence of magnetite. Appl. Geochem. 58, 26–37 (2015).10.1016/j.apgeochem.2015.02.018 ↗
20. Reiser, J. T et al. Scientific basis for nuclear waste management XXXVIII. In MRS Symposium Proceedings, Vol. 1744 (eds Josef Matyáš, Stéphane Gin, Robert Jubin, Eric Vance) 139–144 (Materials Research Society, Warrendale, 2015).10.1557/opl.2015.503 ↗
21. Dillmann, P., Gin, S., Neff, D., Gentaz, L. & Rebiscoul, D. Effect of natural and synthetic iron corrosion products on silicate glass alteration processes. Geochim. Cosmochim. Acta 172, 287–305 (2016).10.1016/j.gca.2015.09.033 ↗
22. Fournier, M., Gin, S. & Frugier, P. Resumption of nuclear glass alteration: state of the art. J. Nucl. Mater. 448, 348–363 (2014).10.1016/j.jnucmat.2014.02.022 ↗
23. Ebert, W. L. & Bates, J. K. Scientific basis for nuclear waste management XIV. In Materials Research Society Symposium Proceedings (ed Teofilo A. Abrajano) (Materials Research Society, Boston, 1991) 89–98. .
24. Inagaki, Y. et al. Aqueous alteration of Japanese simulated waste glass P0798: effects of alteration-phase formation on alteration rate and cesium retention. J. Nucl. Mater. 354, 171–184 (2006).10.1016/j.jnucmat.2006.04.002 ↗
25. Muller, I. S., Ribet, S., Pegg, I. L., Gin, S. & Frugier, P. in Ceramic Transactions Vol. 176 191–199 (American Ceramic Society, Westerville, 2006).
26. Gin, S. Scientific Basis for Nuclear Waste Management XXIV. In Materials Research Society Symposium Proceedings (eds Hart, K. P. & Lumpkin, G. R.) 207–215 (Materials Research Society, Warrendale, 2000).
27. Rebiscoul, D., Frugier, P., Gin, S. SpringerAmpamp; Ayral, A. Protective properties and dissolution ability of the gel formed during nuclear glass alteration. J. Nucl. Mater. 342, 26–34 (2005).10.1016/j.jnucmat.2005.03.018 ↗
28. Gin, S. et al. The controversial role of inter-diffusion in glass alteration. Chem. Geol. 440, 115–123 (2016).10.1016/j.chemgeo.2016.07.014 ↗
29. Gin, S., Ribet, I. & Couillard, M. Role and properties of the gel formed during nuclear glass alteration: importance of gel formation conditions. J. Nucl. Mater. 298, 1–10 (2001).10.1016/S0022-3115(01)00573-6 ↗
30. Bunker, B. C. Molecular mechanisms for corrosion of silica and silicate-glasses. J. Non-Cryst. Solids 179, 300–308 (1994).10.1016/0022-3093(94)90708-0 ↗
31. Valle, N. et al. Elemental and isotopic (Si-29 and O-18) tracing of glass alteration mechanisms. Geochim. Cosmochim. Acta 74, 3412–3431 (2010).10.1016/j.gca.2010.03.028 ↗
32. Geisler, T. et al. Aqueous corrosion of borosilicate glass under acidic conditions: a new corrosion mechanism. J. Non-Cryst. Solids 356, 1458–1465 (2010).10.1016/j.jnoncrysol.2010.04.033 ↗
33. Geisler, T. et al. The mechanism of borosilicate glass corrosion revisited. Geochim. Cosmochim. Acta 158, 112–129 (2015).10.1016/j.gca.2015.02.039 ↗
34. Gin, S. et al. The fate of silicon during glass corrosion under alkaline conditions: a mechanistic and kinetic study with the International Simple Glass. Geochim. Cosmochim. Acta 151, 68–85 (2015).10.1016/j.gca.2014.12.009 ↗
35. Gin, S. et al. Atom-probe tomography, TEM and ToF-SIMS study of borosilicate glass alteration rim: a multiscale approach to investigating rate-limiting mechanisms. Geochim. Cosmochim. Acta 202, 57–76 (2017).10.1016/j.gca.2016.12.029 ↗
36. Gin, S. et al. Origin and consequences of silicate glass passivation by surface layers. Nat. Commun. 6, 8 (2015).10.1038/ncomms7360 ↗
