Abstract
Abstract This paper describes the examination of four copper-containing pigments that catalyze copper corrosion on paper and investigates methods to recreate the damage patterns through artificial aging. The series of tests focused on verdigris as the main catalyst for this damage type but also included atacamite, malachite and azurite in which the damage pattern occurs less frequently. The artificial aging methods include thermal aging, hydrothermal aging, light aging, and combinations thereof. Investigations into pigment changes, the migration behavior of the copper ions and the degree of paper degradation were carried out through Raman spectroscopy, scanning electron microscopy with energy dispersive X-ray analysis (SEM-EDX) and size-exclusion chromatography with multi-angle light scattering (SEC-MALS) and labeling of oxidized functionalities. Hydrothermal aging in a closed glass vessel as well as the combination of hydrothermal and light aging overall yielded results with the closest resemblance to historical examples of copper corrosion on paper.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Advanced Cellulose Research Studies · Material Properties and Processing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Banik, G., Stachelberger, H., Mairinger, F., Vendl, A. & Ponahlo, J. Analytical investigations of the problem of “Kupferfraß” in illuminated manuscripts. Mikrochim. Acta 1, 49–55 (1981).10.1007/BF01198703 ↗
2. Banik, G., Mairinger, F. & Stachelberger, H. Appearance and problems of copper corrosion in book illumination (in German: Erscheinungen und Probleme des Kupferfrasses in der Buchmalerei). Restaurator 1, 71–93 (1983).
3. Banik, G. Discoloration of green copper pigments in manuscripts and works of graphic art. Restaurator 10, 61–73 (1989).
4. Banik, G. & Ponahlo, J. Some aspects of degradation phenomena of paper caused by green copper-containing pigments. Pap. Conserv. 7, 3–7 (1982).10.1080/03094227.1982.9638442 ↗
5. Henniges, U., Prohaska, T., Banik, G. & Potthast, A. A fluorescence labeling approach to assess the deterioration state of aged papers. Cellulose 13, 421–428 (2006).10.1007/s10570-005-9030-3 ↗
6. Pahl, A. Characterization of the Aging Process of Copper Corrosion on Paper (in German: Charakterisierung des Alterungsprozesses von Kupferfraß auf Papier). Unpublished master's thesis, TH Köln (2022).
7. Malešič, J., Kolar, J. & Anders, M. Evaluation of treatments for stabilization of verdigris and malachite containing paper documents. Restaurator 36, 283–305 (2015).
8. Hagadorn, A. An investigation into the use of blue copper pigments in European early printed books. Book Pap. Group Annu. 23, 41–55 (2004).
9. Ahn, K., Hofmann, C., Horsky, M. & Potthast, A. How copper corrosion can be retarded—new ways investigating a chronic problem for cellulose in paper. Carbohydr. Polym. 134, 136–143 (2015).10.1016/j.carbpol.2015.07.040 ↗
10. Hofmann, C. et al. Studies on the conservation of verdigris on paper. Restaurator 36, 147–182 (2015).
11. Reißland, B. & Hofenk de Graaff, J. In ICN-Information Number 1. https://www.cultureelerfgoed.nl/publicaties/publicaties/2001/01/01/condition-rating-for-paper-object-with-iron-gall-ink (Cultural Heritage Agency of the Netherlands, 2001).
12. Schrieder, V. Copper corrosion on paper (in German: Kupferfraß an Papier). Restauro. Z. Konservierung Restaur. 5, 40–50 (2020).
13. Kühn, H. In Artists’ Pigments. A Handbook of Their History and Characteristics, Vol. 2 (ed. Roy, A.) 131–158 (Oxford University Press, 1993).
14. Roller, J., Pataki, A., Potthast, A. & Brückle, I. Aqueous washing treatment aids: how to remove ionic fixatives from paper. Restaurator 36, 307–331 (2015).
15. Meyer, F. & Neumann, A. Recombinant Proteins: a new material for the chemical stabilisation of copper pigment corrosion on paper?. Restaurator 30, 96–130 (2009).
16. Brostoff, L. & Connelly, R. Tracing the alteration of verdigris pigment through combined Raman spectroscopy and X-ray diffraction. Part I. Restaur. 41, 3–10 (2020).
17. Röhrling, J. et al. A novel method for the determination of carbonyl groups in cellulosics by fluorescence labeling. 1. Method development. Biomacromolecules 3, 959–968 (2002).10.1021/bm020029q ↗
18. Röhrling, J. et al. A novel method for the determination of carbonyl groups in cellulosics by fluorescence labeling. 2. Validation and applications. Biomacromolecules 3, 969–975 (2002).10.1021/bm020030p ↗
19. Potthast, A. et al. A novel method for the determination of carbonyl groups in cellulosics by fluorescence labeling. 3. Monitoring oxidative processes. Biomacromolecules 4(3), 743–749 (2003).10.1021/bm025759c ↗
20. Henniges, U., Schröder, K. & Potthast, A. Wallpaper and Copper Corrosion: Considerations on the Feasibility of a Restoration Treatment (in German: Tapeten und Kupferfraß: Überlegungen zur Durchführbarkeit einer Restaurierungsbehandlung) (Berliner Wiss.-Verlag, 2005).
21. Gettens, R. J. & West Fitzhugh, E. In Artists’ Pigments. A Handbook of Their History and Characteristics, Vol. 2 (ed. Roy, A.) 23-35 (Oxford University Press, 1993).