37. Hellmann, R. et al. Nanometre-scale evidence for interfacial dissolution-reprecipitation control of silicate glass corrosion. Nat. Mater. 14, 307–311 (2015).10.1038/nmat4172 ↗
38. Delage, F., Ghaleb, D., Dussossoy, J. L., Chevallier, O. & Vernaz, E. A mechanistic model for understanding nuclear waste glass dissolution. J. Nucl. Mater. 190, 191–197 (1992).10.1016/0022-3115(92)90086-Z ↗
39. Grambow, B. & Muller, R. First-order dissolution rate law and the role of surface layers in glass performance assessment. J. Nucl. Mater. 298, 112–124 (2001).10.1016/S0022-3115(01)00619-5 ↗
40. Gin, S., Beaudoux, X., Angeli, F., Jegou, C. & Godon, N. Effect of composition on the short-term and long-term dissolution rates of ten borosilicate glasses of increasing complexity from 3 to 30 oxides. J. Non-Cryst. Solids 358, 2559–2570 (2012).10.1016/j.jnoncrysol.2012.05.024 ↗
41. Gin, S., Frugier, P., Jollivet, P., Bruguier, F. & Curti, E. New insight into the residual rate of borosilicate glasses: effect of S/V and glass composition. Int. J. Appl. Glass Sci. 4, 371–382 (2013).10.1111/ijag.12048 ↗
42. Frugier, P. et al. SON68 nuclear glass dissolution kinetics: current state of knowledge and basis of the new GRAAL model. J. Nucl. Mater. 380, 8–21 (2008).10.1016/j.jnucmat.2008.06.044 ↗
43. Jollivet, P. et al. Investigation of gel porosity clogging during glass leaching. J. Non-Cryst. Solids 354, 4952–4958 (2008).10.1016/j.jnoncrysol.2008.07.023 ↗
44. Cailleteau, C. et al. Insight into silicate-glass corrosion mechanisms. Nat. Mater. 7, 978–983 (2008).10.1038/nmat2301 ↗
45. Gin, S., Ryan, J. V., Schreiber, D. K., Neeway, J. & Cabie, M. Contribution of atom-probe tomography to a better understanding of glass alteration mechanisms: application to a nuclear glass specimen altered 25 years in a granitic environment. Chem. Geol. 349, 99–109 (2013).10.1016/j.chemgeo.2013.04.001 ↗
46. Cailleteau, C., Devreux, F., Spalla, O., Angeli, F. & Gin, S. Why do certain glasses with a high dissolution rate undergo a low degree of corrosion? J. Phys. Chem. C. 115, 5846–5855 (2011).10.1021/jp111458f ↗
47. Gin, S et al. Origin and consequences of silicate glass passivation by surface layers. Nat. Commun. 6, 6360 (2015).10.1038/ncomms7360 ↗
48. Ledieu, A., Devreux, F., Barboux, P., Sicard, L. & Spalla, O. Leaching of borosilicate glasses. I. Experiments. J. Non-Cryst. Solids 343, 3–12 (2004).10.1016/j.jnoncrysol.2004.06.006 ↗
49. Wild, B. et al. pH-dependent control of feldspar dissolution rate by altered surface layers. Chem. Geol. 442, 148–159 (2016).10.1016/j.chemgeo.2016.08.035 ↗
50. Crovisier, J. L., Advocat, T. & Dussossoy, J. L. Nature and role of natural alteration gels formed on the surface of ancient volcanic glasses (Natural analogs of waste containment glasses). J. Nucl. Mater. 321, 91–109 (2003).10.1016/S0022-3115(03)00206-X ↗
51. Fournier, M., Gin, S. & Frugier, P. Resumption of nuclear glass alteration: state of the art. J. Nucl. Mater. 448, 348–363 (2014).10.1016/j.jnucmat.2014.02.022 ↗
52. Ribet, S., Muller, I. S., Pegg, I. L., Gin, S. & Frugier, P. Scientific basis for nuclear waste management XXVIII . In Materials Research Society Symposium Proceedings (eds Hanchar, J. M., StroesGascoyne, S. & Browning, L.) 309–314 (Materials Research Society, Warrendale, 2004).
53. Fournier, M., Gin, S., Frugier, P. & Mercado-Depierre, S. Contribution of zeolite-seeded experiments to the understanding of resumption of glass alteration. npj Mater. Degrad. 1, 17 (2017).10.1038/s41529-017-0018-x ↗
54. Fett, T., Guin, J. P. & Wiederhorn, S. M. Stresses in ion-exchange layers of soda-lime-silicate glass. Fatigue Fract. Eng. Mater. Struct. 28, 507–514 (2005).10.1111/j.1460-2695.2005.00888.x ↗
55. Barkatt, A. et al. Leach Rate Excursions in Borosilicate Glasses - Effects of Glass and Leachant Composition. Vol. 212 (Materials Research Soc, Warrendale, 1991).10.1557/PROC-212-65 ↗
56. Sang, J. C., Barkatt, A., Talmy, I. G. & Norr, M. K. Scientific basis for nuclear waste management XVI. In Materials Research Society Symposium Proceedings (eds Interrante, C. G. & Pabalan, R. T.) 583–589 (Materials Research Society, Warrendale, 1993).
57. Neill, L. G., et al. Various effects of magnetite on international simple glass (ISG) dissolution: implications for the long-term durability of nuclear glasses. npj Mater. Degrad. 1, 1 (2017).10.1038/s41529-017-0001-6 ↗
58. Peuget, S., Delaye, J. M. & Jegou, C. Specific outcomes of the research on the radiation stability of the French nuclear glass towards alpha decay accumulation. J. Nucl. Mater. 444, 76–91 (2014).10.1016/j.jnucmat.2013.09.039 ↗
59. Tribet, M et al. 2nd international summer school on nuclear glass wasteform: structure, properties and long-term behavior. In Procedia Material Science (eds Angeli, F. et al.) 209-215 (Elsevier Science BV, Amsterdam, 2014).10.1016/j.mspro.2014.10.027 ↗
60. Weber, W. J. et al. Radiation effects in glasses used for immobilization of high-level waste and plutonium disposition. J. Mater. Res. 12, 1946–1978 (1997).10.1557/JMR.1997.0266 ↗
61. Weber, W. J. Radiation and thermal ageing of nuclear waste glass. Procedia Mater. Sci. 7, 237–246 (2014).10.1016/j.mspro.2014.10.031 ↗
62. McGrail, B. P. et al. The structure of Na2O-Al2O3-SiO2 glass: impact on sodium ion exchange in H2O and D2O. J. Non-Cryst. Solids 296, 10–26 (2001).10.1016/S0022-3093(01)00890-0 ↗
63. Shutthanandan, V et al. 16th international conference on the application of accelerators in research and industry. In AIP Conference Proceedings (eds Duggan, J. L. & Morgan, I. L.) 454–457 (American Inst. of Physics, Denton, 2001).
64. Icenhower, J. P., McGrail, B. P. & Luttge, A. Origins of deviations from transition-state theory: affects of ion-exchange kinetics in glass. Geochim. Cosmochim. Acta 66, A351–A351 (2002).
65. Kaneko, T. An ion-exchange model of glass leaching. J. Mater. Sci. Lett. 4, 631–634 (1985).10.1007/BF00720052 ↗
66. McGrail, B. P. et al. Ion-Exchange Processes and Mechanisms in Glasses. Report No. PNNL-13717, (Pacific Northwest National Laboratory, Richland, 1998).
67. Oelkers, E. H., Golubev, S. V., Chairat, C., Pokrovsky, O. S. & Schott, J. The surface chemistry of multi-oxide silicates. Geochim. Cosmochim. Acta 73, 4617–4634 (2009).10.1016/j.gca.2009.05.028 ↗
68. Neeway, J. J. et al. Ion-exchange interdiffusion model with potential application to long-term nuclear waste glass performance. J. Phys. Chem. C. 120, 9374–9384 (2016).10.1021/acs.jpcc.6b03681 ↗
69. Bunker, B. C., Arnold, G. W., Day, D. E. & Bray, P. J. The effect of molecular-structure on borosilicate glass leaching. J. Non-Cryst. Solids 87, 226–253 (1986).10.1016/S0022-3093(86)80080-1 ↗
70. Zapol, P., He, H. Y., Kwon, K. D. & Criscenti, L. J. First-principles study of hydrolysis reaction barriers in a sodium borosilicate glass. Int. J. Appl. Glass Sci. 4, 395–407 (2013).10.1111/ijag.12052 ↗
71. Ford, D. C., He, H. & Zapol, P. Density Functional Theory Calculations of Hydrolysis Reactions on a Sodium Borosilicate Glass Surface. Report No. FCRD-MRWFD-2015-000149, (Argonne National Laboratory, Argonne, 2015).
72. Kerisit, S. N. & Pierce, E. M. Monte Carlo simulations of the dissolution of borosilicate and aluminoborosilicate glasses in dilute conditions. Geochim. Cosmochim. Acta 75, 5296–5309 (2011).10.1016/j.gca.2011.06.036 ↗
73. Kerisit, S., Ryan, J. V. & Pierce, E. M. Monte Carlo simulations of the corrosion of aluminoborosilicate glasses. J. Non-Cryst. Solids 378, 273–281 (2013).10.1016/j.jnoncrysol.2013.07.014 ↗
74. Frugier, P., Martin, C., Ribet, I., Advocat, T. & Gin, S. The effect of composition on the leaching of three nuclear waste glasses: R7T7, AVM and VRZ. J. Nucl. Mater. 346, 194–207 (2005).10.1016/j.jnucmat.2005.06.023 ↗
75. Carriere, C. et al. Influence of iron corrosion on nuclear glass alteration processes: nanoscale investigations of the iron-bearing phases. Corr. Eng. Sci. Tech. 53, 166–172 (2017).10.1080/1478422X.2017.1306962 ↗
76. Ebert, W. L. & Jerden, J. L. Jr. Implementation of the ANL Stage 3 Glass Dissolution Model. Report No. FCRD-MRWFD-2016-000296. (Argonne National Laboratory, Argonne, 2016).
77. Jantzen, C. M., Trivelpiece, C. L., Crawford, C. L., Pareizs, J. M. & Pickett, J. B. Accelerated leach testing of glass (ALTGLASS): II. Mineralization of hydrogels by leachate strong bases. Int. J. Appl. Glass Sci. 8, 84–96 (2017).10.1111/ijag.12264 ↗
78. Ribet, S, Muller, I. S, Pegg, I. L, Gin, S. & Frugier, P. Scientific basis for nuclear waste management XXVIII. In Materials Research Society Symposium Proceedings (eds Hanchar, J. M., Stroes-Gascoyne, S., Browning, L.) 309–314 (Materials Research Society, San Francisco, 2004).
79. Strachan, D. M. & Croak, T. L. Compositional effects on long-term dissolution of borosilicate glass. J. Non-Cryst. Solids 272, 22–33 (2000).10.1016/S0022-3093(00)00154-X ↗
80. Fournier, M. G. S., Frugier, P. & Mercado-Depierre, S. Contribution of zeolite-seeded experiments to the understanding of resumption of glass alteration. npj Mater. Degrad. 1, 17 (2017).10.1038/s41529-017-0018-x ↗
81. Rechard, R. P et al. Basis for Identification of Disposal Options for Research and Development for Spent Nuclear Fuel and High-level Waste. Report No. SAND2011-3781P (Sandia National Laboratories, Albuquerque, 2011).
82. de Combarieu, G. et al. Glass-iron-clay interactions in a radioactive waste geological disposal: an integrated laboratory-scale experiment. Appl. Geochem. 26, 65–79 (2011).10.1016/j.apgeochem.2010.11.004 ↗
83. Michelin, A. et al. Effect of iron metal and siderite on the durability of simulated archeological glassy material. Corros. Sci. 76, 403–414 (2013).10.1016/j.corsci.2013.07.014 ↗
84. Arena, H. et al. Impact of Zn, Mg, Ni and Co elements on glass alteration: additive effects. J. Nucl. Mater. 470, 55–67 (2016).10.1016/j.jnucmat.2015.11.050 ↗
85. Debure, M., De Windt, L., Frugier, P. & Gin, S. HLW glass dissolution in the presence of magnesium carbonate: diffusion cell experiment and coupled modeling of diffusion and geochemical interactions. J. Nucl. Mater. 443, 507–521 (2013).10.1016/j.jnucmat.2013.07.068 ↗
86. Verney-Carron, A., Gin, S., Frugier, P. & Libourel, G. Long-term modeling of alteration-transport coupling: application to a fractured Roman glass. Geochim. Cosmochim. Acta 74, 2291–2315 (2010).10.1016/j.gca.2010.01.001 ↗
87. Verney-Carron, A., Gin, S. & Libourel, G. A fractured roman glass block altered for 1800 years in seawater: analogy with nuclear waste glass in a deep geological repository. Geochim. Cosmochim. Acta 72, 5372–5385 (2008).10.1016/j.gca.2008.08.018 ↗
88. Berner, R. A. Rate control of mineral dissolution under earth surface conditions. Am. J. Sci. 278, 1235–1252 (1978).10.2475/ajs.278.9.1235 ↗
89. Brantley, S. L. in Kinetics of Water-Rock Interaction (eds Brantley, B., Kubicki, J. & White, A.) 151–210 (Springer-Verlag, Berlin, 2008).10.1007/978-0-387-73563-4_5 ↗
90. Lasaga, A. C. in Chemical Weathering Rates of Silicate Minerals. Vol. of 31 Reviews in Mineralogy (eds White, A.F. & Brantley, S.L.) 23–86 (Mineralogical Society of America, Chantilly, 1995).
91. Putnis, A. in Thermodynamics and Kinetics of Water-Rock Interaction. Vol. 70 of Reviews in Mineralogy & Geochemistry (eds Oelkers, E.H. & Schott, J.) 87–124 (Mineralogical Society of America, Chantilly, 2009).
92. Schott, J., Pokrovsky, O. S. & Oelkers, E. H. in Thermodynamics and Kinetics of Water-Rock Interaction. Vol. 70 Reviews in Mineralogy & Geochemistry (eds Oelkersrs E. H. & Schott J.) 207–258 (Mineralogical Society of America, Chantilly, 2009).10.2138/rmg.2009.70.6 ↗
93. Walther, J. V. Relation between rates of aluminosilicate mineral dissolution, pH, temperature, and surface charge. Am. J. Sci. 296, 693–728 (1996).10.2475/ajs.296.7.693 ↗
94. Burgess, J. Ions in Solution—Basic Principles of Chemical Interaction 2nd edn (Woodhead Publishing, Cambridge, 1999).
95. Hellmann, R. & Tisserand, D. Dissolution kinetics as a function of the Gibbs free energy of reaction: an experimental study based on albite feldspar. Geochim. Cosmochim. Acta 70, 364–383 (2006).10.1016/j.gca.2005.10.007 ↗
96. White, W. B. in Corrosion of Glass, Ceramics and Superconductors (eds Clark, D.E. & Zoitos, B.K.) (Noyes, Norwich, 1992).
97. Aagaard, P. & Helgeson, H. C. Thermodynamic and kinetic constraints on reaction-rates among minerals and aqueous-solutions .1. theoretical considerations. Am. J. Sci. 282, 237–285 (1982).10.2475/ajs.282.3.237 ↗
98. Lasaga, A. C. in Kinetics of Geochemical Processes Vol. 8 (eds Lasaga, A.C. & R. J. Kirkpatrick, R.J.) 135–169 (Minerallogical Society of America, Chantilly, 1981).10.1515/9781501508233 ↗
99. Gautier, J. M., Oelkers, E. H. & Schott, J. Experimental-study of k-feldspar dissolution rates as a function of chemical affinity at 150-degrees-c and ph-9. Geochim. Cosmochim. Acta 58, 4549–4560 (1994).10.1016/0016-7037(94)90190-2 ↗
100. Oelkers, E. H. & Schott, J. Experimental study of anorthite dissolution and the relative mechanism of feldspar hydrolysis. Geochim. Cosmochim. Acta 59, 5039–5053 (1995).10.1016/0016-7037(95)00326-6 ↗